Thermodynamics of MgO Atomic Layer Deposition Surface Reactions

Abstract

The realities of atomic layer deposition (ALD) surface reactions often deviate from the simple ligand exchange frequently used to illustrate the technique. A detailed understanding of these reactions is necessary to develop greater surface synthetic control including chemical selectivity for patterning or to target defects. Here, the thermodynamics of surface reactions relevant to MgO ALD were investigated using pyroelectric calorimetry to measure the time-resolved heat generation. These reactions show exothermic heat generation of 0.12 mJ/cm 2 and 0.15 mJ/cm 2 for alternating Mg(CpEt) 2 and H 2 O reactions, respectively. The total reaction heat closely matches the standard reaction enthalpy for bulk MgO, supplemented with first-principles molecular calculations. First-principles models further reveal that while simple ligand exchange is favorable during surface reactions, the required increase in Mg-coordination number from two in the precursor to six in bulk MgO requires additional coverage-dependent surface reactions, which depend on the availability and stability of proximal surface hydroxyls.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Bielinski, Ashley R. [Argonne National Laboratory (ANL), Argonne, IL (United States)] (ORCID:0000000307735782), Xu, Jiayi [Argonne National Laboratory (ANL), Argonne, IL (United States)] (ORCID:0000000317636251), Htun, Swan Yee [Northwestern Univ., Evanston, IL (United States)], Hruszkewycz, Stephan O. [Argonne National Laboratory (ANL), Argonne, IL (United States)] (ORCID:0000000293949252), Liu, Cong [Argonne National Laboratory (ANL), Argonne, IL (United States)] (ORCID:0000000221455034), Martinson, Alex B. F. [Argonne National Laboratory (ANL), Argonne, IL (United States)] (ORCID:0000000339161672). 2025-01-14. Thermodynamics of MgO Atomic Layer Deposition Surface Reactions. https://doi.org/10.1021/acsmaterialslett.4c02078

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