Evaluation of alumina and silica coating materials for the NIF final turning mirrors
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Li 7 La 3 Zr 2 O 12 (LLZO) garnet-type lithium-ion conductors are being investigated as a promising solid electrolyte for solid-state lithium batteries. To enable a functional all-solid-state configuration intensive investigations are needed to reduce the cathode/electrolyte interfacial resistance which contributes the most to cell performance loss. Among the commercial cathode materials investigated so far, LiCoO 2 (LCO) is one of the most stable with garnet electrolytes as only a superficial reaction has been detected between the two materials. However, even this minor reaction would block the Li-ion transport through the interface, resulting in deteriorated cell performance. In this work, we demonstrate that a thin aluminum oxide layer (5 nm) can be an effective interlayer to impede the formation of a harmful interphase and enable facile Li-ion transfer between LCO and the LLZO garnet. Room-temperature-sputtered LCO thin films were employed to form an interface with the garnet electrolyte and annealed at 800 °C to reveal the effect of the interfacial reaction on the Li-ion transfer across the interface. An aluminum oxide layer was then introduced between LCO and the garnet electrolyte by sputtering a metallic aluminum layer which is then annealed together with the upper LCO layer in oxygen, or by direct atomic layer deposition of the oxide. Compared to the LCO/LLZO/Li cells without an aluminum oxide interlayer, those with the interlayer exhibited improved performance, i.e., a stable discharge capacity of up to 90 mAh/(g LCO) at a C/10 rate, a rate capability up to 1.68C and a stable galvanostatic cycling at 0.1C for over 100 cycles with a discharge capacity fade rate of 0.15% per cycle. It was determined that aluminum diffused into the LCO layer after preventing the initial detrimental reaction between LCO and the LLZO garnet from happening during high temperature annealing, suggesting that the coating does not have to remain a physically blocking layer during cycling to function.
The surfaces of most metals immersed in aqueous electrolytes have a several-nanometer-thick oxide/hydroxide surface layer. This gives rise to the existence of both metal|oxide and oxide|liquid electrotlyte interfaces, and makes it challenging to correlate atomic length-scale structures with electrochemical properties such the potential-of-zero-charge (PZC). The PZC has been shown to be correlated the onset potential for pitting corrosion. Here, we conduct large-scale Density Functional Theory and ab initio molecular dynamics to calculate the PZC of a Al(111)| γ -Al 2 O 3 (110)| water double-interface model within the context of aluminum corrosion. By partitioning the multiple interfaces involved into binary components with additive contributions to the overall work function and voltage, we predict the PZC to be -1.53 V vs SHE for this model. Furthermore, we calculate the orbital energy levels of defects like oxygen vacancies in the oxide, which are critical parameters in theories associated with pitting corrosion. We predict that the Fermi level at the PZC lies above the impurity defect levels of the oxygen vacancies, which are therefore uncharged at the PZC. From the PZC estimate, we predict the voltage needed to create oxygen vacancies with net positive charges within a flatband approximation.
Explore the source record for details and available documents.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Abstract not provided.
TMS 2022, Virtual, February 27–March 3, 2022
An austenitic Ni-base alloy, consisting essentially of, in weight percent: 2.5 to 4.75 Al; 21 to 26 Cr; 20 to 40 Fe; 0.75 to 2.5 total of at least one element elected from the group consisting of Nb and Ta; 0 to 0.25 Ti; 0.09 to 1.5 Si; 0 to 0.5 V; 0 to 2 Mn; 0 to 3 Cu; 0 to 2 of at least one element selected from the group consisting of Mo and W; 0 to 1 of at least one element selected from the group consisting of Zr and Hf; 0 to 0.15 Y; 0.3 to 0.55 C; 0.005 to 0.1 B; 0 to 0.05 P; less than 0.06 N and balance Ni (30 to 46 Ni), wherein the weight percent Ni is greater than the weight percent Fe, and wherein the ratio Ni/(Fe+2*C) is between 1.02 and 1.067.