A study of adhesive bonding in metal–metal, metal–CFRP, and CFRP–CFRP material combinations under shear deformation: Fracture morphologies and damage mechanisms

Safe design of adhesive joining in multi-materials in engineered structures requires the accumulation of numerous experimental data on the failure behavior of various adhesively-bonded material combinations under different loading conditions. The deep understanding of mechanical performance, fracturing morphologies, and main damage mechanisms is also quintessential for accelerating the development of proper physics-based and multi-scale models for assisting the design. Towards this goal, this work presents a comprehensive characterization of the failure behavior of adhesively-bonded metal–metal, metal–CFRP, and CFRP–CFRP material combinations under global shear deformation via single lap shear testing. Thanks to a synergistic combination of measurement methods by using Digital Imaging Correlation (DIC) and 3D optical profilometry, adhesive features on the adherend after failure were quantified and the main progressive damage mechanisms were identified. The characterization performed in this work provides quantitative data that contributes to a better understanding of shear failure in adhesive bonding across different bi-material combinations. Finally, the obtained results have practical implications, including the potential to enhance adhesive bonding design, identify failure causes in adhesive joints, and develop or validate computational models capable of capturing the observed behavior in various adhesively-bonded materials under global shear deformation.

36 MATERIALS SCIENCE↗

Detection of voids in hydrogen embrittled iron using transmission X-ray microscopy

Hydrogen embrittlement remains a barrier to widespread adoption of hydrogen as a carbon-neutral energy source. Here, hydrogen embrittlement mechanisms are investigated across length scales in iron using transmission X-ray microscopy (TXM), digital image correlation (DIC), and notched tensile testing during in-situ electrochemical hydrogen charging. TXM reveals void size and spatial distribution ahead of a propagating crack. We find hydrogen charging leads to voids within ~10 μm of the crack tip and suppression of voids beyond this distance. Near the crack tip, voids are elongated in the direction of the crack and are smaller than voids in an uncharged sample. In the presence of hydrogen, these voids lead to quasi-cleavage fracture and a sharper crack tip. DIC shows localization and reduction of plastic strain with hydrogen charging, and tensile testing reveals a reduction in fracture energy and elongation at failure. Finally, these results are discussed in the context of hydrogen embrittlement mechanisms.

08 HYDROGEN↗

An in-situ view cell system for investigating swelling behavior of elastomers upon high-pressure hydrogen exposure

The transition to hydrogen as a clean and efficient energy carrier is impeded by challenges in the compatibility of hydrogen with materials used within hydrogen infrastructure. Elastomers, crucial in sealing components, often exhibit premature failures in high-pressure hydrogen environments due to excessive swelling. This study employs an innovative in-situ view cell system to assess the swelling behavior of hydrogenated nitrile butadiene rubber (HNBR) under various hydrogen conditions. The system, designed to withstand pressures up to 96.5 MPa, incorporates Digital Image Correlation (DIC) for strain measurements and volume estimation. Results reveal non-linear volume increases during depressurization, challenging conventional assumptions. Furthermore, investigations into peak hydrogen pressures and pressure-holding scenarios during decompression highlight complex swelling trends. The introduction of a novel computer vision (CV) method enhances precision in volume estimation, overcoming DIC limitations. The study provides insights into mitigating elastomer swelling, crucial for developing robust materials to support future hydrogen-driven energy systems.

Elastomer↗

3D optical diagnostics for explosively driven deformation and fragmentation

High-speed, optical imaging diagnostics are presented for three-dimensional (3D) quantification of explosively driven metal fragmentation. At early times after detonation, Digital Image Correlation (DIC) provides non-contact measures of 3D case velocities, strains, and strain rates, while a proposed stereo imaging configuration quantifies in-flight fragment masses and velocities at later times. Experiments are performed using commercially obtained RP-80 detonators from Teledyne RISI, which are shown to create a reproducible fragment field at the benchtop scale. DIC measurements are compared with 3D simulations, which have been ‘leveled’ to match the spatial resolution of DIC. Overall, results demonstrate improved ability to identify predicted quantities-of-interest that fall outside of measurement uncertainty and shot-to-shot variability. Similarly, video measures of fragment trajectories and masses allow rapid experimental repetition and provide correlated fragment size-velocity measurements. Measured and simulated fragment mass distributions are shown to agree within confidence bounds, while some statistically meaningful differences are observed between the measured and predicted conditionally averaged fragment velocities. Together these techniques demonstrate new opportunities to improve future model validation.

