Search NASA⌕ Search

SEARCH · Search NASA

Results for “STIRRING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Weld Nugget Temperature Control in Thermal Stir Welding

A control system for a thermal stir welding system is provided. The control system includes a sensor and a controller. The sensor is coupled to the welding system's containment plate assembly and generates signals indicative of temperature of a region adjacent and parallel to the welding system's stir rod. The controller is coupled to the sensor and generates at least one control signal using the sensor signals indicative of temperature. The controller is also coupled to the welding system such that at least one of rotational speed of the stir rod, heat supplied by the welding system's induction heater, and feed speed of the welding system's weld material feeder are controlled based on the control signal(s).

Ding, R. Jeffrey↗

Performance Improvement of Friction Stir Welds by Better Surface Finish

The as-welded friction stir weld has a cross section that may act as a stress concentrator. The geometry associated with the stress concentration may reduce the weld strength and it makes the weld challenging to inspect with ultrasound. In some cases, the geometry leads to false positive nondestructive evaluation (NDE) indications and, in many cases, it requires manual blending to facilitate the inspection. This study will measure the stress concentration effect and develop an improved phased array ultrasound testing (PAUT) technique for friction stir welding. Post-welding, the friction stir weld (FSW) tool would be fitted with an end mill that would machine the weld smooth, trimmed shaved. This would eliminate the need for manual weld preparation for ultrasonic inspections. Manual surface preparation is a hand operation that varies widely depending on the person preparing the welds. Shaving is a process that can be automated and tightly controlled.

Russell, Sam↗

Mechanisms of Oxide Formation in the Self-Reacting Friction Stir Weld Process

The initial objective of this study was to evaluate the effect of an extended delay time between preweld cleaning and the completion of a self-reacting friction stir welding (SRFSW) process on the resulting quality of various thickness panels of AA2219-T87. The current NASA standard specifies no more than a 48 hour delay between preweld cleaning and actual welding. The concern is whether increasing the cleaning delay time results in development of the residual oxide defect (ROD) in SRFSW. This concern emanates from the possibility of increased time correlating with increased oxide layer thickness on the faying surfaces. Oxide content on the faying surfaces has been reported to correlate with the occurrence of the ROD which reduces mechanical properties. When the SRFSW process was first adopted by the NASA Marshall Space Flight Center (MSFC), unexpected low tensile values that resulted were attributed to oxides within the weld that appeared to follow the former faying surface contours. Mitigation of the ROD was achieved through a combination of modifications to the processing parameters, tool designs, and incorporation of a weld seam offset. Two operations are involved in preweld cleaning: the first is removal of oil and grease, and the second is removal of surface oxides. In arc welding, improper cleaning of the faying surfaces of aluminum welded joints can increase the sensitivity toward development of defects. As the aluminum is locally melted, these contaminants contribute toward the development of porosity, inclusions, entrapped oxides, and other discontinuities which can degrade the strength of the weld joint. For weldment of large structures, the weld joint is typically cleaned, fit-up, and tack welded prior to the final full penetration welding pass. Because of the stringent joint fit-up requirements for mismatch and peaking for launch vehicle structures, the joint fit-up can sometimes contribute to lengthy delays between cleaning and tack welding, especially for circumferential weld joints on large diameter components. When the conventional friction stir welding (CFSW) process was introduced at the NASA MSFC, there was no procedure for cleaning prior to the solid-state joining process. As the process expanded to include SRFSW, preparation of the faying, crown, and root surfaces were implemented to overcome the ROD. Although the solid-state process is not expected to reach temperatures high enough for dissociation of the native oxide layer, concern remained regarding the redeposition of the native oxide layer within the stir zone. NASA has previously established the allowable time at 48 hours between preweld cleaning and a SRFSW process. The effect of potential 2 contamination resulting from an extended delay to 188 hours was subsequently evaluated for SRFSWs using tensile testing and metallographic imaging. Tensile specimens were tested at room temperature (RT), and at cryogenic conditions of liquid nitrogen (LN2) and liquid hydrogen. No detrimental effect on weld quality, as determined by weld strength, was reported for cleaning delays of 48, 120, 168, 240 or 288 hours. While no trends were established in this study, which extended the delay from 48 to 188 hours, there were a few outliers in terms of ultimate tensile strength (UTS). According to M. Fisher's 2014 Boeing Company Memo no. EYBF-MAF-14-029, all outliers were above the minimum acceptance criteria, but out of family with respect to the average values. As the robustness and reliability of any process ultimately depends on the average values as well as the outliers, an understanding of the cause of these outliers will ultimately improve the process. This report examines those outliers and their possible causes.

