Hydrogen environment embrittlement of metals

Hydrogen environment embrittlement refers to metals stressed while exposed to a hydrogen atmosphere. Tested in air, even after exposure to hydrogen under pressure, this effect is not observed on similar specimens. Much high purity hydrogen is prepared by evaporation of liquid hydrogen, and thus has low levels for potential impurities which could otherwise inhibit or poison the absorbent reactions that are involved. High strength steels and nickel-base allows are rated as showing extreme embrittlement; aluminum alloys and the austenitic stainless steels, as well as copper, have negligible susceptibility to this phenomenon. The cracking that occurs appears to be a surface phenomenon, is unlike that of internal hydrogen embrittlement.

Jewett, R. P.↗

Vacuum thermal-mechanical fatigue behavior of two iron-base alloys

The present study extends the concept of in-phase grain boundary ratcheting to two iron-base alloys (Type 304 stainless steel and A286 alloy) and provides a clearer interpretation of out-of-phase grain boundary ratcheting effects observed in the A286 alloy which does not exhibit geometric instability. Elevated-temperature low-cycle thermal-mechanical fatigue tests in an ion-pumped ultrahigh vacuum chamber revealed significant effects of frequency and combined temperature-strain cycling on fatigue life. In-phase thermal cycling (tension at high temperature and compression at low temperature) caused large life reductions in both materials due to grain boundary cavitation caused by unreversed grain boundary sliding (grain boundary ratcheting). Out-of-phase thermal cycling (tension at low temperature and compression at high temperature) also caused large cyclic life reductions in both materials. In the A286 alloy, out-of-phase life reductions are attributed to compressive ratcheting.

Sheffler, K. D.↗

Acidic Gas Reduction For Residential Natural Gas Furnace

The United States has more than 119 million homes, and 47% of them rely on natural gas as their primary heating fuel. However, most U.S. homes still use noncondensing units with an annual fuel utilization efficiency (AFUE) of ~80%, rather than efficient condensing furnaces. This is due to the high cost of condensing furnaces, which usually use expensive corrosion resistant super-ferritic stainless steel alloy heatexchangers (HX) to avoid corrosion and fouling acid condensation, along with the cost and difficulty of retrofitting the venting used by the replaced furnace. Here, this article discusses a low-cost acidic gas reduction (AGR) catalyst technology that enables a novel condensing natural gas furnace with an ultraclean (i.e., nearly zero) flue gas and neutral condensate that is environmentally friendly.

03 NATURAL GAS↗

Constitutive model development of aluminum alloy 1100 for elevated temperature forming process

Commercially pure aluminum alloy, AA1100, presents good electrical and thermal conductivity, high formability, and low cost. Those favorable characteristics have the potential to enable bipolar plates with improved economics and enhanced performance compared to current stainless steel bipolar plates for proton exchange membrane fuel cells. An accurate constitutive model is essential to develop and optimize processing parameters and effectively control the forming process. Here, the objective of this work is to develop a constitutive model of AA1100 that is able to simulate stress-strain relation, formed geometry, and predict the onset of fracture strain to avoid forming failure. Initially, a set of tensile tests at temperature between 300 and 500°C and strain rate between 0.005 and 1.0/s were conducted to examine the deformation behavior. Then, a set of damage-based unified visco-plastic constitutive equations is proposed and calibrated based on the results of stress-strain data. A genetic algorithm optimization method is applied to search for best fitting material constants in constitutive equations. The proposed model shows good predictability of both the stress-strain relation and fracture strain at low strain rate and high temperature conditions. The accuracy of proposed model is also evaluated statistically. A comparison of the proposed model with three popular models (Arrhenius-type mode, Johnson-Cook model and Zerilli-Armstrong model) was made. The proposed model shows the best experimental agreement with correlation coefficient of 0.96 in contrast to 0.25, 0.38 and 0.75 for the popular models, respectively. The proposed model can help to optimize the elevated temperature forming process and guide die design to enable optimal geometric features in the formed components.

