Understanding PV Polymer Backsheet Degradation through X-Ray Scattering

Understanding how photovoltaic (PV) module backsheet polymers age and degrade in response to environmental stresses is important for designing polymers that can maintain their structural integrity after decades of outdoor use. X-ray scattering is a powerful technique for exploring backsheet polymer structure at the angstrom- (wide-angle, WAXS) and nanometer- (small-angle, SAXS) length-scales. We present the use of SAXS and WAXS to study pristine and aged polymer backsheets. The structural insight from these techniques can be used to compare the degradation induced by accelerated testing with the degradation seen in field-aged PV materials.

14 SOLAR ENERGY↗

Design, characterization and indoor validation of the optical soiling detector “DUSST”

Nowadays, photovoltaic (PV) technology has reached a high level of maturity in terms of module efficiency and cost competitiveness in comparison with other energy technologies. As PV has achieved high levels of deployment, the development of devices that can help to reduce PV operation and maintenance costs has become a priority. Soiling can be cause of significant losses in certain PV plants and its detection has become essential to ensure a correct mitigation. For this reason, accurate and low-cost monitoring devices are needed. While soiling stations have been traditionally employed to measure the impact of soiling, their high cost and maintenance have led to the development of innovative low-cost optical sensors, such as the device presented in this work and named “DUSST” (Detector Unit for Soiling Spectral Transmittance). The thermal characterization of DUSST’s components and the methodology used to predict soiling transmittance losses are presented in this study. The results demonstrate that the losses can be predicted with an error lower than 1.4%. The method has been verified with an experimental campaign with naturally soiled coupons exposed outdoors in Jaén, Spain.

14 SOLAR ENERGY↗

Measurement of Photovoltaic Module Deformation Dynamics During Hail Impact Using Digital Image Correlation

Stereo high-speed video of photovoltaic modules undergoing laboratory hail tests was processed using digital image correlation to determine module surface deformation during and immediately following impact. The purpose of this work was to demonstrate a methodology for characterizing module impact response differences as a function of construction and incident hail parameters. Video capture and digital image analysis were able to capture out-of-plane module deformation to a resolution of ±0.1 mm at 11 kHz on an in-plane grid of 10 × 10 mm over the area of a 1 × 2 m commercial photovoltaic module. With lighting and optical adjustments, the technique was adaptable to arbitrary module designs, including size, backsheet color, and cell interconnection. Furthermore, impacts were observed to produce an initially localized dimple in the glass surface, with peak deflection proportional to the square root of incident energy. Subsequent deformation propagation and dissipation were also captured, along with behavior for instances when the module glass fractured. Natural frequencies of the module were identifiable by analyzing module oscillations postimpact. Limitations of the measurement technique were that the impacting ice ball obscured the data field immediately surrounding the point of contact, and both ice and glass fracture events occurred within 100 μs, which was not resolvable at the chosen frame rate. Increasing the frame rate and visualizing the back surface of the impact could be applied to avoid these issues. Applications for these data include validating computational models for hail impacts, identifying the natural frequencies of a module, and identifying damage initiation mechanisms.

14 SOLAR ENERGY↗

Towards Validation of Advanced Accelerated Stress Testing Protocols through Failure Analysis and Materials Characterization

As the lifetime of photovoltaic modules increases toward the goal of 50 years, accelerated stress testing is critical to assessing the viability of newer, improved, and often cheaper materials in the field. However, the validation of accelerated testing to reproduce field failure has remained elusive. The recent developments of more advanced stress testing protocols utilizing sequential and combined stressors have provided another opportunity for validation. Using a suite of mechanical, chemical, and structural characterization methods we report the development of our approach using a known bad backsheet “AAA.” We then apply this approach to PVDF-based backsheets to further confirm the generalizability of this approach. The outcome of this work is two-fold: (1) validation of advanced accelerated testing protocols which will enable the prediction of field failures in new materials, and (2) deeper insights into the degradation mechanisms observed through the extensive characterization allowing for improved materials engineering and development.

accelerated aging↗

Spread Spectrum Time Domain Reflectometry (SSTDR) Digital Twin Simulation of Photovoltaic Systems for Fault Detection and Location

