Citrate Effects on Amorphous Calcium Carbonate (ACC) Structure, Stability, and Crystallization
Abstract not provided
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Abstract not provided
Explore the source record for details and available documents.
Not Available
Explore the source record for details and available documents.
Abstract not provided
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Soft magnetic Co{sub 40}Fe{sub 40}B{sub 20} films with different tilt angle were successfully deposited on silicon substrates by using oblique sputtering technique. Different oblique angles are achieved by controlling the position of samples. The corresponding static magnetic properties of these samples were then systematically investigated. Interestingly, with the oblique angle increasing from 38° to 55°, the MOKE hysteresis loop of the thin films displays a unique and special performance with double hard axes. Meanwhile, despite of the measurement magnetic field along PR or AR direction, both of the hysteresis loops have two-stage magnetization reversal that means there are two comparably strong anisotropies in the CoFeB films. Moreover, rotating samples from in-plane to out-of-plane, the hysteresis loops demonstrate the perpendicular anisotropy exist in CoFeB films. The cross-section SEM characterizations further verify that the residual field from the magnetic cylinder will strongly impact the microstructures of thin film.
In this paper, the films were prepared by radio frequency magnetron co-sputtering technique. The effect of different mosaic targets made of nickel strips and graphite pure on the dielectric relaxation time, the carriers hopping rate, the fractal dimensions and the optical loss of films were studied. The values of the optical band gap of films using the cross-point between the tangent of the plot of lower and higher values of the photon energy were calculated. The films deposited at 4.64% have maximum hopping rate of about 8.6 × 10{sup 12} S{sup −1}. It can be seen that the films deposited at 3.92% have minimum value of fractal dimension of 2.27. With increasing Ni content of films a nonmetal–metal transition is observed which it is explainable by the power law of percolation theory. Critical metal content and the critical exponent of films were 87.25% and 1, respectively. With increasing Ni content, the carriers effective mass of films decreased and average lattice separation values of films increased. Films deposited at 3.92% have minimum value of Debye frequency ν{sub D} of about 1.09 × 10{sup 12} Hz. The value of energy loss by free charge carriers when traversing the bulk and surface of films at 3.92% has maximum value and it has an increasing function behavior with energy.