08 HYDROGEN↗

Machine-learning-aided density functional theory calculations of stacking fault energies in steel

A combined large-scale first principles approach with machine learning and materials informatics is proposed to quickly sweep the chemistry-composition space of advanced high strength steels (AHSS). AHSS are composed of iron and key alloying elements such as aluminum and manganese. A systematic exploration of the distribution of aluminum and manganese atoms in iron is used to investigate low stacking fault energies configurations using first principles calculations. To overcome the computational cost of exploring the composition space, this process is sped up using an automated machine learning tool: DeepHyper. Here our results predict that it is energetically favorable for Al to stay away from a stacking fault, but Mn atoms do not affect the stacking fault energy and can stay in the vicinity of the fault. The distribution of Al and Mn atoms in systems containing stacking faults and the effects of their interactions on the equilibrium distribution are systematically analyzed.

36 MATERIALS SCIENCE↗

Fundamental Studies of Tritium Diffusivity in Pure and Defective Zircaloy-4 Getters (Tritium Science Program FY2020 Report)

Zirconium (Zr) alloys are extensively used as tritium (T) getters in nuclear reactors due to their low absorption cross section to thermal neutron, good mechanical properties at high temperature and resistant to corrosion in different environmental conditions. Zr alloys have better thermal properties than many other refractory alloys including stainless steel. The nuclear characteristic is simulated, and T is produced in tritium-producing burnable absorber rods (TPBAR) by the irradiation of neutron flux in pressurized water reactor (PWR). T thus produced diffuses through the pellets and is captured by the getter where it chemically reacts with Zr to form metal hydride (ZrTx). These hydrides are brittle and affect adversely the mechanical properties of alloys. In addition to that, mismatch in the lattice structures after hydride formation creates a stress which needs to be considered in component design and their life evaluation. Therefore, understanding the behavior of T and its species becomes significant as fuel burnup is increased, which leads to increase in hydrogen pickup and oxide formation. The transport of T and its species in pure Zr alloys, and in alloys with certain alloying elements and defects are important to understand in order to enhance the performance of the materials.

36 MATERIALS SCIENCE↗

Low carbon steel: Metallurgical structure vs. mechanical properties

The objective is to provide a low cost, simple experiment for either demonstration purposes or as a laboratory experiment that will teach the student the importance of the thermal-mechanical history of a metallic alloy in determining that material's mechanical behavior. Hairpins are subjected to various treatments. The experimental equipment and procedures are discussed.

Shull, Robert D.↗

Regenerator seal

A method for manufacturing a hot side regenerator cross arm seal assembly having a thermally stablilized wear coating with a substantially flat wear surface thereon to seal between low pressure and high pressure passages to and from the hot inboard side of a rotary regenerator matrix includes the steps of forming a flat cross arm substrate member of high nickel alloy steel; fixedly securing the side edges of the substrate member to a holding fixture with a concave surface thereacross to maintain the substrate member to a slightly bent configuration on the fixture surface between the opposite ends of the substrate member to produce prestress therein; applying coating layers on the substrate member including a wear coating of plasma sprayed nickel oxide/calcium flouride material to define a wear surface of slightly concave form across the restrained substrate member between the free ends thereon; and thereafter subjecting the substrate member and the coating thereon to a heat treatment of 1600.degree. F. for sixteen hours to produce heat stabilizing growth in the coating layers on the substrate member and to produce a thermally induced growth stress in the wear surface that substantially equalizes the prestress in the substrate whereby when the cross arm is removed from the fixture surface following the heat treatment step a wear face is formed on the cross arm assembly that will be substantially flat between the ends.

Davis, Leonard C.↗

Binder Jet Additive Manufacturing Process and Material Characterization for High Temperature Heat Exchangers Used in Concentrated Solar Power Applications

