Search NASA⌕ Search

SEARCH · Search NASA

Results for “Fuel cladding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Ceramic reinforced zirconium alloy nuclear fuel cladding with intermediate oxidation resistant layer

The invention relates to compositions and methods for coating a zirconium alloy (e.g., ceramic-containing) cladding tube for use with fuel rods in a nuclear water reactor. The coating includes an intermediate oxidation resistant layer and a SiC containing layer at least partially deposited on the intermediate oxidation resistant layer. The SiC containing layer can include a plurality of fibers. The SiC containing layer may also be on the outer surface of end plugs. The invention provides improved capability for the zirconium alloy cladding to withstand normal and accident conditions in the nuclear water reactor.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Milestone 1.2.11: H 2 Production from Surrogate Non-Native Corrosion Plumes on Aluminum 6061-T6 Fuel Cladding Surrogates

Thick, localized, “non-native” corrosion plumes have been identified on Advanced Test Reactor fuel elements, raising concern on their impact on the radiolytic formation of molecular hydrogen gas (H 2 ) from aluminum-clad spent nuclear fuel (ASNF) under proposed extended (> 50 years) dry storage conditions. Here, we report our findings on H 2 generation from the gamma irradiation (up to 52 MGy) of surrogate “non-native” corrosion plume coupons: ambient-temperature-corroded (~350 days in water) aluminum alloy 6061 (AA6061) coupons in helium gas environments with ~0% added relative humidity. Additionally, we provide a comparison of proposed ASNF drying techniques— vacuum drying only, vacuum drying + 100 °C for 4 hr, and vacuum drying + 220 °C for 4 hr—on the yield of H 2 from these surrogate systems. The presented data indicates that similar amounts of H 2 (~2 × 10–3 µmol J–1) are formed from gamma irradiated AA6061 coupons corroded under different temperature regimes, i.e., ambient/350 days vs. 90 C/30 days. These findings validate current, complimentary modelling predictions based on high-temperature-corrosion irradiation data only. Further, the application of a heat treatment procedure (100 and 220 °C), in conjunction with vacuum drying, accelerated the rate at which a steady-state H 2 yield was attained, in comparison to vacuum only, due to the removal of H 2 precursors in the form of adsorbed waters. Interestingly, within the confidence limits of our measurements, negligible difference in total H 2 yield was found between the two investigated heat treatment procedures.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Recrystallization driven softening and heating rate dependencies of FeCrAl nuclear fuel cladding during accident transients

A refined understanding of FeCrAl cladding behavior during rapid transients is critical for its potential deployment in light-water reactors. Current assessments focus on transient burst testing metrics such as balloon geometry, burst temperature, and hoop stress, often used as proxies for simpler conventional tensile properties. However, directly correlating isothermal tensile and creep data with accident transient scenarios remains a challenge, although it is essential for high fidelity model development. Recent modeling based on tensile tests up to 800 °C, conducted with both immediate loading and a 10-minute soak, showed that immediate loading better predicts experimental burst temperatures, indicating a thermal softening effect. Building upon this observation, the current study connects transient performance, microstructural evolution, and high-temperature tensile properties by leveraging results from C26M claddings burst tests performed at heating rates of 1–50 °C/s and hoop stresses from 25 to 100 MPa. At 25 MPa, rupture temperatures varied by only 6 °C, but at 100 MPa, the difference reached 116 °C, with faster heating yielding higher burst temperatures. Microstructural analysis identified recrystallization as the primary cause of heating rate-dependent softening, eliminating prior cold-working. In-situ thermomechanical data linked ballooning onset to localized instabilities, similar to ultimate tensile strength behavior in conventional tensile tests. High heating rates correlated with immediate loading tensile data, while lower rates matched soaked data. Furthermore, by linking burst performance to microstructural evolution and tensile properties, this work provides a foundation for more accurate modeling of FeCrAl claddings and potentially other Fe-based materials under accident conditions.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

R&D Progress on Recovery/Recycle of Zirconium from Used Fuel Cladding

There has been significant progress accomplished at Oak Ridge National Laboratory (ORNL) on the development of a dry chlorination process for recovery and purification of zirconium from used nuclear fuel (UNF) cladding by conversion to zirconium tetrachloride, which sublimes to a vapor and is then condensed as a dry salt product, essentially free of fuel and alloy components (impurities). We have accomplished significant progress on developing a chlorination process for removing the zirconium in UNF cladding and purifying the product salt for re-use—possibly in manufacture of new cladding, or at a minimum to meet specifications for disposal as low level waste.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Critical heat flux on zircaloy and accident tolerant fuel cladding under prototypical conditions of pressurized and boiling water reactors

First of a kind high spatial and temporal resolution temperature measurements of Pressurized Water Reactor and Boiling Water Reactor simulated fuel pins (high heat flux cosine profile heaters) in annular rod type geometry during nucleate boiling, departure from nucleate boiling and re-wetting has been performed. Distributed fiber optic measurements of the cladding axial temperature with spatial resolutions down to 2.5 mm axially at up to three equally spaced azimuthal locations per rod have demonstrated the similarities and differences of the different accident tolerant fuel cladding materials. These experiments show the performance of accident tolerant cladding with a precise measurement of the location and evolution of dryout followed by the re-wetting phenomena (see supplementary time history of a critical heat flux event). Experimental parameters varied coolant mass fluxes from 1695 to 2712 kg/m 2 s, pressures from 10 to 20 MPa, and inlet subcooling from 10 to 55 °C. It was found that the coatings and different material have little effect on the value of the critical heat flux. Any discrepancies between the local critical heat flux verified among the cladding material are attributed to different departure from nucleate boiling phenomena captured during the experiment with the high-resolution optical fiber temperature data. Substantial differences in the performance of the different cladding material to survive a critical heat flux event were however observed by post-test X-ray and optical inspection. External evident damage and internal cracks to the simulated fuel pin having the bare zircaloy cladding were observed in regions associated with the occurrence of the critical heat flux for longer periods. Such damages were associated with zirconium oxidation, and not noticed on the Cr coated zircaloy or FeCrAl claddings. These results indicate that the use of FeCrAl or a Cr coated zircaloy as cladding in Pressurized Water Reactor and Boiling Water Reactor may increase the survivability of the cladding material for short transients.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Pool Boiling CHF Experiment for Cr-alloy-coated Accident Tolerant Fuel Cladding

