Improved Creep Testing Approach for Bentonite EBS

Abstract

In the United States, the nuclear reactor contributes 18.7 percent of the nation’s total electricity generation and produces a significant amount of spent nuclear fuel (SNF) and high-level waste. Because SNF is being stored for longer periods than initially envisioned, the U.S. Department of Energy Office of Nuclear Energy, Office of Spent Fuel and Waste Science and Technology is assessing the technical performance of the SNF storage systems after extended durations. The concept of a sustainable geologic repository for SNF disposal relies heavily on the safety provided by multiple barriers, such as repository host rock, overlying rock formation, and human-made engineered barrier systems (EBS). One of the major components of EBS is bentonite-based buffer materials that isolate the nuclear-waste canisters from the host rock and fill the void left in the horizontally drilled boreholes. The resaturated bentonite has a swelling characteristic, which is useful for self-sealing the microcracks in the host rock and supporting the canister’s heavy weight. However, factors such as nonuniformity in the saturation, swelling pressure of bentonite, and the high temperature at the canister-bentonite interface may lead to instability of the waste canister inside the borehole. Therefore, evaluating the long-term deformation of bentonite-based material is necessary. RESPEC Company, LLC recently completed a preliminary study for the U.S. Department of Energy (DE SC0022804) that is attempting to understand the time-dependent deformation in the consolidated sand/bentonite (SB) specimens through triaxial creep experiments and improve the understanding of EBS performance under anticipated repository conditions. The project included developing a standard testing procedure for preparing the consolidated core specimen from a mixture of sand and bentonite in a 50:50 ratio by weight, fabricating a new pressure vessel in-house, modifying existing creep equipment to perform triaxial creep experiments on consolidated SB specimens, and performing six long-term triaxial creep experiments under low-deviatoric stress at two different temperature conditions, which is representative of hypothetical conditions that might be encountered in a geologic repository within a reasonable rate of success in completing creep experiments. The consolidated SB specimen was prepared using the novel specimen preparation procedure and had physical characteristics (e.g., moisture content and bulk density) reasonably comparable with the properties of bentonite-based buffer, which is proposed to be used in the EBS in the Swedish KBS-3H design and the Swiss design of SNF disposal in the horizontal drifts. The newly fabricated pressure vessel could withstand the confining pressure of up to 15 megapascals (MPa) while maintaining the test temperature of up to 90 degrees Celsius (°C) for long-term creep experiments. The preliminary results from the triaxial creep experiments suggested that the consolidated SB specimen may experience time-dependent deformation at a low-deviatoric stress state and room temperature condition. Based on the deformation recorded in the SB specimen from axial and radial linear variable differential transformers (LVDTs) and physical characteristic changes, it is apparent that the time-dependent deformation is a combination of consolidation and creep, which is influenced by the level of deviatoric stresses and temperature. The systematic creep testing of bentonite-based specimens helped develop a standard testing procedure applicable for analyzing the similar characteristics of shale or clay-like materials in different geologic conditions outside repository science, including in civil engineering and infrastructure projects, underground and open pit mining, and deep drilling.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Gupta, Neel, Keffeler, Evan R., Hladysz, Jakub P., Buchholz, Stuart A., Vining, Cody A., Hardin, Ernest L.. 2024-05-14. Improved Creep Testing Approach for Bentonite EBS. https://doi.org/10.2172/2349491

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Spectrophotometric study of erbium (III) speciation in chloride solutions from 25 to 75 °C

In this study, UV-Vis spectrophotometric experiments were conducted from 25 to 75 °C using Er-HClO4-bearing solutions with varying NaCl concentrations. The molar absorbance coefficient of Er3+ decreases with temperature, and the absorbance intensity gradually decreases with increasing mCl/mEr ratios. The number of absorbing species include Er3+ and ErCl2+ even at the highest mCl/mEr ratio. The formation constant (β 1 ) for the ErCl 2+ species was derived and fitted between 50 and 250 °C with existing literature values, yielding the following equation: logβ 1 0 = −22.4315 + 0.0345T + 3.9379·10 3 /T, where T is temperature in Kevin.