The U.S. Department of Energy’s (DOE) Sunshot 2030 initiative has a goal of reducing the cost of concentrating solar power (CSP) to 5 cents per kWh for baseload power plants. One of the potential pathways to this goal includes a reduction in the cost of the supercritical CO2 (sCO2) power block to 0.9 cents per kWh. Recuperators—high and low temperatures, used in the sCO2 power cycle, contribute to >50% of the cost of the power cycle. This work studies the feasibility towards a ≥10% cost reduction for High Temperature Recuperators (HTR) used in the sCO2 power cycle. One way to address the cost reduction is by leveraging low-cost additive manufacturing, specifically, Binder Jet Additive Manufacturing (BJAM) to 3D print HTRs at scale. This study focuses on the development of a BJAM process towards 3D printing HTR cores using Stainless Steel alloy 316L (SS316L). To evaluate the suitability of the BJ process towards the HTR, high level specifications of the application are translated to materials capability requirements. Subsequently, at-temperature materials testing is conducted on as-printed and sintered additively manufactured coupons. Data from the coupons are compared against cast and wrought SS316L data obtained from the literature. Results show that the tensile properties from the BJ process compare well against cast properties. Furthermore, a baseline analysis of creep testing data is established for the BJ process, and insights are drawn from the results towards future improvements of the process.

14 SOLAR ENERGY↗

Corrosion-resistant amorphous metallic films of Mo49Cr33B18 alloy

Corrosion-resistant amorphous metallic alloy films of Mo49Cr33B18 with a crystallization temperature of 590 C were deposited onto glass and quartz substrates by magnetron sputter-quench technique. The amorphous nature of the films was confirmed by their diffuse X-ray diffraction patterns. The deposited films are densely packed (zone T) and exhibit low stress and good adhesion to the substrate. Corrosion current of as-deposited coating of MoCrB amorphous metallic alloy is approximately three orders of magnitude less than the corrosion current of 304 stainless steel in 1N H2SO4 solution.

Ramesham, R.↗

Design and Manufacturing Considerations for Shockproof and Corrosion-Immune Superelastic Nickel-Titanium Bearings for a Space Station Application

An intermetallic nickel-titanium alloy, 60NiTi (60wt%Ni, 40wt%Ti), is a promising tribological material for space mechanisms. 60NiTi offers a broad combination of physical properties that make it unique among bearing materials. 60NiTi is hard, electrically conductive, highly corrosion resistant, readily machined prior to final heat treatment, easily lubricated and is non-magnetic. It also falls within the class of superelastic alloys and can elastically endure large strains (beyond 5 percent) making it highly resistant to excessive and unexpected (shock) loads. Key material properties and characteristics such as elastic modulus, tensile fracture sensitivity and residual stress behavior, however, differ from conventional alloys such as steel and this significantly affects bearing design and manufacturing. In this paper, the preliminary design and manufacture of ball bearings made from 60NiTi are considered for a highly corrosive, lightly loaded, low speed bearing application found inside the International Space Station s water recycling system. The information presented is expected to help guide more widespread commercialization of this new technology into space mechanism and other applications.

DellaCorte, Christopher↗

Stress-controlled fatigue of HfNbTaTiZr high-entropy alloy and associated deformation and fracture mechanisms

The stress-controlled fatigue tests are carried out at a stress ratio of 0.1 and a frequency of 10 Hz, and span both low-cycle and high-cycle regimes by varying the applied stress amplitudes. The high-cycle fatigue regime gives a fatigue strength of 497 MPa and a fatigue ratio of 0.44. At equivalent conditions, the alloy's fatigue strength is greater than all other high-entropy alloys (HEAs) with reported high-cycle fatigue data, dilute body-centered cubic alloys, and many structural alloys such as steels, titanium alloys, and aluminum alloys. Through in-depth analyses of crack-propagation trajectories, fracture-surface morphologies and deformation plasticity by means of various microstructural analysis techniques and theoretical frameworks, the alloy's remarkable fatigue resistance is attributed to delayed crack initiation in the high-cycle regime, which is achieved by retarding the formation of localized persistent slip bands, and its good resistance to crack propagation in the low-cycle regime, which is accomplished by intrinsic toughening backed up by extrinsic toughening. Additionally, the stochastic nature of the fatigue data is neatly captured with a 2-parameter Weibull model.

