Abstract

Mg2Ho2O5 crystallizes in the tetragonal P4/mmm space group. The structure is three-dimensional. Mg2+ is bonded to five O2- atoms to form MgO5 square pyramids that share corners with five equivalent MgO5 square pyramids and faces with four equivalent HoO12 cuboctahedra. There is one shorter (1.89 Å) and four longer (1.95 Å) Mg–O bond length. There are two inequivalent Ho3+ sites. In the first Ho3+ site, Ho3+ is bonded in a body-centered cubic geometry to eight equivalent O2- atoms. All Ho–O bond lengths are 2.40 Å. In the second Ho3+ site, Ho3+ is bonded to twelve O2- atoms to form HoO12 cuboctahedra that share corners with four equivalent HoO12 cuboctahedra, faces with four equivalent HoO12 cuboctahedra, and faces with eight equivalent MgO5 square pyramids. There are four shorter (2.73 Å) and eight longer (2.91 Å) Ho–O bond lengths. There are two inequivalent O2- sites. In the first O2- site, O2- is bonded in a 4-coordinate geometry to two equivalent Mg2+ and four Ho3+ atoms. In the second O2- site, O2- is bonded in a distorted linear geometry to two equivalent Mg2+ and four equivalent Ho3+ atoms.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

2020-09-03. Materials Data on Ho2Mg2O5 by Materials Project. https://doi.org/10.17188/1757293

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