Search NASA⌕ Search

SEARCH · Search NASA

Results for “Hydrogen Concentrations”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Effects of bubbles on the electrochemical behavior of hydrogen-evolving Si microwire arrays oriented against gravity

The size-distribution, coverage, electrochemical impedance, and mass-transport properties of H 2 gas-bubble films were measured for both planar and microwire-array platinized n + -Si cathodes performing the hydrogen-evolution reaction in 0.50 M H 2 SO 4 (aq). Inverted, planar n + -Si/Ti/Pt cathodes produced large, stationary bubbles which contributed to substantial increases in ohmic potential drops. In contrast, regardless of orientation, microwire array n + -Si/Ti/Pt cathodes exhibited a smaller layer of bubbles on the surface, and the formation of bubbles did not substantially increase the steady-state overpotential for H 2 (g) production. Experiments using an electroactive tracer species indicated that even when oriented against gravity, bubbles enhanced mass transport at the electrode surface. Microconvection due to growing and coalescing bubbles dominated effects due to macroconvection of gliding bubbles on Si microwire array cathodes. Electrodes that maintained a large number of small bubbles on the surface simultaneously exhibited low concentrations of dissolved hydrogen and small ohmic potential drops, thus exhibiting the lowest steady-state overpotentials. The results indicate that microstructured electrodes can operate acceptably for unassisted solar-driven water splitting in the absence of external convection and can function regardless of the orientation of the electrode with respect to the gravitational force vector.

25 ENERGY STORAGE↗

Radiolytic Gas Generation and Pressure Buildup in a Closed System Containing Mo-99 Solution

This study measured radiolytic gas generation and pressure buildup in a sealed stainless-steel system containing alkaline Mo-99 solution with added sodium nitrate as a hydrogen suppressant. In each of two experiments, approximately 200 Ci of Mo-99 solution was transferred into a closed experimental vessel inside a hot cell, isolated, and monitored for pressure rise caused by gas generation during radioactive decay. After pressure buildup, headspace gas samples were collected and analyzed by mass spectrometry to determine hydrogen and oxygen concentrations. The purpose was to quantify the magnitude of pressure buildup in a closed system and to characterize the gas composition produced by radiolysis of the Mo-99 target solution under representative handling and storage conditions. The two experiments used similar total Mo-99 activity but differed in solution volume, headspace volume, and leak integrity. In the first experiment, 197.5 Ci of Mo-99 in 16.92 mL of solution was loaded into a vessel with a 31.1-mL headspace; a small leak was later identified, and the measured peak pressure of 46 psig was extrapolated to about 70 psig in the absence of leakage. The headspace gas from this experiment contained about 21.4% H2 and 63.4% O2, but the composition was influenced by preferential hydrogen loss through the leak. In the second experiment, 193 Ci of Mo-99 in 5.41 mL of solution with 0.46 g NaNO3 was loaded into a vessel with a larger 42.61 mL headspace, and no detectable leak was observed. This experiment reached a peak pressure of 38 psig, and the measured gas composition was approximately 28.2% H2 and 51.5% O2. Because the second experiment was leak-free, it is considered the more reliable indicator of the true pressure buildup and intrinsic radiolytic gas composition of the Mo-99 solution.

Chemerisov, Sergey D.↗

Fabrication and characterization of dextran/zein hybrid electrospun fibers with tailored properties for controlled release of curcumin

Abstract BACKGROUND In recent years, there has been considerable interest in the use of biopolymer electrospun nanofibers for various food applications due to the biocompatibility, biodegradability, and high loading capacity. Herein, we fabricated and characterized novel hybrid electrospun fibers from dextran (50%, w/v ) and zein (0–30%, w/v ) solutions, and the effects of various zein concentrations on the properties of the hybrid electrospun fibers were investigated. RESULTS When zein was added at low concentrations (5% and 10%), dextran and zein showed poor miscibility, as reflected by significantly decreased viscosity of the solutions, and the poor mechanical properties of the derived fiber membranes. When zein was added at medium concentrations (15–25%), hydrogen bonds were formed between dextran and zein molecules, as indicated by the red shift of Fourier‐transform infrared bands and β‐sheet to α‐helix structural transformations. The fiber membranes electrospun from a solution with 25% zein showed the most hydrophobic surface, with a water contact angle of 116.9°. The homogenous dispersion of dextran and zein resulted in improved mechanical properties for fibers electrospun from a solution with 30% zein. Curcumin encapsulating dextran/zein electrospun fibers exhibited effective radical scavenging activity and ferric reducing power, along with the desired controlled release behavior for curcumin delivery. CONCLUSION Food grade dextran/zein hybrid electrospun fibers demonstrated tunable properties, and appear to be promising as delivery systems for bioactive and edible antimicrobial food packaging. © 2021 Society of Chemical Industry.

