Search NASA⌕ Search

SEARCH · Search NASA

Results for “MATERIALS EROSION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Electrode erosion in arc discharges at atmospheric pressure

An experimental investigation was performed in an effort to measure and increase lifetime of electrodes in an arcjet thruster. The electrode erosion of various anode and cathode materials was measured after tests in an atmospheric pressure nitrogen arc discharge at powers less than 1 kW. A free-burning arc configuration and a constricted arc configuration were used to test the materials. Lanthanum hexboride and thoriated tungsten had low cathode erosion rates while thoriated tungsten and pure tungsten had the lowest anode erosion rates of the materials tested. Anode cooling, reverse gas flow, an external magnetic fields were all found to reduce electrode mass loss.

Hardy, T. L.↗

Laser supported detonation wave source of atomic oxygen for aerospace material testing

A pulsed high-flux source of nearly monoenergetic atomic oxygen was developed to perform accelerated erosion testing of spacecraft materials in a simulated low-earth orbit (LEO) environment. Molecular oxygen is introduced into an evacuated conical expansion nozzle at several atmospheres pressure through a pulsed molecular beam valve. A laser-induced breakdown is generated in the nozzle throat by a pulsed CO2 TEA laser. The resulting plasma is heated by the ensuing laser-supported detonation wave, and then it rapidly expands and cools. An atomic oxygen beam is generated with fluxes above 10 to the 18th atoms per pulse at 8 + or - 1.6 km/s with an ion content below 1 percent for LEO testing. Materials testing yielded the same surface oxygen enrichment in polyethylene samples as observed on the STS mission, and scanning electron micrographs of the irradiated polymer surfaces showed an erosion morphology similar to that obtained on low earth orbit.

Krech, Robert H.↗

Ground-Laboratory to In-Space Atomic Oxygen Correlation for the Polymer Erosion and Contamination Experiment (PEACE) Polymers

The Materials International Space Station Experiment 2 (MISSE 2) Polymer Erosion and Contamination Experiment (PEACE) polymers were exposed to the environment of low Earth orbit (LEO) for 3.95 years from 2001 to 2005. There were 41 different PEACE polymers, which were flown on the exterior of the International Space Station (ISS) in order to determine their atomic oxygen erosion yields. In LEO, atomic oxygen is an environmental durability threat, particularly for long duration mission exposures. Although spaceflight experiments, such as the MISSE 2 PEACE experiment, are ideal for determining LEO environmental durability of spacecraft materials, ground-laboratory testing is often relied upon for durability evaluation and prediction. Unfortunately, significant differences exist between LEO atomic oxygen exposure and atomic oxygen exposure in ground-laboratory facilities. These differences include variations in species, energies, thermal exposures and radiation exposures, all of which may result in different reactions and erosion rates. In an effort to improve the accuracy of ground-based durability testing, ground-laboratory to in-space atomic oxygen correlation experiments have been conducted. In these tests, the atomic oxygen erosion yields of the PEACE polymers were determined relative to Kapton H using a radio-frequency (RF) plasma asher (operated on air). The asher erosion yields were compared to the MISSE 2 PEACE erosion yields to determine the correlation between erosion rates in the two environments. This paper provides a summary of the MISSE 2 PEACE experiment; it reviews the specific polymers tested as well as the techniques used to determine erosion yield in the asher, and it provides a correlation between the space and ground laboratory erosion yield values. Using the PEACE polymers asher to in-space erosion yield ratios will allow more accurate in-space materials performance predictions to be made based on plasma asher durability evaluation.

Stambler, Arielle H.↗

Angular particle impingement studies of thermoplastic materials at normal incidence

Scanning electron microscope studies were conducted to characterize the erosion resistance of polymethyl methacrylate (PMMA), polycarbonate (PC), polytetrafluorethylene (PTFE), and ultra-high-molecular-weight polyethylene (UHMWPE). Erosion was caused by a jet of angular microparticles of crushed glass at normal incidence. Material built up above the original surface on all of the materials. As erosion progressed, this buildup disappeared. UHMWPE was the most resistant material and PMMA the least. The most favorable properties for high erosion resistance were high values of ultimate elongation, maximum service temperature, and strain energy and a low value of the modulus of elasticity. Erosion-rate-versus-time curves of PC and PTFE exhibited incubation, acceleration, and steady-state periods. PMMA also exhibited a deceleration period, and an incubation period with deposition was observed for UHMWPE.

