At least 181 records · Page 10

Field Validation of Electrochemical Water Filtration System on Open Loop Cooling Towers at Automotive Plants

Open loop cooling towers play a pivotal role in rejecting heat for chilled water systems serving industrial processes, heating, ventilation, and air conditioning loads. Exposure to outside conditions can present certain operating challenges to system performance including scaling, corrosion, and biological growth. These issues are mitigated through the use of effective cooling tower water filtration and treatment systems to reduce contaminants—along with other total suspended solids (TSS) and total dissolved solids (TDS)—in the system. The U.S. Department of Energy’s Industrial Efficiency and Decarbonization Office is interested in an electrochemical-based filtration system with the ability to remove TSS particulate down to 1 micron. The removal of finer particulates reduces the need for blowdown and, in turn, makeup water use and chemical treatment in the cooling tower. Additionally, the removal process can reduce fouling at the condensers, resulting in better heat exchange and energy savings. Two Industrial Technology Validation program projects validated the electrochemical water filtration system at the Toyota Motor Manufacturing, Mississippi plant in Blue Springs, Mississippi, and the Nissan Canton Vehicle Assembly Plant in Canton, Mississippi. Researchers found that installation of both systems resulted in water and chemical treatment savings with minimal impact on energy use.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Nanostructured Black Nickel Coating as Replacement for Black Cr(VI) Finish

This work compares different electrodeposition procedures to produce nickel black coatings as greener and less toxic alternatives to Cr(VI)-based coatings used in different applications. Nickel and nickel-plated brass served as substrates in studies with a Hull cell and polarization curves. After a set of comparative experiments, the best electrodeposition procedure was further studied and optimized. Optimal conditions were found with a bath consisting of 75 g/L NiCl2·6H2O + 30 g/L NaCl and a current density of 0.143 A dm−2 applied for 5 min at room temperature. Furthermore, a pre-treatment with 18.5 vol.% of hydrochloric acid in water was found to be necessary to warrant good coating adhesion to the substrate. The black color is attributed to the development of a nanostructured surface that absorbs the incident light. Corrosion testing was performed in 0.5 M NaCl aqueous solution using electrochemical impedance spectroscopy (EIS) and polarization tests.

Mennucci, Marina M. (ORCID:0000000171886804)↗

Boron/aluminum for space applications

Several experimental boron/aluminum structures have been built for aircraft and space vehicle applications. The success of these structures has led to the decision to use boron/aluminum tubular struts on the mid-fuselage section of the Space Shuttle Orbiter. The suitability of boron/aluminum for this application has been demonstrated in a program that involved fabricating 100 tubes and performing static, fatigue, corrosion, thermal/mechanical fatigue, and damage tolerance tests on them. Other potential applications for boron/aluminum on the Space Shuttle include the wing carry-through panels and side panels for the mid-fuselage, and the landing gear struts. These applications result in significant weight savings over conventional non-composite designs at moderate costs. Boron/aluminum can now be considered a production material that, in many cases, is competitive on a weight and/or cost basis with an all-metal or resin composite system.

Robertson, A. R.↗

Aircraft surface coatings

Liquid, spray on elastomeric polyurethanes are selected and investigated as best candidates for aircraft external protective coatings. Flight tests are conducted to measure drag effects of these coatings compared to paints and a bare metal surface. The durability of two elastometric polyurethanes are assessed in airline flight service evaluations. Laboratory tests are performed to determine corrosion protection properties, compatibility with aircraft thermal anti-icing systems, the effect of coating thickness on erosion durability, and the erosion characteristics of composite leading edges-bare and coated. A cost and benefits assessment is made to determine the economic value of various coating configurations to the airlines.

