VOPO 4 cathode for sodium ion batteries

An electrode comprising a space group Pna2 1 VOPO 4 lattice, capable of electrochemical insertion and release of alkali metal ions, e.g., sodium ions. The VOPO 4 lattice may be formed by solid phase synthesis of KVOPO 4 , milled with carbon particles to increase conductivity. A method of forming an electrode is provided, comprising milling a mixture of ammonium metavanadate, ammonium phosphate monobasic, and potassium carbonate; heating the milled mixture to a reaction temperature, and holding the reaction temperature until a solid phase synthesis of KVOPO 4 occurs; milling the KVOPO 4 together with conductive particles to form a conductive mixture of fine particles; and adding binder material to form a conductive cathode. A sodium ion battery is provided having a conductive NaVOPO 4 cathode derived by replacement of potassium in KVOPO 4 , a sodium ion donor anode, and a sodium ion transport electrolyte. The VOPO 4 , preferably has a volume greater than 90 Å 3 per VOPO 4 .

Whittingham, M. Stanley↗

Regulating Cation Interactions for Zero–Strain and High–Voltage P2–type Na 2/3 Li 1/6 Co 1/6 Mn 2/3 O 2 Layered Oxide Cathodes of Sodium–Ion Batteries

Deep sodium extraction/insertion of sodium cathodes usually causes undesired Jahn–Teller distortion and phase transition, both of which will reduce structural stability and lead to poor long-cycle reliability. Here we report a zero-strain P2- Na 2/3 Li1/6Co 1/6 Mn 2/3 O 2 cathode, in which the lithium/cobalt substitution contributes to reinforcing the host structure by reducing the Mn 3+ /Mn 4+ redox, mitigating the Jahn–Teller distortion, and minimizing the lattice change. 94.5 % of Na + in the unit structure can be reversibly cycled with a charge cut-off voltage of 4.5 V (vs. Na + /Na). Impressively, a solid-solution reaction without phase transitions is realized upon deep sodium (de)intercalation, which poses a minimal volume deviation of 0.53 %. Finally, it attains a high discharge capacity of 178 mAh g –1 , a high energy density of 534 Wh kg –1 , and excellent capacity retention of 95.8 % at 1 C after 250 cycles.

25 ENERGY STORAGE↗

Studying the effect of the upper internal structure design on thermal stratification in sodium fast reactors

Thermal stratification and mixing in large reactor pools can pose significant issues with regard to operation and safety of nuclear plants. While significant work has been done in this area on light water reactors it is more critical for sodium reactors and there is far less data with regard to low Prandtl number fluids. Here this paper focuses on the effect of the upper internal structure on the formation of thermal stratification in a scaled sodium fast reactor upper plenum. Six different upper internal structure configurations were tested to observe the effect on thermal stratification. The degree of stratification was quantified using the stratification number. Each configuration was tested from low to high flow rates at a temperature difference of 50 and 100 °C. Over this broad array of testing, it was observed that higher flow rates, more porosity in the upper internal structure design, and a smaller temperature difference yielded a lower degree of stratification. This information can be used to aid in the design of the upper internal structure in a sodium fast reactor. Furthermore, this high resolved temperature data can be used to verify models under prototypic low Prandtl numbers.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Prognostic model and failure mechanisms of steam generators in Sodium-Cooled fast reactors

