Search NASA⌕ Search

SEARCH · Search NASA

Results for “electron backscatter diffraction (EBSD)”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Micro-structural evolution during diffusion bonding of C-SiC/C-SiC composite using Ti interlayer

Highlights: • Formation of Ti{sub 3}SiC{sub 2} MAX phase in the joint of C-SiC composite • EBSD revealed three zone microstructure of the joint • Formation of a thin continuous layer of TiSi{sub 2} • The apparent shear strength of 19 MPa - Abstract: Diffusion bonding of C-SiC composite was achieved with Ti interlayer at 1500 °C for 3 h with the applied pressure of 20 MPa. The joined C-SiC composite showed the apparent shear strength of 19 MPa and the sample fractured away from the joint. The microstructure of joint consists of Ti{sub 3}SiC{sub 2} MAX phase, TiSi{sub 2} and TiC in which Ti{sub 3}SiC{sub 2} was the major phase. The distribution of phases in the microstructure of joint was categorized into three different zones based on electron backscattered diffraction (EBSD) results. The first zone consists of a thin continuous TiSi{sub 2} phase, which was followed by a thick zone of Ti{sub 3}SiC{sub 2} MAX phase. In the middle of the sample, a mix phase zone was found. The reaction mechanism was established for the evolution above microstructure of joined C-SiC composite.

36 MATERIALS SCIENCE↗

Microstructure evolution of Ag–8Au–3Pd alloy wire during electromigration

As the continuous shrinkage of the interconnect line width in microelectronics devices, there is a growing concern about the electromigration (EM) failure of bonding wire. In addition, an innovative Ag–8Au–3Pd alloy wire has shown promise as an economical substitute for gold wire interconnects due to the cost pressure of gold in the last decade. In present study of the Ag–8Au–3Pd alloy wire, the surface diffusion occupied the dominant position during EM failure, and the activation energy was found to be 0.61 eV. In order to reveal the failure mechanism, the cross-sections of the Ag–8Au–3Pd alloy wire during EM were prepared by focused ion beam (FIB) micro-machining for electron backscatter diffraction (EBSD) analysis. The microstructure evolution of the Ag–8Au–3Pd alloy wire was characterized by the grain size and grain boundary. As a result, the EM failure originates in the atom transportation, which causes grain size increasing and atom diffusion on the wire surface. - Highlights: • The activation energy of Ag–8Au–3Pd alloy wire was obtained as 0.61 eV. • During EM, the silver atoms diffused from negative to the positive terminal on the wire surface. • The microstructure (grain size and grain boundary) was characterized by FIB-EBSD. • During EM, the atom transportation was found to cause grain size growth and atom diffusion on the wire surface.

36 MATERIALS SCIENCE↗

Identifying ferroelectric phase and domain structure using angle-resolved piezoresponse force microscopy

We used angle-resolved piezoresponse force microscopy (AR-PFM), vertical PFM (VPFM), and electron backscatter diffraction (EBSD) to provide a systematic interpretation of domain patterns in polycrystalline, near-morphotropic lead zirconate titanate. This material was used to illustrate the power of AR-PFM methods in resolving complex domain patterns where multiple phases may be present. AR-PFM was carried out with a 30° rotation interval, and the resulting data were analysed to identify the orientation of the underlying axis of piezoelectricity. The additional information provided by AR-PFM was studied, comparing its capabilities to those of 3-dimensional PFM, consisting of one VPFM image and two orthogonal lateral PFM (LPFM) images. We show that, in certain conditions, using AR-PFM can identify the phases present at the sub-grain scale. This was confirmed using VPFM and EBSD data. Furthermore, the method can discriminate laminated domain patterns that appear similar in VPFM and can reliably expose domain patterns that may not be seen in LPFM data from a single orientation, or even in 3D PFM data.

36 MATERIALS SCIENCE↗

Advanced 3D characterisation of iodine induced stress corrosion cracks in zirconium alloys

