Materials Data on Tb4Cu7Sn11 by Materials Project

Abstract

Tb4Cu7Sn11 crystallizes in the tetragonal P4mm space group. The structure is three-dimensional. there are four inequivalent Tb sites. In the first Tb site, Tb is bonded to four equivalent Cu and eight Sn atoms to form a mixture of corner and face-sharing TbCu4Sn8 cuboctahedra. All Tb–Cu bond lengths are 3.09 Å. There are four shorter (3.19 Å) and four longer (3.26 Å) Tb–Sn bond lengths. In the second Tb site, Tb is bonded to five Cu and eight Sn atoms to form a mixture of distorted corner and face-sharing TbCu5Sn8 cuboctahedra. There are four shorter (3.16 Å) and one longer (3.35 Å) Tb–Cu bond lengths. There are four shorter (3.23 Å) and four longer (3.26 Å) Tb–Sn bond lengths. In the third Tb site, Tb is bonded in a 12-coordinate geometry to eight Cu and eight Sn atoms. There are four shorter (3.33 Å) and four longer (3.39 Å) Tb–Cu bond lengths. There are four shorter (3.33 Å) and four longer (3.49 Å) Tb–Sn bond lengths. In the fourth Tb site, Tb is bonded in a 4-coordinate geometry to twelve Cu and four equivalent Sn atoms. There are a spread of Tb–Cu bond distances ranging from 3.12–3.36 Å. All Tb–Sn bond lengths are 3.51 Å. There are five inequivalent Cu sites. In the first Cu site, Cu is bonded in a 9-coordinate geometry to four equivalent Tb and five Sn atoms. There are one shorter (2.47 Å) and four longer (2.61 Å) Cu–Sn bond lengths. In the second Cu site, Cu is bonded in a 9-coordinate geometry to four equivalent Tb, one Cu, and four equivalent Sn atoms. The Cu–Cu bond length is 2.36 Å. All Cu–Sn bond lengths are 2.66 Å. In the third Cu site, Cu is bonded in a 10-coordinate geometry to five Tb and five Cu atoms. All Cu–Cu bond lengths are 2.46 Å. In the fourth Cu site, Cu is bonded in a 12-coordinate geometry to four Tb and four Sn atoms. There are two shorter (2.59 Å) and two longer (2.69 Å) Cu–Sn bond lengths. In the fifth Cu site, Cu is bonded in a 8-coordinate geometry to four Tb, two equivalent Cu, and two equivalent Sn atoms. Both Cu–Sn bond lengths are 2.64 Å. There are seven inequivalent Sn sites. In the first Sn site, Sn is bonded in a 2-coordinate geometry to two equivalent Tb, two equivalent Cu, and five Sn atoms. There are one shorter (2.92 Å) and four longer (3.12 Å) Sn–Sn bond lengths. In the second Sn site, Sn is bonded in a 9-coordinate geometry to two equivalent Tb, two equivalent Cu, and five Sn atoms. There are one shorter (2.97 Å) and four longer (3.12 Å) Sn–Sn bond lengths. In the third Sn site, Sn is bonded in a 8-coordinate geometry to four equivalent Tb and four equivalent Cu atoms. In the fourth Sn site, Sn is bonded in a 8-coordinate geometry to four equivalent Tb and four equivalent Cu atoms. In the fifth Sn site, Sn is bonded in a 7-coordinate geometry to two equivalent Tb and five Sn atoms. All Sn–Sn bond lengths are 3.12 Å. In the sixth Sn site, Sn is bonded in a 7-coordinate geometry to two equivalent Tb and five Sn atoms. All Sn–Sn bond lengths are 3.12 Å. In the seventh Sn site, Sn is bonded in a 9-coordinate geometry to four equivalent Tb and five Cu atoms.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

2020-04-29. Materials Data on Tb4Cu7Sn11 by Materials Project. https://doi.org/10.17188/1747885

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