Fracture surface analysis in composite and titanium bonding

Carbon fibers were obtained from several manufacturers. Surface treatments were performed on these fibers by anodization. The surfaces of these fibers were analyzed by X-ray photoelectron spectroscopy and wetting force measurement. The breaking strength of these fibers was measured at 2.5 cm length. It was seen that the surface treatments reduces the strength of the fibers. It was also seen that the Hercules fibers had a higher breaking strength than the Union Carbide fibers. Fiber critical length measurements showed no difference in critical lengths between AS-4 and AU-4 fibers embedded in polysulfone. However, the fiber lengths were much shorter for the surface treated fibers. This effect could be related to increased adhesion between fiber and matrix, or it could be due to the lower breaking strength of the surface treated fiber.

Devilbiss, T. A.↗

Optimization of aircraft interior panels

Eight different graphite composite panels were fabricated using four different resin matrices. The resin matrices included Hercules 71775, a blend of vinylpolystyrpyridine and bismaleimide, H795, a bismaleimide, Cycom 6162, a phenolic, and PSP 6022M, a polystyrylpyridine. Graphite panels were fabricated using fabric or unidirectional tape. This report describes the processes for preparing these panels and some of their mechanical, thermal and flammability properties. Panel properties are compared with state-of-the-art epoxy fiberglass composite panels.

Kourtides, Demetrius A.↗

Far-infrared properties of cluster galaxies

Far-infrared properties are derived for a sample of over 200 galaxies in seven clusters: A262, Cancer, A1367, A1656 (Coma), A2147, A2151 (Hercules), and Pegasus. The IR-selected sample consists almost entirely of IR normal galaxies, with Log of L(FIR) = 9.79 solar luminosities, Log of L(FIR)/L(B) = 0,79, and Log of S(100 microns)/S(60 microns) = 0.42. None of the sample galaxies has Log of L(FIR) greater than 11.0 solar luminosities, and only one has a FIR-to-blue luminosity ratio greater than 10. No significant differences are found in the FIR properties of HI-deficient and HI-normal cluster galaxies.

Bicay, M. D.↗

Interfacial adhesion of carbon fibers

Relative adhesion strengths between AS4, AS1, and XAS carbon fibers and thermoplastic polymers were determined using the embedded single filament test. Polymers studied included polycarbonate, polyphenylene oxide, polyetherimide, polysulfone, polyphenylene oxide blends with polystyrene, and polycarbonate blends with a polycarbonate polysiloxane block copolymer. Fiber surface treatments and sizings improved adhesion somewhat, but adhesion remained well below levels obtained with epoxy matrices. An explanation for the differences between the Hercules and Grafil fibers was sought using X ray photon spectroscopy, wetting, scanning electron microscopy and thermal desorption analysis.

Bascom, Willard D.↗

Surface characterization in composite and titanium bonding: Carbon fiber surface treatments for improved adhesion to thermoplastic polymers

The effect of anodization in NaOH, H2SO4, and amine salts on the surface chemistry of carbon fibers was examined by X-ray photoelectron spectroscopy (XPS). The surfaces of carbon fibers after anodization in NaOH and H2SO4 were examined by scanning transmission electron microscopy (STEM), angular dependent XPS, UV absorption spectroscopy of the anodization bath, secondary ion mass spectrometry, and polar/dispersive surface energy analysis. Hercules AS-4, Dexter Hysol XAS, and Union Carbide T-300 fibers were examined by STEM, angular dependent XPS, and breaking strength measurement before and after commercial surface treatment. Oxygen and nitrogen were added to the fiber surfaces by anodization in amine salts. Analysis of the plasmon peak in the carbon 1s signal indicated that H2SO4 anodization affected the morphological structure of the carbon fiber surface. The work of adhesion of carbon fibers to thermoplastic resins was calculated using the geometric mean relationship. A correlation was observed between the dispersive component of the work of adhesion and the interfacial adhesion.