Rao, P. V.↗

Ground-Laboratory to In-Space Effective Atomic-Oxygen Fluence Determined for DC 93-500 Silicone

Surfaces on the leading edge of spacecraft in low Earth orbit (e.g., surface facing the velocity direction), such as on the International Space Station, are subject to atomic oxygen attack, and certain materials are susceptible to erosion. Therefore, ground-based laboratory testing of the atomic oxygen durability of spacecraft materials is necessary for durability assessment when flight data are not available. For accurate space simulation, the facility is commonly calibrated on the basis of the mass loss of Kapton (DuPont, Wilmington, DE) as a control sample for effective fluence determination. This is because Kapton has a well-characterized atomic oxygen erosion yield (E(sub y), in cubic centimeters per atom) in the low Earth orbit (LEO) environment. Silicones, a family of commonly used spacecraft materials, do not chemically erode away with atomic oxygen attack like other organic materials that have volatile oxidation products. Instead, silicones react with atomic oxygen and form an oxidized hardened silicate surface layer. Often the loss of methyl groups causes shrinkage of the surface skin and "mud-tile" crazing degradation. But silicones often do not lose mass, and some silicones actually gain mass during atomic oxygen exposure. Therefore, the effective atomic oxygen fluence for silicones in a ground-test facility should not be determined on the basis of traditional mass-loss measurements, as it is with polymers that erode. Another method for determining effective fluence needs to be employed for silicones. A new technique has been developed at the NASA Glenn Research Center for determining the effective atomic oxygen fluence for silicones in ground-test facilities. This technique determines the equivalent amount of atomic oxygen oxidation on the basis of changes in the surface-oxide hardness. The specific approach developed was to compare changes in the surface hardness of ground-laboratory-exposed DC93-500 silicone with DC93-500 exposed to LEO atomic oxygen as part of a shuttle flight experiment. The on-the-ground to in-space effective atomic oxygen fluence was determined on the basis of the Kapton effective fluence in the ground-laboratory facility that produced the same hardness for the fluence in space.

deGroh, Kim K.↗

Falling particle impact erosion testing for particle based CSP systems

CSP systems are currently being examined as an effective method for using solar energy to generate electricity. While much of this research has been conducted using molten salt as the heat transfer medium, in recent years, solid particles have been posited as a cheaper and more energy efficient heat transfer medium for use in CSP systems. Many researchers have looked into the effectiveness of solid particles as a heat transfer medium. However, a concern with the use of particles is that the falling particles will impact various components within the CSP system, such as the hopper, the heat exchanger, and the insulating material, resulting in surface erosion and damage. With repeated impacts from falling particles, material from the surfaces under impact is removed. The degree of erosion depends on whether the substrate is made of brittle or ductile material. Furthermore, factors such as particle shape, size, hardness, concentration, impact angle, particle velocity, and substrate hardness will contribute to the erosion process and determine how much and how quickly erosion will takes place in a system. Three types of erosion will be observed simultaneously: impact erosion from particle impact on receiver, particle storage, and heat exchanger walls, abrasion erosion from particle sliding motion along walls, and attrition erosion as the particles breakdown from particle-to-particle contact and particle-to-wall interactions. It is imperative to understand each of these erosions individually for a more comprehensive understanding and prediction of CSP system durability. In this work, we developed an experimental test setup capable of measuring impact erosion at conditions relevant to 1MW CSP plant. Subsequently, Impact erosion measurements were performed for three different candidate substrate materials at low particle velocities using HSP 40/70 ceramic particles.

14 SOLAR ENERGY↗

Anthropogenic Influences on the Chemical and Mineral Composition in Pond Sediment by X-Ray Absorption Spectroscopy and X-Ray Powder Diffraction

Manmade detention ponds have historically been impacted by anthropogenic activities such as rainwater runoff, car emissions, and drainage from infrastructures, which can lead to complications for pond ecosystems. Sediment samples collected from the northern, southern, western, and eastern regions of a small pond on a suburban high school campus on Long Island, NY, were analyzed for potential chemical changes resulting from an inundation of water by a broken water main. Incorporating synchrotron X-ray techniques, sediment was analyzed using Submicron Resolution Spectroscopy, Tender Energy X-ray Spectroscopy, and X-ray Powder Diffraction to examine heavy metals, light elements, and minerals. Results include a Zn:Cu ratio increase from 4:1 to 10:1 in the eastern zone and a higher heavy metal presence in the western zone for all elements examined, with greater distribution throughout the pond post-inundation. Lighter elements appear to remain relatively unchanged. The appearance of diopside in the eastern zone post-inundation samples suggests contamination from the water main break, while the presence of carbonate minerals in the western zone is consistent with erosion of asphalt material from the adjacent parking lot.

