Effect of electrode manufacturing defects on electrochemical performance of lithium-ion batteries: Cognizance of the battery failure sources

During LIB electrode manufacturing, it is difficult to avoid the certain defects that diminish LIB performance and shorten the life span of the batteries. This study provides a systematic investigation correlating the different plausible defects (agglomeration/blisters, pinholes/divots, metal particle contamination, and non-uniform coating) in a LiNi 0.5 Mn 0.3 Co 0.2 O 2 positive electrode with its electrochemical performance. Additionally, an infrared thermography technique was demonstrated as a nondestructive tool to detect these defects. The findings show that cathode agglomerates aggravated cycle efficiency, and resulted in faster capacity fading at high current density. Electrode pinholes showed substantially lower discharge capacities at higher current densities than baseline NMC 532 electrodes. Metal particle contaminants have an extremely negative effect on performance, at higher C-rates. The electrodes with more coated and uncoated interfaces (non-uniform coatings) showed poor cycle life compared with electrodes with fewer coated and uncoated interfaces. Further, microstructural investigation provided evidence of presence of carbon-rich region in the agglomerated region and uneven electrode coating thickness in the coated and uncoated interfacial regions that may lead to the inferior electrochemical performance. In conclusion, this study provides the importance of monitoring and early detection of the electrode defects during LIB manufacturing processes to minimize the cell rejection rate after fabrication and testing.

25 ENERGY STORAGE↗

Detrimental Effects of Chemical Crossover from the Lithium Anode to Cathode in Rechargeable Lithium Metal Batteries

The interfacial stability is one of the crucial factors affecting long-term cyclability of lithium (Li) metal batteries (LMBs). While cross contamination (such as Mn+2 crossover from cathode to contaminate graphite anode) phenomena has been well studied in Li ion batteries (LIBs), the similar phenomena has rarely been studied in LMBs. Here, we systematically investigated the cathode failure triggered by the chemical crossover between the electrode pair in rechargeable LMBs. In strong contrast to LIBs, the cathode in LMBs suffers more significant and irreversible capacity fade during cycling and its capacity cannot be fully recovered even when Li metal anode has been replaced in the successive cycling. In-depth characterizations of the cathode surface reveal severe CEI deterioration related to the accumulation of highly resistive polymeric components and lithium fluoride. The soluble decomposition products generated by extensive salt-anion decomposition at Li metal surface can diffuse toward cathode side and result in severe deterioration of cathode as well asseparator surfaces. A polydopamine coated separator with selective Li-ion permeability has been developed to mitigate the detrimental chemical crossover and enhance the cathode stability.

Lee, Hongkyung↗

Delineating the impact of Ti/Mg substitution in P2-type Na 2/3 Ni 1/3 Mn 2/3 O 2 with an advanced electrolyte for sodium-ion batteries

Sodium layered oxide cathodes are drawing interest globally as a potential alternative to lithium layered oxides, but they suffer from egregious capacity fade and have intrinsically lower capacity. P2-type Na 2/3 Ni 1/3 Mn 2/3 O 2 is a particularly relevant cathode material as it demonstrates an energy density of up to 550 W h kg −1 at high operating potentials, although this can only be maintained for a handful of cycles with industrial electrolytes. Here, a localized saturated electrolyte (LSE) is shown to significantly improve the cycle life of Na 2/3 Ni 1/3 Mn 2/3 O 2 by suppressing the surface reactivity, despite large volume changes during cycling. The demonstrated influence of surface stability on cycle life in this work challenges the prevailing notion of a popular capacity stabilization strategy with titanium/magnesium co-doping, which is primarily thought to improve cycle life via improved structural stability. Single crystals of Na 2/3 Ni 1/3−x Mg x Mn 2/3−2x Ti 2x O 2 (x = 0, 1/48, 1/24, 1/12) materials are cycled with a traditional electrolyte and the LSE to demonstrate that despite eliminating the phase transition with dopants in Na 2/3 Ni 1/4 Mg 1/12 Mn 1/2 Ti 1/6 O 2 , the predominant role of the dopants is in reducing the parasitic oxygen reactivity at the cathode surface. The different roles these dopants play are systematically disambiguated, and this work can guide future research to focus on reducing the parasitic cathode/electrolyte reactivity further.

