Materials Data on Ca3GaAs3 by Materials Project

Abstract

Ca3GaAs3 crystallizes in the orthorhombic Pnma space group. The structure is three-dimensional. there are three inequivalent Ca2+ sites. In the first Ca2+ site, Ca2+ is bonded to five As3- atoms to form distorted CaAs5 trigonal bipyramids that share corners with nine CaAs6 octahedra, corners with two equivalent GaAs4 tetrahedra, edges with four CaAs6 octahedra, edges with two equivalent GaAs4 tetrahedra, edges with two equivalent CaAs5 trigonal bipyramids, and a faceface with one CaAs6 octahedra. The corner-sharing octahedra tilt angles range from 23–56°. There are a spread of Ca–As bond distances ranging from 2.93–3.06 Å. In the second Ca2+ site, Ca2+ is bonded to six As3- atoms to form CaAs6 octahedra that share corners with seven equivalent CaAs6 octahedra, corners with three equivalent GaAs4 tetrahedra, corners with six equivalent CaAs5 trigonal bipyramids, edges with four equivalent CaAs6 octahedra, edges with two equivalent GaAs4 tetrahedra, an edgeedge with one CaAs5 trigonal bipyramid, a faceface with one CaAs6 octahedra, and a faceface with one CaAs5 trigonal bipyramid. The corner-sharing octahedra tilt angles range from 40–54°. There are a spread of Ca–As bond distances ranging from 2.97–3.29 Å. In the third Ca2+ site, Ca2+ is bonded to six As3- atoms to form CaAs6 octahedra that share corners with seven equivalent CaAs6 octahedra, corners with three equivalent GaAs4 tetrahedra, corners with three equivalent CaAs5 trigonal bipyramids, edges with four equivalent CaAs6 octahedra, edges with three equivalent GaAs4 tetrahedra, edges with three equivalent CaAs5 trigonal bipyramids, and a faceface with one CaAs6 octahedra. The corner-sharing octahedra tilt angles range from 40–54°. There are a spread of Ca–As bond distances ranging from 2.96–3.36 Å. Ga3+ is bonded to four As3- atoms to form GaAs4 tetrahedra that share corners with six CaAs6 octahedra, corners with two equivalent GaAs4 tetrahedra, corners with two equivalent CaAs5 trigonal bipyramids, edges with five CaAs6 octahedra, and edges with two equivalent CaAs5 trigonal bipyramids. The corner-sharing octahedra tilt angles range from 23–51°. There are a spread of Ga–As bond distances ranging from 2.55–2.58 Å. There are three inequivalent As3- sites. In the first As3- site, As3- is bonded to six Ca2+ and one Ga3+ atom to form a mixture of distorted face, edge, and corner-sharing AsCa6Ga pentagonal bipyramids. In the second As3- site, As3- is bonded to six Ca2+ and one Ga3+ atom to form a mixture of distorted face, edge, and corner-sharing AsCa6Ga pentagonal bipyramids. In the third As3- site, As3- is bonded in a 7-coordinate geometry to five Ca2+ and two equivalent Ga3+ atoms.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

2020-07-22. Materials Data on Ca3GaAs3 by Materials Project. https://doi.org/10.17188/1264936

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