Search NASA⌕ Search

SEARCH · Search NASA

Results for “ION IMPLANTATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,801 records · Page 100

Diffusion and recrystallization of B implanted in crystalline and pre-amorphized Ge in the presence of F

Although the diffusion control and dopant activation of Ge p-type junctions are straightforward when using B{sup +} implantation, the use of the heavier BF{sub 2}{sup +} ions or even BF{sup +} is still favored in terms of shallow junction formation and throughput—because implants can be done at higher energies, which can give higher beam currents and beam stability—and thus the understanding of the effect of F co-doping becomes important. In this work, we have investigated diffusion and end-of-range (EOR) defect formation for B{sup +}, BF{sup +}, and BF{sub 2}{sup +} implants in crystalline and pre-amorphized Ge, employing rapid thermal annealing at 600 °C and 800 °C for 10 s. It is demonstrated that the diffusion of B is strongly influenced by the temperature, the presence of F, and the depth of amorphous/crystalline interface. The B and F diffusion profiles suggest the formation of B–F complexes and enhanced diffusion by interaction with point defects. In addition, the strong chemical effect of F is found only for B in Ge, while such an effect is vanishingly small for samples implanted with F alone, or co-implanted with P and F, as evidenced by the high residual F concentration in the B-doped samples after annealing. After 600 °C annealing for 10 s, interstitial-induced compressive strain was still observed in the EOR region for the sample implanted with BF{sup +}, as measured by X-ray diffraction. Further analysis by cross-sectional transmission electron microscopy showed that the {311} interstitial clusters are the majority type of EOR defects. The impact of these {311} defects on the electrical performance of Ge p{sup +}/n junctions formed by BF{sup +} implantation was evaluated.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

AM metal substrates for inkjet-printing of smart devices

Highlights: • An experimental study to characterize 3D-printed metal substrates and their surfaces for inkjet-printing is presented. • Multilayer structures composed of an insulating layer and a superposed conductive layer, inkjet-printed onto various metallic substrates. • Characterization based on microscopic and Focused Ion Beam (FIB) images, profilometer and contact angle measurements of the substrates. • Microscopic images and four-point-probe resistance- and profilometer measurements to gain insight into the quality of the multilayer print. - Abstract: A study to characterize surface and structural properties of 3D-printed metal substrates for multilayer inkjet-printing is presented. Such substrates can enable and alleviate the fabrication of smart and functional packages, implants or spare parts. For the characterization, a multilayer structure composed of an insulating layer and a superposed conductive layer is inkjet-printed onto the various 3D-printed metallic substrates. The printing is done using equivalent settings for all substrates. The characterization is based on microscopic and Focused Ion Beam (FIB) images, as well as profilometer and contact angle measurements of the substrates. Furthermore, microscopic images and four-point-probe resistance- and profilometer measurements are carried out, to gain insight into the quality of the multilayer print. We show the diversity in surface and structural properties of 3D-printed substrates, also for those fabricated using the same process. Also, the 3D-printed samples exhibit different wettability properties than metals processed using standard processes. Finally, we can also demonstrate the suitability of selected substrates for inkjet-printing.

36 MATERIALS SCIENCE↗

Monitoring the Strain Evolution of Lithium‐Ion Battery Electrodes using an Optical Fiber Bragg Grating Sensor

Abstract More advanced characterization and developmental tools are essential to improve the performance and safety of Li‐ion batteries. Conventional tools have been limited to customized test cell configurations that require special facilities and expensive equipment. As a practical solution for the in situ monitoring of realistic battery cells, we have embedded fiber optic sensors within Li‐ion battery pouch cells to monitor the internal electrode strain and temperature during cycling. Here we report the direct monitoring of strain evolution using implanted fiber‐optic sensors within the individual electrodes in a Li‐ion battery. Reproducible peak shifting and splitting in the implanted fiber optic sensor originate from the accumulated longitudinal and transverse strains associated with the expansion or contraction of the anode electrode. These discoveries demonstrate the feasibility and utility of fiber Bragg grating (FBG) sensors to be used as diagnostic tools in the development of new battery materials and structures.