25 ENERGY STORAGE↗

Silicon Based Anodes for Li-Ion Batteries

Silicon is environmentally benign and ubiquitous. Because of its high specific capacity, it is considered one of the most promising candidates to replace the conventional graphite negative electrode used in today's Li ion batteries. Silicon has a theoretical specific capacity of nearly 4200 mAh/g (Li21Si5), which is 10 times larger than the specific capacity of graphite (LiC6, 372 mAh/g). However, the high capacity of silicon is associated with huge volume changes (more than 300 percent) when alloyed with lithium, which can cause severe cracking and pulverization of the electrode and lead to significant capacity loss. Significant scientific research has been conducted to circumvent the deterioration of silicon based anode materials during cycling. Various strategies, such as reduction of particle size, generation of active/inactive composites, fabrication of silicon based thin films, use of alternative binders, and the synthesis of 1-D silicon nanostructures have been implemented by a number of research groups. Fundamental mechanistic research has also been performed to better understand the electrochemical lithiation and delithiation process during cycling in terms of crystal structure, phase transitions, morphological changes, and reaction kinetics. Although efforts to date have not attained a commercially viable Si anode, further development is expected to produce anodes with three to five times the capacity of graphite. In this chapter, an overview of research on silicon based anodes used for lithium-ion battery applications will be presented. The overview covers electrochemical alloying of the silicon with lithium, mechanisms responsible for capacity fade, and methodologies adapted to overcome capacity degradation observed during cycling. The recent development of silicon nanowires and nanoparticles with significantly improved electrochemical performance will also be discussed relative to the mechanistic understanding. Finally, future directions on the development of silicon based anodes will be considered.

25 ENERGY STORAGE↗

Beneficial Effects of La 0.5 Sr 0.5 CoO 3 Coatings on Thin‐Film LiMn 2 O 4 Cathodes for Lithium Ion Batteries

Abstract The severe capacity loss of spinel LiMn 2 O 4 (LMO) limits the utility of this otherwise promising lithium ion battery cathode material. One of the strategies to mitigate capacity fade is applying a coating on LMO particle surfaces. While this approach yields promising results, there is limited understanding of mechanisms whereby coatings improve LMO capacity retention. Herein, the effects of a new protective coating material, La 0.5 Sr 0.5 CoO 3 (LSCO), in a thin‐film battery geometry that is amenable to fundamental studies of electrode processes, are reported. RF sputtering deposition is used to produce high quality 25–100 nm LMO cathodes on Al 2 O 3 substrates with an intervening Pt/Ti back‐side contact layer. Cycling of the un‐coated cathodes results in capacity loss of 18% over 300 cycles. Adding a 2 nm LSCO layer reduces the capacity loss to 3%. While this may be due in part to reduced Mn dissolution, scanning transmission electron microscopy results indicate that the coating helps to preserve crystallinity and reduce lattice structure distortion due to inhibited formation of defect tetragonal spinel. Three‐electrode electrochemical impedance spectroscopy results reveal that the LSCO coating increases charge transfer and ohmic resistances, but the increases are generally too small to significantly impact cell performance even at high C‐rates.

25 ENERGY STORAGE↗

Performance degradation due to anodic failure mechanisms in lithium-ion batteries

Here, we report a mechano-chemical model for anodic degradation during fast-charging of nickel-manganese-cobalt (NMC)/graphite (C) cell due to SEI growth, lithium plating/stripping, dead lithium storage, and film fracture of composite SEI and plated lithium film. Degradation of the battery is analyzed for a range of charging rates from 1 to 6 C-rates, and the influence of plating mechanisms – lithium plating and dead lithium deposition and recovery during stripping – on the film resistance of the anode are accounted for in the model. Dynamic evolution of the interfacial properties is modeled using rule-of-mixture approach. Model predictions of plating associated stress fields are used to compute critical energy release rate for film cracking. The results indicate an increased tendency of fracture for thinner SEI film with lithium plating at higher charging rates. The process of reforming the cracked film absorbs a significant portion of the electrode current thereby reducing the cell capacity and plating efficiency. The mechano-chemical model provides an extensive analytical framework for understanding the synergistic coupling of anodic degradation mechanisms, prognosticating conditions of SEI failure, and evaluating the capacity fade and efficiency of lithium-ion battery.