Luo, Shiyuan↗

Evidence of plasma‐driven decomposition of common plastics exposed to an atmospheric nonthermal discharge

Abstract A nonthermal, pulsed spark discharge is applied to three polymer powders in Ar and Ar– gas mixtures. Hydrogen is introduced to assess plasma‐driven decomposition. Gaseous decomposition products, including methane, acetylene, and ethylene, are observed with Fourier‐transform infrared (FTIR). Surface modifications are observed on the residual polymer via attenuated total internal reflection‐FTIR. Time‐averaged rotational, vibrational, and excitation temperatures are characterized in the discharge. The plasma density is found to be around , with rotational and vibrational temperatures ranging from 1500 to 2200 K and an excitation temperature of 1–2 eV. While spark properties did not change with either gas composition or polymer composition, it was determined that the addition of hydrogen promoted higher concentrations of gaseous phase products (promoting hydrogenolysis).

36 MATERIALS SCIENCE↗

Origins of quench in buffered chemical polished and low temperature baked SRF cavities

Electropolishing (EP) and buffered chemical polishing (BCP) are conventional surface preparation techniques for superconducting radiofrequency (SRF) cavities that remove damaged material from the cavity surface. One main issue with EP and BCP treated SRF cavities is high field Q-slope (HFQS), a drop in quality factor at high gradients that limits quench field. High gradient performance in EP cavities can be improved by applying a low temperature bake (LTB), but LTB does not consistently remove HFQS in BCP cavities. There is no consensus as to the why LTB is not effective on BCP prepared cavities, and the cause of HFQS in BCP cavities is not well understood. We examine the origins of quench in EP, BCP, EP+LTB, and BCP+LTB treated SRF cavities. We also show the effect of these treatments on the onset of HFQS, heating within the cavity up to quench, concentration of free hydrogen, and surface roughness.

43 PARTICLE ACCELERATORS↗

LANL's Contribution to the Design and Preparation of the ANL Bubble Experiment #2

In collaboration with Argonne National Laboratory (ANL), Los Alamos National Laboratory (LANL) is assisting in the design and development of portions of the second ANL Bubble Experiment to be performed in late 2020 at ANL. The ANL Bubble Experiment, as called in this report, is a series of direct electron irradiations of a uranyl sulfate solution to produce radiolysis-induced gas bubbles of hydrogen and oxygen. The gas bubbles formed in the solution enhance mixing and heat transfer. The study of the dynamics, shape, and size of radiolysis-induced gas bubbles is of great importance to understand and characterize the thermal and fluid behavior of the solution, especially for the solution based, neutron-induced fission production technique for Mo-99. During the first experiment performed in 2014, ANL’s 35 MeV electron linear accelerator provided average powers of 6, 12, and 15 kW using a rastered beam to homogeneously heat the 15 x 15 x 80-cm uranyl-sulfate solution. Gas bubble size, shape, velocity, solution temperature, and hydrogen and oxygen concentrations were recorded during the irradiations. The details of the experimental setup and results for the first experiment are described in the ANL reports, Design and Construction of Experiment for Direct Electron Irradiation of a Uranyl Sulfate Solution: Bubble Formation and Thermal Hydraulics Studies and Experimental Results for Direct Electron Irradiation of a Uranyl Sulfate Solution: Bubble Formation and Thermal Hydraulics Studies. The purpose of this report is to describe the issues and lessons learned associated with the first experiment and elaborate on designs to improve and obtain more accurate experimental results for the upcoming experiment.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Evaluation of the Impact of Additional Manganese from the Recycle Collection Tank (RCT) Glycolate Destruction Process on Glass Properties