Schneider, J. A.↗

System and method for light assisted friction stir processing and welding of metallic and non-metallic materials

An apparatus for use in a friction stir operation, such as friction stir welding (FSW) or friction stir processing (FSP). The apparatus may have a rotating tool adapted to be plunged into a material, where the material is susceptible to being softened by heating. The rotating tool may further be adapted to be advanced along a surface of the material. An optical energy generating subsystem may be used to heat a portion of the material using optical energy as the tool is advanced along the material.

42 ENGINEERING↗

X-ray and neutron diffraction measurements of dislocation density and subgrain size in a friction stir welded aluminum alloy

The dislocation density and subgrain size were determined in the base material and friction-stir welds of 6061-T6 aluminum alloy. High-resolution X-ray diffraction measurement was performed in the base material. The result of the line profile analysis of the X-ray diffraction peak shows that the dislocation density is about 4.5 x 10{sup 14} m{sup 02} and the subgrain size is about 200 nm. Meanwhile, neutron diffraction measurements have been performed to observe the diffraction peaks during friction-stir welding (FSW). The deep penetration capability of the neutron enables us to measure the peaks from the midplane of the Al plate underneath the tool shoulder of the friction-stir welds. The peak broadening analysis result using the Williamson-Hall method shows the dislocation density of about 3.2 x 10{sup 15} m{sup -2} and subgrain size of about 160 nm. The significant increase of the dislocation density is likely due to the severe plastic deformation during FSW. This study provides an insight into understanding the transient behavior of the microstructure under severe thermomechanical deformation.

36 MATERIALS SCIENCE↗

X-Ray and Neutron Diffraction Measurements of Dislocation Density and Subgrain Size in a Friction-Stir-Welded Aluminum Alloy

The dislocation density and subgrain size were determined in the base material and friction-stir welds of 6061-T6 aluminum alloy. High-resolution X-ray diffraction measurement was performed in the base material. The result of the line profile analysis of the X-ray diffraction peak shows that the dislocation density is about 4.5 x 10{sup 14} m{sup -2} and the subgrain size is about 200 nm. Meanwhile, neutron diffraction measurements have been performed to observe the diffraction peaks during friction-stir welding (FSW). The deep penetration capability of the neutron enables us to measure the peaks from the midplane of the Al plate underneath the tool shoulder of the friction-stir welds. The peak broadening analysis result using the Williamson-Hall method shows the dislocation density of about 3.2 x 10{sup 15} m{sup -2} and subgrain size of about 160 nm. The significant increase of the dislocation density is likely due to the severe plastic deformation during FSW. This study provides an insight into understanding the transient behavior of the microstructure under severe thermomechanical deformation.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Friction Stir Spot Welding of Advanced High Strength Steels

Friction stir spot welding techniques were developed to successfully join several advanced high strength steels. Two distinct tool materials were evaluated to determine the effect of tool materials on the process parameters and joint properties. Welds were characterized primarily via lap shear, microhardness, and optical microscopy. Friction stir spot welds were compared to the resistance spot welds in similar strength alloys by using the AWS standard for resistance spot welding high strength steels. As further comparison, a primitive cost comparison between the two joining processes was developed, which included an evaluation of the future cost prospects of friction stir spot welding in advanced high strength steels.

AHSS↗

Manufacturing of magnesium/aluminum bimetallic ring components by friction stir assisted simultaneous forging and solid-state joining

Here, a bimetallic ring component is forged by a friction stir assisted forging (FS-forging). A cylindrical bimetallic blank, magnesium AZ31 cylinder (Mg core) tightly fitted inside an aluminum 6061-T6 tube (Al skin), is used. In the FS-forging, the frictional heat and stirring of rotating tool forge the blank into a desired shape, while simultaneously generate a solid-state joint between the Mg core and the Al skin, without additional external heating, as confirmed by the microstructural analysis and mechanical tests. The microstructural analysis also shows that the characteristics of the solid-state joint can be different depending on the process parameters.

42 ENGINEERING↗

Effect of Process Parameters on Abnormal Grain Growth during Friction Stir Processing of a Cast Al Alloy

The effects of process parameters and friction stir processing (FSP) run configurations on the stability of nugget microstructure at elevated temperatures were evaluated. Cast plates of an Al-7Si- 0.6Mg alloy were friction stir processed using a combination of tool rotation rates and tool traverse speeds. All single pass runs showed some extent of abnormal grain growth (AGG), whereas multi-pass runs were more resistant to AGG. Additionally, higher tool rpm was found to be beneficial for controlling AGG. These effects were analyzed by comparing the result of this work with other published results and AGG models.