42 ENGINEERING↗

Implementation and experimental validation of nonlocal damage in a large-strain elasto-viscoplastic FFT-based framework for predicting ductile fracture in 3D polycrystalline materials

Ductile materials, such as metal alloys, can undergo substantial deformation before failure. Additionally, these materials are usually of polycrystalline composition and exhibit strongly anisotropic behavior at small length scales. Previously developed fast Fourier transform (FFT)-based models can model ductile fracture of isotropic materials or the elastic–plastic behavior of anisotropic polycrystalline materials; however, there remains a need to couple both capabilities. This work extends a large-strain FFT-based crystal plasticity model to simulate ductile fracture of polycrystalline materials. In this work, a triaxiality-based continuum damage mechanics (CDM) formulation is incorporated into a large-strain elasto-viscoplastic FFT (LS-EVPFFT) framework. The CDM formulation is augmented with an integral-based nonlocal regularization approach that correctly handles gas-phase material necessary to model unconstrained surfaces. To validate the damage-enabled LS-EVPFFT framework, mesoscale copper tensile coupons were machined using microwire electrical discharge machining and experimentally characterized using electron backscatter diffraction. In-situ optical digital image correlation was performed during uniaxial testing to provide a side-by-side comparison of the experimental and computational strain fields and stress–strain responses. The damage-enabled LS-EVPFFT framework can simulate the complete macroscopic stress–strain response of ductile polycrystals to failure. The model reproduces necking behavior that qualitatively agrees with experimental observations. By leveraging the relatively low computational cost of the damage-enabled LS-EVPFFT framework, the framework presented here allows the ductile fracture response of 3D polycrystalline materials to be tractably predicted.

36 MATERIALS SCIENCE↗

Enhanced joining strength in additive-manufactured polylactic-acid structures fused by embedded heated metallic meshes

Additively manufactured thermoplastic polymers, such as polylactic acid (PLA), hold significant promise for sustainable engineering structures, including wind turbine blades. Upscaling these structures beyond the limitations of 3D printer build volumes is a challenge; fusion joining presents a potential solution. This paper introduces a displacement-controlled resistance welding process for PLA, as an alternative to the typical force-controlled methods. Here, we investigated the bonding quality of resistance-welded and adhesive-bonded PLA beams through three-point bending and measured the surface deformations using digital image correlation. Different metal meshes (30%/0.11 mm Ni—Cu, 34%/0.07 mm Ni—Cu, and 36%/0.25 mm Co—Ni) served as heating elements. The process parameters were varied for the 34%/0.07 mm Ni—Cu mesh to identify an optimum set of parameters. Results showed that this optimized displacement-controlled welding achieved 94% of the original strength of monolithic samples. This indicates that the new welding process not only ensures high-quality bonding and fine surface finishing but also promotes sustainability, recyclability, and economic efficiency in various polymer and composite structural applications.

Additive manufacturing↗

Mitigation of distortion of Al/steel part under simulated paint baking condition: Experiment and numerical model studies

Multi-material joining of lightweight structures is essential to reduce vehicle weight for more energy savings and less greenhouse gas emission. However, mismatch of thermal expansion coefficient for dissimilar materials during the paint baking process can induce part distortion and joint failure for adhesive bonding. Here, in the present work, a thermomechanical model based on contact mechanics and large deformation theory was developed for dissimilar high-strength Al alloy and steel components to study the distortion mechanism and influential factors of the residual gap. The established model was used to optimize joint conditions, such as pitch distance and part geometry. When a weld pitch is shorter than 100 mm, the maximum gap between Al and steel part can be greatly reduced to 0.1 mm, and the local stress and plastic strain around the joint during the oven heating and cooling cycle are also substantially reduced compared with the long pitch case (900 mm). The numerical modeling results revealed that a comparable bending stiffness ratio between the steel and Al cross sections is critical to the minimization of gap and distortion under paint baking condition. Digital image correlation technique was used to measure the overall part distortion and local strain distribution that were used to validate the model prediction. Weld bonding (adhesive bonding with friction bit joining) process was successfully employed to join Al to steel component without gap opening in adhesive after the paint baking and cooling.