Devilbiss, T. A.↗

Fabrication and testing of fire resistant graphite composite panels

Eight different graphite composite panels were fabricated using four different resin matrices. The resin matrices included Hercules 71775, a blend of vinylpolystyrpyridine and bismaleimide, H795, a bismaleimide, Cycom 6162, a phenolic, and PSP 6022m, a polystyrylpyridine. Graphite panels were fabricated using fabric or unidirectional tape. Described are the processes for preparing these panels and some of their mechanical, thermal and flammability properties. Panel properties are compared with state-of-the-art epoxy fiberglass composite panels.

Roper, W. D.↗

Surface and interfacial properties of carbon fibers

Differences in the adhesion of three carbon fibers (Hercules AS1 and AS4, and Hysol-Grafil XAS) to polycarbonate (PC) have been shown to correlate with the absorptivity of PC on the three fiber types. The absorptivity (energy of absorption) was determined using retention time liquid chromatography and the adhesion was measured using the single embedded filament tensile test. A correlation was also found between adhesion strength and the O/N surface element ratio using XPS analysis. The chemical details for these correlations have not yet been determined. A study of filament fracture statistics has been initiated using single and multiple embedded filament tensile tests. Filament fracture has been measured as a function of strain and for different interfiber distances. Preliminary results indicate that fiber fracture is a discontinuous function of increasing strain and may in fact occur at discrete strain intervals. Fiber-fiber interaction effects on fiber fracture have been found for interfiber distances of up to two to three fiber diameters.

Bascom, W. D.↗

Far-infrared properties of cluster galaxies

Far-infrared properties are derived for a sample of over 200 galaxies in seven clusters: A262, Cancer, A1367, A1656 (Coma), A2147, A2151 (Hercules), and Pegasus. The IR-selected sample consists almost entirely of IR normal galaxies, with Log of L(FIR) = 9.79 solar luminosities, Log of L(FIR)/L(B) = 0.79, and Log of S(100 microns)/S(60 microns) = 0.42. None of the sample galaxies has Log of L(FIR) greater than 11.0 solar luminosities, and only one has a FIR-to-blue luminosity ratio greater than 10. No significant differences are found in the FIR properties of HI-deficient and HI-normal cluster galaxies.

Bicay, Michael D.↗

Chemoviscosity modeling for thermosetting resin systems, 4

An experimental study on the changes of chemorheological properties has been conducted and analyzed on commercial Hercules 3501-6 resin system cured under several isothermal conditions between 375 and 435 K. For the cure temperatures equal to or greater than 385 K, the storage modulus curing curves, G prime (t), exhibited abrupt changes in slope which occurred at various times depending on the curing temperatures and were attributed to the onset of gelation reactions. The crossover points between G prime (t) and G double prime (t) curves were observed for curing temperatures equal to or greater than 400 K. The gelation and the crossover points obtained from the chemorheological measurements, therefore, defined two characteristic resin states during cure. Approximately the same value for the degree of cure was reached by the advancement of the reaction at each of these states. The temperature dependency of the viscosities for the characteristic resin states and the rate constants of increase in moduli at different stages of curing were analyzed. Various G prime (t) and G double prime (t) isothermal curing curves were also shown to be capable of being superimposed on one another by the principle of time-temperature superposition. The resultant shift factors a sub t(t) and a Eta(T) were shown to follow the Arrhenius type relationship. Values of the activation energy suggested that the reaction kinetics, instead of the diffusion mechanism, was the limiting step in the overall resin advancement for the cure at temperatures equal to or greater than 385 K.

