Report on technical development in ANL for innovative creep testing and measurement
Abstract
This report summarizes a research effort undertaken by Argonne National Laboratory to accelerate the development of creep data package for ASME code qualification. Progress on the fabrication of a 3-sample load train and the application of a direct current potential drop (DCPD) technique to measure large creep strains are reported. Specifically: (1) The 3-sample load train, with three sets of Linear Variable Differential Transformers (LVDT), has been fabricated and assembled. (2) A DCPD method for creep-strain measurement up to 50% has been demonstrated. The DCPD data matches very well to LVDT results, suggesting its potential application in future creep testing. The technical developments contribute towards shortening the time needed to generate a creep data package for an ASME code case of the laser powder bed fusion 316H stainless steel, an effort under the US Department of Energy’s Advanced Materials and Manufacturing Technologies (AMMT) program.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Zhang, Xuan, Snitzer, John, Listwan, Edward J.. 2024-06-01. Report on technical development in ANL for innovative creep testing and measurement. https://doi.org/10.2172/2375866
Cite the original work for its findings. Save a collection to share your selection of sources.