Bae, Chang‐Jun↗

Effect of H and He Irradiation on Cavity Formation and Blistering in Ceramics

Single- or poly-crystalline specimens of SiC, Si{sub 3}N{sub 4}, MgO, Al{sub 2}O{sub 3} and MgAl{sub 2}O{sub 4} were implanted with 0.4-1 MeV H{sup +} or He{sup +} ion beams at room temperature and 650 C up to fluences of {approx}1 x 10{sup 22}/m{sup 2}. This produced peak implanted gas and displacement damage levels as high as {approx}50 at.% and 34 displacements per atom (dpa). The specimens were subsequently examined optically, and in cross-section using transmission electron microscopy. Subsurface blistering occurred for specimens irradiated to H or He fluences greater than about 3 x 10{sup 21}/m{sup 2} ({approx}15 at.% peak implanted gas concentration), and surface exfoliation occurred for fluences above {approx}1 x 10{sup 22}/m{sup 2} ({approx}40 at.% implanted gas). Both helium and hydrogen had comparable effectiveness for inducing blistering and exfoliation on an atomic basis. The threshold blistering and exfoliation fluences for both ions were weakly dependent on temperature between 25 and 650 C. Both H and He were found to be very effective in inducing matrix cavity formation, due to their low solubility in these ceramics. The implanted gas concentrations that resulted in visible cavity formation generally ranged from 1 to 5 at.%. Visible cavity formation was readily induced during room temperature irradiation despite the limited vacancy mobility in these ceramics at room temperature. Three general types of cavity morphologies were observed: isolated cavities, clusters of small cavities (typically associated with dislocation loops), and two-dimensional platelets. Cavity formation was observed to initiate at the periphery of dislocation loops in some cases. During elevated temperature irradiation, cavity formation was often observed to be preferentially associated with certain low-index habit planes, particularly if the habit plane was oriented nearly parallel to the irradiated surface: (0001) and {l_brace}1{bar 1}00{r_brace} for Al{sub 2}O{sub 3}, (0001) for a-SiC, {l_brace}001{r_brace} and {l_brace}110{r_brace} for MgO, and {l_brace}110{r_brace} and {l_brace}111{r_brace} for MgAl{sub 2}O{sub 4}. The bubble formation and blistering behavior of the ceramics was similar to that observed in other studies of metals irradiated at comparable homologous temperatures. Ionization-induced diffusion effects associated with dual-beam light ion irradiation appeared to exert only a weak effect on cavity and dislocation loop growth compared to the single ion irradiation conditions.

08 HYDROGEN↗

Method of electroplating a conversion electron emitting source on implant

Methods for preparing an implant coated with a conversion electron emitting source (CEES) are disclosed. The typical method includes cleaning the surface of the implant; placing the implant in an activating solution comprising hydrochloric acid to activate the surface; reducing the surface by H.sub.2 evolution in H.sub.2SO.sub.4 solution; and placing the implant in an electroplating solution that includes ions of the CEES, HCl, H.sub.2SO.sub.4, and resorcinol, gelatin, or a combination thereof. Alternatively, before tin plating, a seed layer is formed on the surface. The electroplated CEES coating can be further protected and stabilized by annealing in a heated oven, by passivation, or by being covered with a protective film. The invention also relates to a holding device for holding an implant, wherein the device selectively prevents electrodeposition on the portions of the implant contacting the device.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Conceptual Engineering Method for Attenuating He Ion Interactions on First Wall Components in the Fusion Test Facility (FTF) Employing a Low-Pressure Noble Gas

It has been shown that post detonation energetic helium ions can drastically reduce the useful life of the (dry) first wall of an IFE reactor due to the accumulation of implanted helium. For the purpose of attenuating energetic helium ions from interacting with first wall components in the Fusion Test Facility (FTF) target chamber, several concepts have been advanced. These include magnetic intervention (MI), deployment of a dynamically moving first wall, use of a sacrificial shroud, designing the target chamber large enough to mitigate the damage caused by He ions on the target chamber wall, and the use of a low pressure noble gas resident in the target chamber during pulse power operations. It is proposed that employing a low-pressure (~ 1 torr equivalent) noble gas in the target chamber will thermalize energetic helium ions prior to interaction with the wall. The principle benefit of this concept is the simplicity of the design and the utilization of (modified) existing technologies for pumping and processing the noble ambient gas. Although the gas load in the system would be increased over other proposed methods, the use of a "gas shield" may provide a cost effective method of greatly extending the first wall of the target chamber. An engineering study has been initiated to investigate conceptual engineering metmethods for implementing a viable gas shield strategy in the FTF.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Diffusion Experiment in Lithium Ionic Conductors with the Radiotracer of {sup 8}Li: from Micro- to Nano-diffusion