Source record↗

Pump, and earth-testable spacecraft capillary heat transport loop using augmentation pump and check valves

A spacecraft includes heat-generating payload equipment, and a heat transport system with a cold plate thermally coupled to the equipment and a capillary-wick evaporator, for evaporating coolant liquid to cool the equipment. The coolant vapor is coupled to a condenser and in a loop back to the evaporator. A heated coolant reservoir is coupled to the loop for pressure control. If the wick is not wetted, heat transfer will not begin or continue. A pair of check valves are coupled in the loop, and the heater is cycled for augmentation pumping of coolant to and from the reservoir. This augmentation pumping, in conjunction with the check valves, wets the wick. The wick liquid storage capacity allows the augmentation pump to provide continuous pulsed liquid flow to assure continuous vapor transport and a continuously operating heat transport system. The check valves are of the ball type to assure maximum reliability. However, any type of check valve can be used, including designs which are preloaded in the closed position. The check valve may use any ball or poppet material which resists corrosion. For optimum performance during testing on Earth, the ball or poppet would have neutral buoyancy or be configured in a closed position when the heat transport system is not operating. The ball may be porous to allow passage of coolant vapor.

Baker, David↗

NASA Engineering and Safety Center Technical Bulletin No. 24-01: Material Compatibility of Common Aerospace Metals in MMH/MON-3

The NESC evaluated material compatibility of some common aerospace metals in monomethylhydrazine (MMH) and nitrogen tetroxide (MON-3). Previous work had identified a lack of quantitative compatibility data for nickel alloy 718, 300 series stainless steel, and titanium Ti-6Al-4V in MMH and MON-3 to support the use of zero-failure-tolerant, thin-walled pressure barriers in these propellants. Static (i.e., not flowing) general corrosion and electrochemistry testing was conducted, evaluating varied processing forms and heat treatment of the metals, water content of propellant, and exposure duration. Corrosion-rate data for all tested product forms, fluids, and durations were on the order of 1 x 10 –6 inch per year rather than the previously documented “less than 1 x 10 –3 inch per year”. The majority of the corrosion products were seen in the first 20 days of exposure, with an overall corrosion rate decreasing with time due to the increased divisor (time). It is therefore recommended that corrosion testing be performed at multiple short-term durations to inform the need for longer-duration testing.

Heather K Hickman↗

Corrosion Behavior of Developmental Iron Phosphate Waste Forms: FY20 Status Report

Corrosion tests were performed to assess the dissolution behaviors of developmental iron phosphate materials that are being evaluated as an alternative to the glass-bonded sodalite ceramic waste form to immobilize salt wastes from electrochemical separation operations. Production of the iron phosphate waste form results in dehalogenation of the waste salt that increases potential waste loading. Ferric oxide is added to the waste form to increase the chemical durability. Tests conducted to optimize the amount of ferric oxide used to make the waste form are summarized in this report. Specimens prepared from materials made with between 17 and 34 mole % ferric oxide were subjected to two test methods to assess the effects of the iron content on the relative durability and retention of immobilized salt cations including cesium, strontium, and neodymium. Modified ASTM C1308 test results show the intrinsic durability was significantly higher for materials made with 27 mol % ferric oxide. Further additions generated iron-rich inclusion phases and did not improve durability. Modified ASTM C1285 test results show that solution feedback attenuates the dissolution rate similar to what is observed for borosilicate glasses within seven days. Analyses of test specimens after 42 days show no evidence that surface layers formed. Combined with previous studies addressing the salt loading, a composition region of the ammonium (di)hydrogen phosphate-waste salt-ferric oxide ternary has been defined for durable waste form compositions. Materials with that composition can be used to determine optimal processing conditions, assess long-term performance, and parameterize a degradation model.

