A systematic investigation was conducted on the oxidation behavior of silicon-bond coats within environmental barrier coating (EBC) systems applied to Si-carbide (SiC) substrates, aiming to understand how different underlying SiC substrates influence the bond coat's thermally grown oxide (TGO) and its properties. The study examined (Y/Yb) 2 Si 2 O 7 /Si coatings on three cost-effective surrogate SiC substrates (chemical vapor deposition [CVD]-grown β-SiC, sintered α-SiC, and reaction-bonded [RB] SiC) for SiC fiber /SiC matrix ceramic matrix composites (CMCs). Discrepancies in TGO growth were observed, with noticeably higher growth rates reported for the coated CMC specimens than for the four monolithic SiC specimens. The CMC samples produce an amorphous TGO, whereas the other monolithic substrates formed a crystalline TGO, which lowered the oxygen permeability through the SiO 2 scale. In conclusion, the vitrification of the TGO in the (Y/Yb) 2 Si 2 O 7 /Si/CMC system resulted from the migration of boron species from the CMC substrate to the SiO 2 scale, leading to network modification via boron doping.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Ardrey, Kristyn D. [Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)] (ORCID:0000000184407796), Lance, Michael J. [Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)] (ORCID:0000000151675452), Ridley, Mackenzie J. [Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)] (ORCID:0000000240432209). 2026-01-29. SiC Substrate Composition Effect on TGO Scale Growth in EBC Systems During High‐Temperature Steam Exposure. https://doi.org/10.1111/jace.70540

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Environmental Barrier Coatings for Ceramic Matrix Composites - An Overview

SiC/SiC Ceramic Matrix Composites (CMCs) are increasingly being considered as structural materials for advanced power generation equipment because of their light weight, higher temperature capability, and oxidation resistance. Limitations of SiC/SiC CMCs include surface recession and component cracking and associated chemical changes in the CMC. The solutions pursued to improve the life of SiC/SiC CMCs include the incorporation of coating systems that provide surface protection, which has become known as an Environmental Barrier Coating (EBC). The development of EBCs for the protection of gas turbine hot section CMC components was a continuation of coating development work for corrosion protection of silicon-based monolithics. Work on EBC development for SiC/SiC CMCs has been ongoing at several national laboratories and the original gas turbine equipment manufacturers. The work includes extensive laboratory, rig and engine testing, including testing of EBC coated SiC/SiC CMCs in actual field applications. Another EBC degradation issue which is especially critical for CMC components used in aircraft engines is the degradation from glassy deposits of calcium-magnesium-aluminosilicate (CMAS) with other minor oxides. This paper addresses the need for and properties of external coatings on SiC/SiC CMCs to extend their useful life in service and the retention of their properties.

EBC↗

Thermochemical/Thermomechanical Synergies in High Temperature Solid Particle Erosion of CMAS-Exposed EBCs

Environmental barrier coatings (EBCs) are an enabling technology for the use of SiC-based ceramic matrix composites in next generation gas turbine engines. In the extreme engine environment, EBCs must be able to withstand a variety of individual damage mechanisms and their interactions with each other. Ingested particulates/debris can cause both thermochemical and thermomechanical degradation of EBCs. Siliceous debris primarily based on calcium magnesium aluminosilicates (CMAS) can melt and infiltrate and/or react with EBCs above >1200°C. Similarly, ingested debris can lead to mechanical damage and recession of coatings due to particulate erosion. Both modes of degradation can occur simultaneously during engine operation, and it is crucial to comprehensively understand the mechanisms of coating failure due to high-temperature particulate interactions. This study assesses the erosion durability of Yb2Si2O7-based EBCs exposed to CMAS of various loads in NASA Glenn’s Erosion Burner Rig Facility. CMAS exposures and erosion testing were carried out at 1316°C. The effects of CMAS loading and exposure time on EBC erosion durability were evaluated using Al2O3 as an erodent material.

EBC↗