Search NASA⌕ Search

DOE OSTI · 1916568

Decoding Zeolite Crystallization and Stage III in Nuclear Waste Glasses by Coupled Modeling and Experiments

Abstract

Under specific conditions of pH and temperature, nuclear waste immobilization borosilicate glasses may exhibit a sudden acceleration in their corrosion kinetics (stage III)—a behavior that has been associated with the formation of zeolite crystals. Such accelerated dissolution may compromise the integrity of nuclear wasteforms placed in geological depositories. However, thus far, none of the available models is able to predict the thermodynamic propensity and kinetics of zeolite precipitation as a function of the solution conditions due to (i) a lack of fundamental knowledge regarding the nucleation & growth mechanisms of zeolitic phases, (ii) uncertainty regarding the compositions (types) of zeolites that may form and the rate-limiting step in their precipitation as a function of the solution conditions, and (iii) the complexities that arise due to the vast parametric space (i.e., solution chemistry, temperature, number of secondary phases, etc.) that encompass these systems under conditions of environmental exposure. To resolve these challenges, this project aimed to unambiguously identify the thermodynamic propensity for zeolite precipitation and the kinetics thereof as a function of the solution conditions (composition, pH, and temperature). To achieve this goal: 1) We identified the solution conditions and zeolite phases relevant to nuclear glass dissolution. 2) We performed a series of ab initio molecular dynamics (AIMD) simulations to compute the thermodynamic properties of a group of characteristic zeolites that features a large range of compositions, various hydration levels, a wide range of framework structures, and partial atomic site occupancies. 3) We released a first-of-a-kind self-consistent thermodynamic database that can be used to assess the kinetics and the stability fields of zeolitic phases within a Gibbs energy minimization (GEM) framework. 4) We developed a robust geochemical modeling method allowing us to predict the stability of secondary phases (including zeolites, calcium–silicate–hydrate gels, and clays) upon the dissolution of nuclear waste immobilization glasses. 5) We introduced a model that predicts the dissolution kinetics of a series of borosilicate nuclear waste immobilization glasses in terms of the topology of their atomic network. 6) We investigated the roles of the solution composition on the crystallization kinetics of phillipsite zeolites and tobermorite silicate hydrates. Via PNNL’s collaboration and engagement, this project directly supports DOE’s nuclear waste immobilization activities by offering a technical, science-based foundation that will (i) facilitate predictions of the long-term corrosion rates and extents of existing nuclear waste immobilization glasses to help ensure safe and successful vitrification operations, (ii) inform the development of advanced glass formulations with enhanced durability, and, (iii) enable cost-savings that result from making more decisive and hence less conservative predictions while offering higher levels of nuclear waste embedment in smaller, more compact glass volumes.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Bauchy, Mathieu, Sant, Gaurav, Ryan, Joseph V.. 2023-01-01. Decoding Zeolite Crystallization and Stage III in Nuclear Waste Glasses by Coupled Modeling and Experiments. https://doi.org/10.2172/1916568

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Evaluating transient fission gas release in high burnup light water reactor fuel during loss of coolant accident conditions via new capabilities

In this work, the role of transient fission gas release (tFGR) in the cladding burst behavior of high burnup fuel during a loss-of-coolant accident (LOCA) in commercial light water reactors was further investigated via the use of a new apparatus. During the LOCA-related temperature ramps of high burnup fuel, the release of fission gases exceeds the steady-state release observed under normal operating conditions. An enhancement was made to the Oak Ridge National Laboratory Severe Accident Test Station (SATS) to probe the various factors influencing tFGR. Experiments were performed on commercially irradiated, zirconium-clad uranium dioxide fuel, and this paper details the design of the experimental setup, the initial test results, and the subsequent post-test analyses. Notably, the first test on high burnup fuel demonstrated a LOCA-relevant tFGR of 5.3% from an unpressurized fuel segment. The ultimate tFGR was 10.7% for beyond LOCA conditions. A follow-up test on similar fuel revealed a tFGR of 12.6% under comparable conditions. Microstructural analysis and an analysis of the released gas provide some insight regarding the source of tFGR in the fuel. Finally, a grain boundary bubble model may aid in the interpretation of the results and offer a guide for future work.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Characterization of ceramic fuel powder packing fractions to support INFLUX

Triply periodic minimal surface (TPMS)-based structures show marked potential in novel nuclear reactor fuel designs, as their high surface area-to-volume ratio increases the efficiency of heat transfer out of the fuel, enabling safer, more innovative reactor designs. This milestone report addresses the role of dUO 2 powder processing route on the fill behavior of TPMS-based cladding shells to understand and advance the feasibility of manufacturing TPMS-based nuclear fuel forms. dUO 2 powder was processed through either a dry granulation route, varying consolidation pressure, or through milling, varying milling time, milling method and milled size distribution. The lowest tapped bulk densities (TBD), but best powder flowabilities, were obtained when testing unprocessed dUO 2 powder which was prone to self-agglomeration and formed low-density spheroids. The highest TBD and lowest flowabilities were obtained when using powder produced by hammer-milling dUO 2 powder to pass through a 200-mesh sieve, which led to particles with angular morphologies. Powder produced by dry granulation exhibited TBD that varied according to the consolidation pressure used to form the initial pellets and exhibited improved flowabilities when compared to hammer-milled material. Because of the large span of granule sizes formed as well as the irregular shape associated with the granules, a packing fraction of 0.69 was achieved, exceeding the analytical solution for random close packing of mono-sized spheres. TPMS polymer shells were loaded with unprocessed, granulated, and hammer-milled dUO 2 powders, and their qualitative packing behaviors were analyzed using x-ray computed tomography (xCT). TBDs calculated after loading TPMS polymer shells were 10-20% lower when compared to tapped bulk density measurements taken in a glass graduated cylinder, indicating a non-trivial impact on the tapped bulk density of either the TPMS channel size, TPMS channel surface material, powder cohesiveness, or a combination of the two parameters. A metallic zircaloy-4 TPMS shell will be loaded with hammer-milled dUO 2 powder upon receipt of the shell from Oak Ridge National Laboratory (ORNL) and shipped to Idaho National Labs (INL) for subsequent hot isostatic pressing (HIP) densification experiments.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