Search NASA⌕ Search

SEARCH · Search NASA

Results for “Solid electrolyte interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Effect of Water Concentration in LiPF 6 -Based Electrolytes on the Formation, Evolution, and Properties of the Solid Electrolyte Interphase on Si Anodes

A trace amount of water in an electrolyte is one of the factors detrimental to the electrochemical performance of silicon (Si)-based lithium-ion batteries that adversely affect the formation and evolution of the solid electrolyte interphase (SEI) on Si-based anodes and change its properties. Thus far, a lack of fundamental and mechanistic understanding of SEI formation, evolution, and properties in the presence of water has inhibited efforts to stabilize the SEI for improved electrochemical performance. As such, we investigated the SEI formed in a Gen2 electrolyte (1.2 M LiPF6 in ethylene carbonate/ethyl methyl carbonate, 3:7 wt %, water content: <10 ppm) with and without additional water (50 ppm) at varying potentials (1.0, 0.5, 0.2, and 0.01 V vs Li/Li + ). The impact of additional water on the morphological, (electro)chemical, and structural properties of SEI was studied using microscopic (atomic force microscopy and scanning spreading resistance microscopy) and spectroscopic (X-ray photoelectron spectroscopy, attenuated total reflection Fourier-transform infrared spectroscopy, and time-of-flight secondary ion mass spectrometry) techniques. The SEI exhibits both potential- and water concentration-dependent trends in its morphology and chemical composition. The presence of additional water in the electrolyte causes parasitic reactions, which onset at ~1.0 V, resulting in a reduction of electrolyte components and result in the formation of an insulating, fluorophosphate-rich SEI. In addition, hydrolysis of LiPF 6 creates hydrofluoric acid, which reacts with the surface oxide layer on the Si electrode, leading to a pitted and inhomogeneous SEI structure.

36 MATERIALS SCIENCE↗

Quantification of Inactive Lithium and Solid–Electrolyte Interphase Species on Graphite Electrodes after Fast Charging

Rapid charging of Li-ion batteries is limited by lithium plating on graphite anodes, whereby Li+ ions are reduced to Li metal on the graphite particle surface instead of inserting between graphitic layers, which directly contributes to cell capacity loss because of the low reversibility of the Li plating/stripping process. Furthermore, precisely identifying the onset and amount of Li plating is therefore vital in order to remedy these issues. We demonstrate a titration technique with a detection limit of 20 nmol (5 × 10 –4 mAh) of Li that can be used to quantify inactive Li that remains on the graphite electrode after fast charging. The titration is extended to quantify the total amount of solid carbonate species and lithium acetylide (Li 2 C 2 ) within the solid–electrolyte interphase (SEI), and electrochemical modeling is used to determine the Li plating exchange current density (10 A/m 2 ) and stripping efficiency (65%) of plated Li metal on graphite. These techniques provide a highly accurate measure of the onset of Li plating and quantitative insight into graphite SEI evolution during fast charging.

25 ENERGY STORAGE↗

3D Artificial Solid-Electrolyte Interphase for Lithium Metal Anodes Enabled by Insulator–Metal–Insulator Layered Heterostructures

Despite considerable efforts to prevent lithium (Li) dendrite growth, stable cycling of Li metal anodes with various structures remains extremely difficult due to the direct contact of the liquid electrolyte with Li. Rational design of solid-electrolyte interphase (SEI) for 3D electrodes is a promising but still challenging strategy for preventing Li dendrite growth and avoiding lithium–electrolyte side reactions in Li-metal batteries. Here, a 3D architecture is constructed with g-C 3 N 4 /graphene/g-C 3 N 4 insulator–metal–insulator sandwiched nanosheets to guide uniform Li plating/stripping in the van der Waals gap between the graphene and the g-C 3 N 4 , and the function of which can be regarded as a 3D artificial SEI. Li deposition on the surface of g-C 3 N 4 is suppressed due to its insulating nature. However, its uniform lithiophilic sites and nanopore channels enable homogeneous lithium plating between the graphene and the g-C 3 N 4 , prohibiting the direct contact of the electrolyte with the Li metal. The use of the g-C 3 N 4 -layer-modified 3D anode enables long-term Li deposition with a high Coulombic efficiency and stable cycling of full cells under high cathode loading, limited Li excess, and lean electrolyte conditions. The concept of a 3D artificial SEI will shed light on developing safe and stable Li-metal anodes.