The Defense Waste Processing Facility (DWPF) is planning to implement glycolic acid as a reductant within the waste processing flowsheet. An assessment of the glycolic acid flowsheet has revealed the potential for thermolytic production of hydrogen in the Concentration, Storage and Transfer Facilities (CSTF) from glycolate entrained in the DWPF recycle stream. To mitigate this potential scenario, a glycolate destruction process utilizing sodium permanganate (NaMnO 4 ) is being developed for use in the DWPF Recycle Collection Tank (RCT). The RCT is fed by the Slurry Mix Evaporator Condensate Tank (SMECT) and the Off-Gas Condensate Tank (OGCT). The SMECT could receive glycolate via a foamover from the Sludge Receipt and Adjustment Tank (SRAT) or the Slurry Mix Evaporator (SME), and the OGCT could receive glycolate via carryover of sludge particles in the purge from the melter during surge conditions. The use of NaMnO 4 additions in the RCT will result in additional manganese (Mn) in the waste stream and needs to be evaluated.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Evaluation of δ-Phase ZrH1.4 to ZrH1.7 Thermal Neutron Scattering Laws Using Ab Initio Molecular Dynamics Simulations

Zirconium hydride is commonly used for next-generation reactor designs due to its excellent hydrogen retention capacity at temperatures below 1000 K. These types of reactors operate at thermal neutron energies and require accurate representation of thermal scattering laws (TSLs) to optimize moderator performance and evaluate the safety indicators for reactor design. In this work, we present an atomic-scale representation of sub-stoichiometric ZrH2−x(0.3≤x≤0.6), which relies on ab initio molecular dynamics (AIMD) in tandem with velocity auto-correlation (VAC) analysis to generate phonon density of states (DOS) for TSL development. The novel NJOY+NCrystal tool, developed by the European Spallation Source community, was utilized to generate the TSL formulations in the A Compact ENDF (ACE) format for its utility in neutron transport software. First, stoichiometric zirconium hydride cross sections were benchmarked with experiments. Then sub-stoichiometric zirconium hydride TSLs were developed. Significant deviations were observed between the new δ-phase ZrH2−x TSLs and the TSLs in the current ENDF release. It was also observed that varying the hydrogen vacancy defect concentration and sites did not cause as significant a change in the TSLs (e.g., ZrH1.4 vs. ZrH1.7) as was caused by the lattice transformation from ϵ- to δ-phase.

42 ENGINEERING↗

Operating Characteristics of Metal Hydride-Based Solar Energy Storage Systems

Thermochemical energy storage systems, based on a high-temperature metal hydride coupled with a low-temperature metal hydride, represent a valid option to store thermal energy for concentrating solar power plant applications. The operating characteristics are investigated for a tandem hydride bed energy storage system, using a transient lumped parameter model developed to identify the technical performance of the proposed system. The results show that, without operational control, the system undergoes a thermal ratcheting process, causing the metal hydride concentrations to accumulate hydrogen in the high-temperature bed over time, and deplete hydrogen in the low temperature. This unbalanced system is compared with a ’thermally balanced’ system, where the thermal ratcheting is mitigated by thermally balancing the overall system. The analysis indicates that thermally balanced systems stabilize after the first few cycles and remain so for long-term operation, demonstrating their potential for practical thermal energy storage system applications.