36 MATERIALS SCIENCE↗

Damage evolution and ductile fracture of commercially-pure titanium sheets subjected to simple tension and cyclic bending under tension

This paper describes a study into the evolution of damage in commercial-purity titanium (CP–Ti) sheets subjected to cyclic bending under tension (CBT) and uniaxial tension (simple tension, ST). Sections were taken from sheets that were strained to various levels under both methods and were imaged using X-ray computed tomography (XCT) to reveal insights into the size, density, and distribution of microvoids in the sheets. Digital image correlation (DIC) was also used to observe the surface strain of CBT and ST sheets during testing. These results showed that elongation to failure (ETF) for CBT deformation is about 2.5× higher than for ST, local longitudinal strains in the bulk of the CBT sample are around 1.3× higher than the peak strain in the ST necked region, and 1.7× higher in the localized region of CBT failure. It was found that the volume-density of voids in both sheets followed a similar exponential increase with strain, reaching nearly 45× higher in the CBT than the ST sheets before the onset of failure, mainly due to the higher strain levels achieved. A higher volume density of voids developed in the center of sheets at high levels of strain, for both processes, with the density in the sheet center becoming approximately double that found near the edges. Scanning electron microscopy (SEM) was used to examine the fracture surface of CBT and ST sheets after failure. The observations are presented and discussed highlighting the CBT process as effective to delay ductile fracture of the CP-Ti sheets.

Commercially pure titanium↗

Strength-ductility synergy through microstructural and compositional heterogeneity in directed energy deposition additive manufacturing of face-centered cubic materials

Directed energy deposition (DED) is an additive manufacturing (AM) process based on welding technology and offers the advantages of large build volume, high deposition rate, and ability to fabricate multi-material parts. Epitaxial continuous columnar grain growth is a characteristic microstructural feature of DED processed alloys. In this study, a bamboo-like microstructure (periodic alternation of equiaxed and columnar structure) was produced by adopting an intermittent deposition strategy in 316L stainless steel and Inconel 625. The formation of a bamboo-like alternating microstructure was confirmed through electron backscattered diffraction (EBSD) analysis. Hardness mapping showed that the columnar to equiaxed transition (CET) occurred at the region right below the fusion line. A finite element (FE) model was used to investigate the relationship between the temperature gradient (G) and the solidification rate (R). The FE model showed a low G/R ratio at the region right below the interface promoting the CET. The grain size and material-dependent deformation behaviors are analyzed using digital image correlation (DIC). The lower deformation on the fine-grain regions observed in DIC analysis is attributed to a higher strain hardening rate, which is confirmed through dislocation density analysis on a tensile-interrupted specimen. The periodically alternating grain size coupled with the microstructural changes caused by intermittent deposition strategy result in a better strength-ductility synergy in both single-material and bimetallic specimens.

36 MATERIALS SCIENCE↗

Topology-driven compressive behavior of Inconel 718 lattice structures with Z-strut reinforcement fabricated by laser powder bed fusion

This study investigates the compressive deformation behavior and mechanical performance of Inconel 718 lattice structures fabricated by laser powder bed fusion (LPBF). Four unit-cell topologies—BCC, FCC, BCCZ, and FCCZ—were designed with a unit-cell size of 3 mm and fabricated under identical process conditions to isolate the effect of topology. Measured relative densities ranged from 14.65% to 17.72%. Compressive testing showed that Z-strut-reinforced topologies (BCCZ: 54.6 MPa; FCCZ: 80.2 MPa) exhibited higher strength than their unreinforced counterparts, which may be associated with mixed-mode deformation behavior enabled by the vertically aligned Z-struts. Finite element simulations and Digital Image Correlation (DIC) analysis support the observation of a transition from node-dominated deformation in BCC/FCC to mixed-mode deformation in BCCZ/FCCZ. These findings suggest that unit-cell topology is a key design variable for tailoring deformation mechanisms in LPBF lattice structures.