The severe accident at the Fukushima nuclear power plants forced the nuclear communities to revise and reinforce their safety technology, especially accident tolerance. The main problem of Zr-based alloys is hydrogen generation owing to steam oxidation in a very high temperature environment. Currently, several types of Accident Tolerant Fuel (ATF) claddings that eliminate the steam oxidation problem have been presented as alternatives. Although the ATFs have shown appropriate performances in terms of material engineering, thorough tests including thermal hydraulic concerns are still required to ensure the design compatibilities. In this study, we conducted pool boiling critical heat flux (CHF) experiments using Cr-alloy-coated ATF claddings to verify basic thermal hydraulic performances. (authors)

36 MATERIALS SCIENCE↗

Assessment of Corrosion Resistance of Candidate Alloys for Accident Tolerant Fuel Cladding under Reactor Conditions

The environment of a light water reactor (LWR) core is a combination of high temperatures, high pressures, high neutron and gamma fluxes, mechanical stresses and chemical aggressive coolants. All of these factors combined can induce changes in the microstructure of the fuel and cladding that are very difficult to predict in a systematic fashion [1] and are major challenge for the safety and life extension of current reactors. Throughout reactor transients and accidents, the cladding may experience deterioration caused by a temperature increase, oxidation embrittlement [1], [2], or mechanical interaction with the fuel caused by stress [3]. These events may lead to cracking or rupture of the cladding, causing the release of fission products into the coolant. Such events have been observed at the Three Mile Island and Fukushima accidents. To avoid such occurrences in LWRs, the accident tolerant fuels (ATF) program was initiated to focus on the replacement of zirconium-based alloys with materials that exhibit slower steam oxidation kinetics. This project focuses on several iron-based alloys such as T91, APMT, MA956, experimental Fe-Cr alloys and one experimental nanofeatured alloy (NFA). Experiments have been conducted in both PWR primary water at 320°C and BWR normal water chemistry at 288°C, spanning a large range in electrochemical corrosion potential (ECP). Samples were exposed to either proton irradiation (University of Michigan) or electron irradiation (Notre Dame Radiation Laboratory) to independently assess the roles of displacement damage or radiolysis on the corrosion rate, oxide thickness, morphology, structure and resistivity. Post-irradiation characterization of various regions of the electronirradiated samples was completed by means of microscopy (Notre Dame Integrated Imaging Facility) and spectroscopy (Notre Dame Materials Characterization Facility) techniques to provide high resolution information regarding the oxide layer present on the surface of the material.

Grdanovska, Slavica↗

Completion of a Chlorination Test Using 250 grams of High-Burnup Used Fuel Cladding from a North Anna Pressurized Water Reactor

A second large -scale chlorination test was completed in February 2017 by chlorinating 250 g of used nuclear fuel (UNF) cladding from a North Anna pressurized water reactor (PWR). Analytical results and a Zr mass balance from this test are described and compared with previous results obtained by the Zirconium Recovery and Recycle Project.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Advancing SiC clad fuel performance model: bridging micro- and macro-scale models and experimental validation

This report presents a workflow for advancing fuel performance modeling of SiC composite cladding for light-water reactors by linking microscale, experimental data-informed finite element analysis with rod-scale fuel performance codes such as BISON. The workflow uses X-ray computed tomography (XCT) to capture the actual geometry and processing-induced defects of as-fabricated SiC composite tube specimens, particularly porosity and wall-thickness variations, and converts the segmented XCT volumes into image-based finite element meshes for high fidelity structural analysis.

Koyanagi, Takaaki [Oak Ridge National Laboratory (↗

Single Rod Reflood Quenching Experiments with Simulated Decay Heat for Accident-Tolerant Fuel Claddings

The Loss-of-Coolant Accident (LOCA) is a hypothetical situation which includes a sudden loss of coolant, overheating of fuel rods, and emergency coolant injection. This situation could be modeled as a quenching process of cladding material into the coolants, a reverse process of boiling the coolants. The KAERI have been developing a CrAl-coating type Accident-Tolerant Fuel (ATF) claddings to enhance safety margin in such severe accident situations and evaluations for the performance in various aspects are on process. We established a single-rod type reflood quenching experiment setup to simulate the LOCA process. Unlike other conventional quenching experiment setup, our experiment setup is capable of heating during the reflooding process, simulating the decay heat in the real core. We installed heaters and thermocouples (TC) inside the cladding specimens to minimize any disturbances on the interfacial layer during the experiment. Currently the setup is on test run and we present experiment data and verification with conventional Zircaloy-4 claddings. We are going to conduct the reflood quenching experiment with KAERI's CrAl-coated ATF claddings to evaluate the cooling performances.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