25 ENERGY STORAGE↗

The Chemistry, Formation and Passivation of Solid-Electrolyte Interphase (SEI) from FSI- Breakdown at Li-metal Potential

LiFSI-based liquid electrolytes are promising for realizing high Coulombic efficiency (CE) and long cycle life of next-generation high-energy Li metal battery. Nevertheless, the fundamentals of both the chemistry and formation of solid-electrolyte interphase (SEI) in these electrolytes have remained elusive. Herein, we extensively combine electrochemistry and X-ray photoelectron spectroscopy (XPS) to illustrate the reaction pathways of electrolyte decomposition, especially FSI- breakdown, as well as the dissolution trend of various inorganic SEI components. The SEI-forming reactions at Cu/electrolyte interface manifest a potential (E) dependence, driven by direct electron-transfer (ET) and Li underpotential-deposition (Li UPD) at high and low E regions, respectively. By closely correlating the XPS data obtained with and without solvent washing, we demonstrate that not all the products derived from SEI reactions are incorporated into forming a passivating surface layer, with a notable portion dissolving into liquid electrolyte instead. Importantly, high-CE electrolyte dictated by the chemical identity of solvent, is found to exhibit minimized interfacial reactivity of SEI formation enabling more effective interphasial passivation, via preferential integration of passivating ingredients such as LiF. Overall, this work formulates a systematic understating of bridging the SEI chemistry, formation and passivation while identifying key characteristics of high-performance electrolyte for guiding future design.

Bao, Zhenan [SLAC National Accelerator Laboratory ↗

Knowledge-driven design of solid-electrolyte interphases on lithium metal via multiscale modelling

Abstract Due to its high energy density, lithium metal is a promising electrode for future energy storage. However, its practical capacity, cyclability and safety heavily depend on controlling its reactivity in contact with liquid electrolytes, which leads to the formation of a solid electrolyte interphase (SEI). In particular, there is a lack of fundamental mechanistic understanding of how the electrolyte composition impacts the SEI formation and its governing processes. Here, we present an in-depth model-based analysis of the initial SEI formation on lithium metal in a carbonate-based electrolyte. Thereby we reach for significantly larger length and time scales than comparable molecular dynamic studies. Our multiscale kinetic Monte Carlo/continuum model shows a layered, mostly inorganic SEI consisting of LiF on top of Li 2 CO 3 and Li after 1 µs. Its formation is traced back to a complex interplay of various electrolyte and salt decomposition processes. We further reveal that low local Li + concentrations result in a more mosaic-like, partly organic SEI and that a faster passivation of the lithium metal surface can be achieved by increasing the salt concentration. Based on this we suggest design strategies for SEI on lithium metal and make an important step towards knowledge-driven SEI engineering.

25 ENERGY STORAGE↗

Monolithic solid–electrolyte interphases formed in fluorinated orthoformate-based electrolytes minimize Li depletion and pulverization

Lithium (Li) pulverization and associated large volume expansion during cycling is one of the most critical barriers for the safe operation of Li-metal batteries. Here, we report an approach to minimize the Li pulverization using an electrolyte based on a fluorinated orthoformate solvent. The solid–electrolyte interphase (SEI) formed in this electrolyte clearly exhibits a monolithic feature, which is in sharp contrast with the widely reported mosaic- or multilayer-type SEIs that are not homogeneous and could lead to uneven Li stripping/plating and fast Li and electrolyte depletion over cycling. The highly homogeneous and amorphous SEI not only prevents dendritic Li formation, but also minimizes Li loss and volumetric expansion. Furthermore, this new electrolyte strongly suppresses the phase transformation of the LiNi 0.8 Co 0.1 Mn 0.1 O 2 cathode (from layered structure to rock salt) and stabilizes its structure. In conclusion, tests of high-voltage Li||NMC811 cells show long-term cycling stability and high rate capability, as well as reduced safety concerns.

25 ENERGY STORAGE↗

Preventing Electrolyte Decomposition on a Ca Metal Electrode Interface Using an Artificial Solid‐Electrolyte Interphase

Abstract Calcium ion batteries are gaining attention as alternatives to lithium‐ion technology because they offer comparable properties at reduced cost and improved safety. However, progress has been limited because of the inability to efficiently and reversibly plate and strip Ca metal anodes in organic electrolytes. Moreover, the inorganic components of the solid‐electrolyte interphase (SEI) that form via decomposition of the electrolyte often do not allow for the diffusion of Ca ions. In this work, an approach combining density functional theory and ab initio molecular dynamics (AIMD) simulations is utilized to show that the use of a preformed artificial SEI layer of amorphous can potentially prevent electrolyte decomposition. First, Ca is shown to be able to intercalate into an amorphous layer (up to Ca 1.5 Al 2 O 3 ) and diffuse through on a reasonable time scale. Through calculation of the density of states, the system is found to remain insulating up to the equilibrium stoichiometry. Finally, AIMD simulations with a realistic organic electrolyte environment are used to show that this calcinated layer completely prevents the decomposition of solvent molecules. This approach can provide a route to efficient rechargeable Ca ion batteries, paving the way for cheap large‐scale energy storage.