This paper presents a prognostic model for sodium-cooled fast reactor (SFR) steam generators (SGs). Here, the purpose of the model is to estimate the remaining useful life of SFR SGs and thus to support the decision-making of autonomous control. SFR SGs are of great interest for plant integrity due to their harsh operation environment. They operate at higher temperatures and higher coolant-to-steam pressure differences than those of current light water reactors (LWR). The severity of the SFR SG failure consequences, which include water-sodium contact, is another reason. Understanding its failure mechanisms is important for the development of its prognostic model. Based on our literature review and physics-based analysis, we concluded that creep would be a dominant degradation mode of SFR SGs due to SFR’s high-temperature and high-pressure environment. Thus, creep is the focus of the prognostic model. Various other failure modes were also investigated in this study. The mechanical fatigue due to flow-induced vibration is usually observed in early developmental phases and would not be an important issue during normal operation. The thermal fatigue due to thermal stripping is occasionally observed in other components in SFRs but does not affect SG integrity. Pure water stress corrosive crack, fretting, and so on are commonly observed in LWR SGs but are significantly less important in SFR SGs because of the high temperatures, high pressure differences, and chemical properties of liquid sodium. Based on these investigations, a prognostic model focusing on creep failures was developed. It estimates the failure probability profile by sampling the Larson-Miller parameter (LMP) and temperature and associated uncertainties through Monte Carlo methods. Two case studies were presented. The first one demonstrated the model’s capability to calculate the failure probability for a new specimen within a given time. If the tube is working under temperatures of 500C ± 3 and pressures of 15.2 MPa, which leads to LMP of 20,100 ± 50, the failure probabilities within 50, 70, and 90 years are approximately 0.1 %, 3.2 %, and 17.5 %. The second demonstrated how adjusting the workload can help to protect the integrity of the component. For an old tube reaching 99 % of its lifespan, continuing to run at temperatures of 500C ± 3 and LMP of 20,100 ± 50 leads to a failure probability of about 29.0 % within a year. If the temperature is reduced by 5C, the failure probability can be reduced to 2.5 %, and, if the pressure is also reduced such that the LMP is increased by 100, the failure probability can further be reduced to 0.12 %.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Anomaly Detection in Liquid Sodium Cold Trap Operation with Multisensory Data Fusion Using Long Short-Term Memory Autoencoder

Sodium-cooled fast reactors (SFR), which use high temperature fluid near ambient pressure as coolant, are one of the most promising types of GEN IV reactors. One of the unique challenges of SFR operation is purification of high temperature liquid sodium with a cold trap to prevent corrosion and obstructing small orifices. We have developed a deep learning long short-term memory (LSTM) autoencoder for continuous monitoring of a cold trap and detection of operational anomaly. Transient data were obtained from the Mechanisms Engineering Test Loop (METL) liquid sodium facility at Argonne National Laboratory. The cold trap purification at METL is monitored with 31 variables, which are sensors measuring fluid temperatures, pressures and flow rates, and controller signals. Loss-of-coolant type anomaly in the cold trap operation was generated by temporarily choking one of the blowers, which resulted in temperature and flow rate spikes. The input layer of the autoencoder consisted of all the variables involved in monitoring the cold trap. The LSTM autoencoder was trained on the data corresponding to cold trap startup and normal operation regime, with the loss function calculated as the mean absolute error (MAE). The loss during training was determined to follow log-normal density distribution. During monitoring, we investigated a performance of the LSTM autoencoder for different loss threshold values, set at a progressively increasing number of standard deviations from the mean. The anomaly signal in the data was gradually attenuated, while preserving the noise of the original time series, so that the signal-to-noise ratio (SNR) averaged across all sensors decreased below unity. Results demonstrate detection of anomalies with sensor-averaged SNR < 1.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Dynamic Control of Sodium Cold Trap Purification Temperature Using LSTM System Identification

This study investigates the dynamic regulation of the sodium cold trap purification temperature at Argonne National Laboratory’s liquid sodium test facility, employing long short-term memory (LSTM) system identification techniques. The investigation introduces an innovative hybrid approach by integrating model predictive control (MPC) based on first principles dynamic models with a multi-step time–frequency LSTM model in predicting the temperature profiles of a sodium cold trap purification system. The long short-term memory–model predictive controller (LSTM-MPC) model employs a sliding window scheme to gather training samples for multi-step prediction, leveraging historical data to construct predictive models that capture the non-linearities of the complex system dynamics without explicitly modeling the underlying physical processes. The performance of the LSTM-MPC and MPC were evaluated through simulation experiments, where both models were assessed on their capacity to maintain the cold trap temperature within predefined set-points while minimizing deviations and overshoots. Results obtained show how the data-driven LSTM-MPC model demonstrates stability and adaptability. In contrast, the traditional MPC model exhibits irregularities, particularly evident as overshoots around set-point limits, which can potentially compromise its effectiveness over long prediction time intervals. The findings obtained offer valuable insights into integrating data-driven techniques for enhancing real-time monitoring systems.