36 MATERIALS SCIENCE↗

Spectral Emittance of Uncoated and Ceramic-Coated Inconel and Type 321 Stainless Steel

The normal spectral emittance of Inconel and type 321 stainless steel with different surface treatments was measured at temperatures of 900, 1,200, 1,500, and 1,800 F over a wavelength range of 1.5 to 15 microns. The measurements involved comparison of the radiant energy emitted by the heated specimen with that emitted by a comparison standard at the same temperature by means of a recording double-beam infrared spectrophotometer. The silicon carbide comparison standard had previously been calibrated against a laboratory black-body furnace. Surface treatments included electropolishing, sandblasting, electro-polishing followed by oxidation in air for 1/2 hour at 1,800 F, sandblasting followed by oxidation in air for 1/2 hour at 1,800 F, application of National Bureau of Standards coating A-418, and application of NBS ceramic coating N-143. The normal spectral emittance of both alloys in the electropolished condition was low and decreased very slightly with increasing wavelength while in the sandblasted condition it was somewhat higher and did not vary appreciably with wavelength. The oxidation treatment greatly increased the normal spectral emittance of both the electropolished and sandblasted type 321 stainless steel specimens and of the electropolished Inconel specimens and introduced some spectral selectivity into the curves. The oxidation increased the normal spectral emittance of the sandblasted Inconel specimens only moderately. Of the specimens to which a coating about 0.002 inch thick was applied, those coated with A-418 had higher emittance at all wavelengths than did those coated with N-143, and the coated specimens of Inconel had higher spectral emittance at all wavelengths than did the corresponding specimens of type 321 stainless steel. Both coatings were found to be partially transparent to the emitted energy at this thickness but essentially opaque at a thickness of 0.005 inch. Coated specimens with 0.005 inch or more of coating did not show the effect of the underlying metal on spectral emittance, and there was no significant difference at wavelengths greater than about five microns in the normal spectral emittance of specimens having the two coatings. At shorter wavelengths the normal spectral emittance of specimens coated with A-418 was greater than that of specimens coated with N-143.

Richmond, Joseph C.↗

Brazing Dissimilar Metals

Brazing effective technique for joining ordinary structural metals to brittle, low-thermal-expansion refractory metals. Specifically, brazing process established for joining copper or nickel flanges to ends of vacuum-plasma-sprayed tungsten tubes and for joining stainless-steel flanges to ends of tubes made of alloy of molybdenum with 40 percent of rhenium.

Krotz, Phillip D.↗

Influence of stacking fault energy and hydrogen on deformation mechanisms in high Mn austenitic steels during in-situ tensile testing

High Mn austenitic steels are considered an economical alloy system for hydrogen storage and transport applications. This study used stacking fault energy (SFE) as a design parameter to achieve hydrogen embrittlement (HE)-resistant high Mn austenitic alloys. The role of hydrogen on the deformation mechanisms of low (29 mJ/m 2 ) and high SFE (49 mJ/m 2 ) alloys was evaluated through in-situ neutron diffraction during tensile loading. Hydrogen-precharging increased yield strength, partly due to hydrogen-induced lattice distortion (i.e., solute strengthening). Hydrogen accelerated the increase in defect density, including dislocations and stacking faults. The formation of planar deformation structures (twins and stacking faults), relative to dislocations, plays a critical role in promoting hydrogen-assisted fracture. The stacking fault frequency parameter obtained from neutron diffraction quantifies planar deformation tendencies, correlated with HE sensitivity. The higher SFE alloy exhibited greater resistance to HE, associated with the reduced propensity to form stacking faults and twins upon deformation in the hydrogen-precharged condition.