Stariha, S. A.↗

Environmental Degradation in Advanced Reactor Environments

The Advanced Materials and Manufacturing Technologies (AMMT) program operating under the Department of Energy Office of Nuclear Energy is accelerating the qualification and deployment of additively manufactured materials in advanced reactor environments. Laser powder bed fusion (LPBF) has emerged as a promising additive manufacturing technique to fabricate complex components with the potential of tailored material properties. In the nuclear industry, metal additive manufacturing can offer numerous advantages, such as reduced lead times, streamlined quality assurance, and cost-effective low-volume production of new and replacement components with conventional or novel materials and geometries. The rapid and effective qualification of the effect of processing variability on the performance and degradation of additively manufactured materials is essential for the deployment of these components into advanced reactor environments. This talk presents an overview of the Environmental Effects area activities within AMMT. AMMT is performing irradiation and corrosion testing of several materials built by LPBF, including 316L and 316H stainless steels. Our irradiation efforts encompass neutron irradiation testing and ion irradiation testing to provide a robust technical basis for understanding the effect of process variability on materials degradation. We develop focused irradiation test plans that align well with risk-informed and technologically inclusive approaches to licensing. We will also discuss our plans and specific concerns for corrosion testing additively manufactured material, with a primary focus on molten salt and liquid sodium environments.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Physics-informed machine learning assisted uncertainty quantification for the corrosion of dissimilar material joints

Jointing techniques like the Self-Piercing Riveting (SPR), Resistance Spot Welding (RSW) and Rivet-Weld (RW) joints are used for mass production of dissimilar material joints due to their high performance, short cycle time, and adaptability. However, the service life and safety usage of these joints can be largely impacted by the galvanic corrosion due to the difference in equilibrium potentials between the metals with the presence of electrolyte. Here, in this paper, we focus on Al-Fe galvanic corrosion and develop physics-informed machine learning based surrogate model for statistical corrosion analysis, which enables the reliability analysis of dissimilar material joints under corrosion environment. In this study, a physics-based finite element (FE) corrosion model has been developed to simulate the galvanic corrosion between a Fe cathode and an Al anode. Geometric and environmental factors including crevice gap, roughness of anode, conductivity, and the temperature of the electrolyte are investigated. Further, a thorough Uncertainty Quantification (UQ) analysis is conducted for the overall corrosion behavior of the Fe-Al joints. It is found that the electrolyte conductivity has the largest effects on the material loss and needs to be managed closely for better corrosion control. This will help in designing and manufacturing joints with improved corrosion performance.

42 ENGINEERING↗

The effect of NaCl/g/ on the Na2SO4-induced hot corrosion of NiAl

Studies have been performed to examine the effect of NaCl vapor on the Na2SO4-induced hot corrosion of the alumina former NiAl. In the incubation period associated with such hot corrosion, NaCl(g) has been shown to be effective in removing aluminum from below the protective alumina scale and redepositing it as Al2O3 whiskers on the surface of the Na2SO4-coated sample. Similar effects seen in simple oxidation are associated with isothermal rupturing of the protective alumina scale.

Smeggil, J. G.↗

Test program to demonstrate the stability of hydrazine in propellant tanks

The suitability of stainless steels and Inconel for long-term hydrazine propellant-storage tanks is investigated. Rectangular coupon samples cut from propellent tanks were sealed with a measured amount of hydrazine in glass capsules, stored at 43 or 60 C, and removed after 6 to 24 months, when corrosion of the coupon and decomposition of the hydrazine was determined, and SEM and electron spectroscopy were performed on some coupons. Corrosion was found to be unmeasurably low for all the coupons, and hydrazine decomposition produced less than 1.0 cu cm of gas per sq cm of wetted surface per year, except in those few cases when catalysis or contamination were detected. Especially good stability was observed for type 304L stainless steel. The decomposition rates determined in the coupon tests are confirmed by preliminary results of actual tank storage trials.