Hou, T. H.↗

Mechanical properties of several neat polymer matrix materials and unidirectional carbon fiber-reinforced composites

The mechanical and physical properties of three neat matrix materials, i.e., PEEK (polyetheretherketone) thermoplastic, Hexcel F155 rubber-toughened epoxy and Hercules 8551-7 rubber-toughened epoxy, were experimentally determined. Twelve unidirectional carbon fiber composites, incorporating matrix materials characterized in this or earlier studies (with one exception; the PISO(sub 2)-TPI matrix itself was not characterized), were also tested. These composite systems included AS4/2220-1, AS4/2220-3, T500/R914, IM6/HX1504, T300/4901A (MDA), T700/4901A (MDA), T300/4901B (MPDA), T700/4901B (MPDA), APC2 (AS4/PEEK, ICI), APC2 (AS4/PEEK, Langley Research Center), AS4/8551-7, and AS4/PISO(sub 2)-TPI. For the neat matrix materials, the tensile, shear, fracture toughness, coefficient of thermal expansion, and coefficient of moisture expansion properties were measured as a function of both temperature and moisture content. For the unidirectional composites, axial and transverse tensile, longitudinal shear, coefficient of thermal expansion, and coefficient of moisture expansion properties were determined, at room temperature and 100 C.

Coguill, Scott L.↗

Frequency-dependent dielectric analysis - Monitoring the chemistry and rheology of thermosets during cure

Frequency-dependent dielectric measurements in a curing resin sample were performed using an impedance analyzer and a permittivity sensor, to separate and measure the ionic (sigma) and dipolar (tau) mobilities, used as molecular probes of the cure reaction in the resin. The resin samples were tetraglycidyl 4,4-prime-diaminodiphenylmethane epoxy resins which included catalyzed (Hercules 3501-6) and uncatalyzed l3502 resin samples. The values of sigma and tau were used to quantitatively determine the viscosity, the degree of cure, and the T(g) of the resin. It is shown that the values of the Arrhenius and WLF constants during the cure process reflect the buildup of the crosslink network.

Kranbuehl, D.↗

A semi-empirical approach for the chemoviscosity modeling of reactive resin system

A new analytical model for simulating chemoviscosity of a thermosetting resin is presented. The model is developed on the basis of the Williams-Landel-Ferry (WLF, 1955) polymer rheology theory for the thermoplastic materials, which was modified to account for the factor of reaction time by introducing a relationship between the glass transition temperature and the degree of cure of the resin system. Theoretical predictions of the chemoviscosity profiles under dynamic curing conditions are shown to compare favorably with the experimental data obtained on the Hercules 3501-6 resin system cured under seven isothermal conditions.

Hou, T. H.↗

Filament winding cylinders. II - Validation of the process model

Analytical and experimental studies were performed to validate the model developed by Lee and Springer for simulating the manufacturing process of filament wound composite cylinders. First, results calculated by the Lee-Springer model were compared to results of the Calius-Springer thin cylinder model. Second, temperatures and strains calculated by the Lee-Springer model were compared to data. The data used in these comparisons were generated during the course of this investigation with cylinders made of Hercules IM-6G/HBRF-55 and Fiberite T-300/976 graphite-epoxy tows. Good agreement was found between the calculated and measured stresses and strains, indicating that the model is a useful representation of the winding and curing processes.

Calius, Emilio P.↗

The development of an alternative thermoplastic powder prepregging technique

Discussed is a novel powder prepregging technique that is based on the deposition of the powder onto fibers that have been moistened using an ultrasonic humidifier. The moisture acts as an initial binding agent for the powder until the powder can be melted onto the fiber in a subsequent heating step. LaRC-TPI powder, produced by Mitsui Toastsu, and Hercules AS-4 fiber served as the process development material system. The influence of powder particle size on this process, and the quality of the resulting composite are discussed.

