Deformation behavior of nanoscale Al–Al 2 Cu eutectics studied by in situ micropillar compression

We report deformation behavior of nanoscale laser processed Al–Al 2 Cu eutectics at room temperature is characterized through in situ micro-pillar compression testing in a scanning transmission microscope. Interlamellar spacing of Al–Al 2 Cu eutectics varies from hundreds of nanometers to 20 nm. Three different sizes of micro-pillars are fabricated in order to study the deformation behaviors of single colony and multiple colonies, corresponding to the single crystal and polycrystal respectively. For single colonies, lamellar orientations parallel, normal or inclined to the loading direction were tested. The main findings are: 1) the plasticity mechanisms strongly depend on loading orientation: buckling and kinking in the parallel-loaded eutectics, planar sliding along Al–Al 2 Cu lamellar interfaces in the incline-loaded eutectics and localized shearing in the normal-loaded eutectics. 2) the incline-loaded eutectics exhibits the lowest compression flow strength, and the normal-loaded eutectics has the highest compression flow strength. 3) with decreasing inter-lamellar spacing, the strength increases and plasticity is uniformly distributed, as opposed to shear localization. Highest compressive plasticity is observed in polycrystalline eutectics with an ensemble of lamellar orientations with ~20 nm average spacing: 17.9% at flow stress of 1.63 GPa, and degenerate, bimodal morphology: 11.1% at flow stress of 1.36 GPa.

36 MATERIALS SCIENCE↗

Corrosion analysis of Al-Ce-Ni and Al-Cu-Ce cast alloys in dilute boric acid at room and elevated temperatures

Two Al-Ce-Ni cast alloys, and an Al-Cu-Ce cast alloy, as candidate wet storage materials for spent nuclear fuels, were tested in 0.23 wt% H 3 BO 3 solution to assess the alloy corrosion resistance. Electrochemical and gravimetric corrosion data suggest that the three Al alloys are unlikely to undergo any severe corrosion in dilute H 3 BO 3 at or below 50 °C. Post-exposure characterization of the three Al alloys, including scanning and transmission electron microscopy and electron dispersive spectroscopy, revealed a corrosion product layer, mostly Al 2 O 3 , on the exposed surface and local penetration of oxygen into the alloy matrix. The degree of oxide layer growth and oxygen penetration is greater at 80 °C than the temperature at/below 50 °C. The Al-Cu-Ce alloy is considered less corrosion resistant than the other two alloys studied.

Al-Ce alloy↗

Comparing polysaccharide decomposition between the type strains Gramella echinicola KMM 6050T (DSM 19838T) and Gramella portivictoriae UST040801-001T (DSM 23547T), and emended description of Gramella echinicola Nedashkovskaya et al. 2005 emend. Shahina et al. 2014 and Gramella portivictoriae Lau et al. 2005

Abstract Strains of the genus Gramella (family Flavobacteriacae , phylum Bacteroidetes ) were isolated from marine habitats such as tidal flat sediments, coastal surface seawater and sea urchins. Flavobacteriaceae have been shown to be involved in the decomposition of plant and algal polysaccharides. However, the potential to decompose polysaccharides may differ tremendously even between species of the same genus. Gramella echinicola KMM 6050 T (DSM 19838 T ) and Gramella portivictoriae UST040801-001 T (DSM 23547 T ) have genomes of similar lengths, similar numbers of protein coding genes and RNA genes. Both genomes encode for a greater number of peptidases compared to ’ G. forsetii ’. In contrast to the genome of ’ G. forsetii ’, both genomes comprised a smaller set of CAZymes. Seven polysaccharide utilization loci were identified in the genomes of DSM 19838 T and DSM 23547 T . Both Gramella strains hydrolyzed starch, galactomannan, arabinoxylan and hydroxyethyl-cellulose, but not pectin, chitosan and cellulose (Avicel). Galactan and xylan were hydrolyzed by strain DSM 19838 T , whereas strain DSM 23547 T hydrolyzed pachyman and carboxy-methyl cellulose. Conclusively, both Gramella type strains exhibit characteristic physiological, morphological and genomic differences that might be linked to their habitat. Furthermore, the identified enzymes mediating polysaccharide decomposition, are of biotechnological interest.