36 MATERIALS SCIENCE↗

Friction Stir Processed Repair Welding of Dry Storage Canisters and Mitigation Strategies: Effect of Engineered Barrier Layer on Environmental Degradation

The proposed project aims to develop a friction sir based repair technique to heal cracks of stainless steel dry storage canisters (DSCs), created by the effect of stress corrosion cracking (SCC). In real service conditions, the welded parts of the canisters become prone to SCC under exposure to aggressive chemical environment. The focus of the project is on developing a mitigation strategy that can be implemented for countering SCC in DSCs following a two-pronged approach: (i) apply friction stir processing (FSP) as a crack repair technique while creating compressive residual stresses at the canister material surface, thus improving resistance against SCC; (ii) add molybdenum and/or nitrogen by friction stir based alloying process to create compositions that improve pitting resistance and thus enhance resistance against SCC. The specific project objectives are listed below: • Investigate FSW of 304L SS a potential repair welding technique of dry storage canisters; • Optimize the FSW parameters to introduce surface compressive stress profiles in the weldments; • Develop a FSP method to surface alloy the 304L with nitrogen and Mo by adding CrN and Mo powders; • Evaluate the surface compressive residual stress profile during FSW and FSP processes; • Evaluate the localized corrosion resistance of the FSW and FSP samples as a function of temperature, chloride concentration, and surface alloy composition; • Evaluate the SCC behavior of the FSW and FSP samples as a function of stress, chloride concentration, and temperature at different surface chemistries and induced residual stress profiles.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

In Situ Study on Fracture Behavior of Thick-Section Friction Stir-Welded AA 5083 Alloy

Friction stir welding (FSW) produces a gradient microstructure with distinct metallurgical zones. Here, the present study focuses on characterizing the fracture behavior during uniaxial loading across thick-section FSW joint in nonheat-treatable 5083 aluminum alloy. The hardness variation is linked to microstructural features across the weld zones through correlative microscopy. Notably, the heat-affected zone (HAZ) exhibits a lower hardness of 75 HV, while the thermomechanically affected zone (TMAZ) and stir zones (SZ) display a hardness of around 79HV. A marginal difference in hardness in HAZ prompts strain localization in HAZ on the advancing side of the weld, resulting in offset in fracture from the SZ, which is captured through in situ monitoring of the tensile test. Further, the postdeformation analysis reveals crack propagation along the maximum shear stress plane due to the coalescence of microvoids resulting from the fracturing and debonding of second-phase particles. Overall, this study provides valuable insight for optimizing the FSW process of AA 5083 alloy for thick-section applications.

36 MATERIALS SCIENCE↗

Joining AA7099 to Ni-Cr-Mo Steel using Friction Stir Dovetailing

Friction stir dovetailing (FSD) was used to join 0.5 inch (12.7 mm) AA7099 to 0.5 inch (12.7 mm) Ni-Cr-Mo steel in a lap configuration. Two new FSD approaches are reported that significantly reduce zinc embrittlement of Fe-Al intermetallic compounds (IMCs) which form during conventional friction stir welding (FSW). The first method uses the general FSD approach where a custom designed tool is employed to extrude the AA7099 into the pre-machined dovetail groove of underlying steel by forming mechanical interlocking and metallurgical bonding simultaneously. The second method uses a two-step approach where FSD of AA6061 is first used to form a silicon-rich Fe-Al IMC within the dovetail groove. AA7099 plate is then joined to the AA6061 within the dovetail using conventional FSW. A discussion of the new FSD technique, joint configurations, and process parameters are provided along with joint microstructural analyses and mechanical performance.

Friction stir dovetailing, FSD, AA7099, AA6061, ro↗

Towards High-Speed friction stir welding of 25 mm Thick AA2139-T8: tool innovation and process development

Joining thick plates (≥ 12 mm) of aluminum (Al) alloys is challenging due to high tool forces, uneven material flow, and non-uniform heat distribution through the material’s thickness. Recent advancements in tool design and welding parameters for friction stir welding (FSW) in thick plates butt joining have encountered a developmental plateau, highlighting the need for innovative approaches to overcome existing limitations. Here, this study focuses on the systematic development of single-pass and double-pass FSW processes for high-strength aluminum alloy AA2139-T8, to improve joint efficiency and enable high-speed welding capabilities. Experimental evidence is presented for a novel tool design with opposing pin threads, enabling high-speed (178 mm/min) single-pass friction stir butt welding of 25 mm thick AA2139-T8. A series of FSW trials was conducted both in air and with a trailing water spray, using steel backing plates (BPs) to investigate the impact of quenching and cooling rates on process response and joint performance. A joint efficiency of 83% was attained using the novel tool features and effectively controlling process forces and thermal boundary conditions.