Utilizing spread spectrum time domain reflectometry (SSTDR) to detect, locate, and characterize faults in photovoltaic (PV) systems is examined in this paper. We present a method to obtain the model parameters that are needed to produce digital twin SSTDR responses for PV systems. The digital twin SSTDR responses could be used to predict faults within the PV systems. Here, the model parameters are the reflection and transmission coefficients at each impedance discontinuity in the PV system along with the propagation coefficients across each PV cable segment. We obtain model parameter by applying inverse modeling techniques to experimental SSTDR data associated with PV systems. Our model parameters can be used in any digital twin simulation method for modeling reflectometry in frequency-dependent and complex loads. For validation, we used the model parameters in a graph network simulation engine and adapted it to be used for SSTDR digital twin simulations in PV systems. We produced simulations for 0 to 10 PV modules connected in series. We also simulated SSTDR responses for open circuit disconnections in a PV setup containing 10 PV modules in series. Results show that all but one simulated disconnect locations match experimental disconnection locations of the same setup with an error of less than 5%.

14 SOLAR ENERGY↗

Ligand-Structure-Dependent Coherent Vibrational Wavepacket Dynamics in Pyrazolate-Bridged Pt(II) Dimers

Bimetallic transition metal complexes have gained increasing attention because of their versatile functions in solar energy conversion and photonics applications arising from inter-metal electronic coupling. In bimetallic platinum (Pt) complexes, electronic communication between the Pt-centered and ligand-centered moieties have been shown to be critical for defining their excited-state dynamic trajectories undergoing either localized ligand centered (LC)/metal-to-ligand-charge-transfer (MLCT) transitions or delocalized metal-metal-to-ligand-charge-transfer (MMLCT) transitions. The branching of the excited-state intersystem crossing (ISC) trajectories are modulated through structural factors that alter the relative energies of the different states. In this study, we investigated the correlation of the structural factors influencing the excited state trajectories. Using femtosecond broadband transient absorption (fs-BBTA) spectroscopy, ultrafast dynamics in the excited state of two select Pt(II) dimers have been mapped out using their coherent vibrational wavepacket signatures in corresponding transient absorption spectra. To examine how the ligand moieties of the Pt(II) dimers influence excited-state dynamics and the coherent vibrational wavepacket behavior, here we carried out comparative studies on two pyrazolate-bridged Pt(II) dimers of the general formula [Pt( t Bu 2 Pz)(N^C)] 2 ( t Bu 2 Pz = 3,5-di-tert-butylpyrazole); N^C = 7,8-benzoquinoline (bzq, 1) or 1-phenylisoquinoline (piq, 2)). We found that photoexcitation into the low energy absorption bands of 1 and 2 respectively induce the formation of 1 MMLCT states from which ultrafast ISC proceeds, resulting in stimulated emission quenching and decoherence of the vibrational wavepacket motions. The results obtained in this study suggest that both energetics and the structural rigidity of the aromatic cyclometalating ligands in 1 and 2 can significantly influence dynamics along the excited state trajectory characterized by dephasing of the coherent oscillations. The collective results provide direct evidence of how ligand structure alters electronic dynamics along excited state trajectories associated with ISC processes, providing insight into using ligand design to steer photochemical processes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Generalized and Mechanistic PV Module Performance Prediction From Computer Vision and Machine Learning on Electroluminescence Images

Electroluminescence (EL) imaging of photovoltiac (PV) modules offers high-speed, high-resolution information about device performance, affording opportunities for greater insight and efficiency in module characterization across manufacturing, research and development, and power plant operations and management. Predicting module electrical properties from EL image features is a critical step toward these applications. In this article, we demonstrate quantification of both generalized and performance mechanism-specific EL image features, using pixel intensity-based and machine learning classification algorithms. From EL image features, we build predictive models for PV module power and series resistance, using time-series current-voltage (I-V) and EL data obtained stepwise on five brands of modules spanning three Si cell types through two accelerated exposures: damp heat (DH) (85°C/85% RH) and thermal cycling (TC) (IEC 61215). Overall, 195 pairs of EL images and I-V characteristics were analyzed, yielding 11700 individual PV cell images. A convolutional neural network was built to classify cells by the severity of busbar corrosion with high accuracy (95%). Generalized power predictive models estimated the maximum power of PV modules from EL images with high confidence and an adjusted-R 2 of 0.88, across all module brands and cell types in extended DH and TC exposures. Mechanistic degradation prediction was demonstrated by quantification of busbar corrosion in EL images of three module brands in DH, and subsequent modeling of series resistance using these mechanism-specific EL image features. For modules exhibiting busbar corrosion, we demonstrated series resistance predictive models with adjusted-R 2 of up to 0.73.

