Microstructure and mechanical properties of hypoeutectic Al–6Ce–3Ni-0.7Fe (wt.%) alloy

Here, a hypoeutectic, Fe-modified Al–Ce–Ni alloy (Al–6Ce–3Ni-0.7Fe, wt.%) is studied in terms of microstructure, thermal stability, ambient temperature strengthening, and creep resistance. The as-cast microstructure consists of primary Al dendrites and interdendritic binary eutectic regions (Al–Al11Ce3 and/or Al–Al9(Fe,Ni)2), with micron/submicron lamellar spacing, depending on the location along the height of the ingot. The cast alloy exhibits excellent coarsening resistance at 400 °C, with mostly unchanged microstructure and microhardness after 6 weeks of aging, indicating good thermal stability of Al11Ce3 and Al9(Fe,Ni)2. Orowan strengthening and load transfer are identified as strengthening mechanisms at ambient and elevated temperature. A high volume fraction of the intermetallic phases (providing load transfer) and relatively coarse eutectic spacing (for modest Orowan strengthening) result in a moderate as-cast microhardness of 566 ± 32 MPa. Creep resistance at 300 and 350 °C is similar to a binary Al-12.5Ce eutectic alloy (with twice the Ce content) because of two countering effects: Al–6Ce–3Ni-0.7Fe shows a higher volume fraction of strengthening intermetallic phases, but it also exhibits a large fraction of primary Al dendrites which weaken the alloy. By contrast, the alloy, when laser-remelted at the surface, has a fully eutectic microstructure without primary aluminum dendrites achieved by high undercooling on solidification, with a refined network of eutectic phases that doubles the microhardness as compared to the cast alloy. Whereas coarsening is faster due to the shorter diffusion distances between the eutectic phases, hardness remains ~30% higher than the as-cast alloy after ~6 weeks aging at 400 °C.

36 MATERIALS SCIENCE↗

Treatment and aging studies of GaAs(111)B substrates for van der Waals chalcogenide film growth

GaAs(111)B are commercially available substrates widely used for the growth of van der Waals chalcogenide films. Wafer-scale, high-quality crystalline films can be deposited on GaAs(111)B substrates using molecular beam epitaxy. However, two obstacles persist in the use of GaAs(111)B: first, the surface dangling bonds make it challenging for the growth of van der Waals materials; second, the As-terminated surface is prone to aging in air. This study investigated a thermal treatment method for deoxidizing GaAs(111)B substrates while simultaneously passivating the surface dangling bonds with Se. By optimizing the treatment parameters, we obtained a flat and completely deoxidized platform for subsequent film growth, with highly reproducible operations. Furthermore, through first-principle calculations, we find that the most energetically favorable surface of GaAs(111)B after Se passivation consists of 25% As atoms and 75% Se atoms. Finally, we discovered that the common storage method using food-grade vacuum packaging cannot completely prevent substrate aging, and even after thermal treatment, aging still affects subsequent growth. Therefore, we recommend using N2-purged containers for better preservation.

Engineering↗

Initial Radiation of Nuclear Power Plant Components (CRADA NFE-17-06892 Final Report)

As advanced reactor concepts are developed, instrumentation and control (I&C) cables and sensors will play a significant role in assuring their operation is well understood, and safety-related process information can be collected reliably over the course of their design life. As a first step to develop acceptance criteria and define the limits of currently available nuclear I&C cable and sensor technology, a collaboration between Oak Ridge National Laboratory and Analysis and Measurement Services (AMS) Corporation was initiated under the Gateway for Accelerated Innovation in Nuclear (GAIN) Program. This collaborative effort focused on providing technical information related to the combined thermal and radiation aging of nuclear power plant (NPP) cables, companion NPP cable insulation samples, and two prototype temperature and two pressure sensors. This work was carried out using the instrumented gamma irradiation system that is part of the High Flux Isotope Reactor Gamma Irradiation Facility (HFIR GIF). This system provided the opportunity for the condition of the prototype sensors to be tracked during the irradiation in order to determine their functional limits with greater granularity when compared to a simple irradiation insertion at the HFIRGIF. Experimental assemblies for sensor irradiation were successfully completed, and sensor irradiation to accumulated dose of 3000 kGy at a rate of approximately 6 kGy/hr was carried out. Two prototype temperature assemblies were continuously monitored during exposure to 3000 kGy and found to have no observable degradation from the irradiation. Two pressure sensors were first irradiated to 1000 kGy. At which point, one of the sensors was found to operate normally; however, a second sensor failed the operability test. The operable pressure sensor output was then continuously monitored from 1000 kGy to 3000 kGy. The sensor output exhibited steady trendable drift versus the accumulated radiation dose. At the conclusion of the irradiation, the four test sensors were released for laboratory calibration checks. The calibration check of the temperature sensors found no significant change after irradiation compared to baseline measurements before irradiation; however, both pressure sensors failed the post-test calibration checks and both sensors were not functioning properly. These results will help inform sensor manufacturers and I&C design engineers of potential limitations of these types of sensors for use in high radiation environments associated with the compact configuration of new Small Modular Reactors (SMRs) such as NuScale’s reactor power module. Irradiations on NPP cables and companion samples were not completed due to programmatic delays, however a path forward that was based on lessons learned from this project was defined to accommodate future, comparable instrumented gamma irradiations at the HFIR GIF.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Thermal stability of filler‐based ethylene/vinyl acetate/vinyl alcohol terpolymer in nitroplasticizer oxidative environment