Ogden, A. L.↗

Scale effects in buckling, postbuckling and crippling of graphite-epoxy Z-section stiffeners

The buckling, postbuckling and crippling of Hercules Inc. AS4/3502 graphite-epoxy Z-section stiffeners is investigated as a function of specimen structural parameters. Variables addressed are flange and web widths, flange-to-web corner radius, thickness and stacking sequence. Analytical, numerical and experimental results are discussed. Nondimensional parameters have been obtained from an analytical model which effectively normalize the initial local buckling data reported herein and in the references. The nature of the load redistribution after buckling and its impact on postbuckling stiffness is related to the geometric variables. A normalized total width concept is used to unify the crippling data.

Wieland, Todd M.↗

An infiltration/cure model for manufacture of fabric composites by the resin infusion process

A 1-D infiltration/cure model was developed to simulate fabrication of advanced textile composites by the resin film infusion process. The simulation model relates the applied temperature and pressure processing cycles, along with the experimentally measured compaction and permeability characteristics of the fabric preforms, to the temperature distribution, the resin degree of cure and viscosity, and the infiltration flow front position as a function of time. The model also predicts the final panel thickness, fiber volume fraction, and resin mass for full saturation as a function of compaction pressure. Composite panels were fabricated using the RTM (Resin Transfer Molding) film infusion technique from knitted, knitted/stitched, and 2-D woven carbon preforms and Hercules 3501-6 resin. Fabric composites were fabricated at different compaction pressures and temperature cycles to determine the effects of the processing on the properties. The composites were C-scanned and micrographed to determine the quality of each panel. Advanced cure cycles, developed from the RTM simulation model, were used to reduce the total cure cycle times by a factor of 3 and the total infiltration times by a factor of 2.

Weideman, Mark H.↗

Impact response of graphite/epoxy fabric structures

The impact damage resistance and damage tolerance of graphite/epoxy fabric plate (coupon) and cylinder structures were investigated and compared in an analytical and experimental study. Hercules A370-5H/3501-6 five-harness satin weave cloth in a quasi-isotropic (0,45)(sub s) laminate configuration was utilized. Specimens were impacted with 12.7 mm diameter steel spheres at velocities ranging from 10 m/s to 100 m/s. Damage resistance of the specimens was determined through the use of dye penetrant enhanced x-radiography, sectioning, epoxy burnoff, and visual methods. Damage tolerance of the flat plate structures was assessed in a residual tensile test while damage tolerance of the cylinder structures was assessed via pressurization tests. Impacted fabric laminates exhibited matrix crushing, fiber breakage, delamination, and fiber bundle disbonds; the latter being a unique damage mode for fabric laminates. Plate delamination and bundle disbonding was found to be more extensive around the central core area of fiber damage in the coupon specimens than in the cylinder specimens which showed a cleaner damage area due to impact. Damage resistance and damage tolerance were predicted by utilizing a five-step analysis approach previously utilized for coupon configurations. Two of the five steps were adapted to account for the effects of the structural configuration of the pressurized cylinder. The damage resistance analysis provided good correlation to the fiber damage region of both the coupon and cylinder specimens. There was little difference in the size of this region in the two specimen types. However, the analysis was not able to predict the distribution of damage through-the-thickness. This was important in assessing the damage tolerance of the cylinders. The damage tolerance analysis was able to predict the residual tensile strength of the coupons. A general methodology to predict the impact damage resistance and damage tolerance of composite structures utilizing coupon data is presented.

Lagace, Paul A.↗

Longitudinal splitting in epoxy and K-polymer composites - Shear lag analysis including the effect of fiber bridging

The shear-lag model used previously by Nairn (1988) to derive a fracture mechanics analysis of longitudinal splitting in double-edge notched unidirectional composites was used to investigate the effect of fibers bridging across the longitudinal split in these composites. Using the new analysis, the longitudinal splitting fracture toughness, G(Lc), was determined for Hercules AS4/3501-6 graphite/epoxy laminates and for K-polymer based laminates containing Magnamite IM-6 as the graphite reinforcing fiber. Results show that the inclusion of the fiber bridging in the fracture analysis significantly affects the reported fracture toughness.

Nairn, John A.↗