Moran, C. M.↗

Molecular dynamics of the early stages of high-temperature corrosion

In this work, we performed molecular dynamics simulations of the high-temperature oxidation of metal alloys composed of Al, Cr, and Fe and compared their behavior with that of pure Fe. The metal alloy elements (Al and Cr) segregated to the surface during oxidation, producing a lower stress gradient at the metal/environment interface compared to pure Fe. We have found that the lowered stress gradients produced in the alloy material appear to play a key role in the development of corrosion. Interfaces with lower stress gradients have reduced rates of H 2 O adsorption, especially for the ferritic (bcc) alloys. The diffusivity of oxygen and hydrogen drops more rapidly for the interfaces with reduced stress gradients. The stress gradient is also diminished when the gas pressure is increased, indicating that the Fe-Cr-Al alloy system is more resistant to oxidation than pure Fe at higher pressures. Therefore, we conclude that the lower stress gradients at the alloy/environment interface reduce the stress concentration and can slow down the rate of the initial oxide scale growth. We also compared bcc and fcc alloys with pure Fe based on our three evaluation criteria (peak stress, stress gradient, and summation of stress in the oxide scale). We found that the alloys have lower values under the three criteria compared to pure Fe. The bcc alloy has the best score under a water rich environment and the fcc alloy is proven to be better for peak stress and summation of stress in the oxide scale under an oxygen rich environment. For surface segregation to occur, we find that a minimum content of Al or Cr in the near-surface region must be achieved. We also learned that the role of Al is more important than that of Cr in terms of corrosion resistant behavior at relatively higher temperatures for the Fe-Cr-Al ternary alloys.

36 MATERIALS SCIENCE↗

Grooved electrodes for high-power-density fuel cells

Proton exchange membrane fuel cells (PEMFCs) are leading candidates to decarbonize the transport sector, but widespread deployment will require improvements in lifetime, fuel economy and cost. Here we present the grooved electrode, an alternative electrode structure that enhances PEMFC performance and durability by coupling high ionomer (ion-conducting binder) content for improved H + transport with grooves for rapid O 2 transport. Grooved electrodes provide up to 50% higher performance than state-of-the-art conventional electrodes under standard operating conditions. Fuel cell diagnostics combined with multiphysics modelling demonstrate that grooved electrodes provide facile O 2 transport despite their high ionomer content, enabling improved reaction rate uniformity. Grooved electrodes also provide improved durability, with less performance loss after carbon corrosion compared with baseline electrodes. Machine learning analysis demonstrates the potential to further optimize grooved structures for next-generation PEMFCs with enhanced performance and durability, enabling smaller and cheaper fuel cell stacks with higher fuel efficiency.

25 ENERGY STORAGE↗

A Multi-Scale Computational Platform for Predictive Modeling of Corrosion in Al-Steel Joints (Final Report)

