Failure Analysis of T-38 Aircraft Burst Hydraulic Aileron Return Line

During maintenance troubleshooting for fluctuating hydraulic pressures, a technician found that a right hand aileron return line, on the flight hydraulic side, was ruptured (Fig. 1, 2). This tubing is part of the Hydraulic Flight Control Aileron Return Reducer to Aileron Manifold and is suspected to be original to the T-38 Talon trainer aircraft. Ailerons are small hinged sections on the outboard portion of a wing used to generate rolling motion thereby banking the aircraft. The ailerons work by changing the effective shape of the airfoil of the outer portion of the wing [1]. The drawing, Northrop P/N 3-43033-55 (6/1960), specifies that the line is made from 0.375 inch OD, aluminum 5052-0 tubing with a 0.049 inch wall thickness. WW-T-787 requires the tube shall be seamless and uniform in quality and temper [2]. The test pressure for this line is 3000 psi, and the operational pressure for this line is estimated to be between 45 psi and 1500 psi based on dynamic loading during flight. Examination of the fracture surface found evidence of arrest bands originating on the inner diameter (Fig 3). Ductile dimples are observed on the tube fractures (Fig. 4). The etched cross-section revealed thinning and work-hardening in the burst region (Fig. 5). The wall thickness just outside the work-hardened fracture region measured 0.035". Barlow's Formula: P = 2St/D, where P is burst pressure, S is allowable stress, t is wall thickness and D is the outer diameter of tube. Using the ultimate tensile strength of 28 ksi and a measured wall thickness of 0.035 inches at burst, P = 5.2 ksi (burst pressure). Using the yield of 13 ksi (YS) for aluminum 5052-0, plastic deformation will happen at P = 2.4 ksi suggesting plastic deformation occurred at a proof pressure of 3.0 ksi. Conclusion: The burst resulted from high stress, low-cycle fatigue. Evidence of arrest bands originating on the inner diameter. Fracture is predominately shear dimples, characteristic of high load ductile fractures (Fig 6). Section wall reduction in the burst region. Plastic deformation and thinning of the out-of-specification tube wall likely happened during the initial proof testing years ago. Metallography of tubing away from rupture site confirmed tubing was seamless. Based on the tube microstructure, it is likely that the initial wall thickness was about 30 % thinner than the requirement of 0.049 inches. Fracture initiated on the ID and progressed to the OD (shear lip). The tube is made of the correct material of 5052-0 aluminum as verified using Optical Emission Spectroscopy (Table 2). The tubing hardness tested 77 HV100 (77 HRE). This hardness is slightly above the requirement for 70 HRE maximum for aluminum 5052-0 in AMS 2658C [3].

Martinez, J. E.↗

Data and Modeling of Dendrites Subject to A Step Change in Pressure (TDSE)

There is considerable interest in dendritic solidification because of the influence dendrites have in the determination of microstructure, and thereby in the physical properties of cast metals and alloys. Current theories and models of dendritic growth generally couple diffusion effects in the melt with the physics of the interface. Data and subsequent analysis prior of the tip growth speed and radii of thermal succinonitrile dendrites in the near-convection free, on-orbit, free-fall environment demonstrate that these theories yield predictions that are reasonably in agreement with the results of experiment. However, data and analysis for assessing the interfacial physics component of theory are not sufficiently detailed or definitive. To study fundamental aspects of dendritic interface stability, we are measuring and modeling the kinetics and morphology of dendrites as they evolve from one well-defined steady state at a pre-set supercooling, through a transient stage, to a different well-defined steady state. More specifically, we subject succinonitrile dendrites, growing under steady-state conditions, to a rapid change in pressure. This leads to a rapid change in thermal driving force from the corresponding change in both the equilibrium melting temperature due to the Clapeyron effect, and a change in the far-field temperature due to adiabatic temperature changes in the bulk liquid and solid. Subsequently, we observe transformations from a well-characterized initial state into a new steady-state. Initial data reveal that the dendrite tip velocity changes almost as fast as the pressure charges, while the tip radius changes occur more slowly, taking from 10 60 seconds depending on the size of the step change and the final supercooling. Computer modeling of this process shows both agreements and disagreements with the experimental data. In making these observations and measurements, we are gaining new understandings of interfacial dynamics and state-selection physics.

Koss, Matthew B.↗

Low-Temperature Friction-Stir Welding of 2024 Aluminum

Solid state friction-stir welding (FSW) has been demonstrated to involve dynamic recrystallization producing ultra-fine, equiaxed grain structures to facilitate superplastic deformation as the welding or joining mechanism. However, the average residual, equiaxed, grain size in the weld zone has ranged from roughly 0.5 micron to slightly more than 10 micron, and the larger weld zone grain sizes have been characterized as residual or static grain growth as a consequence of the temperatures in the weld zone (where center-line temperatures in the FSW of 6061 Al have been shown to be as high as 480C or -0.8 T(sub M) where T(sub M) is the absolute melting temperature)). In addition, the average residual weld zone grain size has been observed to increase near the top of the weld, and to decrease with distance on either side of the weld-zone centerline, an d this corresponds roughly to temperature variations within the weld zone. The residual grain size also generally decreases with decreasing FSW tool rotation speed. These observations are consistent with the general rules for recrystallization where the recrystallized grain size decreases with increasing strain (or deformation) at constant strain rate, or with increasing strain-rate, or with increasing strain rate at constant strain; especially at lower ambient temperatures, (or annealing temperatures). Since the recrystallization temperature also decreases with increasing strain rate, the FSW process is somewhat complicated because the ambient temperature, the frictional heating fraction, and the adiabatic heating fraction )proportional to the product of strain and strain-rate) will all influence both the recrystallization and growth within the FSW zone. Significantly reducing the ambient temperature of the base metal or work pieces to be welded would be expected to reduce the residual weld-zone grain size. The practical consequences of this temperature reduction would be the achievement of low temperature welding. This study compares the residual grain sizes and microstructures in 2024 Al friction-stir welded at room temperature (about 30C and low temperature (-30C).