LSTM-MPC↗

Ultralow-Strain Zn-Substituted Layered Oxide Cathode with Suppressed P2–O2 Transition for Stable Sodium Ion Storage

Layered transition metal oxides have drawn much attention as a promising candidate cathode material for sodium-ion batteries. However, their performance degradation originating from strains and lattice phase transitions remains a critical challenge. Herein, a high-concentration Zn-substituted Na x MnO 2 cathode with strongly suppressed P2–O2 transition is investigated, which exhibits a volume change as low as 1.0% in the charge/discharge process. Additionally, such ultralow strain characteristics ensure a stable host for sodium ion storage, which significantly improves the cycling stability and rate capability of the cathode material. Also, the strong coupling between the highly reversible capacity and the doping content of Zn in Na x MnO 2 is investigated. It is suggested that a reversible anionic redox reaction can be effectively triggered by Zn ions and is also highly dependent on the Zn content. Such an ion doping strategy could shed light on the design and construction of stable and high-capacity sodium ion host.

25 ENERGY STORAGE↗

Unblocking Oxygen Charge Compensation for Stabilized High‐Voltage Structure in P2‐Type Sodium‐Ion Cathode

Abstract Layered transition‐metal (TM) oxides are ideal hosts for Li + charge carriers largely due to the occurrence of oxygen charge compensation that stabilizes the layered structure at high voltage. Hence, enabling charge compensation in sodium layered oxides is a fascinating task for extending the cycle life of sodium‐ion batteries. Herein a Ti/Mg co‐doping strategy for a model P2‐Na 2/3 Ni 1/3 Mn 2/3 O 2 cathode material is put forward to activate charge compensation through highly hybridized O 2 p TM 3 d covalent bonds. In this way, the interlayer OO electrostatic repulsion is weakened upon deeply charging, which strongly affects the systematic total energy that transforms the striking P2–O2 interlayer contraction into a moderate solid‐solution‐type evolution. Accordingly, the cycling stability of the codoped cathode material is improved superiorly over the pristine sample. This study starts a perspective way of optimizing the sodium layered cathodes by rational structural design coupling electrochemical reactions, which can be extended to widespread battery researches.

25 ENERGY STORAGE↗

Combining Experimental and Theoretical Techniques to Gain an Atomic Level Understanding of the Defect Binding Mechanism in Hard Carbon Anodes for Sodium Ion Batteries

Sodium ion batteries (NIBs) are an attractive alternative to lithium–ion batteries in applications that require large–scale energy storage due to sodium's high natural abundance and low cost. Hard carbon (HC) is the most promising anode material for NIBs; however, there is a knowledge gap in the understanding of the sodium binding mechanism that prevents a rational design of HC. This study tunes sucrose–derived HC via synthesis temperature then evaluates the structural, physical, and electrochemical properties. Neutron total scattering is used to generate structural models by fitting pair distribution functions (PDF) with a combination of molecular dynamics and reverse Monte Carlo methods. From this model, the number and type of structural features are identified, quantified, and correlated to the galvanostatic charge/discharge. A method of PDF “fingerprinting” binding sites using Na probe atoms is developed and analyzing these PDFs reveals an atomistic view of ion binding sites responsible for “defect” storage mechanisms. Combining these techniques results in an atomic–level study that provides a big picture of the Na–binding mechanism in NIBs, which allows for more precise tuning of the structure–property relationships in the future. Finally, the methodologies developed will also enable new strategies for the analysis of amorphous functional materials.