25 ENERGY STORAGE↗

Life Prediction of Large Lithium-Ion Battery Packs with Active and Passive Balancing

Lithium-ion battery packs take a major part of large-scale stationary energy storage systems. One challenge in reducing battery pack cost is to reduce pack size without compromising pack service performance and lifespan. Prognostic life model can be a powerful tool to handle the state of health (SOH) estimate and enable active life balancing strategy to reduce cell imbalance and extend pack life. This work proposed a life model using both empirical and physical-based approaches. The life model described the compounding effect of different degradations on the entire cell with an empirical model. Then its lower-level submodels considered the complex physical links between testing statistics (state of charge level, C-rate level, duty cycles, etc.) and the degradation reaction rates with respect to specific aging mechanisms. The hybrid approach made the life model generic, robust and stable regardless of battery chemistry and application usage. The model was validated with a custom pack with both passive and active balancing systems implemented, which created four different aging paths in the pack. The life model successfully captured the aging trajectories of all four paths. The life model prediction errors on capacity fade and resistance growth were within +/-3% and +/-5% of the experiment measurements.

25 ENERGY STORAGE↗

Dense Graphene Monolith for High Volumetric Energy Density Li-S Batteries

Despite the outstanding gravimetric performance of lithium-sulfur (Li-S) batteries, their practical volumetric energy density is normally lower than that of lithium-ion batteries, mainly due to the low density of nanostructured sulfur as well as the porous carbon hosts. Here, a novel approach is developed to fabricate high-density graphene bulk materials with ink-bottle-like mesopores by phosphoric acid (H 3 PO 4 ) activation. These pores can effectively confine the polysulfides due to their unique structure with a wide body and narrow neck, which shows only a 0.05% capacity fade per cycle for 500 cycles (75% capacity retention) for accommodating polysulfides. With a density of 1.16 g cm -3 , a hybrid cathode containing 54 wt% sulfur delivers a high volumetric capacity of 653 mA h cm -3 . As a result, a device-level volumetric energy density as high as 408 W h L -1 is achieved with a cathode thickness of 100 mu m. This is a periodic yet practical advance to improve the volumetric performance of Li-S batteries from a device perspective. Furthermore, this work suggests a design principle for the real use Li-S batteries although there is a long way ahead to bridge the gap between Li-S batteries and Li-ion batteries in volumetric performance.

25 ENERGY STORAGE↗

Lithium plating induced degradation during fast charging of batteries subjected to compressive loading

Here we report the lithium plating associated capacity loss during fast charging of compressively loaded lithium-ion batteries (LIBs). The charging and discharging of LIB under compressive loading during service may affect the cell performance or initiate localized defects in the electrodes. Pouch cells of capacity 20 mAh were compressively loaded to nominal pressures of 0–440 kPa and subjected to 10 cycles of fast charging at 1 C and 4 C. Experimental results show that cells charged at 4 C-rate experienced significant capacity fade, and applying compressive loads exacerbated the capacity loss. The coulombic efficiency study shows that active lithium loss was higher for the initial cycles before gradually reducing to a minimal capacity loss for the tenth charging cycle. The cell voltage relaxation immediately after charging was monitored to identify the stripping of plated lithium after fast charging cycles and showed that the duration of lithium stripping was higher for cells under mechanical compressive loading. Scanning electron microscopy (SEM) and electron paramagnetic resonance spectroscopy (EPR) characterization of the anode showed significantly higher lithium deposits on the anodes charged at a 4 C rate under compressive loads. These results indicate that applied mechanical compression causes increased lithium plating during fast charging of batteries.