25 ENERGY STORAGE↗

Scale-Up of Electrode Coating and Flow-Field for Commercial Hydrogen Peroxide Electrolyzer: Cooperative Research and Development Final Report, CRADA Number CRD-17-00687

Hydrogen peroxide is currently produced at central chemical plants via the anthraquinone oxidation process. This process produces environmental pollutants that are costly to remediate, requires hazardous long distance shipping of highly concentrated peroxide (50% or 70%), and necessitates extra handling costs related to storage and dilution. Peroxygen Systems, Inc. (PSi) is developing breakthrough technology for on-site hydrogen peroxide production. PSi’s on-site on-demand electrolyzer can reduce the cost of producing hydrogen peroxide by 50%, while also completely eliminating the cost and safety issues associated with shipping and handling of high concentration hydrogen peroxide. The challenge for PSi is scaling. To support the next step toward commercialization (customer pilot tests), scaling the prototype into larger single cells and 20-40 cell stacks is required. In addition to internal hardware and flow-field design efforts at PSi, NREL will address three critical problems for this scale-up effort: (1) demonstrating a large scale roll-to-roll (R2R) process to coat uniform electrode materials for 100 cm2 and 500 cm2 stack testing, (2) demonstrating an in-line diagnostic to achieve better electrode quality control, and (3) performing in situ cell/stack testing to better understand and optimize the performance of the flow field design.

28 EE - Advanced Manufacturing Office (EE-5A)↗

Sub-second and ppm-level optical sensing of hydrogen using templated control of nano-hydride geometry and composition

Abstract The use of hydrogen as a clean and renewable alternative to fossil fuels requires a suite of flammability mitigating technologies, particularly robust sensors for hydrogen leak detection and concentration monitoring. To this end, we have developed a class of lightweight optical hydrogen sensors based on a metasurface of Pd nano-patchy particle arrays, which fulfills the increasing requirements of a safe hydrogen fuel sensing system with no risk of sparking. The structure of the optical sensor is readily nano-engineered to yield extraordinarily rapid response to hydrogen gas (<3 s at 1 mbar H 2 ) with a high degree of accuracy (<5%). By incorporating 20% Ag, Au or Co, the sensing performances of the Pd-alloy sensor are significantly enhanced, especially for the Pd 80 Co 20 sensor whose optical response time at 1 mbar of H 2 is just ~0.85 s, while preserving the excellent accuracy (<2.5%), limit of detection (2.5 ppm), and robustness against aging, temperature, and interfering gases. The superior performance of our sensor places it among the fastest and most sensitive optical hydrogen sensors.

36 MATERIALS SCIENCE↗

A Thermogravimetric Temperature-Programmed Thermal Redox Protocol for Rapid Screening of Metal Oxides for Solar Thermochemical Hydrogen Production

As combinatorial and computational methods accelerate the identification of potentially suitable thermochemically-active oxides for use in solar thermochemical hydrogen production (STCH), the onus shifts to quickly evaluating predicted performance. Traditionally, this has required an experimental setup capable of directly carrying out a two-stage thermochemical water-splitting process. But this can be a difficult endeavor, as most off-the-shelf equipment cannot adequately deal simultaneously with the high temperatures, varying oxygen partial pressures, and high H 2 O partial pressures required; achieving sufficient temporal sensitivity to accurately quantify the kinetics is also a major challenge. However, as proposed here, a less complicated experiment can be used as a first screening for thermochemical water splitting potential. Temperature-Programmed Thermal Redox (TPTR) using thermogravimetry evaluates the thermal reduction behavior of materials. This technique does not require water splitting or CO 2 -splitting analogs but can nonetheless predict water-splitting performance. Three figures of merit are obtained from the TPTR experiment: reduction onset temperature, extent of reduction, and extent of recovery upon reoxidation. These metrics can collectively be used to determine if a material is capable of thermochemical water-splitting, and, to good approximation, predict whether the thermodynamics are favorable for use under more challenging high-conversion conditions. This paper discusses the pros and cons of using TPTR and proposes a protocol for use within the STCH community.

08 HYDROGEN↗

Experimental measurements of fuel and water crossover in an active DMFC

This work measured polarization curves as well as the high-frequency resistance of active direct methanol fuel cell (DMFC) operates at around 80 °C with active controls of temperature, methanol concentration, airflow rate, and relative humidity. The relative humidity of the air did not have noticeable impacts on the fuel cell unless the operating temperature was near the evaporation temperature of water (100 °C). The hydrophobic water management layer (WML) between the membrane electrode assembly (MEA) and cathode air channel increases the mass transfer resistance and improves the water retention in MEA. Adding a WML increased the peak power density, decreased the ohmic resistance, and improved the fuel efficiency of the fuel cell, especially when it operated near 100 °C. This study also quantitatively measured methanol and water crossover as well as the fuel efficiency at different operating currents. The fuel efficiency increased significantly with the increase of the current density. Using a hydrophobic fuel management layer (FML) between the anode fuel channel and MEA reduced the fuel and water crossover rates and increased the ohmic resistance due to the decrease of the water content of the Nafion membrane. The FML improved fuel efficiency by reducing the methanol crossover. The combination of the FML and WML enabled the steady operation of DMFC using highly concentrated methanol solutions (up to 75 wt%).

