Search NASA⌕ Search

NASA NTRS · 20040082395

Superalloy Lattice Block Structures

Abstract

Initial investigations of investment cast superalloy lattice block suggest that this technology will yield a low cost approach to utilize the high temperature strength and environmental resistance of superalloys in lightweight, damage tolerant structural configurations. Work to date has demonstrated that relatively large superalloy lattice block panels can be successfully investment cast from both IN-718 and Mar-M247. These castings exhibited mechanical properties consistent with the strength of the same superalloys measured from more conventional castings. The lattice block structure also accommodates significant deformation without failure, and is defect tolerant in fatigue. The potential of lattice block structures opens new opportunities for the use of superalloys in future generations of aircraft applications that demand strength and environmental resistance at elevated temperatures along with low weight.

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Nathal, M. V., Whittenberger, J. D., Hebsur, M. G., Kantzos, P. T., Krause, D. L.. 2004-06-01. Superalloy Lattice Block Structures. https://ntrs.nasa.gov/citations/20040082395

Cite the original work for its findings. Save a collection to share your selection of sources.