36 MATERIALS SCIENCE↗

Mechanical failure of fresh nuclear grade iron–chromium–aluminum (FeCrAl) cladding under simulated hot zero power reactivity initiated accident conditions

The reactivity initiated accident (RIA) is a postulated accident in light water reactors initiated by a rapid increase in reactivity which causes an increase in fission rate and fuel temperature. One potential mode of fuel system failure during RIA is pellet cladding mechanical interaction (PCMI) due to the rapid thermal expansion of the fuel pellet. Simulated PCMI experiments were performed by rapidly pressurizing iron-chromium-aluminum (FeCrAl) cladding tube samples using a hydraulic modified burst test system, causing the specimens to burst under a biaxial loading path. Deformation and rupture of the specimens were tracked with a telecentric lens and high-speed camera system. Outer surface strains were calculated using digital image correlation (DIC) on speckle patterns painted on the specimens’ outer surfaces. Experiments were conducted at approximately 275 °C, representative of hot zero power RIA conditions. The failure hoop strain was DIC-calculated between approximately 1.8–3.4%, corresponding to quasi-static energy depositions of approximately 110–260 calories per gram UO 2 assuming initial pellet-cladding contact. These conditions are very similar to the proposed energy deposition limit of 150 calories per gram UO 2 for unirradiated zirconium-based cladding in US Nuclear Regulatory Commission (NRC) Draft Regulatory Guide 1327. A very small strain rate dependence was observed in the data, with the magnitude of the failure hoop strain decreasing slightly with increasing strain rate. This observed dependence may be relevant because the FeCrAl cladding strain rate will be approximately 20% higher than in zirconium-based cladding due to the harder neutron spectrum and resultant shorter neutron generation time.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Influence of neutron irradiation on Al-6061 alloy produced via ultrasonic additive manufacturing

Samples of aluminum alloy 6061 produced via ultrasonic additive manufacturing (UAM) were irradiated in the High Flux Isotope Reactor (HFIR) up to 17.3 dpa at ~70°C while in contact with water using perforated rabbit capsules. The irradiation campaign included as-received (AR) material, specimens subjected to various post-weld heat treatments (PWHTs, including hot isostatic pressing [HIP]), and reference (wrought) alloy samples. Mechanical tensile tests, accompanied by digital image correlation (DIC) analysis, fractography, and metallography, were performed as a part of the post-irradiation evaluation. The X- and Y-specimens (i.e., oriented in the sonotrode moving and vibration directions, respectively) showed pronounced radiation hardening and ductility decrease. Specific serration flow behavior and propagation of deformation bands were observed under various material conditions up to 3.5 dpa but disappeared at 17.3 dpa. In all cases, the fracture mechanism of X- and Y-specimens was ductile; ductile dimples dominated the fracture surface. Irradiated X- and Y-specimens showed good performance, regardless of material conditions (AR or PWHT). The performance of Z-specimens oriented in the build direction was strongly dependent on the PWHT. The AR and aged specimens showed fracture stress decrease with dose, and they experienced fracture under irradiation after 3.5 dpa; specimen cross section analysis revealed specific interface degradation that was likely related to corrosion. Recrystallization significantly improved in-reactor performance. Finally, HIP suppressed interface degradation due to recrystallization and pore removal, which led to good in-reactor performance for Z-specimens.

36 MATERIALS SCIENCE↗

Burst characteristics of advanced accident-tolerant FeCrAl cladding under temperature transient testing

Here assessment of burst characteristics of accident-tolerant fuel (ATF) claddings is essential to evaluate the safety margins of nuclear reactors, and better understanding can enable accelerated licensing for reactor concepts that include the new materials. Therefore, this study investigated the burst behavior of an ATF candidate of C26M, which is an iron–chromium–aluminum alloy (FeCrAl) under transient testing like the simulated loss-of-coolant accident (LOCA) conditions, except the water-quenching phase, in light-water reactors (LWRs). The effect of LOCA specimen length was assessed in terms of post-burst tube parameters. No critical length effect was determined on the burst pressure, burst location, and burst size measurements. Burst temperature showed larger variation likely due to its measurement approach used in this study. The post-test diametral strain was identified as the critical parameter to reduce the specimen length as compared to tube burst length or width. Postmortem optical metrology and digital image correlation were employed to determine the local strain-state during the simulated LOCA, which showed the loading path was close to equibiaxial conditions in regions away from the burst location, rather than internally pressurized conditions (or “plane-strain” tension). Pst-test microstructural characterizations of the FeCrAl revealed that ductile damage was present at the edge of the outer radial surface while the rest of the material was ruptured via cleavage at LOCA burst temperatures. Furthermore, internal grain boundary cracks were observed at locations away from the tube burst region. This behavior was considered to occur during the cooling down period of the simulated LOCA test. Overall, this study aimed to provide essential data for fuel performance code development by considering micromechanics of the deformation and failure.