Highlights: • Macroscopic crack direction is affected by metallurgical state. • High resolution XCT reveals complex crack morphology. • 3D-EBSD used to fully characterise attacked grain boundaries. • Evidence of iodine segregation ahead of a crack tip. - Abstract: In this study, a range of advanced techniques have been used to characterise iodine-induced stress corrosion cracks, and investigate their interaction with microstructure in zirconium alloys used as cladding material in nuclear power reactors. C-ring samples, machined from cladding tubes in a recrystallised and cold worked condition, were subjected to compressive stress while submerged in an iodine-ethanol solution to simulate stress corrosion cracks arising from pellet cladding interaction. The complex morphology of these stress corrosion cracks was imaged in 3D using X-ray computed tomography (XCT), and subsequent analysis using both 2D and 3D electron backscatter diffraction (EBSD) allowed for the interaction of these cracks with microstructure to be investigated. Intergranular cracking modes were observed to dominate in the recrystallised microstructure, resulting in cracking in the radial direction with variations on the order of the grain size. Crack propagation in the cold worked microstructure was observed to be correlated with the direction of the elongated grains, resulting in a more tangential crack path with less local variation and a microstructure potentially more susceptible to iodine-induced stress corrosion cracking. 3D-EBSD using serial sectioning allows for the determination of the full five-parameter grain boundary description, and opens up the possibility of a statistical analysis of susceptible boundaries to SCC. Nanoscale secondary ion mass spectrometry (NanoSIMS) was also used to map the chemical distribution in the crack tip region and provides possible evidence of iodine segregation ahead of the crack tip. The results provide new insight into crack propagation mechanisms in recrystallised and cold worked microstructures, and pave the way for a more mechanistic understanding of crack propagation through advanced characterisation of iodine-induced stress corrosion cracks in zirconium alloys.

36 MATERIALS SCIENCE↗

Electron backscatter diffraction studies of focused ion beam induced phase transformation in cobalt

A focused ion beam microscope was used to induce cubic to hexagonal phase transformation in a cobalt alloy, of similar composition to that of the binder phase in a hardmetal, in a controlled manner at 0°, 45° and 80° ion incident angles. The cobalt had an average grain size of ~ 20 μm, allowing multiple orientations to be studied, exposed to a range of doses between 6 × 10{sup 7} and 2 × 10{sup 10} ions/μm{sup 2}. Electron backscatter diffraction (EBSD) was used to determine the original and induced phase orientations, and area fractions, before and after the ion beam exposure. On average, less phase transformation was observed at higher incident angles and after lower ion doses. However there was an orientation effect where grains with an orientation close to (111) planes were most susceptible to phase transformation, and (101) the least, where grains partially and fully transformed at varying ion doses. - Highlights: •Ion-induced phase change in FCC cobalt was observed at multiple incidence angles. •EBSD was used to study the relationship between grain orientation and transformation. •Custom software analysed ion dose and phase change with respect to grain orientation. •A predictive capability of ion-induced phase change in cobalt was enabled.

36 MATERIALS SCIENCE↗

Phase structures and morphologies of tempered CA6NM stainless steel welded by hybrid laser-arc process

The post-weld tempered microstructure of hybrid laser-arc welded CA6NM, a cast low carbon martensitic stainless steel, was investigated. The microstructural evolutions from the fusion zone to the base metal were characterized in detail using optical microscopy, scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), X-ray diffraction (XRD) and microhardness techniques. The fusion zone, in its post-weld tempered condition, consisted of tempered lath martensite, residual delta-ferrite with various morphologies, reversed austenite and chromium carbides. The reversed austenite, which can be detected through both EBSD and XRD techniques, was found to be finely dispersed along the martensite lath boundaries, particularly at triple junctions. Based on the EBSD analysis, the orientation relationship between the reversed austenite and the adjacent martensite laths seemed to follow the Kurdjumov-Sachs (K-S) model. The results also revealed the presence of the reversed austenite in the different regions of the heat affected zone after post-weld tempering. The microindentation hardness distribution was measured, and correlated to the evolution of the corresponding microstructure across the welds. - Highlights: •The EBSD analysis was performed on hybrid laser-arc welded CA6NM. •The FZ consisted of tempered lath martensite, reversed austenite, carbides and δ ferrite after tempering. •The reversed γ was formed along the α′ lath boundaries, particularly at triple junctions.

36 MATERIALS SCIENCE↗

EBSD and Nanoindentation-Correlated Study of Delamination Fracture in Al-Li Alloy 2090

Al-Li alloys offer attractive combinations of high strength and low density. However, a tendency for delamination fracture has limited their use. A better understanding of the delamination mechanisms may identify methods to control delaminations through processing modifications. A combination of new techniques has been used to evaluate delamination fracture in Al-Li alloys. Both high quality electron backscattered diffraction (EBSD) information and valid nanoindentation measurements were obtained from fractured test specimens. Correlations were drawn between nano-scale hardness variations and local texture along delaminating boundaries. Intriguing findings were observed for delamination fracture through the combined analysis of grain orientation, Taylor factor, and kernel average misorientation.