Young, Joshua↗

Salt-rich solid electrolyte interphase for safer high-energy-density Li metal batteries with limited Li excess

We propose a carbonate-based electrolyte optimized with dual cations and ionic liquid for high-efficiency Li metal batteries with a high-voltage cathode. An average coulombic efficiency of Li deposition of 99.6% is achieved due to the salt-rich solid electrolyte interphase and Na guided uniform Li plating. The Li||NCM811 cells can be cycled with limited Li (N/P = 1) over 90 cycles. An additional advantage is that it improves the thermal stability of the NCM811 cathode.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Anion modification for stable solid electrolyte interphase in anode-free lithium metal batteries

The durability of anode-free Li metal batteries is largely limited by the undesired Li plating/stripping irreversibility on the current collector due to the infinite volume change, uncontrollable Li dendrite growth, and continuous parasitic reactions between Li metal and the electrolyte. To address these challenges, the formation of a stable and robust solid electrolyte interphase (SEI) with high ionic conductivity and strong mechanical strength is critical. Here, we developed an advanced electrolyte by introducing LiNO 3 into the localized high concentration electrolyte (LHCE) with lithium bis(fluorosulfonyl)imide (LiFSI) salt, 1,2-dimethoxyethane (DME) solvent, and 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropylether (TFTE) diluent to in situ construct a LiF and Li x N y O z co-enriched passivation layer on the Cu current collector. The synergetic effect of high mechanical strength of LiF and high ionic conductivity of Li x N y O z endows the Li metal anode with a high Coulombic efficiency (CE) of 99.35%. In conclusion, in anode-free Li metal pouch cell using LiFePO 4 (LFP) as a cathode holds an exceptionally improved capacity retention under the charging/discharging rate of 1/3 C, demonstrating great promise for developing dendrite-free and safe Li metal batteries.

25 ENERGY STORAGE↗

Evaluating the solid electrolyte interphase formed on silicon electrodes: A comparison of ex situ X-ray photoelectron spectroscopy and in situ neutron reflectometry

This work details the in situ characterization of the interface between a silicon electrode and an electrolyte using a linear fluorinated solvent molecule, 0.1 M lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) in deuterated dimethyl perfluoroglutarate (d6-PF5M 2 ) (1.87 x 10 -2 mS/cm -1 ). The solid electrolyte interphase (SEI) composition and thickness determined via in situ neutron reflectometry (NR) and ex situ X-ray photoelectron spectroscopy (XPS) were compared. The data show that SEI expansion and contraction (breathing) during electrochemical cycling was observed via both techniques; however, ex situ XPS suggests that the SEI thickness increases during Si lithiation and decreases during delithiation, while in situ NR suggests the opposite. The most likely cause of this discrepancy is the selective removal of SEI components (top 20 nm of the SEI) during the electrode rinse process, required to remove electrolyte residue prior to ex situ analysis, demonstrating the necessity of performing SEI characterizations in situ.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Solvation Rule for Solid‐Electrolyte Interphase Enabler in Lithium‐Metal Batteries

Abstract Despite the exceptionally high energy density of lithium metal anodes, the practical application of lithium‐metal batteries (LMBs) is still impeded by the instability of the interphase between the lithium metal and the electrolyte. To formulate a functional electrolyte system that can stabilize the lithium‐metal anode, the solvation behavior of the solvent molecules must be understood because the electrochemical properties of a solvent can be heavily influenced by its solvation status. We unambiguously demonstrated the solvation rule for the solid‐electrolyte interphase (SEI) enabler in an electrolyte system. In this study, fluoroethylene carbonate was used as the SEI enabler due to its ability to form a robust SEI on the lithium metal surface, allowing relatively stable LMB cycling. The results revealed that the solvation number of fluoroethylene carbonate must be ≥1 to ensure the formation of a stable SEI in which the sacrificial reduction of the SEI enabler subsequently leads to the stable cycling of LMBs.

