Search NASA⌕ Search

SEARCH · Search NASA

Results for “DEGRADATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Thermal oxidative degradation reactions of perfluoroalkylethers

The mechanisms operative in thermal oxidative degradation of Fomblin Z and hexafluoropropene oxide derived fluids and the effect of alloys and additives upon these processes are investigated. The nature of arrangements responsible for the inherent thermal oxidative instability of the Fomblin Z fluids is not established. It was determined that this behavior is not associated with hydrogen end groups or peroxy linkages. The degradation rate of these fluids at elevated temperatures in oxidizing atmospheres is dependent on the surface/volume ratio. Once a limiting ratio is reached, a steady rate appears to be attained. Based on elemental analysis and oxygen consumption data, CF2OCF2CF2O2, no. CF2CF2O, is one of the major arrangements present. The action of the M-50 and Ti(4 Al, 4 Mn) alloys is much more drastic in the case of Fomblin Z fluids than that observed for the hexafluoropropene derived materials. The effectiveness of antioxidation anticorrosion additives, P-3 and phospha-s-triazine, in the presence of metal alloys is very limited at 316 C; at 288 C the additives arrested almost completely the fluid degradation. The phospha-s-triazine appears to be at least twice as effective as the P-3 compound; it also protected the coupon better. The Ti(4 Al, 4 Mn) alloy degraded the fluid mainly by chain scission processes this takes place to a much lesser degree with M-50.

Paciorek, K. L.↗

The effects of metals and inhibitors on thermal oxidative degradation reactions of unbranched perfluoroalkylethers

Thermal oxidative degradation studies were performed on unbranched perfluoroalkylethers at 288 C in oxygen. Metals and alloys studied included Ti, Al, and Ti (4 Al, 4 Mn). The mechanism of degradation was by chain scission. Ti and Al promoted less degradation than Ti (4 Al, 4 Mn). The two inhibitors investigated (a perfluorophenyl phosphine and a phosphatriazine) reduced degradation rates by several orders of magnitude. Both inhibitors were effective for the same duration (75 to 100 hours). The phosphatriazine appeared to provide more surface protection.

Jones, W. R., Jr.↗

Thermal oxidative degradation reactions of perfluoroalklethers

The objective of this contract was to investigate the mechanisms operative in thermal and thermal oxidative degradation of Fomblin Z and hexafluoropropene oxide derived fluids and the effect of alloys and additives upon these processes. The nature of arrangements responsible for the inherent thermal oxidative instability of the Fomblin Z fluids has not been established. It was determined that this behavior was not associated with hydrogen end-groups or peroxy linkages. The degradation rate of these fluids at elevated temperatures in oxidizing atmospheres was found to be dependent on the surface/volume ratio. Once a limiting ratio was reached, a steady rate appeared to be attained. Based on elemental analysis and oxygen consumption data, -CF2OCF2CF2O-, not -CF2CF2O-, is one of the major arrangements present. The action of the M-50 and Ti(4 Al, 4 Mn) alloys was found to be much more drastic in the case of Fomblin Z fluids than that observed for the hexalfuoropropane oxide derived materials. The effectiveness of antioxidation/anticorrosion additives, P-3 and phospha-s-triazine, in the presence of metal alloys was very limited at 316 C; at 288 C the additives arrested almost completely the fluid degradation. The phospha-s-triazine appeared to be at least twice as effective as the P-3 compound; it also protected the coupon better. The Ti(4 Al, 4 Mn) alloy degraded the fluid mainly by chain scission processes; this took place to a much lesser degree with M-50.

Paciorek, K. L.↗

Interply layer degradation effects on composite structural response

Recent research activities at NASA Lewis Research Center to computationally evaluate the effects of interply layer progressive weakening (degradation) on the structural response of a composite beam are summarized. The structural responses of interest include: (1) bending, (2) buckling, (3) free vibrations, (4) periodic excitation, and (5) impact. Finite element analysis was used for the computational evaluations. The interply layer degradation effects on the various structural responses were determined and assessed as a function of the interply layer modulus varying from 1 million psi down to 1000 psi and even lower for some limiting cases. The results obtained show that the interply layer degradation has generally negligible effects on composite structural response and, therefore, structural integrity, unless the interply layer modulus degrades to about 10,000 psi or less.

