NASA NTRS · 20080004841
Method for forming thin composite solid electrolyte film for lithium batteries
Abstract
A composite solid electrolyte film is formed by dissolving a lithium salt such as lithium iodide in a mixture of a first solvent which is a cosolvent for the lithium salt and a binder polymer such as polyethylene oxide and a second solvent which is a solvent for the binder polymer and has poor solubility for the lithium salt. Reinforcing filler such as alumina particles are then added to form a suspension followed by the slow addition of binder polymer. The binder polymer does not agglomerate the alumina particles. The suspension is cast into a uniform film.
Keep this discovery
Explore connections, maps & timelines
Nagasubramanian, Ganesan, Attia, Alan I.. 1997-02-04. Method for forming thin composite solid electrolyte film for lithium batteries. https://ntrs.nasa.gov/citations/20080004841