54 ENVIRONMENTAL SCIENCES↗

Rocket engine nozzle photographic system

Protective enclosure for a camera, located on the exhaust stream of a rocket engine, permits continuous recording of erosion processes of materials used in nozzle throat structures. The system uses a standard camera in a water-cooled, pressurized enclosure having a unique, inert gas-swept viewing duct.

Bailey, R. L.↗

Solutions for discharge chamber sputtering and anode deposit spalling in small mercury ion thrusters

Proposed solutions to the problems of sputter erosion and sputtered material spalling in the discharge chamber of small mercury ion thrusters are presented. The accelerated life test evaluated three such proposed solutions: (1) the use of tantalum as a single low sputter yield material for the exposed surfaces of the discharge chamber components subject to sputtering, (2) the use of a severely roughened anode surface to improve the adhesion of the sputter-deposited coating, and (3) the use of a wire cloth anode surface in order to limit the size of any coating flakes which might spall from it. Because of the promising results obtained in the accelerated life test with anode surfaces roughened by grit-blasting, experiments were carried out to optimize the grit-blasting procedure. The experimental results and an optimal grit-blasting procedure are presented.

Power, J. L.↗

Mechanistic studies of polymeric samples exposed aboard STS 8

The early Shuttle flights and the attendant opportunity to deploy material samples to the near-Earth space environment, along well-defined trajectories and accompanied by detailed characterization of these samples prior to and following the flight exposure, have brought to light several novel phenomena associated with interaction of these materials with the space environment. JPL, in coordination with other NASA Centers, has carried out a research program to study the degradation and oxidation processes caused by interaction of these materials with atomic oxygen at an energy of 5 eV. In addition, energetic atomic oxygen is believed to be responsible for the shuttle glow first observed during the flight of STS-3. The shuttle glow phenomenon has been extensively studied and modeled because of its long-range potential impact on optical communication schemes and its more immediate impact on the Space Telescope. This report summarizes the results of certian material degradation and erosion experiments carried out aboard STS-8 between August 30, 1983 and September 5, 1983. Based on these data, a generic degradation model has been developed for common structural polymers.

Liang, Ranty H.↗

Weathering of basaltic rocks under cold, arid conditions - Antarctica and Mars

The processes taking part in the chemical weathering of nonvesicular dolerite cobbles producing etch pits and secondary minerals including clays, under cold arid conditions of high-altitude ice-free areas of Victoria Land (Antarctica) are investigated as a possible analog to processes that produced the pitted rocks and clay minerals on Mars. Results suggest that the pits in the dolerite cobbles are formed by the dissolution of the rock by rare snow-melt water during the austral summer, followed by wind erosion of weathered material. The upper interior walls of the pits are lined with a yellow precipitate consisting of illite and quartz mixture, while the pit bottoms contain alteration products including Fe-rich clay minerals and soluble salts. A model is proposed for rock pitting on Mars analogous to that of the Antarctic dolerites.

Allen, C. C.↗

The Zhamanshin impact feature: A new class of complex crater?

The record of 10-km-scale impact events of Quaternary age includes only two 'proven' impact structures: the Zhamanshin Impact Feature (ZIF) and the Bosumtwi Impact Crater (BIC). What makes these impact landforms interesting from the standpoint of recent Earth history is their almost total lack of morphologic similarity, in spite of similar absolute ages and dimensions. The BIC resembles pristine complex craters on the Moon to first order (i.e., 'U'-shaped topographic cross section with preserved rim), while the ZIF displays virtually none of the typical morphologic elements of a 13- to 14-km-diameter complex crater. Indeed, this apparent lack of a craterlike surficial topographic expression initially led Soviet geologists to conclude that the structure was only 5.5 to 6 km in diameter and at least 4.5 Ma in age. However, more recent drilling and geophysical observations at the ZIF have indicated that its pre-erosional diameter is at least 13.5 km, and that its age is most probably 0.87 Ma. Why the present topographic expression of a 13.5-km complex impact crater less than 1 m.y. old most closely resembles heavily degraded Mesozoic shield craters such as Lappajarvi is a question of considerable debate. Hypotheses for the lack of a clearly defined craterlike form at the ZIF include a highly oblique impact, a low-strength 'cometary' projectile, weak or water-saturated target materials, and anomalous erosion patterns. The problem remains unresolved because typical erosion rates within the arid sedimentary platform environment of central Kazakhstan in which the ZIF is located are typically low; it would require at least a factor of 10 greater erosion at the ZIF in order to degrade the near-rim ejecta typical of a 13.5-km complex crater by hundreds of meters in only 0.87 Ma, and to partially infill an inner cavity with 27 cu km (an equivalent uniform thickness of infill of 166 m). Our analysis of the degree of erosion and infill at the ZIF calls for rates in the 0.19 to 0.38 mm/yr range over the lifetime of the landform, which are a factor of 10 to 20 in excess of typical rates for the Kazakhstan semidesert.