High Mn austenitic steel↗

Miniature High-Force, Long-Stroke SMA Linear Actuators

Improved long-stroke shape-memory-alloy (SMA) linear actuators are being developed to exert significantly higher forces and operate at higher activation temperatures than do prior SMA actuators. In these actuators, long linear strokes are achieved through the principle of displacement multiplication, according to which there are multiple stages, each intermediate stage being connected by straight SMA wire segments to the next stage so that relative motions of stages are additive toward the final stage, which is the output stage. Prior SMA actuators typically include polymer housings or shells, steel or aluminum stages, and polymer pads between successive stages of displacement-multiplication assemblies. Typical output forces of prior SMA actuators range from 10 to 20 N, and typical strokes range from 0.5 to 1.5 cm. An important disadvantage of prior SMA wire actuators is relatively low cycle speed, which is related to actuation temperature as follows: The SMA wires in prior SMA actuators are typically made of a durable nickel/titanium alloy that has a shape-memory activation temperature of 80 C. An SMA wire can be heated quickly from below to above its activation temperature to obtain a stroke in one direction, but must then be allowed to cool to somewhat below its activation temperature (typically, less than or equal to 60 C in the case of an activation temperature of 80 C) to obtain a stroke in the opposite direction (return stroke). At typical ambient temperatures, cooling times are of the order of several seconds. Cooling times thus limit cycle speeds. Wires made of SMA alloys having significantly higher activation temperatures [denoted ultra-high-temperature (UHT) SMA alloys] cool to the required lower return-stroke temperatures more rapidly, making it possible to increase cycle speeds. The present development is motivated by a need, in some applications (especially aeronautical and space-flight applications) for SMA actuators that exert higher forces, operate at greater cycle speeds, and have stronger housings that can withstand greater externally applied forces and impacts. The main novel features of the improved SMA actuators are the following: 1) The ends of the wires are anchored in compact crimps made from short steel tubes. Each wire end is inserted in a tube, the tube is flattened between planar jaws to make the tube grip the wire, the tube is compressed to a slight U-cross-section deformation to strengthen the grip, then the crimp is welded onto one of the actuator stages. The pull strength of a typical crimp is about 125 N -- comparable to the strength of the SMA wire and greater than the typical pull strengths of wire-end anchors in prior SMA actuators. Greater pull strength is one of the keys to achievement of higher actuation force; 2) For greater strength and resistance to impacts, housings are milled from aluminum instead of being made from polymers. Each housing is made from two pieces in a clamshell configuration. The pieces are anodized to reduce sliding friction; 3) Stages are made stronger (to bear greater compression loads without excessive flexing) by making them from steel sheets thicker than those used in prior SMA actuators. The stages contain recessed pockets to accommodate the crimps. Recessing the pockets helps to keep overall dimensions as small as possible; and, 4) UHT SMA wires are used to satisfy the higher-speed/higher-temperature requirement.

Cummin, Mark A.↗

A probabilistic creep model incorporating test condition, initial damage, and material property uncertainty

Uncertainty is prevalent in the creep resistance of alloys, where at elevated temperature and low pressure, rupture can range across logarithmic decades. In this study, a probabilistic continuum-damage-mechanics (CDM)-based model is derived to capture the uncertainty of creep resistance. To meet this objective, creep data for alloy 304 Stainless Steel is gathered. A constitutive model, “Sinh”, is calibrated deterministically to determine the statistical variability of the material properties. Three sources of uncertainty are injected into the model: test condition (stress and temperature), initial damage, and material properties. Probabilistic simulations are carried out by (a) calibrating probability distribution functions (pdfs) for each source of uncertainty (b) randomly sampling the pdfs using Monte Carlo methods and (c) executing simulations to replicate the uncertain creep behavior. A sensitivity analysis is performed to evaluate the relative effect of each source of uncertainty. In full probabilistic simulations, the cumulative uncertainty of creep behavior is evaluated. The probabilistic model accurately predicts the creep deformation and rupture of the available experiments. The probabilistic model is validated for interpolation but lacks extrapolation ability. Several future works are proposed to further improve the model.

36 MATERIALS SCIENCE↗

The problem of dimensional instability in airfoil models for cryogenic wind tunnels

The problem of dimensional instability in airfoil models for cryogenic wind tunnels is discussed in terms of the various mechanisms that can be responsible. The interrelationship between metallurgical structure and possible dimensional instability in cryogenic usage is discussed for those steel alloys of most interest for wind tunnel model construction at this time. Other basic mechanisms responsible for setting up residual stress systems are discussed, together with ways in which their magnitude may be reduced by various elevated or low temperature thermal cycles. A standard specimen configuration is proposed for use in experimental investigations into the effects of machining, heat treatment, and other variables that influence the dimensional stability of the materials of interest. A brief classification of various materials in terms of their metallurgical structure and susceptability to dimensional instability is presented.

Wigley, D. A.↗