Abstract To study the thermal stability of ethylene/vinyl acetate/vinyl alcohol (EVA‐OH) composite with filler particles, systematic thermogravimetric analysis (TGA) investigation was conducted in both nonisothermal and isothermal modes. The effect of polymer concentration on the aging behavior of EVA‐OH was investigated in the nitroplasticizer (NP) environment. Fourier transform infrared spectroscopy was used to probe chemical structural changes in the EVA‐OH polymer before and after thermal aging. The results suggest that filler addition accelerates the rate of NP exudation out of the EVA‐OH composites and deteriorates the thermal stability of NP at moderate temperatures (up to 70°C). The degradation of NP, in turn, accelerates the degradation of EVA‐OH polymer in its composite form through oxidation and hydrolysis indicating the importance of antioxidants in such phase blends.

36 MATERIALS SCIENCE↗

Aging of UV curable PDMS developed for large-scale, high viscosity stereolithography

Polydimethylsiloxane (PDMS) elastomers are silicone rubbers that find widespread application in both academic and industrial settings. This study investigates the use of photosensitive platinum catalysts for UV-activated hydrosilylation of PDMS, which enables the additive manufacturing of PDMS objects through techniques such as stereolithography. Specifically, this study focuses on understanding the aging behavior of Pt-catalyzed, UV-curable PDMS samples, including their mechanical behavior under thermal and UV-accelerated aging conditions. The results show that the Pt-catalyzed, UV-curable PDMS introduced in this research is ‘under-cured’ after being printed and will slowly evolve over time resulting in increased stiffness and decreased elongation, likely due to the formation of additional crosslinks. FTIR spectroscopy indicates that no new chemical bonds or functional groups are generated through the aging process, suggesting that no thermal degradation or polymer chain scissions occur in the polymer matrix. Overall, this PDMS formulation exhibits greater mechanical strength and significantly less reduction in strength with aging, compared with the commonly used, UV-curable thiol-ene PDMS.

36 MATERIALS SCIENCE↗

High-temperature stability and thermal expansion behavior of equi-atomic refractory multi-principal element alloys based on MoNbTi system for Gen IV reactor applications

The present study investigates the thermal stability and thermal expansion behavior of seven equi-atomic refractory multi-principal element alloys (MPEAs) based on the MoNbTi ternary system composed of low neutron absorption cross section elements. Through an integrated approach utilizing in-situ high-temperature X-ray diffraction (HT-XRD) in conjunction with differential scanning calorimetry (DSC), dilatometry and ageing heat treatment, the thermal stability of the MPEAs was comprehensively analyzed. In-situ HT-XRD experiment confirmed the stability of the room temperature phases up to 1000 °C with no peaks observed corresponding to additional phases in the HT-XRD patterns at 500, 800 and 1100 °C. DSC thermograms showed the absence of peaks up to 1000 °C, while peaks and valleys corresponding to exothermic and endothermic events were observed above 1000 °C. Coefficient of thermal expansion (CTE) derived from second order polynomial fitting of linear thermal expansion data from the dilatometry experiment showed linear increment up to 1000 °C for all the alloys except those containing Zr. The Cr containing alloys exhibited notably higher CTE values, particularly the Al containing alloy exhibited the highest value. Ageing heat treatment at 800 and 1000 °C for 96 h and subsequent microstructural analysis revealed significant precipitation of secondary phases in MoNbTiZr, MoNbTiZrV and MoNbTiCrAl. In conclusion, a substantial increase in hardness was observed in MoNbTiZr and MoNbTiCrAl due to secondary phase precipitation, while the other alloys maintained hardness values comparable to their as-cast and homogenized states.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Impact of Different Thermal Gradients on the Dynamics of Cylindrical Lithium-ion Cells Subject to Accelerated Aging and on Module Performance