Garvin, J. B.↗

Subscale Injector Testing to Support J-2X Engine Development

The J-2X engine being pursued for the Ares I will be a derivative of the J-2 engine developed by Pratt & Whitney Rocketdyne (PWR). As part of the engine development, a subscale injector was fabricated by PWR and hot-fire tested at NASA s Marshall Space Flight Center (MSFC) to evaluate performance data. This subscale injector had a reduced injector diameter and fewer elements than the full scale design, but the element density (#elements / injector area), and element geometries nearly identical to the full scale design. Three different materials were used for the LOX posts in order to test for durability. The subscale injector included 46 standard elements and 6 baffle elements, corresponding to the ratio of baffled elements to core elements in the full scale design. The baffle elements were included to demonstrate thermal compatibility of the baffles and to more closely represent the full scale performance. Fifteen hot-fire tests were conducted totaling over 200 seconds of mainstage time on the injector. Chamber pressures with oxygen/hydrogen propellants ranged from 870-1380 psig with mixture ratios ranging from 4.8-6.1. Fuel manifold inlet temperatures were varied from 190 to 300 R. Modular, water cooled, calorimeter chamber assemblies were used to provide heating rate data and evaluate the effects of characteristic length (L*). Performance was evaluated relative to the resulting characteristic velocity (C*) efficiency. Performance met the value required in order to proceed with this design for the full scale hardware. Hardware inspections show no evidence of cracking at the tip of the LOX post for any of the materials tested. Minor erosion of the baffle element tips was observed in the early testing. A design change was quickly implemented and tested, and this change resolved the issue. Development of the J-2X is continuing with this element density and design.

Protz, Christopher↗

Development of a Model for the Small-Particle Orbital Debris Population Based on the STS Impact Record

In preparation for the release of the Orbital Debris Engineering Model (ORDEM) version 3.1, the NASA Orbital Debris Program Office (ODPO) revisited how orbiting debris populations of characteristic sizes smaller than 1 cm were modeled. The primary contributor to the population of sub-centimeter debris particles is the surface deterioration or erosion of spacecraft materials exposed to the outer-space environment. Because small particulates are not directly trackable by remote sensing, the primary means of detection is via historical counts of small impact features on flown radiator and window surfaces of the U.S. Space Transportation System (STS, also known as the Space Shuttle) from 1995-2011. Historic NASA studies of high-velocity impact tests have related impact-feature size to particle mass and velocity for certain STS surfaces, so that a corresponding particle size may be inferred from each small-impact feature observed. Micro-debris populations are then estimated by modeling the path and orientation of an STS mission through a simulated debris environment, and the densities of this simulated environment are rescaled to approximate the number of observed STS impact features. Monte-Carlo methods are further employed to gauge the estimation uncertainty of the rescaled environment. A description of the chosen methodologies for estimating and adjusting the micro-debris population model, and the results, are presented.

Seago, J..↗

A Comparison of Space and Ground Based Facility Environmental Effects for FEP Teflon

Fluorinated Ethylene Propylene (FEP) Teflon is widely used as a thermal control material for spacecraft, however, it is susceptible to erosion, cracking, and subsequent mechanical failure in low Earth orbit. One of the difficulties in determining whether FEP Teflon will survive during a mission is the wide disparity of erosion rates observed for this material in space and in ground based facilities. Each environment contains different levels of atomic oxygen, ions, and vacuum ultraviolet (VUV) radiation in addition to parameters such as the energy of the arriving species and temperature. These variations make it difficult to determine what is causing the observed differences in erosion rates. This paper attempts to narrow down which factors affect the erosion rate of FEP Teflon through attempting to change only one environmental constituent at a time. This was attempted through the use of a single simulation facility (plasma asher) environment with a variety of Faraday cages and VUV transparent windows. Isolating one factor inside of a radio frequency (RF) plasma proved to be very difficult. Two observations could be made. First, it appears that the erosion yield of FEP Teflon with respect to that of polyimide Kapton is not greatly affected by the presence or lack of VUV radiation present in the RF plasma and the relative erosion yield for the FEP Teflon may decrease with increasing fluence. Second, shielding from charged particles appears to lower the relative erosion yield of the FEP to approximately that observed in space, however it is difficult to determine for sure whether ions, electrons, or some other components are causing the enhanced erosion.