25 ENERGY STORAGE↗

Inward Lithium-Ion Breathing of Hierarchically Porous Silicon Anodes

Silicon has been identified as one of the most promising candidates as anode for high performance lithium-ion batteries. The key challenge for Si anodes is the large volume change induced chemomechanical fracture and subsequent rapid capacity fading upon cyclic charge and discharge. Improving capacity retention thus critically relies on smart accommodation of the volume changes through nanoscale structural design. In this work, we report a novel fabrication method for hierarchically porous Si nanospheres (hp-SiNSs), which consist of a porous shell and a hollow core. Upon charge/discharge cycling, the hp-SiNSs accommodate the volume change through reversible inward expansion/contraction with negligible particle-level outward expansion. Our mechanics analysis revealed that such a unique volume-change accommodation mechanism is enabled by the much stiffer modulus of the lithiated layer than the unlithiated porous layer and the low flow stress of the porous structure. Such inward expansion shields the hp-SiNSs from fracture, opposite to the outward expansion in solid Si during lithiation. Lithium ion battery assembled with this new nanoporous material exhibits high capacity, high power, long cycle life and high coulombic efficiency, which is superior to the current commercial Si-based anode materials. We find the low cost synthesis approach reported here provides a new avenue for the rational design of hierarchically porous structures with unique materials properties.

25 ENERGY STORAGE↗

Concealed Cathode Degradation in Lithium-Ion Cells with a Ni-Rich Oxide

Difficulties with sourcing cobalt and the interest in increasing cell energy have motivated the development of Ni-rich oxide materials for lithium-ion battery cathodes. Despite the intense research on the topic, there is limited information available on the long-term performance of novel cathode formulations. Here, we evaluate the stability of LiNi 0.9 Mn 0.05 Co 0.05 O 2 in full-cells tested for over five months, assessing how cycling, voltage and electrolyte additives impact cathode aging. We use differential voltage analysis to extract insights about the cathode from the full-cell data and identify the isolation of cathode particles in the delithiated (charged) state as a relevant mode of aging. Importantly, this particular mechanism of cathode aging does not cause immediate cell capacity fade, causing the simple analysis of cell capacity retention to overestimate the cathode stability under the investigated conditions. So, our observations serve as cautionary tale indicating that careful analysis of data from extended testing may be required for assessing the performance of Ni-rich cathodes and for evaluating how these materials are affected by electrolyte additives.

25 ENERGY STORAGE↗

Selecting the Best Graphite for Long-Life, High-Energy Li-Ion Batteries

Here, most lithium-ion batteries still rely on intercalation-type graphite materials for anodes, so it is important to consider their role in full cells for applications in electric vehicles. Here, we systematically evaluate the chemical and physical properties of six commercially-available natural and synthetic graphites to establish which factors have the greatest impact on the cycling stability of full cells with nickel-rich LiNi0.8Mn0.1Co0.1O2 (NMC811) cathodes. Electrochemical data and post-mortem characterization explain the origin of capacity fade. The NMC811 cathode shows large irreversible capacity loss and impedance growth, accounting for much of full cell degradation. However, six graphite anodes demonstrate significant differences with respect to structural change, surface area, impedance growth, and SEI chemistry, which impact overall capacity retention. We found long cycle life correlated most strongly with stable graphite crystallite size. In addition, graphites with lower surface area generally had higher coulombic efficiencies during formation cycles, which led to more stable long-term cycling. The best graphite screened here enables a capacity retention around 90% in full pouch cells over extensive long-term cycling compared to only 82% for cells with the lowest performing graphite. The results show that optimal graphite selection improves cycling stability of high energy lithium-ion cells.

25 ENERGY STORAGE↗

Communication—Ligand-Dependent Electrochemical Activity for Mn 2+ in Lithium-Ion Electrolyte Solutions

Manganese dissolution from metal-oxide cathodes, and subsequent deposition at graphitic anodes, are considered to be key causes of capacity fade in lithium-ion batteries. The Mn2+ redox state is thought to be the major solvated Mn species, but its coordination environment is not well understood. Herein, we present the effects of Mn2+-containing electrolytes (Mn(PF6)(2) and Mn(TFSI)(2)) on the performance of lithium-iron-phosphate//graphite (LFP//Gr) cells. Clear differences in first-cycle capacities and subsequent cycling efficiencies depending on the associated counter-ion indicate that the Mn coordination environment has a profound effect on the associated electrochemical degradation mechanisms.

