Search NASA⌕ Search

DOE OSTI · 1707523

Materials Data on Eu5Mg by Materials Project

Abstract

MgEu5 crystallizes in the hexagonal P-62m space group. The structure is three-dimensional. Mg is bonded to twelve Eu atoms to form MgEu12 cuboctahedra that share corners with eighteen equivalent EuEu9Mg3 cuboctahedra, edges with six equivalent MgEu12 cuboctahedra, edges with twelve equivalent EuEu10Mg2 cuboctahedra, faces with two equivalent MgEu12 cuboctahedra, and faces with eighteen EuEu9Mg3 cuboctahedra. There are six shorter (3.73 Å) and six longer (3.82 Å) Mg–Eu bond lengths. There are two inequivalent Eu sites. In the first Eu site, Eu is bonded to three equivalent Mg and nine Eu atoms to form EuEu9Mg3 cuboctahedra that share corners with nine equivalent MgEu12 cuboctahedra, corners with nine equivalent EuEu9Mg3 cuboctahedra, edges with eighteen EuEu9Mg3 cuboctahedra, faces with three equivalent MgEu12 cuboctahedra, and faces with seventeen EuEu9Mg3 cuboctahedra. There are six shorter (3.80 Å) and three longer (3.82 Å) Eu–Eu bond lengths. In the second Eu site, Eu is bonded to two equivalent Mg and ten Eu atoms to form EuEu10Mg2 cuboctahedra that share corners with eighteen equivalent EuEu10Mg2 cuboctahedra, edges with four equivalent MgEu12 cuboctahedra, edges with fourteen EuEu9Mg3 cuboctahedra, faces with four equivalent MgEu12 cuboctahedra, and faces with sixteen EuEu9Mg3 cuboctahedra. There are two shorter (3.69 Å) and four longer (3.89 Å) Eu–Eu bond lengths.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

2020-05-03. Materials Data on Eu5Mg by Materials Project. https://doi.org/10.17188/1707523

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