The research team proposed to develop innovative multi-scale models to predict corrosion and the resulting mechanical performances in aluminum-steel joints. The methods of joining considered are resistance spot welding, self-piercing riveting, and rivet-welding, all suitable for mass production applications. The multi-scale models integrate high throughput first-principle calculations based on density functional theory (DFT), high throughput calculation of phase diagrams (CALPHAD) modeling, and finite element method (FEM) simulations. These models are to be validated through laboratory experiments. Furthermore, the models are available as open source so as to enable scientists and engineers in the community to adapt and contribute to the development and application. The approaches rely on the research team’s extensive experience on the prediction of properties of individual phases at finite temperatures and variable compositions through DFT calculations, and our broad expertise on dissimilar material joining and their corrosion. The proposed computational framework enables high throughput computations for improved predictions of corrosion and the associated mechanical performance in dissimilar material joints, resulting in significant reduction in computational time needed by the current state-of-the-art methods. With the participation of researchers from three universities, an auto manufacturer, two manufacturing technology/equipment suppliers, and a software developer/vendor, the interdisciplinary research team applies the technical development on both phase-based modeling and laboratory experiments into the automobile body joining processes for validation and technology demonstration. The global cost of corrosion was estimated at about 3.4% of the global GDP in 2013. By using available corrosion control practices, it is estimated a saving between 15-35% of the cost of corrosion. In the U.S., more than $276 billion is spent repairing corrosion damage. Prediction of the corrosion and its impact on performance of the dissimilar material joints is critical for reducing the massive number of the current corrosion-based recalls for automobiles. Thus, the project goal is to develop models to enable predictive maintenance and end-of-life planning of multi-metal joints with risk of corrosion under different conditions such as exposure to high temperatures in summer and salt solutions in winter, quantified through its pH. An academia-industry consortium led by the University of Michigan and including Pennsylvania State University, University of Illinois Urbana-Champaign, University of Georgia, General Motors Company, Livermore Software Technology Corporation, and Optimal Process Technologies, LLC. created multi-scale models for prediction of corrosion in aluminum-steel joint structures such of them used in vehicle subassemblies – chassis and transmission systems. Starting from the first principle calculations, the team developed mathematical and data-driven models to predict the metallic components, which are formed during joining of two metals, for example aluminum and steel - a lightweight multilateral system which is currently used in more than 60% car bodies. These models were used for simulating chemical reactions that are happening when the joining metallic components are exposed to high temperatures and different pH values. The team was able to predict how the corrosion installs on the metallic components and how they lead to a sudden failure of components in cars. Newly developed machine learning algorithms combining Science, Technology, Engineering and Math disciplines, advanced finite element simulation and experimental validations have been integrated in a platform for prediction of the corrosion evolution and prediction the failure of joints under mechanical loadings and fatigue. Moreover, based on machine learning and inverse analysis, the team proposed solutions for designing new metallic alloys less susceptible to corrosion when joining multi-material assembles. An average of 4% error compared with experiments was achieved for the most common joints that are used in vehicle subassemblies.

36 MATERIALS SCIENCE↗

Monitoring the corrosion resistance of cold-spray coatings with membrane-based sensors

In this presentation, the MBES shows the ability to detect the change in exposed environment even with cold-spray coatings. Corrosion rates from the cold-spray coating were comparable to a 316 stainless steel sample. Defects in the coating did not impact sensor performance in terms of corrosion rate or water content detection. Energy dispersive X-ray spectroscopy was used to document ion migration into the membrane.

Rendon, Arnaldo↗

The Test and Evaluation of a Non-Chromate Finishing Agent

This research is focused on the design, development and implementation of an industry, military and commercial standard testing cell for surface coatings, which focuses on advanced non-chromate materials technology and their commercialization. Currently, within both private and commercial sectors, chromates are used in the corrosion prevention. processes. However, there is a great demand for chromate-free systems that are able to provide equal protection. At the end of this effort, it is intended that a patented alternative to chromate conversion coatings would be tested and processed for commercialization. Thus far, research studies have been concerned primarily with current corrosion knowledge and testing methods. Corrosion can be classified into five categories: The first type is uniform corrosion which is dominated by a uniform thinning due to an even and regular loss of metal. The second type is called localized corrosion in which most of the loss occurs in discrete areas. The third type, metallurgically influenced corrosion is a form of attack where metallurgy plays a significant role. The fourth type, titled mechanically assisted degradation is a form of attack where velocity, abrasion, and hydrodynamics control the corrosion process. The last type of corrosion is defined as environmentally induced cracking which occurs when cracks are produced under specific, premeditated stress. Oddly enough, with these varying classifications, there are not as many standardized corrosion testing sites. Two of the most common testing methods for corrosion are salt spray testing and filiform. Although neither has proven to be absolute, in terms of the resulting observations, our research aims to help provide data that may be used to support the standardization for corrosion testing. We would acquire and use a Singleton Cyclic Corrosion Testing Chamber. Singleton test chambers perform a wide range of commonly used catalytic corrosion tests. They are used throughout the industry, some of which are - automotive, aerospace, electronic and many more. In addition to this, Singleton test chambers are fully expandable to accommodate cyclic corrosion testing needs. Singleton chambers are also designed for complete compliance and conformity with ASTM (American Society for Testing and Materials), military and commercial standards.

Gulley, H.↗