Rutledge, Sharon K.↗

Atomic Oxygen Fluence Monitor

This innovation enables a means for actively measuring atomic oxygen fluence (accumulated atoms of atomic oxygen per area) that has impinged upon spacecraft surfaces. Telemetered data from the device provides spacecraft designers, researchers, and mission managers with real-time measurement of atomic oxygen fluence, which is useful for prediction of the durability of spacecraft materials and components. The innovation is a compact fluence measuring device that allows in-space measurement and transmittance of measured atomic oxygen fluence as a function of time based on atomic oxygen erosion yields (the erosion yield of a material is the volume of material that is oxidized per incident oxygen atom) of materials that have been measured in low Earth orbit. It has a linear electrical response to atomic oxygen fluence, and is capable of measuring high atomic oxygen fluences (up to >10(exp 22) atoms/sq cm), which are representative of multi-year low-Earth orbital missions (such as the International Space Station). The durability or remaining structural lifetime of solar arrays that consist of polymer blankets on which the solar cells are attached can be predicted if one knows the atomic oxygen fluence that the solar array blanket has been exposed to. In addition, numerous organizations that launch space experiments into low-Earth orbit want to know the accumulated atomic oxygen fluence that their materials or components have been exposed to. The device is based on the erosion yield of pyrolytic graphite. It uses two 12deg inclined wedges of graphite that are over a grit-blasted fused silica window covering a photodiode. As the wedges erode, a greater area of solar illumination reaches the photodiode. A reference photodiode is also used that receives unobstructed solar illumination and is oriented in the same direction as the pyrolytic graphite covered photodiode. The short-circuit current from the photodiodes is measured and either sent to an onboard data logger, or transmitted to a receiving station on Earth. By comparison of the short-circuit currents from the fluence-measuring photodiode and the reference photodiode, one can compute the accumulated atomic oxygen fluence arriving in the direction that the fluence monitor is pointing. The device produces a signal that is linear with atomic oxygen fluence using a material whose atomic oxygen erosion yield has been measured over a period of several years in low-Earth orbit.

Banks, Bruce A.↗

A digital holography ex situ measurement characterization of plasma-exposed surface erosion from an electrothermal arc source

Digital holography has been proposed to fulfill a need for an imaging diagnostic capable of in situ monitoring of surface erosion caused by plasma–material interaction in nuclear fusion devices. A digital holography diagnostic for 3D surface erosion measurement has been developed at Oak Ridge National Laboratory with the goal of deployment on a plasma device. A proof-of-concept in situ demonstration is planned which would involve measurement of plasma erosion on targets exposed to an electrothermal arc source. This work presents the results of an ex situ characterization of the capability and limitations of holographic imaging of targets exposed to the arc source. Targets were designed to provide a fiducial for comparison of deformed and unaffected areas. The results indicated that the average net erosion was ~150 nm/plasma exposure, which is expected to be within the diagnostic’s measurement capacity. Surface roughness averages determined by holographic image analysis showed good agreement with measurements taken with a profilometer. Finally, the limit of the holography diagnostic’s x–y spatial resolution was characterized by comparison with scanning electron microscope imaging.

