Search NASA⌕ Search

DOE OSTI · 1684030

Materials Data on PrErMn4Co13 by Materials Project

Abstract

ErPrMn4Co13 crystallizes in the monoclinic Cm space group. The structure is three-dimensional. Er is bonded in a 10-coordinate geometry to three Mn and sixteen Co atoms. There are one shorter (2.99 Å) and two longer (3.26 Å) Er–Mn bond lengths. There are a spread of Er–Co bond distances ranging from 2.98–3.27 Å. Pr is bonded in a 10-coordinate geometry to one Mn and sixteen Co atoms. The Pr–Mn bond length is 3.04 Å. There are a spread of Pr–Co bond distances ranging from 2.99–3.32 Å. There are three inequivalent Mn sites. In the first Mn site, Mn is bonded in a 4-coordinate geometry to one Er, three Mn, and ten Co atoms. There are one shorter (2.53 Å) and two longer (2.57 Å) Mn–Mn bond lengths. There are a spread of Mn–Co bond distances ranging from 2.50–2.76 Å. In the second Mn site, Mn is bonded in a 12-coordinate geometry to one Pr, three Mn, and ten Co atoms. Both Mn–Mn bond lengths are 2.59 Å. There are a spread of Mn–Co bond distances ranging from 2.52–2.75 Å. In the third Mn site, Mn is bonded in a 12-coordinate geometry to one Er, two Mn, and eight Co atoms. There are a spread of Mn–Co bond distances ranging from 2.40–2.45 Å. There are eight inequivalent Co sites. In the first Co site, Co is bonded in a 1-coordinate geometry to one Er, one Pr, three Mn, and seven Co atoms. There are a spread of Co–Co bond distances ranging from 2.39–2.61 Å. In the second Co site, Co is bonded in a 1-coordinate geometry to one Er, one Pr, three Mn, and seven Co atoms. There are a spread of Co–Co bond distances ranging from 2.40–2.63 Å. In the third Co site, Co is bonded in a 12-coordinate geometry to one Er, one Pr, four Mn, and six Co atoms. There are a spread of Co–Co bond distances ranging from 2.52–2.67 Å. In the fourth Co site, Co is bonded to one Er, two equivalent Pr, two Mn, and seven Co atoms to form a mixture of distorted edge, corner, and face-sharing CoPr2ErMn2Co7 cuboctahedra. There are one shorter (2.43 Å) and two longer (2.46 Å) Co–Co bond lengths. In the fifth Co site, Co is bonded to one Er, two equivalent Pr, three Mn, and six Co atoms to form distorted CoPr2ErMn3Co6 cuboctahedra that share corners with ten CoPr2ErMn3Co6 cuboctahedra, edges with five CoPr2ErMn2Co7 cuboctahedra, and faces with seven CoPr2ErMn2Co7 cuboctahedra. Both Co–Co bond lengths are 2.46 Å. In the sixth Co site, Co is bonded to two equivalent Er, one Pr, two Mn, and seven Co atoms to form a mixture of distorted edge, corner, and face-sharing CoPrEr2Mn2Co7 cuboctahedra. The Co–Co bond length is 2.43 Å. In the seventh Co site, Co is bonded to two equivalent Er, one Pr, three Mn, and six Co atoms to form distorted CoPrEr2Mn3Co6 cuboctahedra that share corners with ten CoPr2ErMn2Co7 cuboctahedra, edges with five CoPr2ErMn3Co6 cuboctahedra, and faces with seven CoPr2ErMn2Co7 cuboctahedra. In the eighth Co site, Co is bonded in a 12-coordinate geometry to one Er, one Pr, two Mn, and eight Co atoms.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

2020-06-04. Materials Data on PrErMn4Co13 by Materials Project. https://doi.org/10.17188/1684030

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