Su, Chi‐Cheung↗

Polysulfide reduction and Li 2 S phase formation in the presence of lithium metal and solid electrolyte interphase layer

Lithium sulfur battery is an attractive next generation technology that can meet many demands of modern society. Unfortunately, the lithium sulfur battery faces unique issues related to the polysulfide shuttle effect, that is due to reduction products dissolving in the electrolyte and their subsequent reduction on the lithium metal electrode. This adds further problems to the already challenging needs of understanding and engineering a solid electrolyte interphase (SEI) layer with desired properties. One of the most important SEI properties is its passivation of lithium metal which is critically important to the overall battery performance. Passivation is difficult to measure experimentally without the influence of many factors. This study reports an investigation of the reduction of the intermediate Li 2 S 8 over lithium already passivated with Li 2 O, Li 2 CO 3 , LiOH, LiF and Li 2 S along with exploration of Li 2 S 8 reduction over pristine lithium nanoclusters using first principles computational models. Significant formation of Li 2 S phase nucleation is found to stabilize the reduction products of the Li 2 S 8 . Here, the formation of Li 2 S is explored in-depth with lithium nanocluster-based models determining a 2 V potential increase for the reduction of polysulfides due to the formation of Li 2 S. This investigation demonstrates passivation effects of important SEI components including Li 2 S.

25 ENERGY STORAGE↗

Silicon Solid Electrolyte Interphase (SEI) of Lithium Ion Battery Characterized by Microscopy and Spectroscopy

The surface reactions of electrolytes with a silicon anode in lithium ion cells have been investigated. The investigation utilizes two novel techniques that are enabled by the use of binder-free silicon (BF-Si) nanoparticle anodes. The first method, transmission electron microscopy with energy dispersive X-ray spectroscopy, allows straightforward analysis of the BF-Si solid electrolyte interphase (SEI). The second method utilizes multi-nuclear magnetic resonance spectroscopy of D2O extracts from the cycled anodes. The TEM and NMR data are complemented by XPS and FTIR data, which are routinely used for SEI studies. Coin cells (BF-Si/Li) were cycled in electrolytes containing LiPF6 salt and ethylene carbonate or fluoroethylene carbonate solvent. Capacity retention was significantly better for cells cycled with LiPF6/FEC electrolyte than for cells cycled with LiPF6/EC electrolyte. Our unique combination of techniques establishes that for LiPF6/EC electrolyte the BF-Si SEI continuously grows during the first 20 cycles and the SEI becomes integrated with the BF-Si nanoparticles. The SEI predominantly contains lithium ethylene dicarbonate, LiF, and LixSiOy. BF-Si electrodes cycled with LiPF6/FEC electrolyte have a different behavior; the BF-Si nanoparticles remain relatively distinct from the SEI. The SEI predominantly contains LiF, LixSiOy, and an insoluble polymeric species.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Artificial Solid Electrolyte Interphase for Suppressing Surface Reactions and Cathode Dissolution in Aqueous Zinc Ion Batteries

Vanadium-based compounds have been widely used as electrode materials in aqueous zinc ion batteries (ZIBs) due to the multiple oxidation states of vanadium and their open framework structure. However, the solubility of vanadium in aqueous electrolytes and the formation of byproducts during the charge/discharge process cause severe capacity fading and limit cycle life. Here in this paper, we report an ultrathin HfO 2 film as an artificial solid electrolyte interphase (SEI) that is uniformly and conformally deposited by atomic layer deposition (ALD). The inactive hafnium(IV) oxide (HfO 2 ) film not only decreases byproduct (Zn 4 SO 4 (OH) 6 ·xH 2 O) formation on the surface of Zn 3 V 2 O 7 (OH) 2 ·2H 2 O (ZVO) but also suppresses the ZVO cathode dissolution in the electrolyte. As a result, the obtained HfO 2 -coated ZVO cathodes deliver higher capacity and better cycle life (227 mAh g –1 @100 mA g –1 , 90% retention over 100 cycles) compared with pristine ZVO (170 mAh g –1 @100 mA g –1 , 45% retention over 100 cycles). A mechanistic investigation of the role of HfO 2 is presented, along with data showing that our method constitutes a general strategy for other cathodes to enhance their performance in aqueous ZIBs.