14 SOLAR ENERGY↗

A Comparison of Emerging Nonfluoropolymer-Based Coextruded PV Backsheets to Industry-Benchmark Technologies

As the photovoltaic (PV) industry is rapidly expanding around the world, there has been an increasing interest in extending the lifespan of PV modules. Concern has also emerged regarding the recyclability of modules and their component materials, including fluoropolymer-based backsheets. Laminated polyethylene-terephthalate (PET) core backsheets have traditionally been used in the PV industry, but new, coextruded polyolefin (PO) backsheets show promise as an improved alternative. In this work, minimodule and coupon samples of seven different backsheets (made of layers including contemporary PET and fluoropolymers, novel PO, and polyamide materials) were run through hygrometric- or UV photolytic-accelerated aging to identify and better understand each material's degradation modes and the backsheets' field reliability. In addition to the artificial aging, the natural weathering methods used in this article are described. The comprehensive set of chemical, mechanical, and structural characterizations at intermittent read points in this article is presented, including: visual appearance and color; gloss; mechanical tensile testing; I-V performance; electroluminescence (EL) imaging; dielectric breakdown; Fourier-transform infrared-chemical structure; X-ray-polymer structure; and differential scanning calorimetry-crystalline content. After 4000 h of aging, a strong correlation occurs between initial physical characteristics (mechanical tensile test) and operating performance (EL and I-V characteristics).

14 SOLAR ENERGY↗

BACKFLIP: A Comparison of Emerging Non-Fluoropolymer-Based, Co-Extruded PV Backsheets to Industry-Benchmark Technologies

As the photovoltaic (PV) industry is rapidly expanding around the world, there has been an increasing interest in extending the lifespan of PV modules. Concern has also emerged regarding the recyclability of modules and their component materials, including fluoropolymer-based backsheets. Laminated polyethylene-terephthalate (PET) core backsheets have traditionally been used in the PV industry, but new, co-extruded polyolefin (PO) backsheets show promise as an improved alternative. Mini-module and coupon samples of seven different backsheets (made of layers including contemporary PET and fluoropolymers, novel PO, and polyamide (PA) materials) were run through hygrometric- or UV photolytic-accelerated aging to identify and better understand each material's degradation modes and the backsheets' field reliability. In addition to the artificial aging, the natural weathering methods used in this study are described. The comprehensive set of chemical, mechanical, and structural characterizations at intermittent read points in this study is presented, including: visual appearance and color; gloss; mechanical tensile testing; I-V performance; electroluminescence (EL) imaging; dielectric breakdown; FTIR-chemical structure; X-ray-polymer structure (WAXS); and DSC-crystalline content. After 4000 h of aging, a strong correlation occurs between initial physical characteristics (mechanical tensile test) and operating performance (EL and I-V characteristics). This presentation focuses on gloss, FTIR, and breakdown voltage measurements. Results for MiMo power, grayness from EL imaging, optical micrscopy, and specimen morphology (on extraction when cut from MiMos) is also presented.

backsheet↗

Characterization of high-frequency waves in the Martian magnetosphere

Context.Various high-frequency waves in the vicinity of upper-hybrid and Langmuir frequencies are commonly observed in different space plasma environments. Such waves and fluctuations have been reported in the magnetosphere of the Earth, a planet with an intrinsic strong magnetic field. Mars has no intrinsic magnetic field and, instead, it possesses a weak induced magnetosphere, which is highly dynamic due to direct exposure to the solar wind. In the present paper, we investigate the presence of high-frequency plasma waves in the Martian plasma environment by making use of the high-resolution electric field data from the Mars Atmosphere and Volatile Evolution missioN (MAVEN) spacecraft. Aims.This study aims to provide conclusive observational evidence of the occurrence of high-frequency plasma waves around the electron plasma frequency in the Martian magnetosphere. We observe two distinct wave modes with frequency below and above the electron plasma frequency. The characteristics of these high-frequency waves are quantified and presented here. We discuss the generation of possible wave modes by taking into account the ambient plasma parameters in the region of observation. Methods.We have made use of the medium frequency (100 Hz–32 kHz) burst mode-calibrated electric field data from the Langmuir Probe and Waves instrument on board NASA’s MAVEN mission. Due to the weak magnetic field strength, the electron gyro-frequency is much lower than the electron plasma frequency, which implies that the upper-hybrid and Langmuir waves have comparable frequencies. A total of 19 wave events with wave activities around electron plasma frequency were identified by examining high-resolution spectrograms of the electric field. Results.These waves were observed around 5 LT when MAVEN crossed the magnetopause boundary and entered the magnetosheath region. These waves are either a broadband- or narrowband-type with distinguishable features in the frequency domain. The narrowband-type waves have spectral peak above the electron plasma frequency. However, in the case of broadband-type waves, the spectral peak always occurred below the electron plasma frequency. The broadband waves consistently show a periodic modulation of 8–14 ms. Conclusions.The high-frequency narrowband-type waves observed above the electron plasma frequency are believed to be associated with upper-hybrid or Langmuir waves. However, the physical mechanism responsible for the generation of broadband-type waves and the associated 8–14 ms modulation remain unexplained and further investigation is required.