36 MATERIALS SCIENCE↗

BISON validation of FeCrAl cladding mechanical failure during simulated reactivity-initiated accident conditions*

Here, a reactivity-initiated accident (RIA) is a postulated design basis accident in light water reactors (LWRs) in which a rapid reactivity insertion induces a fission rate increase and a fuel pellet temperature rise. During RIA, the fuel pellet thermally expands and may cause pellet-cladding mechanical interaction (PCMI). Separate effects PCMI tests were performed on C26M FeCrAl cladding tube samples, introducing biaxial stress via a well understood modified burst test (MBT) system. A high-speed camera in the MBT system captured the projections, covering a 360° view of the cladding deformation and enabling a digital image correlation (DIC) method to quantify the surface strains with high fidelity. Representative hot zero-power RIA mechanical loading conditions were applied to the sample, and the test duration ranged from 20 to 500 ms at an average temperature of 573 K. BISON finite element–based fuel performance code modeling was performed against the high-fidelity DIC data produced from the MBTs. Validation calculations were conducted with 2D models and systematically compared with test data of the burst time, burst pressure, burst hoop strains, and hoop strain rates. Based on the behaviors from the separate effects test, BISON calculations satisfactorily predicted the cladding deformation behaviors. Sensitivity analysis was conducted to identify highly influential mechanical properties responsible for the cladding failure behavior during the MBT experiments. The results highlight the significance of the cladding's mechanical strength in governing cladding strain, followed by the significance of the mechanical interactions between the pellet and the cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

In-situ determination of strain during transient burst testing and the temperature dependence of Zircaloy-4 claddings

Understanding fuel system behavior during postulated loss-of-coolant accidents is pertinent for continued safe and efficient operation of light water reactors, particularly as higher burnups are being pursued and safety margins re-evaluated. Conventional mechanical models for the incumbent Zr alloys typically rely on the assumption that steady-state creep is the dominant fuel cladding response during transient accident conditions. To investigate this assumption, simulated accident burst testing was performed on Zircaloy-4 claddings with balloon behavior measured in-situ. Here, two distinct loading conditions were utilized during burst testing: (1) constant-gas-inventory where pressure was allowed to increase with temperature and (2) constant pressure. In-situ strains and strain rates were measured via 2-dimensional digital image correlation techniques and synchronized with temperature to determine deformation dependencies. The temperature dependence of strain rate was characterized by a two segment Arrhenius relationship, with a distinct transition between the high and low temperature/strain regimes. The average activation energy of the lower temperature/strain regime was 328 ± 25 kJ/mol, in agreement with the ~320 kJ/mol used for conventional LOCA models. However, the higher temperature/strain segment, which encompassed most of ballooning, showed increased activation energies as well as a dependence on whether the burst region was in view. For tests that burst away from the camera view, the average high temperature/strain segment activation energy was 635 ± 150 kJ/mol. For samples where the rupture opening formed in view, the average activation energy was 1015 ± 179 kJ/mol. This observed shift in temperature dependence indicates a transition in deformation mechanism at the end of life, possibly to time independent failure mechanisms, which has not yet been visualized in the literature for Zr alloys. Parameters at the transition points were analyzed to determine thresholds for this change in behavior, which occurred at an average hoop strain of 6.9 ± 2.1 %.

36 MATERIALS SCIENCE↗

In-situ strain behavior and BISON simulations of Zircaloy cladding subjected to temperature cycling separate-effects tests in a steam environment