We have developed a radiotracer method for diffusion studies in lithium ionic conductors, by using, as the tracer, the short-lived {alpha}-emitting radioisotope of {sup 8}Li from TRIAC (Tokai Radioactive Ion Accelerator Complex). In the method, we measured {alpha}-particles coming out of the sample of interest and have found that the time-dependent yields of {alpha}-particle from the diffusing {sup 8}Li primarily implanted is a good measure of the Li diffusion in the sample. The method has been successfully applied to measure the lithium diffusion coefficients in a typical defect-mediated lithium ionic conductor of LiGa, well demonstrating that the method is very efficient to measure the diffusion in the micro-meter regime per second. Further development, as an extension of the present method, was proposed to measure the diffusion on the nanoscale in lithium ionic conductors.

36 MATERIALS SCIENCE↗

On Boron Diffusion in MgF{sub 2}

The MgF{sub 2} monocrystals were irradiated at room temperature with 390 keV B{sup +} ions up to the fluence of 10{sup 16} cm{sup -2}. The irradiated samples were (isochronally and isothermally) annealed in high vacuum at the temperatures 200 deg. C, 300 deg. C, 400 deg. C, 500 deg. C, 600 deg. C and 700 deg. C for the times ranging from 2-100 hours. After each annealing step, the boron depth distribution was determined using the neutron depth profiling technique. As implanted, the depth distributions of boron exhibited standard Gaussian-like forms, but the evaluated profile parameters, R{sub P} = 960 nm and {delta}R{sub P} = 140 nm, were higher than those calculated using the SRIM code (R{sub P} = 870 nm and {delta}R{sub P} = 115 nm). Annealing at temperatures up to 400 deg. C did not change the depth profiles. Annealing at 600 deg. C, however, led to a one-way gradual transfer of the boron atoms from the site of implantation towards the sample surface, and in this way a bimodal profile was created. The amount of boron atoms, transferred to the sample surface, was an increasing function of the annealing time. After annealing at 700 deg. C for 64 hours the bimodal profile collapsed into a single broad distribution, extending from the sample surface up to the implantation depth. The observed phenomena clearly points out the stability of the as-implanted boron depth profiles at lower annealing temperatures. Thermal annealing above 600 deg. C, however, liberates boron atoms, which then predominantly migrate from the implantation site towards the sample surface, where they are captured on some unspecified surface defects.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Implanting Transition Metal into Li 2 O-Based Cathode Prelithiation Agent for High-Energy-Density and Long-Life Li-Ion Batteries

Compensating the irreversible loss of limited active lithium (Li) is essentially important for improving the energy-density and cycle-life of practical Li-ion battery full-cell, especially after employing high-capacity but low initial coulombic efficiency anode candidates. Introducing prelithiation agent can provide additional Li source for such compensation. Herein, we precisely implant trace Co (extracted from transition metal oxide) into the Li site of Li 2 O, obtaining (Li 0.66 Co 0.11$\square$0.23 ) 2 O (CLO) cathode prelithiation agent. Further, the synergistic formation of Li vacancies and Co-derived catalysis efficiently enhance the inherent conductivity and weaken the Li-O interaction of Li 2 O, which facilitates its anionic oxidation to peroxo/superoxo species and gaseous O 2 , achieving 1642.7 mAh/g ~Li2O prelithiation capacity (≈980 mAh/g for prelithiation agent). Coupled 6.5 wt % CLO-based prelithiation agent with LiCoO 2 cathode, substantial additional Li source stored within CLO is efficiently released to compensate the Li consumption on the SiO/C anode, achieving 270 Wh/kg pouch-type full-cell with 92 % capacity retention after 1000 cycles.