AA2139-T8↗

Computationally inexpensive part-scale thermal history of additive friction-stir deposition

This study presents an analytical model for steady-state power generation and tool heat loss in additive friction-stir deposition (AFSD), developed to enable part-scale thermal simulation while remaining computationally inexpensive. The model predicts total generated power, yielding 3.7–4.7 kW across deposition temperature setpoints of 400–460 °C for the deposition of AA6061 with a Be-Cu tool. This corresponds to 90–95% of the reported spindle power. Tool heat loss is experimentally determined by calibrating a steady-state energy balance between the generated power, the substrate-deposition thermal gradient, and a temperature dependent tool heat loss term: q tool (T) = a + b (T - 400°C) with a = 2.7 x 10 6 Wm -2 and b = 9.5 x 10 3 Wm -2 K -1 . The calibration indicates that about 69% of the generated heat is conducted into the tool for this configuration, which is much higher than previously reported. The calibrated heat-source is implemented in finite element software (Adamantine) to simulate the transient thermal history of a 100 cm 3 representative build in 8 min on a standard desktop (at 0.635 mm build-height resolution). For the first three layers, the substrate temperatures between simulation and experiment are within 10% mean absolute percentage error. Sensitivity analysis indicates that uncertainties in average deposition temperature and deformation localization (stir-zone geometry, depth, and spatial dependance of strain-rate and flow stress) dominate model variance, motivating additional experimental verification.

Additive Friction-Stir Deposition↗

Effect of Friction Stir Processing on Microstructure and Tensile Properties of an Investment Cast Al-7Si-0.6Mg Alloy

Friction stir processing (FSP) is emerging as a promising tool for microstructural modification. The present study assesses the effects of FSP on the microstructure and mechanical properties of an investment cast Al-7Si-Mg alloy. FSP eliminates porosity and significantly refines eutectic Si particles. The extent of particle refinement varied with changes in processing conditions. High tool rotation rate and low to intermediate tool traverse speed generated a higher volume fraction of finer particles. Tensile ductility changed significantly as a result of FSP, whereas UTS improved only marginally. Yield strength was similar in both cast and FSPed samples under various heat treated conditions, with the highest value obtained after a T6 heat treatment. Further, FSP caused significant grain refinement in the stir zone, subsequently transforming into very coarse grains as abnormal grain growth (AGG) occurred during solution treatment at high temperature.

36 MATERIALS SCIENCE↗

Efficient Melt Stirring Induced by the Coupled Effects of Alternating Magnetic Field and Configuration of Cold Crucible

In the present study, the fluid flow in cold crucible and its effects on solute transport were numerically and experimentally investigated. It was found that the coupled effects of alternating magnetic fields and the configuration of cold crucible induce a vigorous three-dimensional melt flow. Further, solute transport results indicate that the three-dimensional flow contributes to more efficient melt stirring, and the stirring efficiency for obtaining uniform melt is improved by 77.5 pct compared with only meridional flow.

36 MATERIALS SCIENCE↗

Evolutions of the Micro- and Macrostructure and Tensile Property of Cu-15Ni-8Sn Alloy During Electromagnetic Stirring-Assisted Horizontal Continuous Casting

The present study investigates the evolution of the micro- and macrostructure and tensile property of the Cu-15Ni-8Sn (weight percent) alloy prepared by horizontal continuous casting and electromagnetic stirring (EMS). The results show that the application of EMS is beneficial for grain refinement and for microstructure transformation from the dendrite to the rosette structure and that it leads to a significant improvement in the tensile property. The forced flow induced by EMS homogenizes the temperature field ahead of the solid-liquid interface, disturbing the heat flow direction and resulting in the columnar to equiaxed transition. The grain refinement under different electromagnetic stirring frequencies is mainly derived from the homogenization of the temperature and the remelting of dendritic arms. In addition, the evolution of the tensile property with and without EMS is discussed from the perspective of fracture mode and fine-grain strengthening.

36 MATERIALS SCIENCE↗

Creep Behavior of Friction Stir Processed Haynes 282

Haynes 282 is a nickel-based superalloy designed for use in hot sections of turbines for aircraft and power generation. In these applications, elevated temperature creep performance is critical. To that end, creep behavior of friction stir processed material was carried out to investigate the high-temperature performance of this alloy. Friction stir processing of Haynes 282 was successfully completed, and the processed region was found to be defect-free. Various mechanical property characterization approaches were carried out in post-heat treated condition. Transverse tensile samples repeatedly failed in the base metal indicating 100% joint efficiency. Creep property evaluation was completed at 760 °C and at various stress levels. The creep-rupture lifetime of the processed material was similar to the base metal. Detailed electron microscopy analysis of the failed sample was carried out to understand the microstructural evolution in various locations of the sample during creep.

creep↗