Understanding fuel system performance during anticipated transients without scram (ATWSs) in boiling water reactors (BWRs) is necessary for refining current and future safety limits. High-fidelity material models and simulations are fundamental to rigorous assessment of zirconium-based cladding performance. However, experimental thermomechanical data during simulated ATWSs to validate these modes are limited. To provide relevant in-situ data, Zircaloy-4 cladding was subjected to cyclic heating in a steam environment to simulate an out-of-pile BWR ATWS. Digital image correlation was used to capture the cladding strain behavior in-situ for comparison against simulations using the BISON finite element code. Conventional high-temperature models were compared using multiple schemes to gain a better understanding of the applicability of three BISON models to BWR ATWS: (1) the default combination of creep models in BISON, (2) the high-temperature Erbacher model alone, and (3) the low-temperature Limback-Andersson model alone. The cases run with the Limback-Andersson model alone produced the lowest root mean square error (RMSE). The lowest RMSE for the Limback-Andersson model alone was 0.659%, and the highest RMSE reported was 4.22%. A data gap within the model in the temperature regime of interest was also identified, and to account for this gap, the current model in BISON is linearly interpolated between two separate datasets. In conclusion, this evaluation highlights the need to either develop a new model or to improve the existing model to capture transient creep effects resulting from a cyclic temperature transient.

Anticipated transient without SCRAM↗

The impact of chromium coatings on Zircaloy cladding deformation behavior under reactivity-initiated accident-like mechanical loading conditions

A reactivity-initiated accident (RIA) occurs when a control rod ejection or control blade drop causes an increase in the fission rate. The injection of energy results in an increase in fuel temperature which in turn causes rapid thermal expansion of the fuel pellet. This thermal expansion may result in pellet-cladding mechanical interaction (PCMI) in which the fuel imparts a mechanical strain to the cladding. PCMI may cause the cladding to fail, and thus, the mechanical response of cladding due to PCMI must be investigated when characterizing new cladding materials. Chromium-coated Zircaloy-4 is a near-term accident-tolerant fuel cladding that exhibits improved high-temperature oxidation resistance. Modified burst testing was utilized to experimentally simulate the effects of PCMI on both uncoated and chromium-coated Zircaloy cladding samples at hot zero power conditions. Samples were coated using either cold spraying or physical vapor deposition to understand the differences in behavior that the coating application method may cause. Digital image correlation was used to analyze images of the deforming specimens to extract the in-situ strain behavior of the cladding. The uncoated specimens burst at hoop strains ranging from 8.8 % to 17.2 %. The cold-spray chromium-coated Zircaloy specimens burst at hoop strains of 7.0 % to 11.0 %. The physical vapor deposition coated tubes burst at hoop strains of 9.1 % to 11.5 %. These results indicate that the chromium coating causes a loss in the ductility of the cladding. Furthermore, the higher burst hoop strains of the physical vapor deposition-coated samples relative to the cold-spray samples indicate that the cold-spraying technique causes more of a loss in ductility than physical vapor deposition. All samples burst at higher hoop strains than those expected to occur in an RIA for fresh cladding.

Accident-tolerant fuel↗

Investigation of nonlinear mechanical behavior of two superfine-grained graphites with DIC assisted disc splitting test

Using standardized uniaxial tensile test specimens is not practical due to the limited volumes in irradiation capsules, molten salt degradation facilities, or oxidation apparatus. The ASTM International Standard Test Method for Tensile Strength Estimate by Disc Compression of Manufactured Graphite (ASTM D8289) was developed to provide a convenient way for estimating tensile strength. Unlike the traditional uniaxial tensile test in ASTM C749 (International Standard Test Method for Tensile Stress–Strain of Carbon and Graphite), which uses dog-bone shaped specimens larger than 12.95 mm × 120.65 mm, the ASTM D8289 standard uses smaller discs with diameters of 6–12.7 mm. A digital image correlation (DIC) system, which uses a full-field noncontact surface displacement measurement technique, was applied along with the ASTM D8289 disc splitting test on IG-110 samples and compared with previous measurements from Mersen 2114 samples. Results confirmed that the DIC technique can measure the surface displacement/strain on these small (Ø6 mm × 3 mm) graphite specimens with good repeatability. However, Mersen 2114 and IG-110 samples exhibited strain discrepancies when DIC measurements were compared with analytical and finite element simulation values. The loading history and strain results also indicated different mechanical behaviors between Mersen 2114 and IG-110, particularly the nonlinear behavior of the IG-110 samples. Good agreement was observed by comparing the splitting tensile strengths of two superfine-grained grades with results from other work. The specimen size effect is discussed when comparing the splitting tensile strength with corresponding uniaxial tensile strength of these two graphite grades.

Lin, Lianshan [ORNL] (ORCID:0000000203399219)↗