High molecular weight first generation PMR polyimides for 343 C applications

Abstract

The effect of molecular weight on 343 C thermo-oxidative stability (TOS), mechanical properties, and processability, of the first generation PMR polyimides was studied. Graphite fiber reinforced PMR-15, PMR-30, PMR-50, and PMR-75 composites (corresponding to formulated molecular weights of 1500, 3000, 5000, and 7500, respectively) were fabricated using a simulated autoclave process. The data reveal that while alternate autoclave cure schedules are required for the high molecular weight resins, low void laminates can be fabricated which have significantly improved TDS over PMR-15, with only a small sacrifice in mechanical properties.

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Malarik, D. C., Vannucci, R. D.. 1992-07-01. High molecular weight first generation PMR polyimides for 343 C applications. https://ntrs.nasa.gov/citations/19920067195

Cite the original work for its findings. Save a collection to share your selection of sources.