Astronomy & Astrophysics↗

Artificial Soiling Replication of Field Losses on Commercial Photovoltaic Modules

Here, this study demonstrates the capabilities of an indoor artificial soiling approach developed to closely replicate the natural, cyclic soil accumulation processes in the field-dust suspension, deposition, and sedimentation/cementation-for a subtropical climate. In this work, a near-field environment is replicated in an artificial soiling cubic chamber through controlled regulation of humidity, temperature, dust type, and dust concentration, based on site-specific historical climate data. Two different models (MA and MB) of full-size commercial photovoltaic modules from a single manufacturer, installed side by side in the mid-Atlantic United States, were retrieved and subjected to artificial soiling experiments and various characterization measurements, including short-circuit current, colorimetry, reflectance, X-ray fluorescence, laser diffraction, and optical microscopy. Both in the field and in our improved field-representative artificial soiling tests, the MA model experienced roughly twice the soiling loss as the MB model. To closely replicate the field soiling losses for a site-specific climate, it is critical to include: 1) The use of field-collected dust with identical dust chemistry and particle distribution instead of standardized ISO 12103 Arizona Road dusts, 2) the use of only a small amount of field-collected dust inside the chamber during the deposition process (e.g., 0.15 g), and 3) the preconditioning of the surface coating for the partial/full dose of UV stress as experienced in the field during sunlight exposure and the abrasion as experienced in the field during regular module cleaning activities, if/as needed. The field-representative artificial soiling method developed here could potentially be adopted for rank ordering of various antisoiling coatings developed by researchers and industry stakeholders.

14 SOLAR ENERGY↗

Wafer-Free Crystalline Silicon Solar Cells (CRADA Final Report)

This CRADA project, based on the DOE Solar Energy Technologies Office (SETO) Solar Prize Voucher program, helped Leap Photovoltaics to develop methodologies to immobilize Si particles by permanently attaching them to an Al-coated substrate and thereby forming carrier-selective electrical contacts to the Si particles. The bigger goal was to help Leap Photovoltaics develop these immobilized and contacted particle arrays into relatively efficient, inexpensive, and industrially relevant solar cells. By using Si particles instead of wafers in a solar cell absorber layer, one can avoid costs associated with growing monocrystalline Si ingots, then diamond-sawing them into wafers, then processing wafers into cells – a mainstream practice in today's high-efficiency Si cell and module technology. Monocrystalline or polycrystalline Si particles can be obtained in various ways: for example, Si kerf from wafer sawing is monocrystalline; recycled Si cell wafers can be ball-milled into particles; particles can be grown using various gas-phase techniques (mostly from SiH4). These Si particles can be assembled onto a substrate and serve as an absorber layer for the solar cell, absorbing photons to generate photocarriers. The challenge with this technique is to collect photocarriers from individual Si particles, with separation of photogenerated electrons to the negative cell’s electrode and positive photogenerated holes to the positive electrode. Therefore, each particle must have two isolated, carrier-selective contacts: one for electrons and one for holes. Plus, particles need to be immobilized onto a solid substrate. The goal of this work was focused on the immobilization of Si particles and creating hole-selective contact to them at the same time, using industrially relevant Si photovoltaic (PV) cell technology: screen printing of Al back-surface field electrodes. This is used in the mainstream Propane Education and Research Council (PERC) technology for hole-collecting contacts at the back of the cell. The work performed at NREL consisted of screen printing of Al metal paste on substrates, spreading Si particles onto it, and thermally processing the structures to form hole-collecting contacts. The final structures were investigated by scanning electron microscopy (SEM) after focused ion beam (FIB) cross-sectioning and polishing. The work was done jointly by NREL staff and Leap Photovoltaics (Leap PV) employees stationed at NREL. The samples were then taken to Leap PV for further processing. Training the Leap PV employee on various NREL techniques (laser cutting, screen printing, thermal processing, characterization) was part of the scope.

