Nucleation dependence of atomic layer deposition on diamond surface termination

Abstract

Surface termination and interfacial interactions are critical for advanced solid-state quantum applications. Here, in this paper, we demonstrate that atomic layer deposition (ALD) can both provide valuable insight on the chemical environment of the surface, having sufficient sensitivity to distinguish between the common diamond (001) surface termination types and passivate these interfaces as desired. We selected diamond substrates exhibiting both smooth and anomalously rough surfaces to probe the effect of morphology on ALD nucleation. We use high resolution in situ spectroscopic ellipsometry to monitor the surface reaction with sub-angstrom resolution, to evaluate the nucleation of an ALD Al 2 O 3 process as a function of different ex and in situ treatments to the diamond surface. In situ water dosing and high vacuum annealing provided the most favorable environment for nucleation of dimethylaluminum isopropoxide and water ALD. Hydrogen termination passivated both smooth and rough surfaces while triacid cleaning passivated the smooth surface only, with striking effectiveness.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Jones, Jessica C., Delegan, Nazar, Heremans, F. Joseph, Martinson, Alex B. F.. 2023-07-10. Nucleation dependence of atomic layer deposition on diamond surface termination. https://doi.org/10.1016/j.carbon.2023.118276

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Frontiers in divalent $f$-block chemistry

Divalent f-block chemistry has undergone rapid expansion in recent years, driven by advances in the stabilization of low-valent lanthanide and actinide complexes. Although f-elements were historically accessed in the +3 or higher oxidation states, the isolation of +2 species has revealed unusual spectroscopic signatures, distinct bonding motifs, and multiple accessible electronic configurations that influence their chemical and physical properties. These developments have generated opportunities in areas including quantum information science, molecular magnetism, catalysis, and luminescence. Computational chemistry has played a pivotal role in interpreting the electronic structure and reactivity of these systems. However, accurately modeling divalent f-block complexes remains challenging because of strong electronic correlation, multiconfigurational character, and the presence of close-in-energy competing electronic states. As experimental capabilities and theoretical methodologies continue to advance, a comprehensive assessment of divalent chemistry is both timely and needed. In this Review, we integrate experimental and theoretical perspectives to provide a systematic analysis of divalent lanthanide and actinide complexes across the f-block series. We critically assess the role of ligands in determining competing ground-state configurations (f n d 1 vs. f n+1 ) resulting in their distinct spectroscopic, magnetic, and bonding properties. Finally, we discuss emerging strategies for predictive modeling and rational design of low-valent f-block molecular systems, with potential applications ranging from dinitrogen reduction to quantum technologies.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Unveiling the electronic structure and chemical bonding of the deprotonated cisplatin anion [(NH 3 )(NH 2 )PtCl 2 ] − via low-temperature photoelectron spectroscopy and theoretical calculations

The dehydrogenated cisplatin anion, [(NH 3 )(NH 2 )PtCl 2 ] − , was investigated via low-temperature photoelectron spectroscopy and theoretical calculations. Seven and four spectral peaks are respectively resolved at 193 and 266 nm, yielding rich electronic structure information for both the anion and neutral. From the threshold and maximum of the lowest electron binding energy band, the experimental adiabatic (ADE) and vertical detachment energies (VDE) are determined to be 3.3 ± 0.1 and 3.525 ± 0.025 eV, respectively. Theoretical calculations indicate the dominant isomer adopting a cis-geometry, in which the platinum center is coplanar with two chlorine and two nitrogen ligands. The calculated VDE of 3.54 eV based on this structure agrees well with the experimental value. Charge analyses reveal that the excess electron in the anion is primarily localized on the Pt and Cl atoms. A suite of theoretical analysis tools was employed to elucidate the bonding characteristics and interaction strength between Pt and its ligands.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Adsorption, charge transfer and a coverage-driven transition of alkali metals on rutile TiO 2 (110)

The interaction of alkali metals with metal oxide surfaces is central to tuning surface reactivity in heterogeneous catalysis and photocatalysis. Here we present a comprehensive DFT+U study of the adsorption of alkali metals (Li, Na, K, Rb, Cs) on the (110) surface of rutile TiO 2 . At low coverage (θ = 1/8), all alkali metals bind preferentially to bridging oxygen sites with adsorption energies in the range −4.06 to −3.33 eV, transferring nearly one full electron (0.92–0.99 |e|) to the substrate and inducing Ti 4+ → Ti 3+ reduction. The excess charge localizes preferentially at subsurface Ti sites in the form of small polarons. Diffusion barriers indicate facile motion along bridging-oxygen rows, whereas inter-row hopping is strongly hindered. Coverage effects were examined systematically for potassium: adsorption energy and charge transfer per K atom decrease monotonically with increasing θ. Strikingly, a sharp energy discontinuity occurs between θ = 4/8 and θ = 5/8 (ΔE ≈ 1 eV per atom), which we identify as a coverage-driven structural transition arising from steric packing constraints and enhanced K–K electrostatic repulsion once every (1×1) surface cell is occupied. This structural transition perfectly correlates with a dramatic drop in the work function down to an ultra-low minimum of 0.84 eV at θ=5/8, followed by a metallization- driven recovery at higher coverages. Ab initio molecular dynamics simulations confirm zigzag K arrangements at moderate coverage (θ = 1/3), while at high coverage (θ = 2/3) short-range K–K correlations emerge without long-range order. These results provide atomistic insight into the structure–activity relationships underlying alkali promotion effects on oxide-supported catalysts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