Chamis, C. C.↗

Laboratory studies of Kapton degradation in an oxygen ion beam

Results are presented from a preliminary laboratory investigation of the degradation of the widely used polyimide Kapton under oxygen ion bombardment. Recent space shuttle flights have shown that Kapton and some other materials exposed to the apparent ram flow of residual atmosphere (at orbital velocity in low Earth orbit) lose mass and change their optical properties. It was hypothesized that these changes are caused by chemical interaction with atomic oxygen, aided by the 5-eV impact energy of atmospheric oxygen atoms in the ram. The reaction rate under O(+) bombardment seemed to be independent of incident energy over a wide range of energies. Although the flux of thermal ions in this experiment was much greater than the accelerated flux, the observed Kapton degradation was limited to the beam area and ram flow direction. This is consistent with an activation energy above the thermal energies but well below the beam energies. The results reproduce well the material loss, optical changes, SEM surface structure, and ram directionality of the samples returned by the shuttle. These factors, along with the lack of degradation under argon ion bombardment, are convincing evidence for ram flow oxidation as the mechanism of degradation.

Ferguson, D. C.↗

Topics in electrochemical degradation of photovoltaic modules

Electrochemical degradation of photovoltaic modules was examined. It is found that the extent of electrochemical damage is dependent on the integrated leakage current. The PV electrochemical degradation mechanisms in the two polarities are different: (1) degradation rates in the two polarities are of the same order of magnitude; (2) center tapped grounded arrays are a preferred system configuration to minimize electrochemical degradation. The use of thicker pottant layers and polymer substrate films to reduce equilibrium leakage current values is suggested. A metallized substrate layer, if used, should be isolated from the pottant and the frame by polyester layers, and EVA modules appear to be consistent with 30 year life allocation levels for electrochemical damage. Temperature acceleration factors are well behaved and moderately well understood; humidity acceleration factors vary radically with module construction and materials and require additional research.

Mon, G. R.↗

Laboratory degradation of Kapton in a low energy oxygen ion beam

An atomic oxygen ion beam, accelerated from a tunable microwave resonant cavity, was used at Lewis Research Center to bombard samples of the widely used polyimide Kapton. The Kapton experienced degradation and mass loss at high rates, which may be comparable to those found in Space Shuttle operations if the activation energy supplied by the beam enabled surface reactions with the ambient oxygen. The simulation reproduced the directionality (ram-wake dependence) of the degradiation, the change in optical properties of the degraded materials, and the structure seen in scanning electron micrographs of samples returned on the Shuttle Trails with a substituted argon ion beam produced no rapid degradation. Energy Dispersive X-ray Analysis (EDAX) showed significant surface composition changes in all bombarded samples. Mass loss rates and surface composition changes are discussed in terms of the possible oxidation chemistry of the interaction. Finally, the question of how the harmful degradation of materials in low earth orbit can be minimized is addressed.

Ferguson, D. C.↗

Interply layer degradation effects on composite structural response

Recent research activities at NASA Lewis Research Center to computationally evaluate the effects of interply layer progressive weakening (degradation) on the structural response of a composite beam are summarized. The structural responses of interest include: (1) bending, (2) buckling, (3) free vibrations, (4) periodic excitation, and (5) impact. Finite element analysis was used for the computational evaluations. The interply layer degradation effects on the various structural responses were determined and assessed as a function of the interply layer modulus varying from 1 million psi down to 1000 psi and even lower for some limiting cases. The results obtained show that the interply layer degradation has generally negligible effectss on composite structural response and, therefore, structural integrity, unless the interply layer modulus degrades to about 10,000 psi or less.

Chamis, C. C.↗

The effects of metals and inhibitors on thermal oxidative degradation reactions of unbranched perfluoroalkyl ethers

Thermal oxidative degradation studies were performed on unbranched perfluoroalkylethers at 288 C in oxygen. Metals and alloys studied included Ti, Al, and Ti (4 Al, 4 Mn). The mechanism of degradation was by chain scission. Ti and Al promoted less degradation than Ti (4 Al, 4 Mn). The two inhibitors investigated (a perfluorophenyl phosphine and a phosphatriazine) reduced degradation rates by several orders of magnitude. Both inhibitors were effective for the same duration (75 to 100 hours). The phosphatriazine appeared to provide more surface protection.