25 ENERGY STORAGE↗

Tailoring P2/P3‐Intergrowth in Manganese‐Based Layered Transition Metal Oxide Positive Electrodes via Sodium Content for Na‐Ion Batteries

High-manganese content sodium-ion positive electrodes have received heightened interest as an alternative to contemporary Li-ion chemistries due to their high abundance, low toxicity, and even geographical distribution. However, these materials typically suffer from poor capacity, unstable cycling performance, and sluggish Na + kinetics. Herein, we explore a manganese-based layered transition metal oxide (Na x N 0.25 Mn 0.75 O 2 ) and show by X-ray diffraction (XRD) and high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM) that careful variation of the sodium content can instigate the formation of a biphasic intergrowth. This intergrown P2/P3 material offered a higher capacity than its monophasic P2 counterpart due to the P3 structure having greater low-voltage Mn 3+/4+ redox. Further, the intergrowth material offers greatly enhanced kinetics and cycling stability when compared to single-phase P3 material, due to the stabilizing nature of the P2 structure, elucidated by galvanostatic intermittent titration technique (GITT) and operando synchrotron X-ray diffraction. These results highlight the beneficial effect that the intergrowth structure has on the electrochemical performance of high-manganese content positive electrode for future sodium-ion batteries.

25 ENERGY STORAGE↗

Incorporating Diamondoids as Electrolyte Additive in the Sodium Metal Anode to Mitigate Dendrite Growth

Abstract Owing to the high abundance and gravimetric capacity (1165.78 mAh g −1 ) of pure sodium, it is considered as a promising candidate for the anode of next‐generation batteries. However, one major challenge needs to be solved before commercializing the sodium metal anode: The growth of dendrites during metal plating. One possibility to address this challenge is to use additives in the electrolyte to form a protective solid electrolyte interphase on the anode surface. In this work, we introduce a diamondoid‐based additive, which is incorporated into the anode to target this problem. Combining operando and ex situ experiments (electrochemical impedance spectroscopy, optical characterization, and cycling experiments), we show that molecular diamondoids are incorporated into the anode during cycling and successfully mitigate the growth of dendrites. Furthermore, we demonstrate the positive effect of the additive on the operation of sodium‐oxygen batteries by means of increased energy density.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Molten-Salt Synthesis of O 3 -Type Layered Oxide Single Crystal Cathodes with Controlled Morphology towards Long-Life Sodium-Ion Batteries

Sodium layered oxides show great promise as affordable alternatives to lithium layered oxides, but their poor cycle life and air stability limit their practical potential. Micron-scale single crystals with greater packing density and lower surface area can overcome these challenges and improve performance compared to the traditional polycrystalline morphology. Herein, the authors present the synthesis of layered O 3 -type Na(Ni 0.3 Fe 0.4 Mn 0.3 )O 2 single-crystals with greatly improved cycle life and air stability. A molten-salt synthesis technique is adopted with excess sodium hydroxide to obtain platelet-like single crystals. Because the main mechanisms of both capacity fade and air degradation occur as a result of surface reactions at the opening of the sodium diffusion channels, particle morphology is found to be a critical metric for materials performance. More important than particle size or total surface area, the smaller proportion of exposed edge planes in the platelet morphology greatly reduces the amount of harmful surface reactions. Furthermore, the molten-salt method is found to eliminate the need for coprecipitated precursors and even form better morphology, starting from metal oxides instead of coprecipitated hydroxides.