25 ENERGY STORAGE↗

Ultrafast charging of energy-dense lithium-ion batteries for urban air mobility

Urban air mobility (UAM) demands batteries with high energy density, long cycle life, and fast rechargeability. In this paper, we demonstrate an energy-dense lithium-ion battery (LiB) with ultralong cycle life under ultrafast charging. By using the asymmetric temperature modulation (ATM) method, i.e., charging at an elevated temperature and discharging around the ambient temperature, it is experimentally shown that the 209 Wh/kg LiB is charged to 88% state of charge (SOC) in ~5 min under UAM cycling while retaining 97.7% capacity after 1,000 cycles. Moreover, an experimentally validated electrochemical-thermal (ECT) model is developed to elucidate the fast charging process and the degradation mode of UAM batteries, quantitatively capturing lithium plating during fast charging. We find that the LiBs for UAM applications are most prone to lithium plating due to their higher initial SOC required as the reserve for safety; nevertheless, the ATM method is effective in minimizing or preventing lithium plating in the high SOC range of 30-90%. In addition to slowing down capacity fade, the ATM method also raises the usable capacity by 10%, which boosts the battery energy density and ensures the battery to perform full UAM cycles even at the end of life.

25 ENERGY STORAGE↗

High capacity and good cycling stability of multi-walled carbon nanotube/SnO{sub 2} core-shell structures as anode materials of lithium-ion batteries

The multi-walled carbon nanotube/SnO{sub 2} core-shell structures were fabricated by a wet chemical route. The electrochemical performance of the core-shell structures as anode materials of lithium-ion batteries was investigated. The initial discharge capacity and reversible capacity are up to 1472.7 and 1020.5 mAh g{sup -1}, respectively. Moreover, the reversible capacity still remains above 720 mAh g{sup -1} over 35 cycles, and the capacity fading is only 0.8% per cycle. Such high capacities and good cyclability are attributed to SnO{sub 2} network structures, excellent mechanical property and good electrical conductivity of the multi-walled carbon nanotubes.

36 MATERIALS SCIENCE↗

Approaching the capacity limit of lithium cobalt oxide in lithium ion batteries via lanthanum and aluminium doping

Here, lithium cobalt oxides (LiCoO 2 ) possess a high theoretical specific capacity of 274 mAh/g. However, cycling LiCoO 2 -based batteries to voltages greater than 4.35 V vs. Li/Li + causes significant structural instability and severe capacity fade. Consequently, commercial LiCoO 2 exhibits a maximum capacity of only ~165 mAh/g. Here we develop a doping technique to tackle this long-standing issue of instability and thus increase the capacity of LiCoO 2 . La and Al are concurrently doped into Co-containing precursors, followed by high-temperature calcination with lithium carbonate. The dopants are found to reside in the crystal lattice of LiCoO 2 , where La works as a pillar to increase the c-axis distance and Al as a positively charged center, facilitating Li + diffusion, stabilizing the structure and suppressing the phase transition during cycling, even at a high cut-off voltage of 4.5 V. This doped LiCoO 2 displays an exceptionally high capacity of 190 mAh/g, cyclability with 96% capacity retention over 50 cycles and significantly enhanced rate capability.

25 ENERGY STORAGE↗

The Chemistry of Electrolyte Reduction on Silicon Electrodes Revealed by in Situ ATR-FTIR Spectroscopy

While silicon is the most promising next-generation anode material for lithium-ion batteries (LIBs), silicon electrodes exhibit significant capacity fade with cycling. A common hypothesis is that the capacity loss is due to the solid electrolyte interphase (SEI) forming in the first cycle and becoming destabilized by large cyclic volume changes. A cell for in situ attenuated total reflection-Fourier transform infrared spectroscopy with controllable penetration depth was used to study the chemistry at the electrode–electrolyte interface. The SEI product precursors at the interface were successfully identified and differentiated from free or solvated solvent molecules in the bulk electrolyte. Intriguingly, for the most common electrolyte consisting of ethylene carbonate and diethyl carbonate, ethylene carbonate was found to directly reduce to lithium ethylene dicarbonate on the lithiated silicon surface and diethyl carbonate to selectively reduce to diethyl 2,5-dioxahexane dicarboxylate on the surface of the native silicon-oxide film. In conclusion, understanding this surface dependence of the SEI composition is critical to tuning the silicon electrode surface condition and, ultimately, enhancing the performance of future LIBs.

25 ENERGY STORAGE↗