59 BASIC BIOLOGICAL SCIENCES↗

Compression studies on particulate composites of ternary Al-Ti-Fe, and quaternary Al-Ti-Fe-Nb and Al-Ti-Fe-Mn L1(2) compounds

Compression studies were conducted on monolithic and TiB2 particulate-reinforced composites of Al22Fe3Ti8, both with and without minor quaternary alloying additions (2 at. pct Nb and 2 at. pct Mn) as a function of temperature and as a function of strain rate at high temperature. The volume fraction of reinforcement was varied between 0 and 20 percent. The particulate reinforcements were found to be effective in increasing ambient- and warm-temperature strength; at high temperatures, the monolithic material is stronger than the composites, although the composites are superior at slow strain rates. The microstructures of the monolithic and composite specimens were examined before and after deformation to explain these observations.

Kumar, K. S.↗

Hot-Tearing Assessment of Multicomponent Nongrain-Refined Al-Cu Alloys for Permanent Mold Castings Based on Load Measurements in a Constrained Mold

The hot-tearing resistance of multicomponent Al-Cu alloys during permanent mold casting was investigated using a constrained permanent mold in which the load and temperature were measured. The nominal Cu composition was varied from 5 to 8 wt pct. Casting experiments were conducted without adding any grain-refining inoculants. The following variables, which were obtained from the measured load data during casting, were considered to assess the hot-tearing resistance of the Al-Cu multicomponent alloys: “V”-like signature in the load rate variation, load at solidus point, and load rate average over the freezing range. In addition, a hot-tearing criterion based on the variation of the fraction of solid in the late stages of solidification was used. It was found that all criteria considered can accurately predict the alloys with the lowest and highest hot-tear resistance, respectively. It was found that the rate of measured load during casting could be used to indicate substantial hot tearing. However, the load rate variation could not be used to detect when small hot tears were present. Among all the criteria considered, the load at the solidus point shows an excellent agreement with experimentally observed hot-tearing resistance for all but one alloy. The poorly resistant hot-tearing alloys exhibited mainly coarse columnar grains while the most hot-tearing resistant alloys exhibited a much more refined grain microstructure. This is the first study in which good hot-tear resistance is demonstrated for multicomponent Al-Cu alloys with nominal Cu content greater than 7 wt pct.

36 MATERIALS SCIENCE↗

Dynamic Wetting of High-Al Steel by CaO-SiO{sub 2}- and CaO-Al{sub 2}O{sub 3}-Based Mold Fluxes

Wetting of steel by mold fluxes affects the surface quality of steel products. Reaction between [Al] and mold fluxes in the continuous casting of high-Al steel leads to a dynamic interfacial phenomenon. This work investigated the wetting of the high-Al steel substrate by CaO-SiO{sub 2}-based and CaO-Al{sub 2}O{sub 3}-based mold fluxes. The interfacial tensions were estimated and related to their high-temperature structures. The interface morphology revealed that CaO-SiO{sub 2}-based mold flux and CaO-Al{sub 2}O{sub 3}-based mold flux with CaO/Al{sub 2}O{sub 3} = 1 exhibited deep reaction zones in the steel substrates and irregular flux/steel interfaces, while CaO-Al{sub 2}O{sub 3}-based mold fluxes with CaO/Al{sub 2}O{sub 3} = 2 and 3 showed smooth interfaces and superficial reaction zones. The sedation of dynamic wetting behavior in Samples 3 and 4 was related to the high viscosity in the flux droplet after the initial composition change, which led to the stabilization of the interface.

