Fracture in Hydrogen-Implanted Germanium

Abstract

We have studied the mechanism of fracture in hydrogen-implanted Ge. First, the as-implanted Ge state and its evolution during subsequent annealing were characterized via TEM and FTIR-MIR spectroscopy. Results showed that the extended defects formation and growth follow the same basic mechanism in Ge as in Si, which is the reference material. Nevertheless, the global damage level in the implanted Ge layer is higher compared to Si. Second, the fracture step was studied via the fracture kinetics analysis, SIMS and AFM on the transferred layer. An activation energy comparable to the reported data from blistering studies was obtained. Just like in Si, the Cmax of H in Ge measured via SIMS was found to decrease during the fracture anneal. This decrease is associated with the formation of gaseous H{sub 2} that pressurizes the internal cavities and then contributes to the fracture. Finally, a high roughness of the Ge transferred layer was measured, which results from the large thickness of the implantation damaged zone.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Mazen, F, Tauzin, A, Sanchez, L, Chieux, F, Deguet, C, Augendre, E, Clavelier, L, Akatsu, T, Richtarch, C. 2008-11-03. Fracture in Hydrogen-Implanted Germanium. https://doi.org/10.1063/1.3033596. https://searchnasa.com/record/osti%3A21251659/fracture-in-hydrogen-implanted-germanium

Citations retain the original authors and DOI and include this site’s record URL. If this discovery service contributed to your research, you can also cite Search NASA by Indiciae: BibTeX · RIS.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