Simple Creep Test For Ceramic Fibers

Abstract

Simple bend-stress-relaxation test yields information on creep-related properties of polycrystalline ceramic fibers. Determination of these properties important part of efforts to develop ceramic composite materials that retain mechanical strength and resistance to creep at high temperatures. Present test measures effects of time, temperature, and applied strain on creep-related relaxation of bend stress in ceramic fiber of almost any diameter in almost any environment, without need for contact sensors. Degree of relaxation of bend stress determined from radii of curvature.