Search NASA⌕ Search

SEARCH · Search NASA

Results for “Tensile”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Characterization and modeling of tensile behavior of ceramic woven fabric composites

This paper examines the tensile behavior of SiC/SiC fabric composites. In the characterization effort, the stress-strain relation and damage evolution are studied with a series of loading and unloading tensile test experiments. The stress-strain relation is linear in response to the initial loading and becomes nonlinear when loading exceeds the proportional limit. Transverse cracking has been observed to be a dominant damage mode governing the nonlinear deformation. The damage is initiated at the inter-tow pores where fiber yarns cross over each other. In the modeling work, the analysis is based upon a fiber bundle model, in which fiber undulation in the warp and fill directions and gaps among fiber yarns have been taken into account. Two limiting cases of fabric stacking arrangements are studied. Closed form solutions are obtained for the composite stiffness and Poisson's ratio. Transverse cracking in the composite is discussed by applying a constant failure strain criterion.

Kuo, Wen-Shyong↗

An evaluation of the +/-45 deg tensile test for the determination of the in-plane shear strength of composite materials

The applicability of the +/-45 deg tensile test for the determination of the in-plane shear strength of advanced composite laminates is studied. The assumptions used for the development of the shear strength formulas were examined, and factors such as the specimen geometry and stacking sequence were assessed experimentally. It was found that the strength of symmetric and balanced +/-45 deg laminates depends primarily upon the specimen thickness rather than the specimen width. These findings have important implications for the +/-45 deg tensile test which is recommended by several organizations for the determination of the in-plane shear stress/strain response and the shear strength of continuous fiber reinforced composites. Modifications to the recommended practices for specimen selection and shear strength determination are suggested.

Kellas, S.↗

Delamination analysis of tapered laminated composites under tensile loading

A study was conducted to analyze tapered composite laminates under tensile loading. A tapered construction made of S2/SP250 glass/epoxy laminate was used to achieve a thickness reduction using three consecutive dropped plies over a distance of 60 ply thicknesses. The principle of minimum complementary potential energy was used to determine interlaminar stresses. The interlaminar peel stress distribution shows a higher tensile intensity at the taper/thin portion juncture. The total strain energy release rate is determined using a simplified membrane model. Results are compared with a finite element simulation.

Armanios, Erian A.↗

Relevance of impacter shape to nonvisible damage and residual tensile strength of a thick graphite/epoxy laminate

A study was made to determine the relevance of impacter shape to nonvisible damage and tensile residual strength of a 36 mm thick graphite/epoxy motor case. The shapes of the impacters were as follows: 12.7 mm and 25.4 mm diameter hemispheres, a sharp corner, and a 6.3 mm diameter bolt-like rod. The investigation revealed that damage initiated when the contact pressure exceeded a critical level. However, the damage was not visible on the surface until an even higher pressure was exceeded. The impact energy to initiate damage or cause visible damage on the surface increased approximately with impacter diameter to the third power. The reduction in strength for nonvisible damage increased with increasing diameter, 9 and 30 percent for the 12.7 mm and 25.4 mm diameter hemispheres, respectively. The corner impacter made visible damage on the surface for even the smallest impact energy. The rod impacter acted like a punch and sliced through the composite. Even so, the critical level of pressure to initiate damage was the same for the rod and hemispherical impacters. Factors of safety for nonvisible damage increased with increasing kinetic energy of impact. The effects of impacter shape on impact force, damage size, damage visibility, and residual tensile strength were predicted quite well assuming Hertzian contact and using maximum stress criteria and a surface crack analysis.

Poe, Clarence C., Jr.↗

Tensile strain measurements of ceramic fibers using scanning laser acoustic microscopy

A noncontacting technique using scanning laser acoustic microscopy for making in situ tensile strain measurements of small diameter fibers was implemented for the tensile strain analysis of individual Nicalon SiC fibers (nominal diameter 15 microns). Stress vs strain curves for the fibers were plotted from the experimental data. The mean elastic modulus of the fibers was determined to be 185.3 GPa. Similar measurements were made for Carborundum SiC fibers (nominal diameter 28 microns) and Saphikon sapphire fibers (nominal diameter 140 microns).

Kent, Renee M.↗

Failure mechanisms of 3-D woven SiC/SiC composites under tensile and flexural loading at room and elevated temperatures

Nicalon silicon carbide 3D yarn with silicon carbide matrix composites made through a chemical vapor infiltration (CVI) process were investigated under tensile and flexural loading at 23, 1200 and 1550 C in air. The effectiveness of a chemical vapor deposition (CVD) SiC surface coating was also evaluated in severe oxidizing environment. Acoustic emission sensors and in situ optical microscopy were used at room temperature to monitor the failure mechanisms. It is shown that the level of tensile stress at which nonlinear behavior begins is not drastically reduced at 1200 and 1550 C when composites were protected by a SiC surface coating. Extensive fiber pull-out was observed only in the 1550 C specimen. Similar behaviors were also found in flexural specimens.

