Decoupling the capacity fade contributions in polymer electrolyte-based high-voltage solid-state batteries

Abstract

Polymer electrolyte (PE)-based solid-state batteries (PE-SSBs) made with high-voltage cathodes are known to suffer from severe capacity fade, stemming primarily from the poor oxidative stability of most PEs under high-voltage cycling conditions. PEs also suffer from greater ion-transport limitations compared to liquid or solid electrolytes. However, often, these limitations are collectively stated to be responsible for the observed capacity fade, and it is challenging to decouple the contributions of different factors. Herein, a tunable cell fabrication platform was developed to systematically investigate and decouple the two primary capacity fade drivers (cell impedance growth and kinetic limitations), while keeping the other cell parameters constant. Three PE types with distinct transport characteristics were compared. By utilizing a voltage profile analysis method, the contribution of the cell's internal impedance growth was quantitatively decoupled from the kinetic limitations stemming from the high concentration gradient in the polymer catholyte and slow charge transfer reactions. We demonstrate that the high interfacial impedance did not necessarily correlate with the high capacity fade rate. Kinetic limitations that are not reflected by impedance measurements can play a dominant role in causing cumulative capacity decay.

Keep this discovery

BibTeXRIS

Ock, Ji-young [Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)] (ORCID:0000000211591753), Kalnaus, Sergiy [Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)] (ORCID:0000000274653034), Zachman, Michael J. [Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)] (ORCID:0000000319101357), Ullman, Andrew M. [Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)] (ORCID:0000000338759648), Owensby, Kyra D. [Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States); Univ. of Tennessee, Knoxville, TN (United States). Bredesen Center for Interdisciplinary Research and Graduate Education], Long, Oliver [Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)] (ORCID:0009000567865601), Chen, Xi Chelsea [Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)] (ORCID:0000000311887658), Sahore, Ritu [Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)] (ORCID:0000000223909570). 2025-12-15. Decoupling the capacity fade contributions in polymer electrolyte-based high-voltage solid-state batteries. https://doi.org/10.1039/D5TA07799K

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related discoveries

Improving Ionic Conformality Across Polymer Electrolyte|Electrode Interfaces

Maintaining uniform ionic transport at electrode|electrolyte interfaces, i.e., ionic conformality, remains challenging in polymer electrolyte (PE)-based solid-state batteries. Morphological conformality does not necessarily imply ionic conformality. In PEs, which typically consist of a mechanically supporting component and distinct ionically conductive components, the rearrangement or depletion of mobile ion-conductive domains at interfaces can disrupt ionic transport pathways. Such localized ionic depletion contributes to interfacial instability and capacity degradation in high-voltage lithium-metal batteries. Herein, an electrolyte design approach aimed at minimizing interfacial heterogeneities is demonstrated through compositional adjustments, characterized by spatially resolved structural and chemical X-ray techniques and NMR diffusometry to elucidate ion transport dynamics. This approach improves ionic conformality at electrode interfaces, enhancing cycling stability in Li||LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NMC811) coin and pouch cells cycled at high voltages. These results contribute to understanding interfacial behaviors in multiphase PEs and inform strategies for improving stability across solid-state battery interfaces.

36 MATERIALS SCIENCE

Novel Zwitterionic Polyurethane-in-Salt Electrolytes with High Ion Conductivity, Elasticity, and Adhesion for High-Performance Solid-State Lithium Metal Batteries

This study presents a novel polymer-in-salt (PIS) zwitterionic polyurethane-based solid polymer electrolyte (zPU-SPE) that offers high ionic conductivity, strong interaction with electrodes, and excellent mechanical and electrochemical stabilities, making it promising for high-performance all solid-state lithium batteries (ASSLBs). The zPU-SPE exhibits remarkable lithium-ion (Li+) conductivity (3.7 × 10⁻⁴ S cm−1 at 25 °C), enabled by exceptionally high salt loading of up to 90 wt.% (12.6 molar ratio of Li salt to polymer unit) without phase separation. It addresses the limitations of conventional SPEs by combining high ionic conductivity with a Li+ transference number of 0.44, achieved through the incorporation of zwitterionic groups that enhance ion dissociation and transport. The high surface energy (338.4 J m−2) and elasticity ensure excellent adhesion to Li anodes, reducing interfacial resistance and ensuring uniform Li+ flux. When tested in Li||zPU||LiFePO₄ and Li||zPU||S/C cells, the zPU-SPE demonstrated remarkable cycling stability, retaining 76% capacity after 2000 cycles with the LiFePO4 cathode, and achieving 84% capacity retention after 300 cycles with the S/C cathode. Molecular simulations and a range of experimental characterizations confirm the superior structural organization of the zPU matrix, contributing to its outstanding electrochemical performance. The findings strongly suggest that zPU-SPE is a promising candidate for next-generation ASSLBs.

Wang, Kun

Making Plasticized Polymer Electrolytes Stable Against Sodium Metal for High‐Energy Solid‐State Sodium Batteries

Solid polymer electrolytes based on plastic crystals are promising for solid-state sodium metal (Na 0 ) batteries, yet their practicality has been hindered by the notorious Na 0 -electrolyte interface instability issue, the underlying cause of which remains poorly understood. Here, in this study, by leveraging a model plasticized polymer electrolyte based on conventional succinonitrile plastic crystals, we uncover its failure origin in Na 0 batteries is associated with the formation of a thick and non-uniform solid electrolyte interphase (SEI) and whiskery Na 0 nucleation/growth. Furthermore, we design a new additive-embedded plasticized polymer electrolyte to manipulate the Na 0 deposition and SEI formulation. For the first time, we demonstrate that introducing fluoroethylene carbonate (FEC) additive into the succinonitrile-plasticized polymer electrolyte can effectively protect Na 0 against interfacial corrosion by facilitating the growth of dome-like Na 0 with thin, amorphous, and fluorine-rich SEIs, thus enabling significantly improved performances of Na//Na symmetric cells (1,800 h at 0.5 mA cm −2 ) and Na//Na 3 V 2 (PO 4 ) 3 full cells (93.0 % capacity retention after 1,200 cycles at 1 C rate in coin cells and 93.1 % capacity retention after 250 cycles at C/3 in pouch cells at room temperature). Our work provides valuable insights into the interfacial failure of plasticized polymer electrolytes and offers a promising solution to resolving the interfacial instability issue.

25 ENERGY STORAGE