25 ENERGY STORAGE↗

Nano-Oxide-Dispersed Ferritic Steel for Fusion Energy Systems

The role of oxide nanoparticles in cavity formation of a nano-oxide-dispersed ferritic steel subjected to (Fe + He) dual-ion and (Fe + He + H) triple-ion irradiations has been studied using transmission electron microscopy to elucidate the synergistic effects of helium and hydrogen on radiation tolerance of nano-oxide-dispersed ferritic steel for fusion energy systems. The effect of oxide nanoparticles on suppressing radiation-induced void swelling is clearly revealed from the observation of preferred trapping of helium bubbles at oxide nanoparticles, which results in a unimodal distribution of cavities in the (Fe + He) dual-ion irradiated specimen . An adverse effect of hydrogen implantation, however, is revealed from the observation of a bimodal distribution of cavities with large and facetted voids in association with the formation of HFe 5 O 8 -based hydroxide in local regions of the (Fe + He + H) triple-ion irradiated specimen.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Quantifying the mechanical effects of He, W and He + W ion irradiation on tungsten with spherical nanoindentation

Here, recent advances in spherical nanoindentation protocols have proven very useful for capturing the grain-scale mechanical response of different metals. This is achieved by converting the load–displacement response into an effective indentation stress–strain response which reveals latent information such as the elastic–plastic transition or indentation yield strength and work-hardening behavior and subsequently correlating the response with the material structure (e.g., crystal orientation) at the indentation site. Using these protocols, we systematically study and quantify the microscale mechanical effects of He, W, and He + W ion irradiation on commercially pure, polycrystalline tungsten. The indentation stress–strain response is correlated with the crystal orientation from electron backscatter diffraction, the defect structure from transmission electron microscopy micrographs, and the stopping range of ions in matter calculations of displacement damage and He concentration. He-implanted grains show a much higher indentation yield strength and saturation stress compared to W-ion-irradiated grains for the same displacement damage. There is also good agreement between the dispersed barrier hardening model with a barrier strength of 0.5–0.8 and void models (Bacon–Kochs–Scattergood and Osetsky–Bacon models) with the experimentally observed changes in indentation strength due to the presence of He bubbles. This finding indicates that a high density (~ 9 × 10 23 m –3 ) and concentration (~ 1.5 at.%) of small (~ 1 nm diameter) He bubbles can be moderate to strong barriers to dislocation slip in tungsten.

36 MATERIALS SCIENCE↗

Order-of-magnitude differences in retention of low-energy Ar implanted in Si and SiO{sub 2}

The retention of 1 and 5 keV Ar implanted at 45° in Si and 4.3 nm SiO{sub 2} on Si was studied at fluences between 3 × 10{sup 14} and 1.5 × 10{sup 16} cm{sup −2}. X-ray photoelectron spectroscopy (XPS) served to monitor the accumulation of Ar as well as the removal of SiO{sub 2}. Bombardment induced changes in oxygen chemistry caused the O 1s peak position to move toward lower binding energies by as much as 2.2 eV. Plotted versus depth of erosion, the fluence dependent changes in oxygen content, and peak position were similar at 1 and 5 keV. The Ar content of Si increased with increasing exposure, saturating at fluences of ∼2 × 10{sup 15} cm{sup −2} (1 keV) and ∼6 × 10{sup 15} cm{sup −2} (5 keV). Much less Ar was retained in the SiO{sub 2}/Si sample, notably at 1 keV, in which case the low-fluence Ar signal amounted to only 8% of the Si reference. The results imply that essentially no Ar was trapped in undamaged SiO{sub 2}, i.e., the Ar atoms initially observed by XPS were located underneath the oxide. At the lowest fluence of 5 keV Ar, the retention ratio was much higher (43%) because the oxide was already highly damaged, with an associated loss of oxygen. The interpretation was assisted by TRIM(SRIM) calculations of damage production. Partial maloperation of the ion beam raster unit, identified only at a late stage of this work, enforced a study on the uniformity of bombardment. The desired information could be obtained by determining x,y line scan profiles of O 1s across partially eroded SiO{sub 2}/Si samples. Fluence dependent Ar retention in Si was described using an extended version of the rapid relocation model which takes into account that insoluble implanted rare-gas atoms tend to migrate to the surface readily under ongoing bombardment. The range parameters required for the modeling were determined using TRIM(SRIM); sputtering yields were derived from the literature. The other three parameters determining the Ar signal, i.e., (1) the thickness w of the near-surface Si region devoid of Ar, (2) the relocation efficiency Ψ{sub rlc}, and (3) the effective attenuation length L in XPS analysis were varied within reasonable limits until the calculated retention curves for 1 and 5 keV Ar in Si agreed with experimental data to better than 8%, using the same XPS sensitivity factor throughout. Results: w = 1.4 ± 0.1 nm, Ψ{sub rlc} = 6.6 ± 0.5, and L = 2.7 ± 0.2 nm. Combining experimental and calculated data, it was found that the Ar trapping efficiency of the damaged oxide is intimately correlated with the loss of oxygen. The calculated stationary areal densities of all retained Ar are compared with results obtained by high-resolution medium-energy ion scattering spectrometry. Attractive areas of future research in rare gas retention and nanobubble formation are sketched briefly.

