Materials Data on Ca2Ni10H by Materials Project

Abstract

Ca2Ni10H crystallizes in the orthorhombic Amm2 space group. The structure is three-dimensional. Ca is bonded in a distorted single-bond geometry to fourteen Ni and one H atom. There are a spread of Ca–Ni bond distances ranging from 2.84–3.20 Å. The Ca–H bond length is 2.36 Å. There are six inequivalent Ni sites. In the first Ni site, Ni is bonded in a 12-coordinate geometry to three equivalent Ca and nine Ni atoms. There are a spread of Ni–Ni bond distances ranging from 2.41–2.87 Å. In the second Ni site, Ni is bonded in a 12-coordinate geometry to three equivalent Ca and nine Ni atoms. There are a spread of Ni–Ni bond distances ranging from 2.42–2.44 Å. In the third Ni site, Ni is bonded to four equivalent Ca and eight Ni atoms to form distorted NiCa4Ni8 cuboctahedra that share corners with sixteen NiCa4Ni8 cuboctahedra, edges with ten NiCa4Ni8 cuboctahedra, an edgeedge with one HCa2Ni2 tetrahedra, faces with two equivalent NiCa4Ni8 cuboctahedra, and faces with two equivalent HCa2Ni2 tetrahedra. There are two shorter (2.46 Å) and two longer (2.47 Å) Ni–Ni bond lengths. In the fourth Ni site, Ni is bonded in a single-bond geometry to six Ni and one H atom. The Ni–H bond length is 1.57 Å. In the fifth Ni site, Ni is bonded to four equivalent Ca and eight Ni atoms to form NiCa4Ni8 cuboctahedra that share corners with eight NiCa4Ni8 cuboctahedra, corners with four equivalent HCa2Ni2 tetrahedra, edges with two equivalent NiCa4Ni8 cuboctahedra, and faces with ten NiCa4Ni8 cuboctahedra. All Ni–Ni bond lengths are 2.47 Å. In the sixth Ni site, Ni is bonded to four equivalent Ca and eight Ni atoms to form NiCa4Ni8 cuboctahedra that share corners with eight NiCa4Ni8 cuboctahedra, corners with four equivalent HCa2Ni2 tetrahedra, edges with six NiCa4Ni8 cuboctahedra, and faces with eight NiCa4Ni8 cuboctahedra. There are one shorter (2.47 Å) and one longer (2.48 Å) Ni–Ni bond lengths. H is bonded to two equivalent Ca and two equivalent Ni atoms to form HCa2Ni2 tetrahedra that share corners with twelve NiCa4Ni8 cuboctahedra, an edgeedge with one NiCa4Ni8 cuboctahedra, and faces with two equivalent NiCa4Ni8 cuboctahedra.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

2018-07-19. Materials Data on Ca2Ni10H by Materials Project. https://doi.org/10.17188/1725258. https://searchnasa.com/record/osti%3A1725258/materials-data-on-ca2ni10h-by-materials-project

Citations retain the original authors and DOI and include this site’s record URL. If this discovery service contributed to your research, you can also cite Search NASA by Indiciae: BibTeX · RIS.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