Materials Data on Ho13(Mg2Zn27)2 by Materials Project

Abstract

Ho13(Mg2Zn27)2 crystallizes in the hexagonal P6_3/mmc space group. The structure is three-dimensional. there are two inequivalent Mg sites. In the first Mg site, Mg is bonded in a 6-coordinate geometry to three equivalent Ho and twelve Zn atoms. All Mg–Ho bond lengths are 3.11 Å. There are six shorter (2.82 Å) and six longer (3.15 Å) Mg–Zn bond lengths. In the second Mg site, Mg is bonded in a body-centered cubic geometry to eight Zn atoms. There are a spread of Mg–Zn bond distances ranging from 2.61–2.71 Å. There are four inequivalent Ho sites. In the first Ho site, Ho is bonded in a 3-coordinate geometry to sixteen Zn atoms. There are a spread of Ho–Zn bond distances ranging from 3.01–3.22 Å. In the second Ho site, Ho is bonded in a 12-coordinate geometry to one Mg and fourteen Zn atoms. There are a spread of Ho–Zn bond distances ranging from 3.00–3.29 Å. In the third Ho site, Ho is bonded in a 11-coordinate geometry to thirteen Zn atoms. There are a spread of Ho–Zn bond distances ranging from 2.96–3.24 Å. In the fourth Ho site, Ho is bonded in a 6-coordinate geometry to fourteen Zn atoms. There are a spread of Ho–Zn bond distances ranging from 2.88–3.49 Å. There are ten inequivalent Zn sites. In the first Zn site, Zn is bonded in a 10-coordinate geometry to four Ho and six Zn atoms. There are a spread of Zn–Zn bond distances ranging from 2.60–2.90 Å. In the second Zn site, Zn is bonded in a 1-coordinate geometry to two Mg, three Ho, and three Zn atoms. There are two shorter (2.62 Å) and one longer (2.63 Å) Zn–Zn bond lengths. In the third Zn site, Zn is bonded in a 9-coordinate geometry to three Ho and six Zn atoms. There are two shorter (2.55 Å) and two longer (2.88 Å) Zn–Zn bond lengths. In the fourth Zn site, Zn is bonded to two equivalent Ho and ten Zn atoms to form face-sharing ZnHo2Zn10 cuboctahedra. There are a spread of Zn–Zn bond distances ranging from 2.59–2.77 Å. In the fifth Zn site, Zn is bonded in a 12-coordinate geometry to four Ho and eight Zn atoms. There are a spread of Zn–Zn bond distances ranging from 2.54–2.97 Å. In the sixth Zn site, Zn is bonded in a 10-coordinate geometry to one Mg, four Ho, and five Zn atoms. There are two shorter (2.57 Å) and one longer (2.59 Å) Zn–Zn bond lengths. In the seventh Zn site, Zn is bonded in a 11-coordinate geometry to five Ho and six equivalent Zn atoms. In the eighth Zn site, Zn is bonded to three equivalent Ho and nine Zn atoms to form face-sharing ZnHo3Zn9 cuboctahedra. All Zn–Zn bond lengths are 2.65 Å. In the ninth Zn site, Zn is bonded in a 1-coordinate geometry to one Mg, three Ho, and five Zn atoms. In the tenth Zn site, Zn is bonded in a 1-coordinate geometry to one Mg, four Ho, and three Zn atoms.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

2020-09-03. Materials Data on Ho13(Mg2Zn27)2 by Materials Project. https://doi.org/10.17188/1757341

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