25 ENERGY STORAGE↗

Effect of sodium loading on Pt/ZrO 2 during ethanol steam reforming

Ethanol steam reforming (ESR) was investigated on unpromoted and several sodium promoted Pt/ZrO 2 catalysts. From DRIFTS experiments, the following steps during ESR were inferred: dissociation of ethanol to produce ethoxy species; oxidative dehydrogenation of ethoxy species to acetate; and acetate decomposition. Acetate decomposition depends on the catalyst formulation. Decarboxylation is the most favored route at high sodium loading (2.5 and 5 wt.%); acetate decomposes in the forward direction to CH 4 and a carbonate, which further decomposes to CO 2 . In contrast, decarbonylation is prevalent for the unpromoted catalyst or catalysts having low sodium loading. Furthermore, acetate likely decomposes to CH 3 OH and CO. Adsorbed methanol may undergo further steam reforming by oxidative dehydrogenation to formate species, which decarbonylates via reverse decomposition to CO and H 2 O. Temperature programmed desorption/reaction and activity data confirmed that alkali promotion, especially at 1.8 %Na and higher loading, facilitates the forward acetate decomposition step, favoring decarboxylation over decarbonylation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Thermal-striping analysis methodology for sodium-cooled reactor design

Computational fluid dynamics simulations have been performed to study the applicability of engineering CFD methods for thermals striping analysis. Thermal striping is the fluctuating temperature profile in a solid caused by fluctuating fluid temperature, and the resulting fluctuating thermal stresses cause high cycle fatigue and eventual material failure. Here this study presents the methodology for thermal striping analysis that including a transient conjugate heat transfer RANS model and benchmark the results against a sodium triple jet experiment. The multiphysics calculations are implemented to analyze the thermal stresses in the solid domain caused by the coupled heat transfer between the fluid and solid domains. Validation data from a liquid sodium triple jet experiment include time-averaged temperature measurements and power spectra of the temperature signal. The numerical results agree well with these experimental measures, demonstrating key features such as the dominant frequency of temperature fluctuations. The applicability of a low-cost wall treatment method is demonstrated, enabling key computational savings. Finally, the performance of two finite element stress analysis software packages is compared, and the validity of the lower-cost method is confirmed. These results demonstrate the applicability of engineering methods for computational thermal striping calculations, enabling thermal striping estimations in large fluid systems such as the core of a Sodium-cooled nuclear reactor.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Thermal management of a high temperature sodium sulphur battery stack

The sodium sulfur battery is an advanced secondary battery with high potential for grid-level storage due to their high energy density, low cost of the reactants, and high open-circuit voltage. However, as the operating temperature of the battery is high (about 300 °C), effective thermal management is required to prevent thermal runaway under high current density operation. Here, to develop efficient thermal management strategies, a detailed, thermo-electrochemical, non-isothermal, distributed dynamic model of a sodium-sulfur battery stack is developed. Models of three thermal management strategies are developed and analyzed in this work: active cooling, passive cooling, and hybrid cooling. The active cooling strategy uses air as the cooling medium whereas, the passive cooling strategy uses a phase change material. In the hybrid cooling strategy, both active and passive cooling strategies are used. Due to the high operating temperature of the sodium sulfur batteries, the rejected heat can be utilized effectively and consequently a high variability in the heat rejection rate may not be acceptable. Performance of these strategies is analyzed under high current density operation by evaluating the variability in the cell temperature during charge/discharge cycles, temperature difference between the cells based on their locations, and variability in the heat rejection rate. The phase change-based hybrid thermal management strategy with an embedded controller maintained the temperature variation within ±/- 2.8 °C. Considering the tradeoff between the capital cost for PCM, fan power requirement, and variability in the heat rejection rate, the optimal quantity of the PCM and the maximum air velocity for the maximum current density of 260 mA/cm 2 (0.55 C-rate) were found be 0.74 g/Wh and 3 m/s, respectively.

25 ENERGY STORAGE↗

Construction of MoS 2 /NiS 2 heterostructure with fast interfacial reaction kinetics for ultrafast sodium storage