Chulya, Abhisak↗

Graphite/Polyimide Tabs For High-Temperature Tensile Tests

Delamination from ceramic composite specimens prevented. Tabs made from composite of graphite and PMR-15 polyimide enable high-temperature tensile testing of flat coupons of ceramic-matrix composites. Also used in high-temperature tensile testing of flat coupons of ceramics, metals, and metal-matrix composites.

Gyekenyesi, John Z.↗

Tensile properties of cast titanium alloys: Titanium-6Al-4V ELI and Titanium-5Al-2.5Sn ELI

This work was performed to determine the tensile properties of cast, hot isostatic pressed (HIP'ed), and annealed titanium alloys, Ti-6Al-4V ELI and Ti-5Al-2.5Sn ELI, that are candidate materials for the space transportation main engine (STME) liquid hydrogen turbopump impeller. Samples of the cast alloys were HIP'ed, annealed, and machined into tensile specimens. The specimens were tested in air at ambient temperature (70 F) and also at -423 F in liquid hydrogen. The Ti-6Al-4V alloy had an average ultimate strength of 129.1 ksi at 70 F and 212.2 ksi at -423 F. The Ti-5Al-2.5Sn alloy had an average ultimate strength of 108.4 ksi at 70 degrees F and 185.0 ksi at -423 F. The ductility, as measured by reduction of area, for the Ti-6Al-4V averaged 15.2 percent at 70 F and 8.7 percent at -423 F, whereas for the Ti-5Al-2.5Sn alloy average reduction of area was 24.6 percent at 70 F and 11.7 percent at -423 F.

Billinghurst, E. E., Jr.↗

Acousto-Ultrasonic analysis of failure in ceramic matrix composite tensile specimens

Three types of acousto-ultrasonic (AU) measurements, stress-wave factor (SWF), lowest antisymmetric plate mode group velocity (VS), and lowest symmetric plate mode group velocity (VL), were performed on specimens before and after tensile failure. Three different Nicalon fiber architectures with ceramic matrices were tested. These composites were categorized as 1D (unidirectional fiber orientation) SiC/CAS glass ceramic, and 2D and 3D woven SiC/SiC ceramic matrix materials. SWF was found to be degraded after tensile failure in all three material categories. VS was found to be degraded only in the 1D SiC/CAS. VL was difficult to determine on the irregular specimen surfaces but appeared unchanged on all failed specimens. 3D woven specimens with heat-treatment at high temperature exhibited degradation only in SWF.

Kautz, Harold E.↗

Tensile strain-rate sensitivity of tungsten/niobium composites at 1300 to 1600 K

The tensile behavior of continuous tungsten fiber reinforced niobium composites (W/Nb), fabricated by an arc-spray process, was studied in the 1300 to 1600 K temperature range. The tensile properties of the fiber and matrix components as well as of the composites were measured and were compared to rule of mixtures (ROM) predictions. The deviation from the ROM was found to depend upon the chemistry of the tungsten alloy fibers, with positive deviations for ST300/Nb (i.e., stronger composite strength than the ROM) and negative or zero deviations for 218/Nb.

Yun, H. M.↗

Effect of tensile mean stress on fatigue behavior of single-crystal and directionally solidified superalloys

Two nickel base superalloys, single crystal PWA 1480 and directionally solidified MAR-M 246 + Hf, were studied in view of the potential usage of the former and usage of the latter as blade materials for the turbomachinery of the Space Shuttle main engine. The baseline zero mean stress (ZMS) fatigue life (FL) behavior of these superalloys was established, and then the effect of tensile mean stress (TMS) on their FL behavior was characterized. A stress range based FL prediction approach was used to characterize both the ZMS and TMS fatigue data. In the past, several researchers have developed methods to account for the detrimental effect of tensile mean stress on the FL for polycrystalline engineering alloys. These methods were applied to characterize the TMS fatigue data of single crystal PWA 1480 and directionally solidified MAR-M 246 + Hf and were found to be unsatisfactory. Therefore, a method of accounting for the TMS effect on FL, that is based on a technique proposed by Heidmann and Manson was developed to characterize the TMS fatigue data of these superalloys. Details of this method and its relationship to the conventionally used mean stress methods in FL prediction are discussed.

Kalluri, Sreeramesh↗

Tensile creep and creep-recovery behavior of a SiC-fiber-Si3N4-matrix composite

The tensile creep and creep-recovery behavior of a hot-pressed unidirectional SiC-fiber/Si3N4-matrix composite was investigated at 1200 C in air, in order to determine how various sustained and cyclic creep loading histories would influence the creep rate, accumulated creep strain, and the amount of strain recovered upon specimen unloading. The data accumulated indicate that the fundamental damage mode for sustained tensile creep at stresses of 200 and 250 MPa was periodic fiber fracture and that the creep life and the failure mode at 250 MPa were strongly influenced by the rate at which the initial creep stress was applied. Cyclic loading significantly lowered the duration of primary creep and the overall creep-strain accumulation. The implications of the results for microstructural and component design are discussed.

