Search NASA⌕ Search

SEARCH · Search NASA

Results for “fade”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Insight into the Capacity Fading Mechanism of Amorphous Se 2 S 5 Confined in Micro/Mesoporous Carbon Matrix in Ether-Based Electrolytes

In contrast to the stable cycle performance of space confined Se-based cathodes for lithium batteries in carbonate-based electrolytes, their common capacity fading in ether-based electrolytes has been paid less attention and not yet well-addressed so far. In this work, the lithiation/delithiation of amorphous Se2S5 confined in micro/mesoporous carbon (Se2S5/MPC) cathode was investigated by in situ X-ray near edge absorption spectroscopy (XANES) and theoretical calculations. The Se2S5/MPC composite was synthesized by a modified vaporization-condensation method to ensure a good encapsulation of Se2S5 into the pores of MPC host. In situ XANES results illustrated that the lithiation/delithiation reversibility of Se component was gradually decreased in ether-based electrolytes, leading to an aggravated formation of long-chain polyselenides during cycling and further capacity decay. Moreover, ab initio calculations revealed that the binding energy of polyselenides (Li2Sen) with carbon host is in an order of Li2Se6 > Li2Se4 > Li2Se. The insights into the failure mechanism of Se-based cathode gain in this work are expected to serve as a guide for future design on high performance Se-based cathodes.

ab initio calculations↗

Corrosion/Fragmentation of Layered Composite Cathode and Related Capacity/Voltage Fading during Cycling Process

Pristine and cycled layered structure cathode of Li[Li0.2Ni0.2M0.6]O2 samples are characterized by aberration-corrected scanning transmission electron microscopy and electron energy loss spectroscopy. These analyses provide new insights on capacity/voltage fading mechanism of Li[Li0.2Ni0.2M0.6]O2. Sponge-like structure and fragment pieces were found on the surface of cathode after cycling. Mn2+ species and reduced Li content in the fragments caused significant capacity loss. These results also reveal the functional mechanism of surface coatings, e.g. AlF3, which can protect the electrode from etching by acidic species in the electrolyte, suppress cathode degradation and improve long-term cycling stability.

Voltage fading, fragmentation, etched surface, Mn2↗

Optimizing Lunar Map Partitioning for Multipath Fade Loss Analyses

A methodology is presented pertaining to the run-time optimization of quasi-optical ray-tracing simulations. These shooting-and-bouncing ray methods are used for assessing multipath fade loss in cislunar communication links. Our approach employs partitioning lunar terrain maps in shapes that approximate two-dimensional projections of Fresnel zone cross-sections. This technique drastically reduces computational run-time without causing significant loss of simulation accuracy.

Digital elevation models↗

Performance Study of Hybrid DS/FFH Spread-Spectrum Systems in the Presence of Frequency-Selective Fading and Multiple-Access Interference

Hybrid spread-spectrum (HSS) systems have recently received considerable interest in commercial, Smart Grid, and military communication systems because they accommodate high data rates with high link integrity, even in the presence of significant multipath effects and interfering signals. A highly useful form of this modulation scheme is the specific code-related combination of standard direct-sequence spread spectrum (DSSS) with fast frequency-hopping (FFH) spread spectrum, denoted hybrid DS/FFH, wherein multiple frequency hops occur within a single data-bit time. In this paper we perform a simulation-based study of the DS/FFH performance as compared to the existing standard DSSS and FHSS wireless networks. The performance metrics are bit-error probability and multiple-access capability. The parameter space of DS/FFH, including the DS spreading rate, frequency hopping rate, carrier frequencies, and numbers of users, is explored to show its performance under frequency-selective Rayleigh fading environments and multiuser interference. Direct digital synthesizers to achieve fast hopping speeds are also considered in our study.

