High-Throughput Uniformity and Defect Monitoring in Low-Temperature Electrolysis Porous Transport Layers Using X-Ray Radiography

Effective quality control (QC) for manufacturing proton exchange membrane water electrolysis (PEMWE) components is critical to enabling widespread adoption of the technology for hydrogen generation. This study investigates X-ray radiography as a novel, high-throughput, potentially in-line QC technique for detecting defects and assessing material property distributions in titanium-based porous transport layers (PTLs) which constitute a crucial component of low temperature PEMWE stacks. We obtain radiographs of a set of fifteen PTLs and model their absorbance of the broadband radiation as a second-order polynomial to account for the non-monoenergetic radiation source used in this study. The resulting model serves as a basis for predicting the areal density and porosity distributions of the PTLs. We find radiography successful in detecting multiple instances of defects, including holes/depressions, cracks, and excess material on the surface or in the pores of the material, demonstrating its potential as a robust in-line QC tool for PTL manufacturing.

08 HYDROGEN

Optimizing Porous Transport Layer Porosity for Proton Exchange Membrane Water Electrolysis

An empirical model is presented that describes anode-side losses related to porous transport layer (PTL) morphology in proton exchange membrane water electrolysis (PEMWE). The model is based on an advanced voltage breakdown analysis that links various overpotentials to PTL morphology. Custom Ti PTLs, spanning uncommonly low porosities (22 - 31%), were fabricated and analyzed with X-ray CT to obtain pore and particle size distributions. Particle size distributions were consistent across samples with an average particle diameter of 12.0?..mu..m, whereas average pore diameters ranged from 6.0 to 7.0?..mu..m. The PTLs were tested in standard PEMWE cell assemblies with anode catalyst loadings of 0.1 mgIr cm-2 to obtain polarization curves, electrochemical impedance spectra, and augmented Tafel analysis. The PTL-dependent anode side losses were deconvoluted and assigned to excess utilization, concentration, ion transport resistance, and electrical contact resistance overpotentials. The data and model reveal an optimal 20 - 28% PTL porosity region where utilization and contact resistance overpotentials are minimized without triggering concentration and ion transport losses related to water deprivation. The optimal PTL porosity depends on the operating current density and is demonstrated at realistic PEMWE water flow rates to establish PTL design guidance for operation at scale.

08 HYDROGEN