DOE OSTI · 3682464

Automated 4D X-ray Computed Tomography Registration and Flaw Tracking Across Interrupted Creep Testing of Additively Manufactured Steel

Abstract

The source did not provide an abstract. Follow the original record for more information.

Keep this discovery

BibTeXRIS

Ziabari, Amir [ORNL] (ORCID:000000034776457X), Franklin, Rahul [ORNL] (ORCID:0000000232662362), Rahman, Obaid [ORNL] (ORCID:0000000277810840), Joslin, Chase [ORNL] (ORCID:0000000246246511), Knapp, Gerry [ORNL] (ORCID:000000022023992X), Dryepondt, Sebastien [ORNL] (ORCID:0000000312651612), Massey, Caleb [ORNL], Nandwana, Peeyush [ORNL] (ORCID:0000000251471668), Dehoff, Ryan [ORNL] (ORCID:0000000194569633). 2026-08-01. Automated 4D X-ray Computed Tomography Registration and Flaw Tracking Across Interrupted Creep Testing of Additively Manufactured Steel. https://doi.org/10.2172/3682464

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Thermal Inspection for the Assessment of Adhesively Bonded Metal Adherents

Certification of adhesively bonded structures is currently a challenge for aircraft manufacturers. The ability to certify bonds in primary structure can reduce dependence on fasteners and this will enable more efficient manufacturing. For example, drilling holes and installing fasteners in bonded joints can be a potentially significant bottleneck in airframe manufacturing. In addition, fasteners increase the airframe weight and can add stress concentration areas. Reducing fastener count can accelerate manufacturing and improve aircraft performance. NASA is currently investigating nondestructive evaluation (NDE) techniques to assess bond integrity. For example, bond thickness influences bond strength and therefore NDE techniques are being investigated to determine bond thickness. For bonded metal structures, there is a large difference in the thermal diffusivity between the 7075 aluminum alloy metal adherends and aircraft grade adhesive. Multi-layered thermal models show a large variation in the thermal response for bondline adhesive thicknesses that vary from 100 to 300 microns for adherend thicknesses of 0.163 cm. Experimental through-transmission thermal measurements reveal promise to quantitatively characterize the bondline thickness. Results were validated with X-ray computed tomography and optical microscopy measurements, and influence of porosity on the thermal model and measurements are investigated.

bondline thickness

Thermal Inspection for the Assessment of Adhesively Bonded Metal Adherends

Certification of adhesively bonded structures is currently a challenge for aircraft manufacturers. The ability to certify bonds in primary structure can reduce dependence on fasteners and this will enable more efficient manufacturing. For example, drilling holes and installing fasteners in bonded joints can be a potentially significant bottleneck in airframe manufacturing. In addition, fasteners increase the airframe weight and can add stress concentration areas. Reducing fastener count can accelerate manufacturing and improve aircraft performance. NASA is currently investigating nondestructive evaluation (NDE) techniques to assess bond integrity. For example, bond thickness influences bond strength and therefore NDE techniques are being investigated to determine bond thickness. For bonded metal structures, there is a large difference in the thermal diffusivity between the 7075 aluminum alloy metal adherends and aircraft grade adhesive. Multi-layered thermal models show a large variation in the thermal response for bondline adhesive thicknesses that vary from 100 to 300 microns for adherend thicknesses of 0.163 cm. Experimental through-transmission thermal measurements reveal promise to quantitatively characterize the bondline thickness. Results were validated with X-ray computed tomography and optical microscopy measurements, and influence of porosity on the thermal model and measurements are investigated.

X-ray computed tomography

X-ray tomography of damage dynamics in advanced materials using a laser wakefield accelerator

Additively manufactured (AM) metals offer the potential for customizable, cost-effective components, but qualification and certification are crucial. Key to this process is understanding pore dynamics under stress, typically analyzed using micro-computed tomography. This study introduces laboratory-scale “betatron” x-rays from laser wakefield acceleration as a high-throughput alternative for x-ray tomography of advanced materials, such as AM AlSi10Mg alloys. Coupled with 3D finite element modeling, this method provides detailed insights into stress-porosity interactions. The approach delivers high-resolution scans, revealing that pore shape and local triaxiality significantly influence fracture dynamics, supporting advanced material characterization. This work also demonstrates the potential and versatility of laser-betatron x-ray μCT for generating large datasets to accelerate our understanding of the stochastic, process-specific nature of pore formation in AM alloys.

Senthilkumaran, Vigneshvar