Advanced PGM-free Cathode Engineering for High Power Density and Durability

Abstract

Polymer electrolyte fuel cells (PEFCs) are among the most promising technologies for future electric vehicles by using clean H2 with much-improved energy conversion efficiency, longer range, and rapid refueling. However, due to a large amount of platinum group metal (PGM) catalyst used in their electrodes, their prohibitively high cost hinders broad commercialization of PEFCs for transportation. Therefore, there is a critical need to develop low-cost, high-performance PGM-free cathode catalysts that have the potential to dramatically transform the economics of PEFC commercialization by reducing catalyst costs by one to two orders of magnitude. However, before PGM-free cathodes become viable, several technical challenges associated with PGM-free cathodes must be addressed, including insufficient activity and stability of the catalysts, as well as severe water flooding and large transport losses in the electrodes. Overcoming those barriers and ultimately meeting the challenging automotive PEFC performance targets was the focus of this comprehensive research and development effort on new PGM-free cathodes. To this end, we assembled a team including leading researchers from universities and industry with different but complementary expertise and capabilities. The project combined three novel and promising approaches: Advanced metal-organic framework (MOF)-derived M-N-C catalysts with a high activity and impressive durability, Novel PGM-free specific cathode architectures and fabrication strategies capable of addressing the substantial flooding and transport resistances in thicker cathodes by introducing engineered hydrophobicity through additives and support layers, and Advanced electrode ionomers with high proton conductivity for low ohmic losses across the electrode and more uniform catalyst utilization. The implementation of these new materials and electrode designs was supported by a suite of advanced experimental and simulation tools that allows us to identify performance and durability bottlenecks, devise solutions, and establish rational material design and synthesis targets. These methods include advanced electrochemical characterization, high-resolution imaging, and multi-scale modeling. In addition, the project team leveraged a broad cross-section of the ElectroCat consortium’s national laboratory facilities and expertise in advancing these materials and design strategies. Finally, the industry partners on the project facilitated the evaluation of scaled-up synthesis and manufacturing in the United States. Over its four-year period, the project made significant year-over-year advances in PGM-free cathode performance and viability. A combination of high activity and highly durable catalysts were developed through novel catalyst synthesis strategies, which met several performance and durability targets. More specifically, a catalyst prepared from MOFs and Fe2O3 nanoparticles with ammonium chloride and chemical vapor deposition treatments yielded a significant advancement in PGM-free cathode durability. Several novel strategies for fabricating cathodes were demonstrated, including those designed to reduce flooding and thickness of the cells for significantly increased volumetric power density. An optimized cathode with high conductivity ionomer and tuned ink processing for hydrophobicity yielded high fuel cell performance with new levels power density and maximum current. The scientific studies and modeling assessment also provided an outlook for future efforts, including a focus on catalysts with an increased density of the highly stable active sites developed in this project.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Litster, Shawn, Wu, Gang, Xu, Hui. 2021-11-29. Advanced PGM-free Cathode Engineering for High Power Density and Durability. https://doi.org/10.2172/1832890

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Elucidating key reducing species beyond ions in hydrogen plasma smelting reduction of iron ore

Hydrogen plasma smelting reduction (HPSR) of iron ore has attracted significant attention over the past decade due to its high-temperature operation, rapid plasma mediated reduction kinetics, and simpler density-based separation of molten iron product, compared to H2-based solid-state reduction. All of these attributes enable processing of low-grade ores for downstream use in electric-arc furnaces, as virgin iron with low gangue content is required for high quality steel and improved furnace operation. While positive ions exist within the plasma arc, this work demonstrates that near the anodic ore surface, hydrogen radicals and vibrationally excited hydrogen species dominate and their densities correlate well with observed reduction rates. Species concentrations in the transferred plasma arc and at the plasma-ore interface are evaluated using coupled thermal plasma and near-wall non-equilibrium plasma models. The thermal plasma model is validated against experimental voltage data and spectroscopic measurements of plasma temperature and density for varying current inputs. Modeling of the near surface thermochemical non-equilibrium and micrometer scale anode sheath layer reveals, in addition to the expected H + , significant concentrations of ArH + and H$^+_3$ ions, typically not observed in thermal plasmas under thermodynamic equilibrium. Our results show that the inverted sheath structure at the anodic ore surface strongly suppresses reactive positive ion fluxes, while non-equilibrium electron-impact processes generate abundant hydrogen radicals and vibrationally excited species. These findings highlight the critical role of non-equilibrium effects in hydrogen arc-driven iron ore reduction and advance understanding beyond prevailing hypotheses centered on hydrogen ion-driven mechanisms.

08 HYDROGEN↗

SimH 2 : an integrated techno-economic modeling framework for hydrogen pipeline infrastructure and network optimization

Large-scale hydrogen (H 2 ) pipeline transport design and network optimization have seldom been reported due to the lack of a cost model accounting for the relationship between transport cost and hydrogen mass flow rate. Here, this work introduced a system-level cost model for hydrogen pipeline transport at supercritical state and integrated it with an existing CO 2 pipeline network tool, SimCCS, for hydrogen-specific pipeline design and optimization. The Intermountain West (I-West) region of the U.S., historically dependent on fossil fuel-based economies, is chosen to demonstrate the capabilities of our H 2 pipeline cost model and transport network optimization platform called SimH 2 . Two scenarios are examined: one where the pipeline is not allowed to pass through disadvantaged communities and the other where it is permitted. The results highlight that incorporating disadvantaged-community constraints lead to longer pipeline routes and increased transport costs, reflecting the trade-offs involved in equitable infrastructure development. It is demonstrated that the newly developed SimH 2 tool not only enables the efficient design of H 2 transportation pipelines but also optimizes the network by accounting for local terrain and the presence of disadvantaged areas.

08 HYDROGEN↗

Disordered hydrogen adsorption at the three-fold site of W(110)

Hydrogen often forms disordered phases on metals; however, deciphering the atomic-scale behavior requires experimental and modeling techniques that directly probe the short-range order between neighboring hydrogen adsorbates. Here, to address this challenge, we applied direct recoil spectroscopy (DRS) to investigate hydrogen adsorption on the W(110) surface. We show that the recoiled hydrogen flux measured during DRS is sensitive to the short range order of the adsorbed hydrogen. Ordered hydrogen neighbors are much more efficient at dechanneling incident ions along low-index surface channels, strongly suppressing the recoiled hydrogen flux along these directions. By modeling the DRS measurements with molecular dynamics for ordered and disordered hydrogen phases, we find that at a hydrogen surface coverage of approximately Θ = 0.6, the hydrogen adsorbates are bound to three-fold sites in a disordered phase at room temperature. This finding is consistent with transfer-matrix scaling model calculations that suggest the transition to an ordered hydrogen phase occurs at a greater surface coverage of Θ = 0.83.