Jones, W. R., Jr.↗

Degradation mechanisms of materials for large space systems in low Earth orbit

Degradation was explored of various materials used in aerospace vehicles after severe loss of polymeric material coatings (Kapton) was observed on an early shuttle flight in low Earth orbit. Since atomic oxygen is the major component of the atmosphere at 300 km, and the shuttle's orbital velocity produced relative motion corresponding to approx. 5 eV of oxygen energy, it was natural to attribute much of this degradation to oxygen interaction. This assumption was tested using large volume vacuum systems and ion beam sources, in an exploratory effort to produce atomic oxygen of the appropriate energy, and to observe mass loss from various samples as well as optical radiation. Several investigations were initiated and the results of these investigations are presented in four papers. These papers are summarized. They are entitled: (1) The Space Shuttle Glow; (2) Laboratory Degradation of Kapton in a Low Energy Oxygen Ion Beam; (3) The Energy Dependence and Surface Morphology of Kapton Degradation Under Atomic Oxygen Bombardment; and (4) Surface Analysis of STS 8 Samples.

Gordon, William L.↗

Solar cell design for avoiding LILT degradation

Growing concerns about radioisotope thermoelectric generator (RTG) performance potential, cost, safety, and availability have renewed interest in utilizing photovoltaic energy conversion for future JPL interplanetary missions such as the Mariner Mark II set. Although lightweight solar array technology has advanced to the point where it would appear to provide an alternative power source, anomalous silicon cell curve shape degradation at conditions of low intensity and low temperature (LILT) severely restricts photovoltaic applications for missions beyond 3 AU solar distance. In order to extend photovoltaic applications to distances of 5 AU, ways to minimize the deleterious impact of LILT cell degradation were investigated. These investigations have ranged from consideration of individual cell selection for LILT behavior to the examination of methods for reducing or eliminating cell LILT degradation by modifying the cell processing. Use of a partial oxide barrier between the cell n+ contacts and the silicon has been shown to reduce significantly both the occurrence and magnitude of the LILT degradation.

Stella, P. M.↗

Degradation of graphite-epoxy due to electron radiation

Experimental results are presented showing that electron irradiation has a variable effect on the properties of graphite-epoxy depending upon the test temperature and the property of interest. In general, compression properties are improved at cold temperature and degraded at elevated temperature. With the exception of some moduli, tensile and shear properties are degraded at both cold and elevated temperatures. Electron irradiation lowers the glass transition temperature of graphite/epoxy significantly. Property degradation of irradiated materials at the elevated temperature is associated with the reduction in Tg. It is shown that a (0) compression-strength test is the most sensitive test for exhibiting the effects of electron irradiation. Results from tests on neat resin also show that the bulk matrix is degraded after irradiation, and that the correlation between resin and composite response is good.

Herakovich, C. T.↗

Degradation and crosslinking of perfluoroalkyl polyethers under X-ray irradiation in ultrahigh vacuum

Degradation of three types of commercially available perfluoroalkyl polyethers (PFPE)-Demnum S200, Fomblin Z25, and Krytox 16256-by X-ray irradiation was studied by using X-ray photoemission spectroscopy (XPS) and a mass spectrometer under ultra-high-vacuum conditions. The carbons in the polymers were characterized by chemical shifts of Cls binding energies. Gaseous products containing COF2 and low-molecular-weight fluorocarbons were formed. From Fomblin Z25, which has acetal linkages (-OCF2O-), a large quantity of COF2 gas was evolved. Liquid products became tacky after a long irradiation time, and some did not dissolve in Freon. High-pressure liquid chromatography (HPLC) showed that molecular weight distribution became broader and that higher molecular weight polymers were formed from Demnum and Krytox. We concluded from these results that degradation and cross-linking took place simultaneously. Demnum crosslinked more easily than the other fluids. The time dependence of both XPS spectra of Cls and mass spectra showed that C-O-bonded carbons in PFPE'S were removed faster than other carbons. There was no substrate effect on the degradation reaction because the first-order rate constants calculated from the change of gaseous products were similar when stainless steel (440C) and gold-coated surfaces were used. Metal fluorides were formed on stainless steel during the reaction. A mechanism for the degradation of PFPE'S is discussed on the basis of their molecular structures.