99 GENERAL AND MISCELLANEOUS↗

Elucidating Instabilities Contributing to Capacity Fade in Bipyridine‐Based Materials for Non‐aqueous Flow Batteries

Abstract Metal‐based non‐aqueous redox flow batteries have the potential for long‐term energy storage if stability requirements can be achieved. One such stability issue in metal coordination complexes arises from ligand shedding in the anolyte upon reduction. Recognizing that the free ligands are relatively more stable than the metal coordination complex under highly reducing conditions, we evaluated a family of metal‐free bipyridinium materials as flow battery anolytes with the corresponding iron coordination complex as the catholyte. Bipyridinium compounds were functionalized for increased electrochemical stability, cycled in flow cells to understand efficiencies, and analyzed for degradation products. Methylation of the bipyridine nitrogens increased electrochemical stability yet left the reduced molecule susceptible to radical‐induced bond cleavage. Subsequent functionalization of bipyridine with carbomethoxy groups resulted in good battery performance with 96 % Coulombic and 90 % voltage efficiency, and improved cycling stability over a methoxy‐substituted anolyte with 14 % vs 36 % capacity fade in the first charge‐discharge cycle.

Kolesnichenko, Claudina X.↗

Underlying limitations behind impedance rise and capacity fade of single crystalline Ni-rich cathodes synthesized via a molten-salt route

Layered oxide LiNi x Mn y Co z O 2 (NMC) cathodes are often synthesized as polycrystalline secondary particles. Due to intergranular fracture stemming from volume changes of randomly oriented primary particles during charge/discharge, the synthesis of larger single-crystalline cathodes is of high interest. In this work, molten salt assisted growth of micron-sized Ni-rich crystals is achieved with excellent crystallinity, low cation mixing, and negligible impurities. However, electrochemical performance is compromised by high surface reactivity resulting in decomposition of electrolyte and subsequent formation of a thick CEI layer. While intergranular fracture is eliminated, planar gliding and severe intragranular fracture along the (003) plane occurs in the high voltage region within the first few cycles and is associated primarily with H2 to H3 structural transitions. In addition, H2 to H3 transitions are highly irreversible with cyclic voltammograms revealing polarization growth within <5 cycles. Subsequently, the single-crystalline material exhibited markedly reduced available capacity and enhanced capacity fade from sharp impedance growth compared to its polycrystalline counterpart. Here, this work furthers a fundamental understanding into the limitations of single-crystalline Ni-rich cathodes, and the obstacles limiting the advantages offered by the single-crystalline morphology.

25 ENERGY STORAGE↗

Synthesis and Characterization of the Lithium-Rich Core-Shell Cathodes with Low Irreversible Capacity and Mitigated Voltage Fade

Lithium-rich layered Ni–Mn–Co oxide materials have been intensely studied in the past decade. Mn-rich materials have serious voltage fade issues, and the Ni-rich materials have poor thermal stability and readily oxidize the organic carbonate electrolyte. Core–shell (CS) strategies that use Ni-rich material as the core and Mn-rich materials as the shell can balance the pros and cons of these materials in a hybrid system. The lithium-rich CS materials introduced here show much improved overall electrochemical performance compared to the core-only and shell-only samples. Energy dispersive spectroscopy results show that there was diffusion of transition metals between the core and shell phases after sintering at 900 °C compared to the prepared hydroxide precursors. A Mn-rich shell was still maintained whereas the Co which was only in the shell in the precursor was approximately homogeneous throughout the particles. The CS samples with optimal lithium content showed low irreversible capacity (IRC), as well as high capacity and excellent capacity retention. Sample CS2-3 (the third sample in the 0.67Li 1+x (Ni₀.₆₇Mn₀.₃₃) 1–x O₂·0.33Li 1+y (Ni₀.₄Mn₀.₅Co₀.₁) 1–y O₂ CS2 series) had a reversible capacity of ~218 mAh/g with 12.3% (~30 mAh/g) irreversible capacity (IRC) and 98% capacity retention after 40 cycles to 4.6 V at 30 °C at a rate of ~C/20. Differential capacity versus potential (dQ/dV versus V) analysis confirmed that cells of the CS samples had stable impedance as well as a very stable average voltage. Apparently, the Mn-rich shell can effectively protect the Ni-rich core from reactions with the electrolyte while the Ni-rich core renders a high and stable average voltage.