This study investigates the impacts of applying different thermal gradient patterns to cylindrical lithium-ion cells in a module on cell dynamics (temperatures, current flows, state of charge), module performance (evolution of resistance, capacity, and energy versus cycle number), and module lifetime. The thermal gradients were generated using cooling plates (CPs) with three different flow-field designs, namely, straight, perpendicular, and U-turn. The study uses computational fluid dynamics (CFD), the pseudo-two-dimensional (P2D) battery model, capacity loss and increased impedance due to the growth of a solid-electrolyte-interphase, and the electric current distribution from module terminals to cells that depends on the series-parallel electrical connections among the cells. The impact of the thermal gradient (resulting from the CP designs) on the variability in resistance, current, state of charge, and voltage among the cells was analyzed and linked to differences in the module's performance. Applying a thermal gradient to parallel-connected strings of series-connected cells led to variation in the current through each parallel string and an imbalance in the voltage of series-connected cells. Module performance is poorer when the thermal gradient causes a voltage imbalance than when it causes a current imbalance. Module performance becomes the worst when both current variation and voltage imbalance happen together. For instance, the module's lifetime (estimated as reaching 80% of its initial capacity) varied by 5% to 17.5%, depending on the magnitude and pattern of the imposed thermal gradient. As the relative orientation between thermal gradients and cells' electrical connectivity influences the module's performance, appropriate consideration should be given to the choice of the CP, especially if large thermal gradients are allowed.

Battery thermal management↗

High-Resolution Thermal Profiling of a High-Power Diode Laser Facet During Aging

Here, we study the facet temperature distribution of a high-power diode laser over its lifetime using a noncontact, high spatial resolution CCD-based thermoreflectance technique. Based on the known correlation between non-radiative defects and heating, thermal maps can provide valuable information regarding the formation and evolution of small point defects that are at or near the facet during aging. In the laser under study in this work we measure the appearance of local hot spots on the facet, including concentrated hot spots that appear just before or just after COD and are correlated with loss of local light emission. The locations of these hot spots do not exhibit morphology changes in high-resolution SEM imaging of the facet, indicating that the related defects are too small to be observable in SEM or are located at some depth under the facet. Prior to COD, we measure a gradual facet temperature increase accompanied by a gradual optical power decrease and gradual facet optical absorption increase, indicating gradual degradation of the laser.

47 OTHER INSTRUMENTATION↗

2023 Status Report - Fiberboard Properties and Degradation Rates for Storage of 9975 Shipping Package in KAC

Thermal, mechanical, and physical properties have been measured on fiberboard samples aging for up to 18 years at accelerated conditions. The aging environments include elevated temperature up to 250 ºF (the maximum allowed service temperature for fiberboard in 9975 packages) and elevated humidity. Accelerated aging results have been analyzed and used to build aging models. Correlations relating several properties (thermal conductivity, energy absorption, weight, dimensions, and density) to their rate of change in potential storage environments have been developed. Combined with an estimate of the actual conditions the fiberboard experiences in K-Area Complex (KAC), these models allow development of service life predictions.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Thermal Decomposition Kinetics of 4,6‐Diamino‐5,7‐dinitro‐benzo‐furazan

This experimental study investigated the thermal decomposition kinetics of 4,6-diamino-5,7-dinitro-benzo-furazan (referred to as F1 hereafter)—an important decomposition product of 1,3,5-triamino-2,4,6-trinitrobenzene (TATB—a prototypical insensitive high explosive). Simultaneous differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), and mass spectrometry (MS) measurements were employed to determine the decomposition kinetics of F1 and to track the evolution of product gases. The DSC profiles were measured at 10 different heating rates between 0.025°C/min and 10°C/min. The measured exotherms were influenced by F1 melting at heating rates above 0.25°C/min, and corresponding changes in decomposition enthalpy and TGA mass-loss-rate profiles indicated a transition from solid-to-gas decomposition to an increasing contribution from liquid-to-gas decomposition. Analysis of low-heating-rate DSC data between 0.025°C/min and 0.17°C/min with the extended Prout–Tompkins model yielded an activation energy of 305 kJ/mol for solid-to-gas F1 decomposition, higher than previous values inferred from TATB decomposition models involving F1. This study provides the first direct experimental determination of the energy barrier for F1 decomposition. MS measurements showed that the major gaseous products matched species previously reported for TATB decomposition (e.g., CO 2 , HCN, C 2 N 2 , etc.), with water identified as the dominant product. Furthermore, these results provide important experimental constraints for improving chemical kinetics models of TATB decomposition and for predicting the reactivity, stability, and safety of TATB-based high explosives under long-term aging conditions and abnormal thermal environments.