Constructing heterostructure is a valid method to reinforcing sodium storage performance of transition metal chalcogenides materials. Herein, a simple, safe and controllable one step hydrothermal method is proposed to synthesize MoS 2 /NiS 2 heterostructure. Due to the difference in band gaps and work functions of MoS 2 and NiS 2 , the charges are redistributed at the MoS 2 /NiS 2 heterointerfaces, thereby accelerating the migration of electrons and Na + . The heterointerfaces provide extra active sites for storing Na + , thus increasing the sodium storage capacity of the heterostructure. Furthermore, the distinct redox potentials of NiS 2 and MoS 2 promote the structural stability of MoS 2 /NiS 2 heterostructure during the electrochemical reaction processes. Consequently, the obtained MoS 2 /NiS 2 heterostructure exhibits superior rate properties (339.4 mAh g –1 at 10 A g –1 ) and ultra-stable cycling stability (480.5 mAh g –1 after 350 cycles at 1 A g –1 ). Finally, this paper presents a valid strategy for creating heterostructure anodes with excellent sodium storage properties.

25 ENERGY STORAGE↗

Experimental validation of simplified radionuclide transport bubble scrubbing code in sodium coolant pool

Solid radionuclides released following fuel pin failure may become entrained in gaseous fission products and be rapidly transported through the coolant pool to the cover gas region. Sensitivity studies on radionuclide transport have identified this potential pathway as one of both high concern and high uncertainty. The simplified radionuclide transport scrubbing code utilizes classical aerosol scrubbing mechanisms to model this phenomenon and predict aerosol masses reaching the cover gas region. This paper serves to validate this code in a sodium environment while conducting a parametric study to analyze the effects of aerosol size, bubble size, pool temperature, pool depth, aerosol density, and aerosol concentration. Through a series of experimental tests, it was determined that aerosol sizes ranging from 0.001 to 1.0 µm are of primary concern as aerosols in this range have a ratio of aerosol mass entering the sodium pool from the fuel pin to aerosol mass exiting the sodium pool to the cover gas region of less than 10. Further, the experimental results were found to match the trends found in the scrubbing model closely, but significantly more scrubbing was seen experimentally. Decreasing bubble size and increasing pool depth and aerosol density were all found to increase scrubbing both experimentally and theoretically. Pool temperature was found to have a negligible effect on scrubbing amounts; however, this was largely due to a subsequent increase in bubble size corresponding to increasing temperatures which offset the increase in scrubbing due to increased temperature. Varying aerosol concentration was found to have no effect on scrubbing ratios. A final series of tests was conducted for a more prototypic fuel pin failure with a heterogenous bubble swarm. From these tests, it was found that the experimental scrubbing quantities were larger than for the single bubble case. Overall, it was found that the simplified bubble transport scrubbing code accurately models the trends of the bubble scrubbing but provides a conservative estimate of scrubbing quantities. Model limitations fail to model the complex phenomena present for fission product scrubbing via bubble transport, but match trends seen experimentally.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Miniature DC electromagnetic pumps of molten lead and sodium to support development of Gen-IV nuclear reactors

This work developed designs of submerged, dual-regions, miniature DC-EM pumps for circulating molten lead and liquid sodium at ≤500 °C without active cooling for use in ex-pile and in-pile test loops to support of materials and fuel developments for Gen-IV sodium and molten lead fast nuclear reactor. These pumps with two pumping regions are 57 mm, 66.8 mm, 95.4 mm, and 133.5 mm in diameter and have two Alnico 5 permanent magnets with Hiperco-50 pole pieces for focusing the magnetic field lines in the flow duct. The Equivalent Circuit Model (ECM) linked to the Finite Element Method Magnetics (FEMM) software in MATLAB platform calculated the pumps characteristics for a wide range of parameters. Also determined are the pumps dimensions for the highest cumulative pumping power and peak efficiency. These dimensions are the height, width, and length of the flow duct, the thickness of the Alnico magnets, the length of current electrodes, and the separation distance between the two pumping regions. For molten lead, the pumping power increases from 368 W to 728 W, and the peak efficiency from 14.7% to 31.6% with increased pump diameter from 57 mm to 133.5 mm. In conclusion, for liquid sodium, both the pumping power and peak efficiency are higher, increasing from 392 W to 767 W and from 44.3 to 51.2%, respectively, with increased pump diameter from 57 mm to 133.5 mm.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