Stable high conductivity oxide electrolyte
Abstract
The present invention relates to rhomboidal phase bismuth oxide that maintains electric conductivity of at least about 1×10 −2 S/cm at temperature of about 500° C. for at least about 100 hours. In particular, the bismuth oxides of the invention have stable conductivity at a temperature range from about 500° C. to about 550° C.