Holmes, John W.↗

Corrosion Embrittlement of Duralumin VI The Effect of Corrosion Accompanied by Stress on the Tensile Properties of Sheet Duralumin

The effect of corrosion on the tensile properties of duralumin while stressed is shown in graphical form. According to the test results, duralumin sheet, coated with aluminum, maintains its initial properties unimpaired for corrosion periods as long as 60 days with an applied tensile stress as high as 20,000 lb/sq.in., which is approximately one-half the stress corresponding to the yield point as defined here. In these tests, that material which had been heat-treated by being quenched in cold water, though far inferior to similar material having the aluminum coating, was superior to the sheet material which was heat treated by being quenched in hot water. These results are in excellent agreement with the results of previous laboratory and exposure tests.

Rawdon, Henry S↗

Tensile and pack compressive tests of some sheets of aluminum alloy, 1025 carbon steel, and chromium-nickel steel

Tensile and compressive stress-strain curves, stress-deviation curves, and secant modulus-stress curves are given for longitudinal and transverse specimens of 17S-T, 24S-T, and 24S-RT aluminum-alloy sheet in thicknesses from 0.032 to 0.081 inch, 1025 carbon steel sheet in thicknesses of 0.054 and 0.120 inch, and chromium-nickel steel sheet in thicknesses form 0.020 to 0.0275 inch. Significant differences were found between the tensile and the compressive stress-strain curves, and also the corresponding corollary curves; similarly, differences were found between the curves for the longitudinal and transverse directions. These differences are of particular importance in considering the compressive strength of aircraft structures made of thin sheet. They are explored further for the case of compression by giving tangent modulus-stress curves in longitudinal and transverse compression and dimensionless curves of the ratio of tangent modulus to Young's modulus and of the ratio of reduced modulus for a rectangular section to Young's modulus, both plotted against the ratio of stress to secant yield strength.

Atchison, C S↗

Interaction of Bearing and Tensile Loads on Creep Properties of Joints

The interaction of bearing and tensile loads on the creep behavior of joints was studied. A specimen was designed for this study which possessed some of the general features of pin and rivet joint connections and an apparatus was constructed to apply both bearing and tensile loads to the joint model. Deformation measurements were made by use of a photogrid printed on the joint model.

CONNECTIONS, STRUCTURAL↗

Plastic Stress-strain Relations for 75S-T6 Aluminum Alloy Subjected to Biaxial Tensile Stresses

In this investigation, the material tested was a 75S-T6 aluminum alloy and the stresses were essentially biaxial and tensile. The biaxial tensile stresses were produced in a specially designed testing machine by subjecting a thin-walled tubular specimen to axial tension and internal pressure. Plastic stress-strain relations for various biaxial stress conditions were obtained using a clip-type SR-4 strain gage. Three types of tests were made: Constant-stress-ratio tests, variable-stress-ratio tests, and special tests. The constant-stress-ratio test results gave control data and showed the influence of biaxial stresses on the yield, fracture, and ultimate strength of the material. By means of the variable-stress-ratio tests, it is possible to determine whether there is any significant difference between the flow and deformation type of theory. Finally, special tests were conducted to check specific assumptions made in the theories of plastic flow. The constant-stress-ratio tests show that the deformation theory based on the octahedral, effective; or significant stress-strain relations is in approximate agreement with the test results. The variable-stress-ratio tests show that both the deformation and flow theory are in equally good agreement with the test results.

Marin, Joseph↗

Through-the-thickness tensile strength of textile composites

A series of tests was run to characterize the through-the-thickness tensile strength for a variety of composites that included 2D and 3D braids, 2D and 3D weaves, and prepreg tapes. A new test method based on a curved beam was evaluated. The through-the-thickness deformations were characterized using moire interferometry. Failures were significantly different between the 2D and 3D materials. The 2D materials delaminated between layers due to out-of-plane tensile stresses. The strength of the 2D textile composites did not increase relative to the tapes. The 3D materials failed due to the formation of radial cracks caused by high circumferential stresses along the inner radius. A circumferential crack similar to the 2D materials produced the final failure. Final failure in the 3D materials occurred at a lower bending moment than in other materials. The early failures were caused by radial crack formation rather than low through-the-thickness strength.

Jackson, Wade C.↗

Heat Treatment Effects on the Tensile Properties and Microstructures of a SiC/RBSN Composite in Nitrogen

The room-temperature tensile properties and constituent microstructures of a unidirectionally reinforced SiC/reaction bonded silicon nitride (RBSN) composite have been investigated after heat treatments at 1400, 1600, or 1800 C in nitrogen for up to 100 hr. The composite consisted of approximately 24 vol% of aligned 140 micron diameter, continuous length, chemically vapor deposited SiC fibers in an approximately 40% porous silicon nitride matrix. The composites heat treated at 1400 C for up to 100 hr showed elastic modulus, first matrix cracking strength, and ultimate tensile strength values similar to those of the as-fabricated composites, but those heat treated for 1 hr beyond this temperature displayed losses in all three properties. Recrystallization of the SiC fibers, reaction between the carbon-rich interface coating on the fibers and the RBSN matrix, and dissociation of the RBSN matrix are the reasons for the loss of mechanical properties.

Bhatt, R. T.↗