14 SOLAR ENERGY↗

Accelerated Aging of PV Cables - The Development of Methods Towards Combined-Accelerated Stress Testing

PV cables allow the collection and distribution of electricity from modules to the energy grid. Durable cabling allows continuous operation of PV installations. Cables with a life less than that of the modules must be replaced - reducing electricity generation and adding to the system operating expense. We have examined the durability of a variety of representative cable samples using artificial UV weathering (IEC TS 62788-7-2) and combined accelerated stress testing (C-AST). Jackets in this study include PV-rated (polyolefin), building wire (PVC/PA), and multi-conductor (rubber, as in PV trackers), with some examples of black and red cables. Characterizations at read points include appearance (camera and optical microscope), surface roughness (linear profilometry), instrumented indentation, surface morphology (SEM), chemical composition (EDS), thermal decomposition (TGA), phase transition (DSC), crystalline structure (WAXS), and polymer chemical structure (FTIR). Complimentary examinations confirm damage to the external and interior layer(s) of less durable samples, including changes in morphology (e.g., cracking), chemistry (e.g., oxidation), structure, and mechanical performance (e.g., through-thickness modulus and hardness). The results may be generally compared to other examples from the field (PV installations) or after accelerated testing (IEC 61215). The methods in this study are presently being applied in a follow-on C-AST study, incorporating both dynamic and kinematic fixtures.

balance of systems↗

Field Study of Nighttime Leakage Currents in Bifacial PV Modules: Correlation with Atmospheric Electric Field Data

Leakage currents measured on PV modules in the field originate from a potential difference between the modules' frame and the cells. They can be a relative indicator of Potential-Induced Degradation (PID) severity, especially when comparing the same module design in a different environment. As modules are not operating at night, no leakage current should be observed but our team has reported several events of nighttime leakage currents on bifacial PV modules. These events have been firstly observed during a thunderstorm that are characterized by strong atmospheric electrical field values. This lead us to believe that nighttime leakage currents could originate from the atmospheric electric charges. In this paper, we correlate nighttime leakage currents measured on bifacial PV modules with field mill data to identify the origin of nighttime leakage currents. Our results show that so far, no leakage currents at night occur when the atmospheric electric field is between 0 and 150–200 V/m (standard value for fair weather). As soon as the atmospheric electric field is out of this range, leakage currents are observed with or without rain involved. This suggests a transport of charged particles from the atmosphere to the modules' frame. A combination of heavy rain with strong atmospheric electric field results into high nighttime leakage currents with a magnitude up to 8 times higher than what observed during the day with -1500V applied. This is explained by an easier transport of the charged particles through the water droplets. Based on these results, leakage currents observed during the day might not be only due to the inherent potential difference between the frame and the cells depending on the atmospheric electric field activity. We believe that it should be taken into account in PID studies.

14 SOLAR ENERGY↗

Performance and durability of electrically conductive tape for shingled Si heterojunction technology cells

We report electrically conductive tape (ECT) was characterized and used to assemble shingled cell strings at low temperature to achieve high reliability Pb- and Ag-free interconnections. The volume resistivity for two considered ECTs are 0.13 ± 0.06 mΩ·cm and 0.47 ± 0.20 mΩ·cm and specific contact resistances, 6.85± 2.00 mΩ·cm 2 and 6.30 ± 0.37 mΩ·cm 2 using the emerging IEC 62788-8-1 Technical Specification for assessment of electrically conductive adhesives (ECA). Durability and performance of the technology in glass–glass mini modules were evaluated with temperature cycling, damp heat testing, and combined-accelerated stress testing (CAST). Through temperature cycling (-40°C to 85°C) applying five times the mini module short-circuit current in forward bias and in the multi climate CAST protocol, there was negligible degradation of fill factor after replacing connectors at the modules' cable leads; however, CAST resulted in short circuit current loss attributed to degradation in light collection by the cells, not the ECT. The IEC 61215-2 85°C, 85% relative humidity damp heat testing showed susceptibility of the HJT cells to effects of humidity in the electroluminescence intensity around the module perimeter that degraded power performance by 4% (relative). Contrasting the IEC 61215-2 qualification testing-based damp heat testing with CAST, factors such as the optical stress of CAST may precipitate the degradation of the modules whereas the humidity levels and duration of IEC 61215-2 damp heat testing may lead to excessive levels of humidity diffused into the modules, potentially resulting in degradation that is unrepresentative of the field.