4,6-Diamino-5,7-dinitro-benzo-furazan↗

Experimental Aging and Lifetime Prediction in Grid Applications for Large-Format Commercial Li-Ion Batteries

Due to the growth of electric vehicle and stationary energy storage markets, the production and use of lithium-ion batteries has grown exponentially in recent years. For many of these applications, large-format lithium-ion batteries are being utilized, as large cells have less inactive material relative to their energy capacity and require fewer electrical connections to assemble into packs. And especially for stationary energy storage systems, where energy delivered is the only revenue source, the economics of these battery systems is highly dependent on cell lifetime. However, testing of large-format lithium-ion batteries is time consuming and requires high current channels and large testing chambers, making information on the performance of commercial, large-format lithium-ion batteries hard to come by. Here, accelerated aging test data from four commercial large-format lithium-ion batteries is reported. These batteries span both NMC-Gr and LFP-Gr cell chemistries, pouch and prismatic formats, and a range of cell designs with varying power capabilities. Accelerated aging test results are analyzed to examine both cell performance, in terms of efficiency and thermal response under load, as well as cell lifetime. Cell thermal response is characterized by measuring temperature during cycle aging, which is used to calculated a normalized thermal resistance value that may help estimate both cell cooling needs or to help extrapolate aging test results to different thermal environments. Cell lifetime is evaluated qualitatively, considering simply the average calendar and cycle life across a range of conditions, as well as quantitatively, using statistical modeling and machine-learning methods to identify predictive aging models from the accelerated aging data. These predictive aging models are then used to investigate cell sensitivities to stressors, such as cycling temperature, voltage window, and C-rate, as well as to predict cell lifetime in various stationary storage applications. Results from this work show that cell lifetime and sensitivity to aging conditions varies substantially across commercial cells, necessitating testing for specific cell formats to make quantitative lifetime predictions. That being said, all commercial cells tested here are predicted to reach at least 10-year lifetimes for stationary storage applications. Based on the aging test results and modeling, some cells are expected to be relatively insensitive to temperature and use-case, making them suited for simple use cases with little or no thermal management and simple controls, while the lifetime of other cells could be extended to 20+ years if operated with thermal management and degradation-aware controls.

battery↗

Radiation-Induced Modifications in Copper Oxide Growth

Radiation-induced effects and their influence on oxidation processes were evaluated for their use as a forensic tool for special nuclear material (SNM). A beam of 10 MeV Au³⁺ ions was used to mimic the accumulation of microstructural damage from self-irradiation through the decay of radionuclides. Several copper samples were irradiated as suitable surrogate materials at 200 °C with a flux of 1x10¹² ions/cm·s to damage levels of 5, 10, and 15 displacements per atom (dpa). This corresponds to about 50, 100, and 150 years, respectively, of accumulated α-decay damage in a PuGa alloy assuming a damage rate of 0.1 dpa/year. After irradiation, all samples were exposed to an accelerated aging process induced by thermal treatment at 350 °C for 1 hour in air. This resulted in the growth of a mixed oxide layer (Cu₂O and CuO) which was characterized in detail using several complementary analytical techniques: Scanning Electron Microscopy, Raman spectroscopy, Synchrotron X-ray diffraction (transmission mode), and Grazing Incidence X-ray diffraction. The oxide layer growth of irradiated Cu at 350°C is distinctly modified as a result of the ion irradiation. Most notably, the growth of the CuO phase is suppressed with increasing radiation damage on the Cu substrate, and structural changes occurred in the Cu₂O phase. These results indicate that damage from self-irradiation over time can cause quantifiable modifications in the oxidation process of metals that could be harnessed for their use as a novel forensic tool.