Tayon, Wesley A.↗

Three-dimensional FIB/EBSD characterization of irradiated HfAl{sub 3}-Al composite

A thermal neutron-absorbing composite comprised of 28.4 vol.% HfAl{sub 3} intermetallic particles in an Al matrix, developed for use in a conduction-cooled thermal neutron filter, will enable fast flux irradiation of materials and fuels in an existing pressurized water test reactor. In this paper, an EBSD-FIB characterization approach is used to observe the microstructural changes of the HfAl{sub 3}-Al composite in response to simulated long-term neutron irradiation. Using a focused ion beam (FIB), the sample was fabricated to 25 μm x 25 μm x 20 μm and mounted on a transmission electron microscopy (TEM) grid. A series of operations were carried out repeatedly on the sample's top surface to prepare it for scanning electron microscopy (SEM). First, a ∼ 100-nm layer was removed by high voltage FIB milling. Then, several cleaning passes were performed on the newly exposed surface using low voltage FIB milling to improve the SEM image quality. The surface was then scanned by Electron Backscattering Diffraction (EBSD) to obtain a two-dimensional image. After 50 to 100 two-dimensional images were collected, the images were stacked to reconstruct a three-dimensional model using DREAM.3D software. Two such reconstructed three dimensional models were obtained from samples of the original and post-irradiation HfAl{sub 3}-Al composite, from which the most significant microstructural change caused by neutron irradiation appears to be the size reduction of both HfAl{sub 3} and Al grains. Possible causes include thermal expansion and related thermal strain from thermal neutron capture. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Effect of Annealing Treatment on Mechanical and Magnetic Softening Behaviors of Cold Rolled Interstitial-Free Steel

The recovery and recrystallization behaviors of low-carbon interstitial-free steel are investigated at different annealing temperatures (200-690 °C) through correlation between the changes in magnetic parameters (coercivity and r.m.s. voltage), hardness, tensile strength and high-angle grain boundary fractions (HAB). Magnetic parameters and tensile strength show a significant change within recovery region (200-500 °C), while the hardness variation is very minimal at this temperature region. On the other hand, the hardness is abruptly changed compared to magnetic properties at higher annealing temperature (550-640 °C). The grain boundary characteristics and microtexture evolution occurring at recrystallization regime are evaluated by orientation imaging microscopy (OIM) and orientation distribution function (ODF) through electron backscattered diffraction (EBSD). The increase in recrystallization fraction noticeably affects microtexture property, justifying with the strengthening of γ-fiber, weakening of α-fiber and disappearance of rotated cube component with increasing annealing temperatures.

36 MATERIALS SCIENCE↗

High (1 1 1) orientation poly-Ge film fabricated by Al induced crystallization without the introduction of AlO{sub x} interlayer

High (1 1 1) orientation poly-Ge film was fabricated by Al induced crystallization (AIC), where Al and amorphous Ge (a-Ge) layers were continuously deposited by magnetron sputtering, avoiding the deliberate introduction of an AlO{sub x} interlayer. To improve the quality of poly-Ge film, the ratio of thicknesses of Al and a-Ge was adjusted. Electron backscattered diffraction (EBSD) results revealed that the (1 1 1) fraction of poly-Ge film reached 97% and the average crystal grain size surpassed 100 μm.

36 MATERIALS SCIENCE↗

Liquid metal embrittlement in laser lap joining of TWIP and medium-manganese TRIP steel: The role of stress and grain boundaries

Highlights: • This work shows liquid metal embrittlement in externally loaded laser lap welding. • Results confirmed a direct relation between external load and LME susceptibility. • TWIP steel showed a higher LME susceptibility compared to medium-Mn TRIP steel. • Results indicated stress-assisted diffusion of Zn into austenite grain boundaries. • High angle grain and Σ3 twinning boundaries play major role in Zn penetration. - Abstract: High-Manganese austenite-containing steels with superior combination of strength and ductility have shown potential for enhancement of passenger safety and body-in-white (BIW) weight reduction. Even though Zn-coated austenitic steels have improved corrosion resistance, they are highly susceptible to liquid metal embrittlement (LME) during welding. The present work is aimed to address LME susceptibility during restrained laser lap joining of high-Mn twinning induced plasticity (TWIP) and medium-Mn transformation induced plasticity (MMn-TRIP) steels. Electron probe micro-analysis (EPMA) results showed that stress-assisted diffusion of Zn into the austenite grain boundaries and further liquid Zn formation by a peritectic reaction lead to grain boundary decohesion. Electron backscatter diffraction (EBSD) results demonstrated that high angle and special grain boundaries are prone to Zn-penetration within the heat-affected-zone (HAZ). Additionally, LME sensitivity was observed to be highly dependent on the magnitude of applied stress.