58 GEOSCIENCES↗

The future of subsurface monitoring: AEC’s breakthroughs in CCS technology

Carbon capture and storage (CCS) has emerged as a key solution in the fight against climate change. However, for CCS to succeed, it is crucial to ensure that the sequestered CO2 stays safely trapped underground. The U.S. Department of Energy (DOE) has emphasized the need for advancements in subsurface monitoring, measurement, reporting, and verification. Aside from caprock integrity failure, the other primary failure points usually involve defective cement in the casing annulus of wellbores or plugged and abandoned wells. In addition, many energy producers (e.g., oil and gas, geothermal) and storage and disposal operators (e.g., H2 and water) must deal with the same issue. Poorly placed or degraded cement can create pathways for gas or fluid to escape from casing annuli and in plugged and abandoned or orphan wells, posing environmental risks. Yet, a reliable and cost-effective way to monitor cement and well integrity over multiple decades is still unavailable. Traditional geophysical methods like 4D seismic imaging and surface-based electromagnetic monitoring lack the resolution and accuracy for detecting these types of failures (Vasco et al., 2022; Fawad and Mondol, 2021). Wireline logging is expensive to run continuously and is obtrusive to the operation. While fiber optics can potentially be a solution, its bulkiness can significantly compromise the cement's integrity. To address these challenges, the Advanced Energy Consortium (AEC) at The University of Texas at Austin’s Bureau of Economic Geology (the Bureau) has been pioneering research in subsurface monitoring using its portfolio of distributed autonomous microfabricated sensors for harsh subsurface environments since 2008. A class of these microsensors [System on a Chip (SoC)] can be mixed in cement and permanently placed without compromising the cement column; the sensors would then communicate with each other or a data acquisition (DAQ) master node. Another class of the AEC microsensors can be fully autonomous, with rechargeable micro-batteries capable of exceeding 100°C, flash memory, and, currently, a pressure and temperature sensor. They are designed to circulate in mud, geothermal fluids, U-loops, or pipelines. They can log data into memory and are unobtrusive to operations. Our team has been working on a multi-year DOE-funded project (DE-FE0031856)—supported by $2.95M in federal funding and $0.75M in cost-matching from the AEC—to demonstrate SoC sensor utility for CO2 leakage monitoring in CCS applications. This multi-institutional collaboration developed a novel sensing architecture utilizing radiofrequency (RF) microsensors embedded within the cement sheath. These sensors detect CO2 migration and are interrogated via a Smart Casing Collar (SCC).

58 GEOSCIENCES↗

Hydrogeological assessment of CO2 containment assurance and wellbore integrity at a Gulf Coast storage site

Abstract A large-scale carbon capture and storage (CCS) initiative on the Texas Gulf Coast serves as a premier demonstration of the U.S. Department of Energy’s CarbonSAFE program. Targeting deep saline formations, specifically Oligo-Miocene deltaic sequences, the project aims to establish technical and commercial viability for geologic CO2 storage within a major industrial corridor. This study provides a rigorous hydrogeological assessment to support Class VI permitting by quantifying the high degree of containment security. Utilizing a compositional reservoir simulator, we developed a suite of 27 distinct simulation cases to evaluate vertical plume dynamics near both planned injection wells and proximal legacy infrastructure. To ensure numerical accuracy near wellbores, we implemented a refined mesh strategy, determining that a 5.6 ft × 5.6 ft grid refinement offered the optimal balance between computational efficiency and descriptive precision. The modeling framework utilized a systematic sensitivity-based approach to evaluate the mechanical redundancy of the subsurface system by performing a bounding analysis of wellbore interfaces against hypothetical high-permeability microannuli. By systematically isolating competing physical drivers, including permeability, porosity, gas hysteresis, thermal gradients, salinity, and solubility trapping (quantified via Henry’s law with dynamically adjusted coefficients), this work moves beyond binary assessments to establish a nuanced hierarchy of containment factors. The results confirm that primary trapping mechanisms (e.g., gas hysteresis and solubility), combined with the site's unique geomechanical stratigraphy, significantly restrict vertical mobility and reinforce the robust containment security of the reservoir. Baseline results demonstrate substantial vertical separation between the CO2 plume and the upper confining system, ensuring robust containment. Sensitivity analysis reveals that even under highly conservative bounding scenarios—assuming theoretical 10-Darcy pathways at specific wellbore locations—the 2,900-ft thick multi-layered confining zone remains a reliable barrier. In these hypothetical upper-bound cases, peak upward fluxes of CO2 and saltwater after 15 years of injection remain localized and dissipate rapidly within the lower sections of the confining interval, leaving the integrity of the seal uncompromised. Furthermore, the study identifies that while localized wellbore pathways define theoretical upper bounds of vertical migration, the Area of Review (AoR) is primarily sensitive to regional thermal gradients and hysteresis, which can influence the AoR by over 3,000 acres in pessimistic configurations. Also, primary trapping mechanisms, specifically gas hysteresis and solubility, work in tandem with the Gulf Coast’s unique geomechanical stratigraphy to significantly restrict vertical mobility. Ductile, smectite-rich mudstones facilitate natural borehole convergence and the self-healing of potential conduits, creating a natural geomechanical bridge that effectively mitigates migration potential at both current injection points and legacy-well locations. This comprehensive modeling effort demonstrates that the integration of high-resolution wellbore simulations and regional geomechanical observations confirms the long-term storage security of the studied site, providing a physics-based foundation for industrial-scale CCS deployments. This modeling framework establishes a baseline for future research into coupled geomechanical effects, such as time-dependent borehole convergence, to further refine long-term containment projections. Acknowledgements We thank the Gulf Coast Carbon Center (GCCC) at the Bureau of Economic Geology for foundational research support. We appreciate Alex Bump for technical guidance and David Hoffman for model mesh generation. This work used TACC’s Frontera cluster for simulations and CMG Ltd. software licenses provided to UT-Austin. This material is based upon work supported by the Department of Energy under Award Number DE-FE0032338. Disclaimer This material is based upon work supported by the U.S. Department of Energy’s Fossil Energy and Carbon Management Office under the CarbonSAFE program, award Number DE-FE0032338. The views expressed herein do not necessarily represent the views of the U.S. Department of Energy or the United States Government.

58 GEOSCIENCES↗