36 MATERIALS SCIENCE↗

Simulation of First-Charge Oxygen-Dimerization and Mn-Migration in Li-Rich Layered Oxides x Li 2 MnO 3 ·(1 – x )Li M O 2 and Implications for Voltage Fade

The instabilities of Li-rich layered oxide xLi 2 MnO 3 •(1-x)LiMO 2 (lithium-ion-battery cathode materials) during the first charge are investigated using first-principles dynamical simulation. To complement our earlier simulations for (x = 0.4, M = Ni 0.5 Mn 0.5 ), we address here: pure Li 2 MnO 3 ; small x; M compositions that include Co; a composite with Co spinel: Li 2 MnO 3 •Li 2 M 2 O 4 ; a Li 2 MnO 3 slab. Lastly, we discuss how the threshold fraction f of Li 2(1-f) MnO 3 delithiation at which instabilities occur at the surface, fth(surface), differs from that in the bulk, f th (bulk). Approaches to inhibit voltage fade are discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of Morphology and Manganese Valence on the Voltage Fade and Capacity Retention of Li[Li 2/12 Ni 3/12 Mn 7/12 ]O 2

We have determined the electrochemical characteristics of the high voltage, high capacity Li-ion battery cathode material Li[Li 2/12 Ni 3/12 Mn 7/12 ]O 2 prepared using three different synthesis routes: sol-gel, hydroxide co-precipitation, and carbonate co-precipitation. Each route leads to distinct morphologies and surface areas while maintaining the same crystal structures. X-ray photoelectron spectroscopy (XPS) measurements reveal differences in their surface chemistries upon cycling, which correlate with voltage fading. As expected, we observed the valence state of Mn on the surface to decrease upon lithiation, and this reduction is specifically correlated to discharging below 3.6V. Furthermore, the data shows a correlation of the formation of Li 2 CO 3 with Mn oxidation state from the

25 ENERGY STORAGE↗

Progressive growth of the solid–electrolyte interphase towards the Si anode interior causes capacity fading

The solid–electrolyte interphase (SEI), a layer formed on the electrode surface, is essential for electrochemical reactions in batteries and critically governs the battery stability. Active materials, especially those with extremely high energy density, such as silicon (Si), often inevitably undergo a large volume swing upon ion insertion and extraction, raising a critical question as to how the SEI interactively responds to and evolves with the material and consequently controls the cycling stability of the battery. Here, by integrating sensitive elemental tomography, an advanced algorithm and cryogenic scanning transmission electron microscopy, we unveil, in three dimensions, a correlated structural and chemical evolution of Si and SEI. Furthermore, corroborated with a chemomechanical model, we demonstrate progressive electrolyte permeation and SEI growth along the percolation channel of the nanovoids due to vacancy injection and condensation during the delithiation process. Consequently, the Si–SEI spatial configuration evolves from the classic ‘core–shell’ structure in the first few cycles to a ‘plum-pudding’ structure following extended cycling, featuring the engulfing of Si domains by the SEI, which leads to the disruption of electron conduction pathways and formation of dead Si, contributing to capacity loss. The spatially coupled interactive evolution model of SEI and active materials, in principle, applies to a broad class of high-capacity electrode materials, leading to a critical insight for remedying the fading of high-capacity electrodes.

36 MATERIALS SCIENCE↗

Evaluation of the sensitivity and fading characteristics of an image plate system for x-ray diagnostics

Image plates (IPs) are a reusable recording media capable of detecting ionizing radiation, used to diagnose x-ray emission from laser-plasma experiments. Due to their superior performance characteristics in x-ray applications [C. C. Bradford, W. W. Peppler, and J. T. Dobbins III, Med. Phys. 26, 27 (1999) and J. Digit. Imaging. 12, 54 (1999)], the Fuji Biological Analysis System (BAS) IPs are fielded on x-ray diagnostics for the HELEN laser by the Plasma Physics Department at AWE. The sensitivities of the Fuji BAS IPs have been absolutely calibrated for absolute measurements of x-ray intensity in the energy range of 0-100 keV. In addition, the Fuji BAS IP fading as a function of time was investigated. We report on the characterization of three Fuji BAS IP responses to x-rays using a radioactive source, and discrete x-ray line energies generated by the Excalibur soft x-ray facility and the Defense Radiological Standards Centre filter-fluorescer hard x-ray system at AWE.

07 ISOTOPE AND RADIATION SOURCES↗