47 OTHER INSTRUMENTATION↗

Plasma Wall Interaction with 3-D Plasma Boundaries

The interaction of the edge plasma and the material surfaces is one of the most critical challenges on the path to harness fusion power as new, fundamental energy source. This challenge typically combines the thrust to reach high density, low temperature (detached) plasmas in front of the divertor target plates as well as understanding the plasma material interaction (PMI) in particular in this regime. The combination of both research thrusts represents an extraordinarily challenging subject encompassing spatial scales spanning nanometers to meters in all states of matter and across a broad energy range. Modeling capabilities, which help to interpret data from nowadays experiments and enable extrapolation to future devices are urgently required. This is in particular true for toroidal magnetic confinement devices with three-dimensional (3D) plasma boundaries. Such plasma boundary geometries occur in tokamaks, when small amplitude magnetic perturbations are used to stabilize the unruly edge plasma or in stellarators, that are inherently 3D plasma confinement devices. In this project, the impact of 3D plasma boundaries on the plasma material interaction (PMI) was assessed. This work focused on plasma boundary conditions, in which high-density conditions at the material surfaces yield mitigation of the otherwise immense heat and particle loads that these materials would see. These so-called high recycling and eventually detached plasma regimes are of great interest for future reactor operation. In the project, key features that are unique to 3D boundaries were explored in comparison to canonically assumed axisymmetric plasma edge situations in tokamaks. In particular, the relevance of the 3D boundary situation in the extrapolation to the plasma boundary solution at ITER, the next step fusion energy experiment under construction as a multi-national, world-wide large-science experiment in southern France, has been explored. The EMC3-EIRENE plasma edge fluid and kinetic neutral transport code has been advanced to cope with the challenging and unprecedented conditions in the ITER boundary plasma including 3D fields that are planned to be used to suppress harmful edge instabilities, the so-called edge localized modes. This is a vital integration challenge for ITER and the results from this grant have provide a leading capability for this assessment. It was shown that the detachment process in a 3D edge solution for ITER follows the recycling regimes that are known from axisymmetric solutions, but that multiple plasma exhaust channels connected to the material surfaces are established which feature individual recycling characteristics. Because these channels touch the material surfaces in the divertor in a 3D geometry, the compatibility with the plasma material interaction (PMI), including erosion and impurity generation has been found to be an important part of the integration challenge. To address this, the fully 3D plasma material interaction code ERO2 has been adapted to these ITER specific geometries and a homogeneous mixing model was implemented, that allows to consider the mixing of Be and Was used at ITER in the PMI modeling. This model enhancement has been used to study non-local migration of Be in the JET ITER like wall configuration and it has been shown that with this model such complex migration processes in ITER relevant plasma shapes and with ITER relevant plasma boundary conditions can be addressed. The combined modeling approach using EMC3-EIRENE as a plasma boundary transport code and the ERO2 specialized PMI model will be an asset for the continued preparations of ITER operation as well as for Fusion Pilot Plant efforts that have emerged in the U.S. during the evolution of this grant. The predictive capability of this numerical tool has been validated at the DIII-D US national fusion facility. Here, dedicated plasma edge diagnostics were implemented to measure the impurity household around a 3D edge plasma during ELM suppression by 3D fields. Dedicated experiments with local material probes using these diagnostics and the state-of-the-art suite of boundary measurements at DIII-D have shown that the 3D perturbation of the plasma edge that is excreted by such 3D control fields yield a perturbation of the plasma boundary flux structure and hence also of the resulting PMI. The 3D boundary plasma is composed out of helical magnetic flux channels that intersect the divertor targets at an angle relative to the main guiding field, i.e., the toroidal magnetic field component of the tokamak. A similar effect has been measured as well on limiter surfaces during the startup campaign at the new stellarator experiment Wendelstein 7-X. These experiments ad initial analysis with the ERO plasma material interaction model, suggested that the place of erosion for a given particle from the surface and its re-deposition can be different in such 3D field geometries yielding potentially a significant level of net-erosion. This is not the case for axisymmetric solutions, where it was shown in the past that the eroded particles are effectively re-deposited into gaps produced by erosion at the same position and hence the net-erosion levels are small. For ITER, the quest to suppress the ELMs and at the same time maintain the integrity of the divertor is an issue, which these fundamental findings will help to resolve. The coupling of this work to the extrapolation in the ITER program has been addressed by both the PI and the lead numerical scientist being ITER Science Fellows in the duration of the contract and forward. A second focus in the exploration of 3D boundary effects on tokamaks and stellarators has been set on the measurement of helium exhaust features with such 3D fields. This is important because He represents the ash of the fusion process and needs to be exhausted. It was shown that 3D field application compatible with suppression of ELMs yields an increase of the helium exhaust performance. The ratio of the effective helium confinement time over the energy confinement time was reduced by almost 50% which demonstrated that the impact of helium accumulation in the plasma core with respect to the confinement of energy to sustain the fusion reaction is significantly improved with such 3D control fields. It was shown that this is the case for tokamaks as well as stellarators. At the Large helical Device in Japan, a similar enhancement of the helium exhaust features when small amplitude additional 3D fields were applied was measured. This is an important additional function of 3D field application and its impact on ITER is presently being studied in combination with investigations of helium exhaust in 3D field geometries of stellarator devices.

3D plasma edge transport↗