Mori, Shigeyuki↗

Accuracy of telemetry signal power loss in a filter as an estimate for telemetry degradation

When telemetry data is transmitted through a communication link, some degradation in telemetry performance occurs as a result of the imperfect frequency response of the channel. The term telemetry degradation as used here is the increase in received signal power required to offset this filtering. The usual approach to assessing this degradation is to assume that it is equal to the signal power loss in the filtering, which is easily calculated. However, this approach neglects the effects of the nonlinear phase response of the filter, the effect of any reduction of the receiving system noise due to the filter, and intersymbol interference. Here, an exact calculation of the telemetry degradation, which includes all of the above effects, is compared with the signal power loss calculation for RF filtering of NRZ data on a carrier. The signal power loss calculation is found to be a reasonable approximation when the filter follows the point at which the receiving system noise is introduced, especially if the signal power loss is less than 0.5 dB. The signal power loss approximation is less valid when the receiving system noise is not filtered.

Koerner, M. A.↗

Martian impact crater degradation studies: Implications for localized obliteration episodes

Early spacecraft missions to Mars revealed that impact craters display a range of degradational states, but full appreciation of the range of preservational characteristics was not revealed until the Mariner 9 and Viking missions in the 1970's. Many studies have described the spatial and temporal distribution of obliteration episodes based on qualitative descriptions of crater degradation. Recent advances in photoclinometric techniques have led to improved estimates of crater morphometric characteristics. The present study is using photoclinometry to determine crater profiles and is comparing these results with the crater geometry expected for pristine craters of identical size. The result is an estimate of the degree of degradation suffered by Martian impact craters in selected regions of the planet. Size-frequency distribution analyses of craters displaying similar degrees of degradation within localized regions of the planet may provide information about the timing of obliteration episodes in these regions.

Barlow, N. G.↗

LEO degradation of graphite and carbon-based composites aboard Space Shuttle Flight STS-46

Six different types of carbon and carbon-boron nitride composites were exposed to low Earth orbit aboard Space Shuttle flight STS-46. The samples received a nominal atomic oxygen fluence of 2.2 x 10(exp 20) atoms/sq cm in 42 hours of exposure. Pyrolytic graphite and highly oriented pyrolytic graphite showed significant degradation, and the measured erosion yield was within a factor of two of published values. The erosion yield of pyrolytic boron nitride was found to be 2.6 x 10(exp 26) cu cm/atom in plasma asher exposure, over 42 times lower than that of pyrolytic graphite. This low erosion yield makes graphite plus boron nitride mixtures quite resistant to low Earth orbit exposure. Evidence suggests that the graphitic component was preferentially etched, leaving the surface boron nitride rich. Degradation resistance increases with boron nitride composition. Carbon fiber/carbon composites degraded in low Earth orbit, and the carbon pitch binder was found to etch more easily than the graphite fibers which have much higher degradation resistance.

Spady, Blaine R.↗

Degradation of TCE using sequential anaerobic biofilm and aerobic immobilized bed reactor

Bacteria capable of degrading trichloroethylene (TCE) were isolated from contaminated wastewaters and soil sites. The aerobic cultures were identified as Pseudomonas aeruginosa (four species) and Pseudomonas fluorescens. The optimal conditions for the growth of aerobic cultures were determined. The minimal inhibitory concentration values of TCE for Pseudomonas sps. were also determined. The aerobic cells were immobilized in calcium alginate in the form of beads. Degradation of TCE by the anaerobic and dichloroethylene (DCE) by aerobic cultures was studied using dual reactors - anaerobic biofilm and aerobic immobilized bed reactor. The minimal mineral salt (MMS) medium saturated with TCE was pumped at the rate of 1 ml per hour into the anaerobic reactor. The MMS medium saturated with DCE and supplemented with xylenes and toluene (3 ppm each) was pumped at the rate of 1 ml per hour into the fluidized air-uplift-type reactor containing the immobilized aerobic cells. The concentrations of TCE and DCE and the metabolites formed during their degradation by the anaerobic and aerobic cultures were monitored by GC. The preliminary study suggests that the anaerobic and aerobic cultures of our isolates can degrade TCE and DCE.

Chapatwala, Kirit D.↗

Degradation in finite-harmonic subcarrier demodulation

Previous estimates on the degradations due to a subcarrier loop assume a square-wave subcarrier. This article provides a closed-form expression for the degradations due to the subcarrier loop when a finite number of harmonics are used to demodulate the subcarrier, as in the case of the buffered telemetry demodulator. We compared the degradations using a square wave and using finite harmonics in the subcarrier demodulation and found that, for a low loop signal-to-noise ratio, using finite harmonics leads to a lower degradation. The analysis is under the assumption that the phase noise in the subcarrier (SC) loop has a Tikhonov distribution. This assumption is valid for first-order loops.