Optimizing cathodoluminescence microscopy of buried interfaces through nanoscale heterostructure design
Spatial resolution and brightness in cathodoluminescence can be tuned by nanoscale design of samples.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Spatial resolution and brightness in cathodoluminescence can be tuned by nanoscale design of samples.
Core–shell particles with a Prussian blue analogue Rb a Co b [Fe(CN) 6 ] c · m H 2 O core and different shell thicknesses are studied as the cores undergo both thermal and light-induced spin transitions, revealing different mechanisms for accommodating strain.
Group IV-based germanium-tin (Ge1-ySny) compositional materials have recently shown great promise for infrared detection, light emission and ultra-low power transistors. High carrier lifetimes are desirable for enhancing the detection limit and efficiency of photodetectors, low threshold current density in lasers, and low tunneling barrier height by lowering defects and dislocations at the heterointerface of a source and a channel. Here, carrier lifetimes in epitaxial germanium (Ge) and variable tin (Sn) compositional Ge1-ySny materials were experimentally determined on GaAs substrates using the contactless microwave photoconductive decay (u-PCD) technique at an excitation wavelength of 1500 nm. Sharp (2 x 2) reflection high energy electron diffraction patterns and low surface roughness were observed from the surface of the Ge0.97Sn0.03 epilayer. X-ray rocking curves from Ge0.97Sn0.03 and Ge0.94Sn0.06 layers demonstrated the pseudomorphic and lattice-matched growth on AlAs and In0.12Al0.88As buffers, respectively, further substantiated by reciprocal space maps and abrupt heterointerfaces evident from the presence of Pendellosung oscillations. High effective carrier lifetimes of 150 ns to 450 ns were measured for Ge1-ySny epilayers as a function of Sn composition, surface roughness, growth temperature, and layer thickness. The observed increase in the carrier lifetime with an increasing Ge layer thickness and a reducing surface roughness, by incorporating Sn, were explained. The enhancement of the carrier lifetime with an increasing Sn concentration was achieved by controlling the defects with lattice-matched Ge0.94Sn0.06/In0.12Al0.88As heterointerfaces or the pseudomorphic growth of Ge0.94Sn0.06 on GaAs. Therefore, our monolithic integration of variable Sn alloy compositional Ge1-ySny materials with high carrier lifetimes opens avenues to realize electronic and optoelectronic devices.
High-throughput combinatorial synthesis of Al 1− x RE x N (RE = Pr, Tb) thin films with 0 < x < 0.4 was performed to assess composition-phase-property relationships in an emerging materials family.
Colossal ionic conductivity was recently discovered in YSZ/SrTiO3 multilayers and was ex- plained in terms of strain and interface-enhanced disorder of the O sublattice. In the present paper we use a combination of scanning transmission electron microscopy and electron energy loss spectroscopy (EELS) and theoretical EELS simulations to confirm the presence of a disordered YSZ O sublattice in coherent YSZ/SrTiO3 multilayers. O K-edge fine structure simulated for the strained disordered O sublattice phase of YSZ possess blurred-out features compared to that of ordered cubic bulk YSZ, and experimental EELS fine structure taken from the strained YSZ of coherent YSZ/SrTiO3 thin films is similarly blurred out. Elemental mapping is shown to be capable of resolving ordered YSZ O sublattices. Elemental mapping of O in the coherent YSZ/STO multilayers is presented in which the O sublattice is seen to be clearly resolved in the STO but blurred out in the YSZ, indicating it to be disordered. In addition, we present imaging and EELS results which show that strained regions exist at the incoherent interfaces of YSZ islands in STO with blurred out fine structure suggesting these incoherent regions may also support high ionic conductivites. Recently, Cavallaro et al. reported electronic conductivities in samples of incoherent disconnected islands embedded in STO that are similar to the islands described herein. The presence of a region of O depleted STO at the interface with incoherent YSZ islands is revealed by EELS elemental mapping, implying the n-type doping of STO/YSZ nanocomposites with disconnected incoherent YSZ islands.