36 MATERIALS SCIENCE↗

SR19021 Tritium Aging of Regenerated LANA.75 (Final Project Report)

The Savannah River Tritium Enterprise (SRTE) has used the metal hydride LaNi 4.25 Al 0.75 (LANA.75) in the Tritium Facilities for over two decades. The objective of this project was to expand upon the understanding of LANA.75 regeneration. Three distinct scopes were identified: monitor tritium aging of the single sample regenerated, regenerate a second tritium-aged sample, and perform thermal stability testing on a non-tritiated sample of LANA.75.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

2025 Status Report - Fiberboard Properties and Degradation Rates for Storage of 9975 Shipping Package in KAC

Fiberboard assemblies in the 9975 package were identified as susceptible to aging and degradation under long-term storage conditions. Thermal, mechanical, and physical properties have been measured on fiberboard samples aging for up to 20 years at accelerated conditions. The aging environments include elevated temperature up to 250 ºF (the maximum allowed service temperature for fiberboard in 9975 packages) and elevated humidity. Accelerated aging results have been analyzed and used to build aging models. Correlations relating several properties (thermal conductivity, energy absorption, weight, dimensions, and density) to their rate of change in potential storage environments have been developed. Combined with an estimate of the actual conditions the fiberboard experiences in K-Area Complex (KAC), these models allow development of service life predictions. KAC completed calculations that supported extending the service life of 9975 packages with 3013 containers in storage from 20 years to 40 years. These calculations addressed the potential for degraded fiberboard properties following 40 years in storage using degradation models. The 40 year storage evaluations assumed the degradation rates from initial values for density, dimensional, and thermal properties were 0.5% per year (i.e., after 40 years, the density, dimensional, and thermal properties of fiberboard were 80% of its initial values). The updated degradation models developed in this report were compared to the assumptions in those calculations, and the current results for fiberboard dimensions, density, axial and radial thermal conductivities, and energy absorption remain consistent with those calculations. Additional data will continue to be collected to permit future refinements to the models and assumptions. Some of the predicted degradation rates presented in this report are purposely high to accelerate aging. These rates relate to environments that do not exist within KAC or are postulated to only occur as upset conditions that are unlikely to persist for an extended period. For a typical package stored in KAC with approximately 10-12 watts internal heat load or less, and ambient temperatures below 90 ºF, the fiberboard assemblies experience storage conditions less severe than any of the aging environments (i.e., under 125 °F) used in this study. Fiberboard in conforming packages with lower internal heat loads should experience little or no degradation and is expected to provide a service life beyond the currently approved 40 year storage period. Packages with higher internal heat loads may not continue to perform their required safety functions beyond 40 years. Ultimately, service life will be determined by the cumulative effect of degradation from all the conditions these packages might encounter. The results and model predictions presented in this report are applicable to 9975 packages with cane or softwood fiberboard overpack assemblies. These degradation models do not address the effects of nonconforming conditions such as the presence of excess moisture and mold or beetle infestations.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Unraveling the Combined Photothermal Stability of Common Perovskite Solar Cell Compositions

In halide perovskite solar cells, certain compositions, especially those with a high mixture of anions, degrade rapidly. Here, in this study, a degradation study compares the photo (exposure to light), thermal (exposure to elevated temperatures), and photo-plus-thermal (combination) stability of three representative perovskite compositions chosen for their relatively high performance and to independently test anion versus cation effects. Based upon experience and reports, the compositions studied are triple cation with a high Br ratio (Cs 0.05 (FA 0.98 MA 0.02 ) 0.95 Pb(I 0.5 Br 0.5 ) 3 ), all iodide with a moderately high Cs ratio (FA 0.8 Cs 0.2 PbI 3 ), and FA-dominated triple cation (Cs 0.05 (FA 0.98 MA 0.02 ) 0.95 Pb(I 0.98 Br 0.02 ) 3 ). Cs 0.05 (FA 0.98 MA 0.02 ) 0.95 Pb(I 0.98 Br 0.02 ) 3 displayed the best combined photo-plus-thermal stability. Degradation mechanisms were investigated by comparing the morphology, surface composition, and bulk and interface carrier dynamics. Under the harshest aging conditions (photo-plus-thermal), phase segregation and vaporization of organic cations occurred, along with the appearance of high-energy states indicating the interaction with C 60 . The findings were verified on perovskite films blade-coated in air used in devices (FTO/NiOx/SAM/Perovskite/C 60 /BCP/Cu), achieving an efficiency of 21.9% alongside correlated stability.