36 MATERIALS SCIENCE↗

Formation of Al{sub 15}Mn{sub 3}Si{sub 2} Phase During Solidification of a Novel Al-12%Si-4%Cu-1.2%Mn Heat-Resistant Alloy and Its Thermal Stability

The formation of Al{sub 15}Mn{sub 3}Si{sub 2} phase in Al-12Si-4Cu-1.2Mn (wt.%) alloy during solidification was investigated by adopting CALPHAD method and microstructural observation by optical microscopy, SEM–EDS, TEM–EDS/SAD and XRD analysis; SEM fixed-point observation method was applied to evaluate its thermal stability. As-cast microstructural observation consistently demonstrates the solidification sequence of the studied alloy predicted by phase diagram calculation. Based on the phase diagram calculation, SEM–EDS, TEM–EDS/SAD and XRD analysis, as well as evidences on Al-Si-Mn-Fe compounds from the literature, the primary and eutectic Mn-rich phases with different morphologies in the studied alloy are identified to be Al{sub 15}Mn{sub 3}Si{sub 2} that has a body-centered cubic (BCC) structure with a lattice constant of a = 1.352 nm. SEM fixed-point observation and XRD analysis indicate that Al{sub 15}Mn{sub 3}Si{sub 2} phase has more excellent thermal stability at high temperature than that of CuAl{sub 2} phase and can serve as the major strengthening phase in heat-resistant aluminum alloy that has to face a high-temperature working environment. Results of tension test show that addition of Mn can improve the strength of Al-Si-Cu alloy, especially at elevated temperature.

36 MATERIALS SCIENCE↗

Evaluating the Discharge Performance of Heat-Treated Al-Sb Alloys for Al-Air Batteries

In this work, the combined effects of heat treatment and Sb addition on the discharge performance of Al-Sb alloys as anode for Al-air batteries have been evaluated experimentally. The results indicate that heat treatment decreases the electrochemical and discharge activities of Al-Sb alloys. Heat-treated Al-Sb alloys at 550 °C for 3 h show an improved anode performance. The Al-0.02Sb alloy exhibits a high discharge capacity and anodic efficiency of 2758 Ah kg{sup −1} and 92.6%, respectively. Further prolonging the heat treatment time results in a decrease in anode performance. Microstructure characterization indicates that such negative effect is due to the higher-temperature and prolonged heat treatment to bring out significant grain growth and coarsening of Al-Sb precipitates. The corresponding corrosion behaviors are also discussed in detail.

36 MATERIALS SCIENCE↗

The role of the laser fluence on the Al{sub 2}O{sub 3} target in the nanostructure and morphology of VO{sub x} : Al{sub 2}O{sub 3} thin films prepared by pulsed laser deposition.

The role played by the laser fluence on the Al{sub 2}O{sub 3} target when depositing VO{sub x}:Al{sub 2}O{sub 3} nanocomposite thin films by alternate ablation from ceramic alumina (Al{sub 2}O{sub 3}) and metallic vanadium (V) targets in vacuum has been studied. The fluence and number of pulses on the V target to prepare the nanoparticles has been maintained constant, while the fluence used to grow the Al{sub 2}O{sub 3} host has been varied from 1.3 to 3.9 J cm{sup -2}. The optical properties of the films, namely in-situ reflectivity during growth and extinction coefficient, evidence that the properties of the nanoparticles change as a function of the laser fluence on the Al{sub 2}O{sub 3} host. Transmission electron microscopy analysis shows the formation of vanadium oxide nanoparticles with average diameters in the range of 4.6 nm. Structural analysis of the nanoparticles shows that they are mainly crystalline. Phases of VO{sub x} with average [O]/[V] ratios from 1.7 to 2.2 have been identified with the most commonly observed being V{sub 3}O{sub 5}. This is in agreement with low heat of formation of this oxide. It is shown that the oxidation of the nanoparticles induced during the deposition of Al{sub 2}O{sub 3} is very efficient since no metallic V nanoparticles are formed even for the lowest fluence used.

36 MATERIALS SCIENCE↗