Abstract not provided
Single crystal AlN thin films were epitaxially grown on GaN/sapphire (0001) substrates on a macroscopic scale by magnetron sputtering. The microscopic structure and orientation degree of the AlN epilayers were studied by high-resolution transmission electron microscopy, high-resolution x-ray diffraction, and reciprocal spacing mapping. It was revealed that the AlN epilayers have high in-plane and out-of-plane orientation degrees and low defect density. The electrical and optical properties of the AlN epilayers were also studied, and the results suggest that the AlN epilayers grown by sputtering may be employed in the fabrication of GaN-based light-emitting diode devices with increased efficiency.
We demonstrate that a controllable cracking can be realized in Si with a buried strain layer when hydrogen is introduced using traditional H-ion implantation techniques. However, H stimulated cracking is dependent on H projected ranges; cracking occurs along a Si{sub 0.8}Ge{sub 0.2} strain layer only if the H projected range is shallower than the depth of the strained layer. The absence of cracking for H ranges deeper than the strain layer is attributed to ion-irradiation induced strain relaxation, which is confirmed by Rutherford-backscattering-spectrometry channeling angular scans. The study reveals the importance of strain in initializing continuous cracking with extremely low H concentrations.
We report the controlled growth of vertically aligned GaAs/AlGaAs core-shell nanowires. By optimizing the shell deposition temperature and catalyst density we maintain high temperature stability and achieve defect-free epitaxial AlGaAs shell deposition with high aluminum incorporation. Energy dispersive x-ray analysis determines the shell composition to be Al{sub 0.9}Ga{sub 0.1}As and measures the uniformity of the shell thickness. Lattice-resolved high-angle annular dark-field scanning transmission electron microscopy images confirm the core-shell interface to be defect-free, epitaxial, and atomically sharp. The ability to realize GaAs/AlGaAs core-shell nanowires with precise control over the morphology and composition is essential to the development of nanowire-based high mobility electronics.
The authors have investigated changes in the electronic structures of digitally controlled La{sub 0.6}Sr{sub 0.4}MnO{sub 3} (LSMO) layers sandwiched between SrTiO{sub 3} as a function of LSMO layer thickness in terms of hard x-ray photoemission spectroscopy (HX-PES). The HX-PES spectra show the evolution of Mn 3d derived states near the Fermi level and the occurrence of metal-insulator transition at 8 ML. The detailed analysis for the thickness dependent HX-PES spectra reveals the existence of the less conducting and nonmagnetic transition layer with a film thickness of about 4 ML in the interface region owing to significant interaction through the interface.
We have developed a method for photoelectrochemical etching of p-type semiconductors, including GaN, that relies on the built-in bandbending already inherent to optical devices. Electron-hole pairs are generated by filtered light in a buried small bandgap layer, and a pn junction separates the charge. Electrons are sent into the n-type layer, where they are extracted, and holes to the surface, where they participate in etching reactions. This technique is rapid and inexpensive, and it requires no applied bias or elevated temperatures. This technique has widespread applications to GaN optical devices where ion-damage-free etching or wide tunability of etch parameters is desired.
The defect structure of Ge(111) epilayers grown by molecular beam epitaxy on cubic Pr{sub 2}O{sub 3}(111)/Si(111) support systems was investigated by means of transmission electron microscopy and laboratory-based x-ray diffraction techniques. Three main types of defects were identified, namely, rotation twins, microtwins, and stacking faults, and studied as a function of Ge film thickness and after annealing at 825 deg. C in ultrahigh vacuum. Rotation twins were found to be localized at the Ge(111)/cubic Pr{sub 2}O{sub 3}(111) interface and their amount could be lowered by the thermal treatment. Microtwins across (111) were detected only in closed Ge films, after Ge island coalescence. The fraction of Ge film volume affected by microtwinning is constant within the thickness range of approx20-260 nm. Beyond 260 nm, the density of microtwins is clearly reduced, resulting in thick layers with a top part of higher crystalline quality. Microtwins resulted insensitive to the postdeposition annealing. Instead, the density of stacking faults across (111) planes decreases with the thermal treatment. In conclusion, the defect density was proved to diminish with increasing Ge thickness and after annealing. Moreover, it is noteworthy that the annealing generates a tetragonal distortion in the Ge films, which get in-plane tensely strained, probably due to thermal mismatch between Ge and Si.