36 MATERIALS SCIENCE↗

In situ analysis of plasticity and damage nucleation in a Ti-6Al-4V alloy and laser weld

Highlights: • EBSD in situ tensile test on a Ti-6Al-4V alloy and laser weld • Mainly prismatic, basal and pyramidal a slip activity in the base metal • Damage nucleation in the vicinity of the β phase and at α grain boundaries • Alignment of 10-10 crystallographic direction with the tensile axis in the α′ laths of the weld metal • Crack initiation along specific laths interfaces, former β grain boundary or twinned martensite laths in the weld metal The present work addresses the mechanisms of plasticity and damage nucleation in a Ti-6Al-4V alloy and its laser weld. To this end, in situ tensile tests are performed in a Scanning Electron Microscope (SEM) equipped with a Electron BackScatter Diffraction (EBSD) camera. The slip activity is automatically analyzed using a modified Schmid analysis. It is shown that the slip activity of the base metal consists mainly in prismatic, basal and pyramidal a slip. Damage nucleation in the vicinity of the β phase and at α grain boundaries is also evidenced in the base metal. In the α{sup ′} weld metal (a microstructure similar to the one often obtained in additive manufacturing Ti-alloy parts), plastic deformation results in a crystallographic rotation of the laths tending to align the 〈10 1-bar 0〉 direction with the tensile axis. The rare events of crack initiation in the martensite are shown to occur along specific laths interfaces, former β grain boundary or twinned martensite needles.

36 MATERIALS SCIENCE↗

Thermomechanical characterization and modeling for TSV structures

Continual scaling of devices and on-chip wiring has brought significant challenges for materials and processes beyond the 32-nm technology node in microelectronics. Recently, three-dimensional (3-D) integration with through-silicon vias (TSVs) has emerged as an effective solution to meet the future technology requirements. Among others, thermo-mechanical reliability is a key concern for the development of TSV structures used in die stacking as 3-D interconnects. This paper presents experimental measurements of the thermal stresses in TSV structures and analyses of interfacial reliability. The micro-Raman measurements were made to characterize the local distribution of the near-surface stresses in Si around TSVs. On the other hand, the precision wafer curvature technique was employed to measure the average stress and deformation in the TSV structures subject to thermal cycling. To understand the elastic and plastic behavior of TSVs, the microstructural evolution of the Cu vias was analyzed using focused ion beam (FIB) and electron backscattering diffraction (EBSD) techniques. Furthermore, the impact of thermal stresses on interfacial reliability of TSV structures was investigated by a shear-lag cohesive zone model that predicts the critical temperatures and critical via diameters.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure and mechanical properties development of micro channel tubes in extrusion, rolling and brazing

Highlights: • Rolling and brazing greatly affect the properties of micro-channel tubes (MCTs). • The properties of MCTs are investigated by the evolution of the microstructure. • Strength is decreased by 47% at 5%-rolling reduction ratio and 3-minute brazing. • Ductile fracture mode is observed by OM at failure of MCTs under inner pressure. - Abstract: In addition to extrusion, the post-processing of rolling and brazing has significant effect on the mechanical properties of multi-port tubes. The aluminum micro channel tubes, especially the seam welding zone in the internal webs, are investigated in terms of mechanical tests, microstructure characterization, and finite element analysis. The effect of the post-process of rolling are quantified by varying amount of rolling reduction ratios. Tensile strength and pressure bearing capacity are determined by tensile tests and burst pressure tests, respectively. The evolution of the microstructure within the seam wielding zone is characterized by Electron backscattered diffraction (EBSD) and optical microscopy (OM). The fracture profile observed by OM indicates ductile fracture mode. The pressure bearing capacity is reduced by ~47% at 5% reduction ratio of rolling followed by 3-minute brazing, where largest grains are obtained due to abnormal grain growth.

36 MATERIALS SCIENCE↗

The role of titanium and vanadium based precipitates on hydrogen induced degradation of ferritic materials