25 ENERGY STORAGE↗

Tailoring solid-electrolyte interphase and solvation structure for subzero temperature, fast-charging, and long-cycle-life sodium-ion batteries

The sluggish Na + reaction kinetics with carbon materials limits the fast-charging capability, Coulombic efficiency, and cycle life of sodium-ion batteries, especially at low temperatures. Herein, free-standing carbon nanofiber films, with controllable crystallinity and surface chemistry, are used as a platform to investigate the correlation between Na + reaction kinetics, storage mechanism, and electrolyte environment. The ion solvation effect and solid-electrolyte interphase (SEI) properties determine the kinetics and storage mechanism. A strong Na + -solvent interaction, such as Na + -diglyme, tends to form a "pseudo-SEI" layer dominated by anion decomposition, enabling fast Na + -solvent co-intercalation kinetics. Tuning the SEI chemistries by pre-cycling in the weakly solvated electrolyte (e.g., ester electrolyte), the intercalation capacity rapidly disappears due to the high energy barrier for Na + transport. Finally, such mechanistic insights allow us to develop the optimal combination of electrode materials and electrolyte chemistry to achieve high initial Coulombic efficiency, ultra-long cycle life under fast charging, and excellent low-temperature performance.

25 ENERGY STORAGE↗

High Current Cycling in a Superconcentrated Ionic Liquid Electrolyte to Promote Uniform Li Morphology and a Uniform LiF-Rich Solid Electrolyte Interphase

High-energy-density systems with fast charging rates and suppressed dendrite growth are critical for the implementation of efficient and safe next-generation advanced battery technologies such as those based on Li metal. However, there are few studies that investigate reliable cycling of Li metal electrodes under high-rate conditions. in this work, by employing a superconcentrated ionic liquid (IL) electrolyte, we highlight the effect of Li salt concentration and applied current density on the resulting Li deposit morphology and solid electrolyte interphase (SEI) characteristics, demonstrating exceptional deposition/dissolution rates and efficiency in these systems. Operation at higher current densities enhanced the cycling efficiency, e.g., from 64 ± 3% at 1 mA cm –2 up to 96 ± 1% at 20 mA cm –2 (overpotential <±0.2 V), while resulting in lower electrode resistance and dendrite-free Li morphology. A maximum current density of 50 mA cm –2 resulted in 88 ± 3% cycling efficiency, displaying tolerance for high overpotentials at the Ni working electrode (0.5 V). X-ray photoelectron microscopy (XPS), time-of-flight secondary-ion mass spectroscopy (ToF-SIMS), and scanning electron microscopy (SEM) surface measurements revealed that the formation of a stable SEI, rich in LiF and deficient in organic carbon species, coupled with nondendritic and compact Li morphologies enabled enhanced cycling efficiency at higher currents. Reduced dendrite formation at high current is further highlighted by the use of a highly porous separator in coin cell cycling (1 mAh cm –2 at 50 °C), sustaining 500 cycles at 10 mA cm –2 .

25 ENERGY STORAGE↗

Buildup of the Solid Electrolyte Interphase on Lithium-Metal Anodes: Reactive Molecular Dynamics Study

Using reactive molecular dynamics simulations, we evaluate atomistic-level interactions leading to the formation of surface films on a Li-metal (100) surface in contact with an electrolyte solution. We observe the evolution of the interfacial region and the formation of well-defined regions with varying density and oxidation state of Li; the penetration of electrolyte molecules and in some cases their electron transfer-driven decomposition leading to the initial formation of solid electrolyte interphase products. The simulations are done in the absence of a bias potential and using various electrolyte compositions including highly reactive solvents such as ethylene carbonate and less reactive solvents such as 1,3-dioxolane mixed with a 1 M concentration of a lithium salt. The structure and oxidation state of Li and some of the fragments are followed through the metal dissolution process. The results are important to understand the nature of the Li-metal anode/electrolyte interface at open-circuit potential.

25 ENERGY STORAGE↗

Efficient Lithium Metal Cycling over a Wide Range of Pressures from an Anion-Derived Solid-Electrolyte Interphase Framework

Advanced electrolytes were developed to improve the cyclability of lithium (Li) metal anodes, yet their working mechanisms remain unclear. Here, we study the Li cycling performance under different pressures in a 1 M Li bis(fluorosulfonyl)imide/fluorinated 1,4-dimethoxybutane electrolyte. A consistently long cycle life is achieved over a wide range of pressures (30–600 psi). We find that this is due to a completely different Li plating mode with more favorable deposition morphologies compared to that in a conventional carbonate electrolyte, which exhibits increasing cycle stability with increased pressure. We show that this is enabled by the properties of an anion-derived residual solid-electrolyte interphase (rSEI) framework on the electrode surface, an undercharacterized structure with profound implications for Li metal cycling. This anion-derived rSEI chemistry is likely the key to a prolonged cycle life of Li metal batteries and should be vigorously addressed in future electrolyte designs.

25 ENERGY STORAGE↗