Solidification processing superalloys in an electric field

Abstract

The phase morphology of a given superalloy's microstructure is established during solidification. Solidification-processing in an applied electric field is a technique currently undergoing experimental characterization at NASA-Marshall. The method is predicated on the simplest model of a metallic solid, in which ions are arranged in basic space lattices that are permeated by an 'electron gas' whose valence electrons are free to move in the solid. When in a superheated liquid state, the metal is seen as a dense 'cold plasma' of electrons and ions. The application of an electric field during solidification establishes a steady, continuous current flow; the direction of propagation of the plasma waves coincides with the direction of the electric field. Such an alignment introduces an ordered arrangement of the electric vectors and introduces an additional degree of order in an already highly ordered alloy.

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Ahmed, Shaffiq, Bond, Robert, Mckannan, Eugene C.. 1991-10-01. Solidification processing superalloys in an electric field. https://ntrs.nasa.gov/citations/19920044301

Cite the original work for its findings. Save a collection to share your selection of sources.