14 SOLAR ENERGY↗

Fiberboard Properties and Degradation Rates for Storage of 9975 Shipping Packages in KAC (2021 Status Report)

Thermal, mechanical, and physical properties have been measured on fiberboard samples following accelerated aging for up to 16 years. The aging environments include elevated temperature up to 250 ºF (the maximum allowed service temperature for fiberboard in 9975 packages) and elevated humidity. Accelerated aging results have been analyzed and used to build aging models. Correlations relating several properties (thermal conductivity, energy absorption, weight, dimensions, and density) to their rate of change in potential storage environments have been developed. Combined with an estimate of the actual conditions the fiberboard experiences in K-Area Complex (KAC), these models allow development of service life predictions. KAC completed calculations that supported extending the service life of 9975 packages with 3013 and non3013 containers in storage from 15 years to 20 years. These calculations addressed the potential for degraded fiberboard properties following 20 years in storage using degradation models developed previously. The updated degradation models developed in this report have been compared to the assumptions in these calculations, and the current results for fiberboard dimensions, density, radial thermal conductivity, and energy absorption remain consistent with those calculations. The axial thermal conductivity degradation rate slightly exceeds calculations estimate of 0.5% per year between 130 and 160 °F. Additional data will continue to be collected to permit future refinements to the models and assumptions. Some of the predicted degradation rates presented in this report are extreme. However, these relate to environments that do not exist within KAC or would be postulated only as upset conditions that would not likely persist for an extended period. For a typical package stored in KAC with approximately 10-12 watts internal heat load or less, and ambient temperatures below 90 ºF, the fiberboard assemblies experience storage conditions less severe than any of the aging environments. Fiberboard in conforming packages with lower internal heat loads should experience little or no degradation and is expected to provide a service life beyond the currently approved 20 year storage period. Packages with higher internal heat loads may not continue to perform their required safety functions beyond 20 years. Ultimately, service life will be determined by the cumulative effect of degradation from all the conditions these packages might encounter. The results and model predictions presented in this report are applicable to 9975 packages with cane or softwood fiberboard overpack assemblies. These degradation models do not address the effects of nonconforming conditions such as the presence of excess moisture and mold or beetle infestations.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Fiberboard Properties and Degradation Rates for Storage of 9975 Shipping Package in KAC (2022 Status Report)

Thermal, mechanical, and physical properties have been measured on fiberboard samples following accelerated aging for up to 17 years. The aging environments include elevated temperature up to 250 °F (the maximum allowed service temperature for fiberboard in 9975 packages) and elevated humidity. Accelerated aging results have been analyzed and used to build aging models. Correlations relating several properties (thermal conductivity, energy absorption, weight, dimensions, and density) to their rate of change in potential storage environments have been developed. Combined with an estimate of the actual conditions the fiberboard experiences in K-Area Complex (KAC), these models allow development of service life predictions. KAC completed calculations that supported extending the service life of 9975 packages with 3013 containers in storage from 20 years to 40 years. These calculations addressed the potential for degraded fiberboard properties following 40 years in storage using degradation models developed previously. Due to differences in containers, 9975 packages with non-3013 containers are only approved for 20 years of storage. The updated degradation models developed in this report have been compared to the assumptions in those calculations, and the current results for fiberboard dimensions, density, radial thermal conductivity, and energy absorption remain consistent with those calculations. The axial thermal conductivity degradation rate slightly exceeds calculations estimate of 0.5% per year between 130 and 160 °F. Additional data will continue to be collected to permit future refinements to the models and assumptions. Some of the predicted degradation rates presented in this report are extreme. However, these relate to environments that do not exist within KAC or would be postulated only as upset conditions that would not likely persist for an extended period. For a typical package stored in KAC with approximately 10-12 watts internal heat load or less, and ambient temperatures below 90 °F, the fiberboard assemblies experience storage conditions less severe than any of the aging environments. Fiberboard in conforming packages with lower internal heat loads should experience little or no degradation and is expected to provide a service life beyond the currently approved 40 year storage period. Packages with higher internal heat loads may not continue to perform their required safety functions beyond 40 years. Ultimately, service life will be determined by the cumulative effect of degradation from all the conditions these packages might encounter. The results and model predictions presented in this report are applicable to 9975 packages with cane or softwood fiberboard overpack assemblies. These degradation models do not address the effects of non-conforming conditions such as the presence of excess moisture and mold or beetle infestations.

36 MATERIALS SCIENCE↗