Anodizing And Sealing Aluminum In Nonchromated Solutions
Abstract
Improved process for anodizing and sealing aluminum involves use of 5 volume percent sulfuric acid in water as anodizing solution, and 1.5 to 2.0 volume percent nickel acetate in water as sealing solution. Replaces process in which sulfuric acid used at concentrations of 10 to 20 percent. Improved process yields thinner coats offering resistance to corrosion, fatigue life, and alloy-to-alloy consistency equal to or superior to those of anodized coats produced with chromated solutions.
Keep this discovery
Explore connections, maps & timelines
Emmons, John R., Kallenborn, Kelli J.. 1995-05-01. Anodizing And Sealing Aluminum In Nonchromated Solutions. https://ntrs.nasa.gov/citations/19950065397