Materials Data on YbEu by Materials Project

Abstract

EuYb is alpha La-derived structured and crystallizes in the trigonal R-3m space group. The structure is three-dimensional. there are two inequivalent Yb sites. In the first Yb site, Yb is bonded to six equivalent Yb and six Eu atoms to form YbYb6Eu6 cuboctahedra that share corners with twelve YbYb6Eu6 cuboctahedra, edges with twelve YbYb6Eu6 cuboctahedra, edges with twelve EuYb6Eu6 cuboctahedra, faces with six equivalent YbYb6Eu6 cuboctahedra, and faces with twelve EuYb6Eu6 cuboctahedra. All Yb–Yb bond lengths are 3.89 Å. All Yb–Eu bond lengths are 3.91 Å. In the second Yb site, Yb is bonded to ten equivalent Yb and six Eu atoms to form YbYb10Eu6 cuboctahedra that share corners with ten EuYb6Eu6 cuboctahedra, corners with twelve YbYb6Eu6 cuboctahedra, edges with eight EuYb6Eu6 cuboctahedra, edges with sixteen YbYb6Eu6 cuboctahedra, faces with sixteen equivalent YbYb10Eu6 cuboctahedra, and faces with eighteen EuYb6Eu6 cuboctahedra. There are a spread of Yb–Yb bond distances ranging from 3.89–7.77 Å. All Yb–Eu bond lengths are 3.91 Å. There are three inequivalent Eu sites. In the first Eu site, Eu is bonded to six equivalent Yb and six equivalent Eu atoms to form EuYb6Eu6 cuboctahedra that share corners with twelve EuYb6Eu6 cuboctahedra, edges with twelve equivalent YbYb6Eu6 cuboctahedra, edges with twelve EuYb6Eu6 cuboctahedra, faces with six equivalent EuYb6Eu6 cuboctahedra, and faces with twelve equivalent YbYb6Eu6 cuboctahedra. All Eu–Eu bond lengths are 3.89 Å. In the second Eu site, Eu is bonded to six Yb and six equivalent Eu atoms to form EuYb6Eu6 cuboctahedra that share corners with five equivalent YbYb10Eu6 cuboctahedra, corners with twelve EuYb6Eu6 cuboctahedra, edges with ten YbYb6Eu6 cuboctahedra, edges with twelve EuYb6Eu6 cuboctahedra, faces with six equivalent EuYb6Eu6 cuboctahedra, and faces with fifteen YbYb6Eu6 cuboctahedra. All Eu–Yb bond lengths are 3.91 Å. All Eu–Eu bond lengths are 3.89 Å. In the third Eu site, Eu is bonded to six Yb and six equivalent Eu atoms to form EuYb6Eu6 cuboctahedra that share corners with five equivalent YbYb10Eu6 cuboctahedra, corners with twelve EuYb6Eu6 cuboctahedra, edges with ten YbYb6Eu6 cuboctahedra, edges with twelve EuYb6Eu6 cuboctahedra, faces with six equivalent EuYb6Eu6 cuboctahedra, and faces with fifteen YbYb6Eu6 cuboctahedra. All Eu–Eu bond lengths are 3.89 Å.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

2020-05-02. Materials Data on YbEu by Materials Project. https://doi.org/10.17188/1695107

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