Benavides, S.↗

Imaging the End-to-End Dynamics of the Global Solar Wind-Magnetosphere Interaction

Much of what we know about the solar wind’s interaction with the Earth’s magnetosphere has been gained from isolated in situ measurements by single or multiple spacecraft. Based on their observations, we know that reconnection, whether on the dayside magnetopause or deep within the Earth’s magnetotail, controls the flow of solar wind energy into and through the global system. We know that nightside activity provides the energized particles that power geomagnetic storms. But by their very nature these isolated in situ measurements cannot provide an instantaneous global view of the entire system or its cross-scale dynamics. As a result, we don’t know which mode of reconnection prevails on the dayside magnetopause or within the magnetotail as a function of solar wind and geomagnetic conditions. We don’t know which mode or modes of nightside activity supply the most energized particles to the ring current. Nor do we know the dominant loss mode for ring current decay: precipitation, magnetopause outflow, or charge exchange with neutrals. Nor do we know how processes deep within the magnetosphere provide feedback to those happening in the outer magnetosphere. The answers to these questions could have an impact far beyond magnetospheric physics, since magnetic reconnection, particle acceleration, and charge-exchange are fundamental plasma processes that operate at other planets and throughout the universe. Comprehensive end-to-end global imaging of the key micro, meso-, and macro-scale plasma structures that comprise the magnetosphere will provide the answers to these questions via observations with a spatial resolution that exceeds anything possible with in situ measurements. Each proposed interaction mechanism generates a diagnostic plasma structure or boundary signature. Global, end-to-end, imaging provides the pathway to understanding the system as a whole, its constituent parts, and its cross-scale processes on a continuous basis, as needed to quantify the flow of solar wind energy through the global magnetospheric system. The significance of each mechanism is the product of its amplitude and occurrence rate. This white paper describes how a comprehensively-instrumented single spacecraft in a high-latitude circular polar orbit can provide the essential observations needed to track and quantify the flow of solar wind energy through the magnetosphere, including the solar wind plasma and magnetic field input, the magnetopause location in soft X-rays, the auroral oval in far ultraviolet, the ring current in energetic neutrals, the plasmasphere in extreme ultraviolet, the exosphere in Lyman-, the microstructure of the nightside auroral oval in ground-based all sky cameras, and the magnetic perturbations of ionospheric current patterns seen by ground-based magnetometers.

D G Sibeck↗

Gravitational Effects on the Morphology and Kinetics of Photodeposition of Polydiacetylene Thin Films From Monomer Solutions

The goal of this proposed work is to study gravitational effects on the photodeposition of polydiacetylene thin films from monomer solutions onto transparent substrates. Polydiacetylenes have been an extensively studied class of organic polymers because they exhibit many unusual and interesting properties, including electrical conductivity and optical nonlinearity. Their long polymeric chains render polydiacetylenes readily conducive to thin film formation, which is necessary for many applications. These applications require thin polydiacetylene films possessing uniform thicknesses, high purity, minimal inhomogeneities and defects (such as scattering centers), etc. Also, understanding and controlling the microstructure and morphology of the films is important for optimizing their electronic and optical properties. The lack of techniques for processing polydiacetylenes into such films has been the primary limitation to their commercial use. We have recently discovered a novel method for the formation of polydiacetylene thin films using photo-deposition from monomer solutions onto transparent substrates with UV light. This technique is very simple to carry out, and can yield films with superior quality to those produced by conventional methods. Furthermore, these films exhibit good third-order properties and are capable of waveguiding. We have been actively studying the chemistry of diacetylene polymerization in solution and the photo-deposition of polydiacetylene thin films from solution. It is well-known that gravitational factors such as buoyancy-driven convection and sedimentation can affect chemical and mass transport processes in solution. One important aspect of polydiacetylene thin film photodeposition in solution, relevant to microgravity science, is that heat generated by absorption of UV radiation induces thermal density gradients that under the influence of gravity, can cause fluid flows (buoyancy-driven convection). Additionally, changes in the chemical composition of the solution during polymerization may cause solutal convection. These fluid flows affect transport of material to and from the film surface and thereby affect the kinetics of the growth process. This manifests itself in the morphology of the resulting films; films grown under the influence of convection tend to have less uniform thicknesses, and can possess greater inhomogeneities and defects. Specifically, polydiacetylene films photodeposited from solution, when viewed under a microscope, exhibit very small particles of solid polymer which get transported by convection from the bulk solution to the surface of the growing film and become embedded. Even when carried out under conditions designed to minimize unstable density gradients (i.e., irradiating the solution from the top), some fluid flow still takes place (particles remain present in the films). It is also possible that defect nucleation may be occurring within the films or on the surface of the substrate; this, too, can be affected by convection (as is the case with crystal growth). Hence films grown in 1-g will, at best, still possess some defects. The objective of this proposal is to investigate, both in 1-g and in low-g, the effects of gravitational factors (primarily convection) on the dynamics of these processes, and on the quality, morphology, and properties of the films obtained.

Paley, Mark S.↗