14 SOLAR ENERGY↗

Characterization of Field-Exposed Photovoltaic Modules Featuring Signs of Contact Degradation

Here, this work investigates several photovoltaic (PV) modules that have shown signs of metal contact corrosion due to field exposure in a hot and humid climate. This includes two multicrystalline silicon aluminum back surface field systems with 10 and 14 years of exposure and one monocrystalline silicon passivated emitter and rear cell system with four years of exposure. A comprehensive, multiscale characterization process is used to evaluate these PV modules in great detail. Current–voltage (I−V), Suns-V OC measurements, electroluminescence imaging, infrared imaging, and ultraviolet fluorescence imaging were performed, and locations of interest were cored and analyzed using cross-sectional scanning electron microscopy (SEM). A rigorous, quantitative analysis procedure for the cross-sectional SEM images is proposed and implemented. Careful characterization does reveal that some of these PV modules do indeed exhibit the same classic signs of acetic-acid-based corrosion of the glass frit that is present at the silver/silicon interface, which have been observed previously in PV modules exposed to damp heat in an environmental chamber.

14 SOLAR ENERGY↗

A Custom High-Throughput Optical Mapping Instrument (OMI) for Accelerated Stress Testing of PV Module Materials

The performance and integrity of photovoltaic (PV) modules and materials may be assessed through optical characterizations. We have developed a custom Optical Mapping Instrument (OMI) to improve measurement throughput time, facilitate automated measurements, and obtain spatial information relative to commercial benchtop spectrophotometer instruments. Both the key components and the methods used to improve the measurements are described. The measurement precision for the OMI is benchmarked for hemispherical transmittance relative to a previous round-robin study for commercial spectrophotometers. Example mapping measurements and their implications are given for specimens from other studies, including: (1) the depletion of the UV absorber is revealed for specimens beyond a certain size after standardized artificial ultraviolet (UV) weathering, (2) an optical degradation by internal haze formation is confirmed following Damp Heat (85°C/85% relative humidity) testing, (3) the better uniformity of the wear pattern for falling sand abrasion is used to select the DIN 52348 fixture over the ASTM D968 fixture, and (4) the local (millimeter-scale) heterogeneity of surface contamination in the soiling-prone location of Dubai relative to Kuwait. The results of the UV study have already been used to improve the standardized weathering of encapsulants. The example for Damp Heat testing is given to increase awareness of a degradation believed to be ubiquitously occurring in safety and design-type qualification testing of PV modules.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Failure Analysis of a New Polyamide-Based Fluoropolymer-Free Backsheet After Combined-Accelerated Stress Testing

The viability of novel coextruded, fluoropolymer-free backsheets for photovoltaic (PV) modules has been questioned as a result of a large number of early-life backsheet failures in PV installations containing one of the earliest co-extruded polyamide (PA)-based backsheet to reach the market, “AAA.” New PV reliability testing protocols have been recently developed and applied to backsheets to reproduce failures observed in the field and evaluate the durability of novel backsheet materials and designs prior to commercialization. A new co-extruded PA-based backsheet was tested using combined-accelerated stress testing (C-AST) and demonstrated a greater lifetime than AAA, and some other fluoropolymer-based backsheets such as polyvinylidene fluoride. The improved PA-based backsheet also eventually failed by through-thickness cracking. Using surface and bulk material characterization techniques, we performed a comprehensive study of material properties before and after the stress testing. Aging of the backsheet resulted in an increase of surface roughness by erosion of the outer PA layer. However the failure is more likely related to an increase in crystallinity of the polyolefin core layer reducing the backsheet tearing energy. The analysis can ultimately inform on the specific weaknesses of the materials so that the manufacturer can improve the backsheet design to extend its lifetime.

14 SOLAR ENERGY↗