08 HYDROGEN↗

Full-Scale Hydrogen Mitigation Installation and Testing at Nevada Solar One

This project was performed under a Cooperative Research & Development Agreement (CRADA) between the National Renewable Energy Laboratory (NREL) and Acciona Energy USA (AE). The purpose was to advance an NREL TRL 3 technology that was developed during the previous CRADA from completed laboratory testing to full-scale process installation and testing at AE's Nevada Solar One (NSO) power plant. The project's objective was to complete full-scale implementation and performance verification of the NREL hydrogen mitigation technology at the Nevada Solar One (NSO) power plant in Boulder City, Nevada.

08 HYDROGEN↗

Heteroatom-Doped Graphenes as Actively Interacting 2D Encapsulation Media for Mg-Based Hydrogen Storage

Nanoencapsulation using graphene derivatives enables the facile fabrication of two-dimensional (2D) nanocomposites with unique microstructures and has been generally applied to many fields of energy materials. Particularly, metal hydrides such as MgH 2 encapsulated by graphene derivatives have emerged as a promising hybrid material for overcoming the disadvantageous properties of Mg-based hydrogen storage. Although the behavior of the graphene–Mg nanoencapsulation interface has been studied for many composite materials, the direct modification of graphene with nonmetal foreign elements for changing the interfacial behavior has been limitedly reported. In this regard, using B-doped graphene and N-doped graphene as nanoencapsulation media for tuning the interfacial behavior of graphene derivative–Mg nanoparticles, we present altered hydrogen storage kinetics of heteroatom-doped (B and N) graphene–Mg composites. The effect of heteroatom doping is studied in terms of bonding configurations and heteroatom doping concentrations. The enhancement in hydrogen uptake was observed for all of the heteroatom-doped graphene–Mg nanocomposites. On the other hand, a few samples exhibit significantly low activation energy at the early stage of desorption, which can be related to the facilitated nucleus formation. Density functional theory calculation indicates that B-doping and N-doping accelerate hydrogen absorption kinetics in different ways, aiding charge transfer and inducing surface deformation of Mg nanoparticles, respectively. Their effects can be augmented in the presence of structural defects on graphene, such as vacancies, pores, or graphene edges. These results demonstrate that hydrogen storage kinetics of Mg-based systems can be altered by utilizing heteroatom-doped graphene oxide derivatives as 2D nanoencapsulation media, suggesting that the addition of a nonmetal doping element can also be applied to Mg-based hydrogen storage by modifying the nanoencapsulation interface without forming Mg alloy phases.

08 HYDROGEN↗

A chemo-mechanical model for describing sorption hysteresis in a glassy polyurethane

Abstract Hysteretic sorption and desorption of water is observed from 0 to 95% relative humidity and 298–333 K on a glassy polyurethane foam. It is postulated that sorption-induced swelling of the glassy polyurethane increases the concentration of accessible hydrogen-bonding adsorption sites for water. The accessibility of sites is kinetically controlled due to the restricted thermal motions of chains in the glassy polymer, causing a difference in accessible site concentrations during sorption and desorption. This discrepancy leads to hysteresis in the sorbed concentrations of water. A coupled chemo-mechanical model relating volumetric strain, adsorption site concentration, and sorbed water concentration is employed to describe water sorption hysteresis in the glassy polyurethane. This model not only describes the final mass uptake for each relative humidity step, but also captures the dynamics of water uptake, which exhibit diffusion and relaxation rate-controlled regimes.

36 MATERIALS SCIENCE↗