GaAs-MnAs core-shell structures are grown by molecular-beam epitaxy using wurtzite GaAs nanowires on GaAs(111)B. The nanowire structures curve due to the strain at the heterointerface when the substrate is not rotated during the growth, evidencing the diffusion length in the MnAs overgrowth being less than the perimeter of the columns. The MnAs growth is thus demonstrated to take place by direct deposition on the sidewall. The MnAs envelope is m-plane-oriented with the c-axis along the nanowire axis. The magnetic easy axis hence lies in the surface plane of the substrate, which is confirmed by magnetization measurements and magnetic-force microscopy.
Measurement results of the acoustoelectric effects [surface acoustic waves (SAW) attenuation and velocity] in a high-mobility p-SiGe/Ge/SiGe structure are presented. The structure was low-energy plasma-enhanced chemical vapor deposition grown with a two-dimensional (2D) channel buried in the strained Ge layer. The measurements were performed as a function of temperature (1.5-4.2 K) and magnetic field (up to 8.4 T) at different SAW intensities at frequencies 28 and 87 MHz. Shubnikov-de Haas-like oscillations of both SAW attenuation and the velocity change have been observed. Hole density and mobility, effective mass, quantum and transport relaxation times, as well as the Dingle temperature were measured with a method free of electric contacts. The effect of heating of the 2D hole gas by the electric field of the SAW was investigated. Energy relaxation time tau{sub e}psilon and the deformation potential constant determined.
Al{sub x}Ga{sub 1-x}N films grown on nonpolar m (1100) and (1122) semipolar orientations of freestanding GaN substrates were investigated over a range of stress states (x<=0.17). Cracking on the (0001) plane was observed beyond a critical thickness in the (1100) oriented films, while no cracking was observed for (1122) films. Theoretical analysis of tensile stresses in Al{sub x}Ga{sub 1-x}N for the relevant planes revealed that anisotropy of in-plane biaxial stress for the nonpolar (1100) planes results in the highest normal stresses on the c-planes, consistent with experimental observations. Shear stresses are significant in the semipolar case, suggesting that misfit dislocation formation provides an alternative mechanism for stress relief.
Explore the source record for details and available documents.
Superlattices (SLs) with different periodicity of ferromagnetic La{sub 0.7}Sr{sub 0.3}MnO{sub 3} (LSMO) and ferroelectric Ba{sub 0.7}Sr{sub 0.3}TiO{sub 3} as constitutive layers were fabricated on conducting LaNiO{sub 3} coated (001) oriented MgO substrates using pulsed laser deposition. The crystallinity, ferroelectric, and magnetic properties of the SLs were studied over a wide range of temperatures and frequencies. The structure exhibited ferromagnetic behavior at 300 K and ferroelectric behavior over a range of temperatures between 100 and 300 K. A frequency-dependent change in dielectric constant and tangent loss were observed above the ferromagnetic-paramagnetic temperature. The frequency-dependent dielectric anomalies are attributed to the change in metallic and magnetic nature of LSMO and also the interfacial effect of two different phases that are connected alternatively in series. The effect of ferromagnetic LSMO layers on ferroelectric properties of the SLs indicated strong influence of the interfaces. The asymmetric behavior of ferroelectric loop and the capacitance-voltage relationship suggest development of a built field in the SLs due to high strain across the interfaces.
Refine your search to explore more results.