42 ENGINEERING↗

Local and systemic changes associated with long-term, percutaneous, static implantation with titanium alloys in rhesus macaques (Macaca mulatta)

Metal alloys are frequently used as implant materials in veterinary medicine. Recent studies suggest that many types of metal alloys may induce both local and systemic inflammatory responses. In this study, 37 rhesus macaques with long-term skull-anchored percutaneous titanium alloy implants (0-14 years duration) were evaluated for changes in their hematology, coagulation and serum chemistry profiles. Negative controls (n=28) did not have implants. All of the implanted animals were on IACUC-approved protocols and were not implanted for the purpose of this study. Animals with implants had significantly higher plasma D-dimer and lower antithrombin III concentrations compared with nonimplanted animals (p-values < 0.05). Additionally, animals with implants had significantly higher globulin, and lower albumin and calcium concentrations compared with nonimplanted animals (p-values < 0.05). Many of these changes were positively correlated with duration of implantation as well as the number of implants. Chronic bacterial infection was observed on the skin around many of the implant sites, and within deeper tissues. Representative histopathology around the implant site of two implanted animals revealed chronic suppurative to pyogranulomatous inflammation extending from the skin to the dura mater. X-ray fluorescence microscopy of tissue biopsies from the implant site of the same two animals revealed significant increases in free metal ions within the tissue, including titanium and iron. Free metal ions persisted in the tissues up to 6 months postexplant. These results suggest that long-term skull-anchored percutaneous titanium alloy implants results in localized inflammation, chronic infection, and leaching of metal ions into local tissues.

Frydman, Galit F.↗

Microstructure Evolution and Mechanical Response of Nanolaminate Composites Irradiated with Helium at Elevated Temperatures

In this paper, we summarize recent work on helium (He) interaction with various heterophase boundaries under high temperature irradiation. We categorize the ion-affected material beneath the He-implanted surface into three regions of depth, based on the He/vacancy ratio. The differing defect structures in these three regions lead to the distinct temperature sensitivity of He-induced microstructure evolution. The effect of He bubbles or voids on material mechanical performance is explored. Finally, overall design guidelines for developing materials where He-induced damage can be mitigated in materials are discussed.

36 MATERIALS SCIENCE↗

Nanotube array controlled carbon plasma deposition

Finding approaches to control the elementary processes of plasma-solid interactions and direct the fluxes of matter at nano-scales becomes an important aspect in science. This letter reports that, by taking advantages of the spacing characteristics of discrete TiO{sub 2} nanotube arrays, the flying trajectories and the subsequent implantation and deposition manner of energetic carbon ions can be directed and controlled to fabricate hollow conical arrays. The study provides an alternative method for plasma nano-manufacturing.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

A Novel Experimental Setup for Rare Events Selection and Its Potential Application to Super-heavy Elements Search

The paper presents a novel instrumentation for rare events selection which was tested in our research of short lived super heavy elements production and detection. The instrumentation includes an active catcher multi elements system and dedicated electronics. The active catcher located in the forward hemisphere is composed of 63 scintillator detection modules. Reaction products of damped collisions between heavy ion projectiles and heavy target nuclei are implanted in the fast plastic scintillators of the active catcher modules. The acquisition system trigger delivered by logical branch of the electronics allows to record the reaction products which decay via the alpha particle emissions or spontaneous fission which take place between beam bursts. One microsecond wave form signal from FADCs contains information on heavy implanted nucleus as well as its decays.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Method of making a high voltage V-groove solar cell

A method is provided for making a high voltage multijunction solar cell. The cell comprises a plurality of discrete voltage generating regions, or unit cells, which are formed in a single semiconductor wafer and are connected together so that the voltages of the individual cells are additive. The unit cells comprise doped regions of opposite conductivity types separated by a gap. The method includes forming V-shaped grooves in the wafer and thereafter orienting the wafer so that ions of one conductivity type can be implanted in one face of the groove while the other face is shielded. A metallization layer is applied and selectively etched away to provide connections between the unit cells.

Evans, J. C., Jr.↗

Refine your search to explore more results.