Multi-principal element alloys for fast reactor cladding applications

Abstract

Given the extensive list of multi-principal element alloys (MPEAs) within literature and the overwhelming number of alloys that can be made from only a handful of elements, this article proposes a methodology for prioritizing alloys for use as cladding within advanced reactors. This paper applies neutronic, mechanical, and chemical assessments to a collection of MPEAs available within literature for use as advanced reactor cladding. The results are compared to a reference design of HT9, a ferritic/martensitic steel, for employed in sodium-cooled fast reactor. Mechanical assessments determined pressure limits for a thin-walled tube pressure boundary, thus relating the material's mechanical properties to a minimum acceptable wall thickness. Neutronic analyses reveal a maximum allowable wall thickness that a given material must meet to provide a level of neutronic economy that is equivalent to than that of HT9. Lastly, each alloying element is compared to typical fission products found in a fast reactor fuels to mitigate deleterious phenomena such as fuel-cladding chemical interactions (FCCI). These analyses indicate that Mo-Nb-Ti-V-based alloys are likely to be advantageous and that the inclusion of elements with a high neutronic penalty (e.g., Hf) could be considered with minimal consequences.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Beausoleil, G. L., Curnutt, Byron J., Moorehead, Michael J., Bascom, Andrew John. 2024-11-05. Multi-principal element alloys for fast reactor cladding applications. https://doi.org/10.1016/j.net.2024.11.005

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Evaluating transient fission gas release in high burnup light water reactor fuel during loss of coolant accident conditions via new capabilities

In this work, the role of transient fission gas release (tFGR) in the cladding burst behavior of high burnup fuel during a loss-of-coolant accident (LOCA) in commercial light water reactors was further investigated via the use of a new apparatus. During the LOCA-related temperature ramps of high burnup fuel, the release of fission gases exceeds the steady-state release observed under normal operating conditions. An enhancement was made to the Oak Ridge National Laboratory Severe Accident Test Station (SATS) to probe the various factors influencing tFGR. Experiments were performed on commercially irradiated, zirconium-clad uranium dioxide fuel, and this paper details the design of the experimental setup, the initial test results, and the subsequent post-test analyses. Notably, the first test on high burnup fuel demonstrated a LOCA-relevant tFGR of 5.3% from an unpressurized fuel segment. The ultimate tFGR was 10.7% for beyond LOCA conditions. A follow-up test on similar fuel revealed a tFGR of 12.6% under comparable conditions. Microstructural analysis and an analysis of the released gas provide some insight regarding the source of tFGR in the fuel. Finally, a grain boundary bubble model may aid in the interpretation of the results and offer a guide for future work.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Characterization of ceramic fuel powder packing fractions to support INFLUX

Triply periodic minimal surface (TPMS)-based structures show marked potential in novel nuclear reactor fuel designs, as their high surface area-to-volume ratio increases the efficiency of heat transfer out of the fuel, enabling safer, more innovative reactor designs. This milestone report addresses the role of dUO 2 powder processing route on the fill behavior of TPMS-based cladding shells to understand and advance the feasibility of manufacturing TPMS-based nuclear fuel forms. dUO 2 powder was processed through either a dry granulation route, varying consolidation pressure, or through milling, varying milling time, milling method and milled size distribution. The lowest tapped bulk densities (TBD), but best powder flowabilities, were obtained when testing unprocessed dUO 2 powder which was prone to self-agglomeration and formed low-density spheroids. The highest TBD and lowest flowabilities were obtained when using powder produced by hammer-milling dUO 2 powder to pass through a 200-mesh sieve, which led to particles with angular morphologies. Powder produced by dry granulation exhibited TBD that varied according to the consolidation pressure used to form the initial pellets and exhibited improved flowabilities when compared to hammer-milled material. Because of the large span of granule sizes formed as well as the irregular shape associated with the granules, a packing fraction of 0.69 was achieved, exceeding the analytical solution for random close packing of mono-sized spheres. TPMS polymer shells were loaded with unprocessed, granulated, and hammer-milled dUO 2 powders, and their qualitative packing behaviors were analyzed using x-ray computed tomography (xCT). TBDs calculated after loading TPMS polymer shells were 10-20% lower when compared to tapped bulk density measurements taken in a glass graduated cylinder, indicating a non-trivial impact on the tapped bulk density of either the TPMS channel size, TPMS channel surface material, powder cohesiveness, or a combination of the two parameters. A metallic zircaloy-4 TPMS shell will be loaded with hammer-milled dUO 2 powder upon receipt of the shell from Oak Ridge National Laboratory (ORNL) and shipped to Idaho National Labs (INL) for subsequent hot isostatic pressing (HIP) densification experiments.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