Highlights: • Hydrogen induced damage is studied in Fe-C-Ti and Fe-C-V ferritic alloys. • Fe-C-Ti is less susceptible to hydrogen embrittlement than Fe-C-V. • Fe-C-V is less susceptible to blistering than Fe-C-Ti. • The role of diffusible hydrogen depends on the damage mechanism. - Abstract: The hydrogen induced damage of generic Fe-C-Ti and Fe-C-V ferritic alloys was investigated to assess the influence of precipitates on the hydrogen sensitivity of a material. The precipitates, formed during heat treatment, were evaluated by scanning transmission electron microscopy (STEM). The hydrogen/material interaction was evaluated by: 1) melt and hot extraction to determine the total and diffusible hydrogen content, respectively, 2) permeation experiments to calculate the diffusion coefficient, 3) thermal desorption spectroscopy to determine the hydrogen trapping characteristics of the materials. Furthermore, two different types of hydrogen induced damage were evaluated, i.e. hydrogen assisted cracking and blistering, resulting from electrochemical hydrogen charging with and without the application of an external load, respectively. Evaluation of the hydrogen induced damage and the role of the precipitates was performed by combining optical microscopy, scanning electron microscopy (SEM), and electron backscatter diffraction (EBSD). An important though divertive role of diffusible hydrogen is observed in both damage mechanisms for the investigated microstructures. On the one hand, a large amount of diffusible hydrogen compared to strongly trapped hydrogen promotes hydrogen assisted cracking of materials, while on the other hand, the blistering phenomenon is delayed under such conditions.

36 MATERIALS SCIENCE↗

Precipitation behavior of ωo phase and texture evolution of a forged Ti-45Al-8.5Nb-(W, B, Y) alloy during creep

Highlights: • The morphology of ω{sub o} and residual β{sub o} phases depends on creep temperature and stress. • Stress can increase the tendency of the α{sub 2} to ω{sub o} phase transformation. • The strength of the texture components depend on temperature and stress. • β{sub o}(ω{sub o}) precipitation retards the growth of recrystallized γ grains. • ω{sub o} precipitation resists and deflects the crack during the crack propagation. - Abstract: Creep rupture tests of the as-forged Ti-45Al-8.5Nb-(W,B,Y) alloy with a duplex microstructure were carried out at 750–850 °C and 130–300 MPa. An investigation was performed to study the effects of temperature and stress on the microstructure and texture evolution, as well as on the creep properties of the forged high Nb-containing TiAl alloy with a duplex microstructure. The results show that the stress exponent n = 2.8–3.3, and the creep activation energy values are in the range of 300–400 kJ/mol. After creep, a regular arrangement of ω{sub o} precipitations was observed in the β{sub o} region. The un-transformed β{sub o} phase, which remained in the ω{sub o} interval, was examined using high resolution transmission electron microscope (HRTEM). It is shown that the growth of ω{sub o} precipitations and the morphology of residual β{sub o} phases are related to the creep temperature and stress. Certain β{sub o} stabilizer elements, such as Nb, segregate into α{sub 2} plates and cause ω{sub o} precipitation during dissolution of α{sub 2} plates at high temperature. The interfacial structure between the ω{sub o} and α{sub 2} phases was studied in detail using HRTEM. Meanwhile, texture evolution and dynamic recrystallization of the γ phase were studied using electron backscatter diffraction (EBSD). Observations on the deformation structure also demonstrate that ω{sub o} precipitation acts as an obstacle inhibiting crack propagation and growth of the γ phase. The corresponding formation mechanism and possible effects on creep are discussed.

36 MATERIALS SCIENCE↗

Influence of the grain size on deleterious phase precipitation in superduplex stainless steel UNS S32750

In the present work, the effect of grain size on deleterious phase precipitation in a superduplex stainless steel was investigated. The materials studied were heat treated isothermally at 800 deg. C, 850 deg. C and 900 deg. C for times up to 120 min. Hardness tests, light optical microscopy, scanning electron microscopy and X-ray diffraction were carried out to detect sigma and other harmful precipitate phases. The ferritic and austenitic grain sizes in the solution treated condition of the two steels analyzed were measured by electron backscattered diffraction (EBSD). Cyclic polarization corrosion tests were performed to evaluate the effect of grain size on the corrosion resistance. The results presented show that the precipitation of deleterious phases such as {chi}, {sigma} and {gamma}{sub 2}, which can occur during welding and forming operations, is retarded by grain growth.

36 MATERIALS SCIENCE↗

Strain softening mechanism at meso scale during micro-compression in an ultrafine-grained pure copper

Strain softening behavior has been found at meso scale using micro-compression testing in an ultrafine-grained (UFG) pure copper by comparison with the typical strain hardening in conventional coarse-grained (CG) material. Microstructural observations show that grain size remains nearly the same including the fraction of high-angle grain boundaries during micro-compression in UFG pure copper. The Kernel average misorientation(KAM) distribution measured by electron backscatter diffraction (EBSD), as a statistical method, is applied to qualitatively evaluate dislocation density in the interior of the grains. It is suggested that the deformation mechanisms are dominated by grain boundary sliding and grain rotation accompanied by dislocation slip in UFG pure copper, which demonstrates that the strain softening behavior is primarily caused by dislocation annihilation during micro-compression.

36 MATERIALS SCIENCE↗